CN103337627A - 一种锂离子电池及其磷酸铁锂正极材料 - Google Patents

一种锂离子电池及其磷酸铁锂正极材料 Download PDF

Info

Publication number
CN103337627A
CN103337627A CN2013102348448A CN201310234844A CN103337627A CN 103337627 A CN103337627 A CN 103337627A CN 2013102348448 A CN2013102348448 A CN 2013102348448A CN 201310234844 A CN201310234844 A CN 201310234844A CN 103337627 A CN103337627 A CN 103337627A
Authority
CN
China
Prior art keywords
iron phosphate
lithium
ion battery
lithium iron
phosphate positive
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102348448A
Other languages
English (en)
Inventor
赖晓芳
Original Assignee
SUZHOU NUOXIN INNOVATION ENERGY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU NUOXIN INNOVATION ENERGY CO Ltd filed Critical SUZHOU NUOXIN INNOVATION ENERGY CO Ltd
Priority to CN2013102348448A priority Critical patent/CN103337627A/zh
Publication of CN103337627A publication Critical patent/CN103337627A/zh
Pending legal-status Critical Current

Abstract

本发明提供了一种锂离子电池及其磷酸铁锂正极材料,所述正极材料为具有橄榄石结构的纳米磷酸铁锂,其以三氯化铁为铁源,以聚乙烯为还原剂,在原料中添加过量碳粉合成的球形碳磷酸铁锂复合颗粒,颗粒直径为500-700纳米,放电容量为150mAh/g。相较于现有技术,本发明的所述正极材料可以提高锂离子电池的容量,改善其循环性能和充放电性能。

Description

一种锂离子电池及其磷酸铁锂正极材料
技术领域
本发明涉及一种锂离子电池及其磷酸铁锂正极材料。
背景技术
锂离子电池已经广泛应用众多电子产品中,其体积较小、没有充放电记忆效应,因此受到市场的广泛欢饮。然而目前的锂离子电池的容量不足,尤其是在智能手机中,经常由于待机时间不理想而影响市场前景。
发明内容
本发明主要解决的技术问题是目前的锂离子电池的容量不足。
为了解决上述技术问题,本发明实施例公开了一种用于锂离子电池的磷酸铁锂正极材料,所述正极材料为具有橄榄石结构的纳米磷酸铁锂,其以三氯化铁为铁源,以聚乙烯为还原剂,在原料中添加过量碳粉合成的球形碳磷酸铁锂复合颗粒,颗粒直径为500-700纳米,放电容量为150mAh/g。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料中,碳为包裹在碳磷酸铁锂表面的碳膜。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料还掺杂有钛或者钒。
为了解决上述技术问题,本发明实施例公开了一种锂离子电池,其包括正极,所述正极材料为具有橄榄石结构的纳米磷酸铁锂,其以三氯化铁为铁源,以聚乙烯为还原剂,在原料中添加过量碳粉合成的球形碳磷酸铁锂复合颗粒,颗粒直径为500-700纳米,放电容量为150mAh/g。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料中,碳为包裹在碳磷酸铁锂表面的碳膜。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料还掺杂有钛或者钒。
相较于现有技术,本发明的所述正极材料可以提高锂离子电池的容量,改善其循环性能和充放电性能。
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅是本发明的一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其它实施例,都属于本发明保护的范围。
为了解决上述技术问题,本发明实施例公开了一种用于锂离子电池的磷酸铁锂正极材料,所述正极材料为具有橄榄石结构的纳米磷酸铁锂,其以三氯化铁为铁源,以聚乙烯为还原剂,在原料中添加过量碳粉合成的球形碳磷酸铁锂复合颗粒,颗粒直径为500-700纳米,放电容量为150mAh/g。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料中,碳为包裹在碳磷酸铁锂表面的碳膜。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料还掺杂有钛或者钒。
为了解决上述技术问题,本发明实施例公开了一种锂离子电池,其包括正极,所述正极材料为具有橄榄石结构的纳米磷酸铁锂,其以三氯化铁为铁源,以聚乙烯为还原剂,在原料中添加过量碳粉合成的球形碳磷酸铁锂复合颗粒,颗粒直径为500-700纳米,放电容量为150mAh/g。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料中,碳为包裹在碳磷酸铁锂表面的碳膜。
在本发明的一较佳实施例中,所述磷酸铁锂正极材料还掺杂有钛或者钒。
相较于现有技术,本发明的所述磷酸铁锂正极材料可以提高锂离子电池的容量,改善其循环性能和充放电性能。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其它相关的技术领域,均同理包括在本发明的专利保护范围内。

Claims (4)

1.一种用于锂离子电池的磷酸铁锂正极材料,其特征在于,所述正极材料为具有橄榄石结构的纳米磷酸铁锂,其以三氯化铁为铁源,以聚乙烯为还原剂,在原料中添加过量碳粉合成的球形碳磷酸铁锂复合颗粒,颗粒直径为500-700纳米,放电容量为150mAh/g。
2.根据权利要求1所述的用于锂离子电池的磷酸铁锂正极材料,其特征在于,所述磷酸铁锂正极材料中,碳为包裹在碳磷酸铁锂表面的碳膜。
3.根据权利要求1所述的用于锂离子电池的磷酸铁锂正极材料,其特征在于,所述磷酸铁锂正极材料还掺杂有钛或者钒。
4.一种锂离子电池,其特征在于,包括权利要求1-3任一所述的磷酸铁锂正极材料。
CN2013102348448A 2013-06-14 2013-06-14 一种锂离子电池及其磷酸铁锂正极材料 Pending CN103337627A (zh)