JPWO2010119680A1 - 連続鋳造設備 - Google Patents
連続鋳造設備 Download PDFInfo
- Publication number
- JPWO2010119680A1 JPWO2010119680A1 JP2011509217A JP2011509217A JPWO2010119680A1 JP WO2010119680 A1 JPWO2010119680 A1 JP WO2010119680A1 JP 2011509217 A JP2011509217 A JP 2011509217A JP 2011509217 A JP2011509217 A JP 2011509217A JP WO2010119680 A1 JPWO2010119680 A1 JP WO2010119680A1
- Authority
- JP
- Japan
- Prior art keywords
- slab
- roll
- support
- rolls
- support roll
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
本願は、2009年4月14日に、日本に出願された特願2009−097681号に基づき優先権を主張し、その内容をここに援用する。
A≦0.001×B2−1.5×B+735・・・・(1)
400≦B<680・・・・(2
なお、上記式(2)において下限値である400mmは、連続鋳造設備において支持ロールを実際に設置可能な最小の間隔として決定した。
また、中心固相率は、伝熱・凝固計算によって求めることができ、伝熱・凝固計算としては、エンタルピー法や等価比熱法などが広く知られており、いずれの方法を用いても良い。また、簡易的には、下記の式が広く知られており、この式を用いても良い。
中心固相率=(液相線温度−溶融部温度)/(液相線温度−固相線温度)
ここで、溶融部温度とは、鋳片厚み方向の中心部で、かつ、鋳片幅方向の溶融部分の温度を意味しており、伝熱・凝固計算によって求めることができる。また、液相線温度は、例えば、「鐵と鋼、日本鐡鋼協會々誌、Vol.55、No.3(19690227)S85、社団法人日本鉄鋼協会」を参照して、また、固相線温度は、例えば、「平居、金丸、森;学振19委、第5回凝固現象協議会資料、凝固46(1968年12月)」を参照して、それぞれ算出することができる。
A≦0.001×B2−1.5×B+735・・・・(1)
400≦B<680・・・・(2)
但し、Aは支持ロール10a中の鋳片幅方向D2に隣り合う分割ロール30a、30b間の間隔(mm)であり、Bは支持ロール10aの鋳造方向D1の両隣の支持ロール10b、10c間の間隔(mm)である。
また、非支持帯幅Aが0mmで支持ロールが分割されていない場合、実際には前述の通り、支持ロールがたわむことによりバルジングが生じるという問題がある。しかし、ここでは、非支持帯幅Aおよび非支持帯長さBを変化させた場合の検討を行う際に、非支持帯幅Aが0mmの場合をバルジング量が最も少ない場合の基準とするために、支持ロールがたわむことなく操業できるものと仮定した。
ここで、非支持帯幅Aが0mm、かつ非支持帯長さBが560mmにおけるバルジング量を基準としたのは、分割されていない支持ロール(A=0mm)を用いる場合に、通常、設定されている鋳造方向D1の支持ロール間隔が280mm程度であることに基づいている。そこで、発明者らが調べたところ、バルジング指数が2.8以下であると鋳片Hの中心偏析を十分に抑制できることが分かった。すなわち、図5中の太い点線より下の範囲が中心偏析を抑制できる範囲であることが分かった。
2 タンディッシュ
3 鋳型
4 ノズル
5 鋳片通路
6、7 ロール群
10、11 支持ロール
20 ロールセグメント装置
21、22 フレーム
23 支持部材
24 油圧シリンダ
30、40 分割ロール
31、41 シャフト
32、42 端部軸受部
33、43 中間軸受部
H 鋳片
S 非支持帯
Claims (1)
- 鋳片の通路を挟んで対向配置される複数の支持ロールを備えた連続鋳造設備であって、
それぞれの前記支持ロールは、前記鋳片の幅方向に沿って配置された複数の分割ロールを有し、
連続鋳造工程中の前記鋳片の中心固相率が0.2以上かつ1.0未満となる前記通路上の位置に配置された前記各支持ロールについて:
前記支持ロール中の前記鋳片の前記幅方向で隣り合う前記分割ロール間の間隔を間隔A(mm)と定義し、
前記支持ロールの鋳造方向下流側の隣の支持ロールから前記支持ロールの鋳造方向上流側の隣の支持ロールまでの距離を距離B(mm)と定義したとき、間隔A及び距離Bが、
A≦0.001×B2−1.5×B+735・・・・(1)
および
400≦B<680・・・・(2)
を満たすことを特徴とする連続鋳造設備。