CN201390777Y - 内加热式热浸镀锌设备用加热棒 - Google Patents

内加热式热浸镀锌设备用加热棒 Download PDF

Info

Publication number
CN201390777Y
CN201390777Y CN200820301693U CN200820301693U CN201390777Y CN 201390777 Y CN201390777 Y CN 201390777Y CN 200820301693 U CN200820301693 U CN 200820301693U CN 200820301693 U CN200820301693 U CN 200820301693U CN 201390777 Y CN201390777 Y CN 201390777Y
Authority
CN
China
Prior art keywords
heating
zinc
type hot
heating rod
dip galvanized
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200820301693U
Other languages
English (en)
Inventor
王青松
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200820301693U priority Critical patent/CN201390777Y/zh
Application granted granted Critical
Publication of CN201390777Y publication Critical patent/CN201390777Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型涉及一种加热棒,由于其在金属壳外表面涂覆了具有耐液态金属锌侵蚀,耐锌渣侵蚀的陶瓷涂层。使得该加热棒较耐蚀的石英玻璃棒具有较高强度,不易破损;较金属棒具有较高耐侵蚀性,不被锌和锌渣腐蚀。极大提高了该种设备部件的寿命。可用于内热式热浸镀锌设备的直接加热。采用了该部件的内加热的热浸镀锌锅较传统的外加热锅具有节能、减排、降耗、环保的优点。

Description

内加热式热浸镀锌设备用加热棒
所属技术领域
本实用新型设计属于腐蚀与防护工程领域。
背景技术
采用热浸镀的方法在钢铁表面形成耐蚀镀层可以提高钢铁的耐蚀性。通常采用的方法是在钢铁表面热浸镀锌、铝或锌铝合金。
目前,公知的热浸镀锌/锌铝锅大都采用外加热,由于其加热体在锅外,其热能不能被充分利用。而采用内加热式锅可以充分利用热能。
内加热式锅要求其关键部件——浸在金属镀液中的加热体能够具有一定的强度并同时能耐金属镀液和镀液氧化物渣的侵蚀。目前这一问题还没有得到很好的解决。保护套管采用金属材料会被金属镀液溶解,采用耐热玻璃或二氧化硅保护套,虽然能够耐金属镀液和镀液氧化物渣侵蚀但是其强度太低,容易碰碎,而采用一般陶瓷保护套,其抗热振性差,容易炸裂。因此,需要一种具有一定强度、能够耐金属镀液和镀液氧化物渣侵蚀的加热体保护套。
发明内容
为了克服现有加热体的不足,本实用新型提供了一种加热棒,由于该加热棒保护套外表面涂覆了能够耐金属镀液和镀液氧化物渣侵蚀且具有良好的抗热振性的陶瓷涂层,使其可以应用于内加热式热浸镀锌/锌铝设备锌锅的加热。
本实用新型解决其技术问题采用的技术方案是:加热体外保护套采用金属管,如普通钢管、不锈钢管或耐热钢管,在金属管外表面采用等离子或氧乙炔火焰喷涂工艺喷涂一层能够同时耐液态金属锌/锌铝和镀液渣侵蚀的陶瓷涂层。
本实用新型的有益效果是:该加热棒可以长期浸在热浸镀锌/锌铝锅中加热液态金属锌/锌铝合金。这使得内加热型热浸镀锌/锌铝锅的广泛采用成为可能。采用内加热技术可以极大降低能耗,减少污染物排放,提高热浸镀的质量。
下面结合附图和实例具体说明:
附图说明
图1内加热式热浸镀锌设备用加热棒示意图。
图中:1.金属套管  2.陶瓷涂层  3.绝缘体  4.电热丝
具体实施方式
制造一端封闭的电热棒金属套管,并在套管外表面采用氧-乙炔火焰热喷涂工艺
喷涂主要成分为氧化铝、氧化锌及其化合物的陶瓷粉,在表面形成一层致密的陶瓷保护层。***由缠绕了电加热丝的陶瓷绝缘体构成的加热体,按照图1组装,构成加热棒。该加热棒可应用于热浸镀锌/锌铝锅内加热。

Claims (1)

1.一种内加热式热浸镀锌设备用加热棒,其特征是:该加热棒内部为缠绕加热丝的陶瓷绝缘体,外部为有陶瓷涂层的金属外保护套管构成。
CN200820301693U 2008-08-01 2008-08-01 内加热式热浸镀锌设备用加热棒 Expired - Fee Related CN201390777Y (zh)