JP2000347394A5 - 感光性ペーストおよびディスプレイ用部材の製造方法 - Google Patents
感光性ペーストおよびディスプレイ用部材の製造方法 Download PDFInfo
- Publication number
- JP2000347394A5 JP2000347394A5 JP1999159229A JP15922999A JP2000347394A5 JP 2000347394 A5 JP2000347394 A5 JP 2000347394A5 JP 1999159229 A JP1999159229 A JP 1999159229A JP 15922999 A JP15922999 A JP 15922999A JP 2000347394 A5 JP2000347394 A5 JP 2000347394A5
- Authority
- JP
- Japan
- Prior art keywords
- photosensitive paste
- display members
- manufacturing photosensitive
- photosensitive
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
【特許請求の範囲】
【請求項1】 ガラス転移点が400〜550℃である低融点ガラスおよび感光性有機成分を含む感光性ペーストであって、厚さ50μmの塗布膜の全光線透過率が60%以上、焼成後にXYZ表色系におけるY値が15以下であることを特徴とする感光性ペースト。
【請求項2】 ガラス転移点が400〜550℃である低融点ガラス、感光性有機成分ならびにRu、Mn、Ni、Cr、Fe、CoおよびCuからなる群から選ばれる少なくとも一種の金属のアルコキシド誘導体類、β−ジケトン類の錯体、β−ケト酸エステル類の錯体または有機カルボン酸誘導体類を含むことを特徴とする感光性ペースト。
【請求項3】 基板上に請求項1または2に記載の感光性ペーストを塗布、乾燥して得た感光性ペースト膜を露光、現像、焼成することによって隔壁を形成する工程を含むディスプレイ用部材の製造方法。
【請求項1】 ガラス転移点が400〜550℃である低融点ガラスおよび感光性有機成分を含む感光性ペーストであって、厚さ50μmの塗布膜の全光線透過率が60%以上、焼成後にXYZ表色系におけるY値が15以下であることを特徴とする感光性ペースト。
【請求項2】 ガラス転移点が400〜550℃である低融点ガラス、感光性有機成分ならびにRu、Mn、Ni、Cr、Fe、CoおよびCuからなる群から選ばれる少なくとも一種の金属のアルコキシド誘導体類、β−ジケトン類の錯体、β−ケト酸エステル類の錯体または有機カルボン酸誘導体類を含むことを特徴とする感光性ペースト。
【請求項3】 基板上に請求項1または2に記載の感光性ペーストを塗布、乾燥して得た感光性ペースト膜を露光、現像、焼成することによって隔壁を形成する工程を含むディスプレイ用部材の製造方法。
【0012】
【課題を解決するための手段】
すなわち本発明は、ガラス転移点が400〜550℃である低融点ガラスおよび感光性有機成分を含む感光性ペーストであって、厚さ50μmの塗布膜の全光線透過率が60%以上、焼成後にXYZ表色系におけるY値が15以下であることを特徴とする感光性ペーストである。また、ガラス転移点が400〜550℃である低融点ガラス、感光性有機成分ならびにRu、Mn、Ni、Cr、Fe、CoおよびCuからなる群から選ばれる少なくとも一種の金属のアルコキシド誘導体類、β−ジケトン類の錯体、β−ケト酸エステル類の錯体または有機カルボン酸誘導体類を含むことを特徴とする感光性ペーストである。
【課題を解決するための手段】
すなわち本発明は、ガラス転移点が400〜550℃である低融点ガラスおよび感光性有機成分を含む感光性ペーストであって、厚さ50μmの塗布膜の全光線透過率が60%以上、焼成後にXYZ表色系におけるY値が15以下であることを特徴とする感光性ペーストである。また、ガラス転移点が400〜550℃である低融点ガラス、感光性有機成分ならびにRu、Mn、Ni、Cr、Fe、CoおよびCuからなる群から選ばれる少なくとも一種の金属のアルコキシド誘導体類、β−ジケトン類の錯体、β−ケト酸エステル類の錯体または有機カルボン酸誘導体類を含むことを特徴とする感光性ペーストである。
さらに、本発明は、基板上に上記の感光性ペーストを塗布、乾燥して得た感光性ペースト膜を露光、現像、焼成することによって隔壁を形成する工程を含むディスプレイ用部材の製造方法である。