JPS6323623B2 - - Google Patents

Info

Publication number
JPS6323623B2
JPS6323623B2 JP1920079A JP1920079A JPS6323623B2 JP S6323623 B2 JPS6323623 B2 JP S6323623B2 JP 1920079 A JP1920079 A JP 1920079A JP 1920079 A JP1920079 A JP 1920079A JP S6323623 B2 JPS6323623 B2 JP S6323623B2
Authority
JP
Japan
Prior art keywords
charging
battery
capacity
circuit
recovery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP1920079A
Other languages
English (en)
Other versions
JPS55111079A (en
Inventor
Akio Watanabe
Masashi Wakamatsu
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panasonic Holdings Corp
Original Assignee
Matsushita Electric Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Matsushita Electric Industrial Co Ltd filed Critical Matsushita Electric Industrial Co Ltd
Priority to JP1920079A priority Critical patent/JPS55111079A/ja
Publication of JPS55111079A publication Critical patent/JPS55111079A/ja
Publication of JPS6323623B2 publication Critical patent/JPS6323623B2/ja
Granted legal-status Critical Current

Description

【発明の詳細な説明】 本発明は、過放電によつて充電不能となつた鉛
蓄電池の容量を回復させる方法に関するものであ
る。
過放電によつて充電不能となつた蓄電池を回復
させる従来からの方法は、電池に高い電圧をかけ
て微小電流により充電する方法が唯一のものであ
つた。この方法では、特殊な充電器を用い、かつ
回復完了までに長時間を要し、実用性に乏しいこ
とが問題であつた。この回復充電時間を短縮する
ために大きな電流で充電を行なつた場合、電池が
発熱し、電池の性能及び寿命を損うおそれがあつ
た。
本発明は過放電により充電不能になつた蓄電池
では正極格子表面と活物質との界面に生成した粗
大粒子化した硫酸鉛などが半導体的な整流作用を
呈し、正規の充電方向に電流を流す際には高い内
部抵抗を示すのに反し、放電方向へは比較的小さ
い内部抵抗を示す性質を有することを利用し、こ
のような状態の蓄電池に交流電圧を印加すること
により、最初は充電方向よりも放電方向へ流れる
電気量が多いが、漸時両方向が等量もしくはそれ
に近くなることを見出したものである。そしてこ
の初期放電の後、通常の充電方法で正規の充電を
可能にしたものである。
以下、本発明の実施例を図により説明する。第
1図において充電器の全てのスイツチSWをa側
に接続すると定電圧回路Cが動作して正規の定電
圧充電回路が構成され、b側に接続すると電池1
に交流電圧2が印加される回路が構成される。な
おTは降圧トランス、Rは全波整流器である。
今、スイツチSWをa側に倒して充電できなかつ
た過放電状態の電池1を充電端末に接続し、スイ
ツチSWをbに倒して接続状態とし、交流電圧を
電池1に印加して発光ダイオードLが点灯した時
点で再びスイツチSWをa側に倒して正規の充電
を行なう。
このような充電により容量の回復を図つた電池
について過放電以前の初期容量に比べると次のよ
うな状態であつた。
初期容量 3.2Ah 回復充電後の容量 3.1Ah 容量回復率 96.9% 同様の原理により、第2図に示すトランスTの
ない充電回復回路において過放電状態の電池1に
高圧の交流を印加した後、定電圧充電器に接続し
て正規の回復充電した場合の回復情況も前記の結
果とまつたく同様であつた。
前述のごとき過放電電池の特性から第3図に示
す充電回路を用い、連動スイツチSWをa側に倒
して正規の充電を施しても電流が流れない電池に
ついては、スイツチSWをb側に倒して放電方向
電流を流して逆充電し、その後スイツチSWをa
側に倒して充電を行なつても、ほぼ前記と同様の
回復率が得られる。
このような本発明の容量回復法によれば、過放
電して正規の充放方法では充電不能な蓄電池であ
つても交流電圧を印加するか、又は逆充電を施す
ことで、正極格子表面と活物質との界面に生成し
た整流作用を呈する半導体的生成物質で破壊し
て、この物質の通電を可能とすることで、短時間
で充電回復可能な状態にすることができ、実用的
に大きな価値がある。
さらに本発明では通常の充電回路に低廉な回路
を付加するか、又は別個に用意することで電池の
容量を回復させることができるので経済的価値が
高いという利点がある。
【図面の簡単な説明】
第1図は本発明の実施例における容量回復のた
めに用いた充電回路を示す図、第2図、第3図は
他の実施例における回路図である。 1……過放電した電池、2……交流電源、T…
…トランス、R……全波整流器、C……定電圧回
路、SW……スイツチ。

Claims (1)

    【特許請求の範囲】
  1. 1 過放電により充電不能となつた鉛蓄電池に、
    交流電圧を印加するか又は逆充電して正極格子表
    面と活物質との界面に生成した半導体的物質を破
    壊し、その後に正規の充電を施すことを特徴とし
    た鉛蓄電池の容量回復法。
JP1920079A 1979-02-20 1979-02-20 Capacity recovery method in lead acid battery Granted JPS55111079A (en)