DE373944C - Verfahren zur Herstellung von glasierten Schutzrohren fuer elektrische Waermemesser - Google Patents
Verfahren zur Herstellung von glasierten Schutzrohren fuer elektrische WaermemesserInfo
- Publication number
- DE373944C DE373944C DEH86418D DEH0086418D DE373944C DE 373944 C DE373944 C DE 373944C DE H86418 D DEH86418 D DE H86418D DE H0086418 D DEH0086418 D DE H0086418D DE 373944 C DE373944 C DE 373944C
- Authority
- DE
- Germany
- Prior art keywords
- production
- protective tubes
- tubes
- glazed
- glazed protective
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Herstellung von glasierten Schutzrohren für elektrische Wärmemesser. Bei der Erfindung handelt es sich um die Herstellung vonSchutzrohrenfür elektrischeWärmemesser (Widerstandsthermometer, Thermoelemente u. dgl.). Man sucht solche Rohre mit einer feuerfesten Glasur zu überziehen, um die Schutzrohre selbst vor den Wirkungen der Gase zu sichern. Es hat sich dabei herausgestellt, daß, je länger das Schutzrohr ist, es um so schwieriger wird, daß dem stärksten Feuer ausgesetzte Ende gut zu emaillieren; denn man muß diese Rohre während des Prozesses drehen und muß sie, um bei der Erwärmung durch die hohe Temperatur ein Verbiegen zu verhüten, etwas aufstützen. An diesen, also gerade an den wichtigsten Stellen, wird aber regelmäßig die Emaille beschädigt oder schlechter ausfallen.
- Gemäß der Erfindung wird das Rohr mit geeigneten Wulsten, Ansätzen o. dgl. versehen, welche zum Auflegen dienen, und bei welchen eine schadhafte Emaillierung nebensächlich ist. Zwei besonders zweckmäßige Ausbildungen des Rohres sind figürlich dargestellt. In Abb. x ist das Rohr mit einem flachen ringförmigen Wulst w versehen, der in eine scharfe Kante ausläuft. An dieser Kante wird also die Glasur zweifellos beschädigt. Es ist dies aber deshalb unerheblich, weil die schädliche Einwirkung der Gase, wenn sie an dieser Stelle angreift, vernachlässigt werden kann.
- Dem gleichen Gedankengang entspricht die Ausführung nach Abb. 2. Es ist dort ein zylindrischer Verlängerungsstift s an dem Rohr- l ende angebracht. Auch dort ist die Metallmasse so groß und liegt von der eigentlichen Rohrwand so weit weg, daß ein starkes Zerfressen des Schutzrohres infolge schlechter Emaillierung nicht zu befürchten ist. Es steht nichts im Wege, die genannten Teile w und s, deren Ausgestaltung eine mannigfache sein kann, nach erfolgter Emaillierung teilweise zu entfernen.
- Gegenüber den bekannten Verstärkungen der Rohre, welche entweder den besseren Halt oder die größere Steifheit der Rohre bezwecken, kommen dem Sinn der Erfindung gemäß nur diejenigen Verstärkungen in der Nähe des unteren Endes der Rohre in Frage, welche dazu dienen können, gerade das Rohrende in einwandsfreier Weise mit einem Überzuge zu versehen.
Claims (1)
- PATENT-ANSPRUCII: Verfahren zur Herstellung von glasierten Schutzrohren für elektrische Wärmemesser, dadurch gekennzeichnet, daß die Rohre vor dem Emaillieren mit besonderen schmalen Wulsten, Ansätzen und ähnlichen Stützen versehen sind, welche während der Emaillierung als Auflageflächen für das Drehen des Rohres dienen, die bei dem Aufliegen unvermeidliche Beschädigung des Emailleübcrzuges an unwichtige Stellen verlegen und nach Fertigstellung entfernt werden können.