DE846523C - Verfahren zur Erniedrigung der Viskositaet von waesserigen Braunkohlenfilteraschen- oder Zementsuspensionen - Google Patents
Verfahren zur Erniedrigung der Viskositaet von waesserigen Braunkohlenfilteraschen- oder ZementsuspensionenInfo
- Publication number
- DE846523C DE846523C DEV3031A DEV0003031A DE846523C DE 846523 C DE846523 C DE 846523C DE V3031 A DEV3031 A DE V3031A DE V0003031 A DEV0003031 A DE V0003031A DE 846523 C DE846523 C DE 846523C
- Authority
- DE
- Germany
- Prior art keywords
- viscosity
- filter ash
- aqueous
- reducing
- lignite
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Erniedrigung der Viskosität von wässerigen Braunkohlenfilteraschen- oder Zementsuspensionen Bei der Verwendung von Filterasche, insbesondere Bratinkolilenfilterasche, der gegebenenfalls io bis doo/o*Sand, Kalk, Zement, Traß oder Tuff zugesetzt werden können, als Putzmörtel, machen sich nach dem _anmachen mit Wasser beim Verteilen die schwankende Viskosität des Stoffgemisches und die rasche Erstarrung hindernd bemerkbar. Aber auch bei der Herstellung von Bausteinen aus Filterasche, insbesondere Braunkohlenfilterasclie, mit oder ohne Zugabe obengenannter Zusätze. gleichgültig ob Luft- oder dampfgehärtet wird, macht sich heim Anmachen die schwankende Viskosität störend bemerkbar, die zur Regulierung verschiedener Mengen zusätzlichen Wassers bedarf, was die Festigkeit ungünstig und schwankend beeinflußt.
- Es wurde gefunden, daß durch geringe Zusätze von 0,5 his 4% Di- oder Trinatriumphosphat die Viskosität wässeriger Aufschlämmungen von 13raunkohlenfilterasche erniedrigt und das Produkt bedeutend langsamer viskos wird. Die verflüssigende Wirkung ist um so größer, je mehr Di- oder Trinatriumphospliat verwendet wird. Dasselbe tritt ein hei Mörteln aus hydraulischen Zementen.
- Die Erscheinung der Verflüssigung von Tonschlicker durch Phosphatzusätze war bekannt. Es war aber nicht vorauszusehen, daß durch diesen Zusatz die Viskosität von Aufschlämmungen aus Braunkoblenfilterasc'he, Portlandzement oder auch anderen Zementen erniedrigt wird, wodurch diese erst für viele Zwecke Anwendung finden können. Es war auch keineswegs anzunehmen, daß durch diese A ,Ikaliphosphate die Erstarrurigszeit dieser Aufschlämmungen maßgeblich verlängert wird. Braunkohlenfilterasche besteht z. B, aus
Ca0: 52 bis 580/0 Fe203 : 15 bis 200/0 Mg0: 6 bis 9% Unlöslichen SiO.: 4 bis 10%.
Claims (2)
- PATEN TANSPRCCHE: i. Verfahren zur Erniedrigung der Viskosität und Verlängerung der Erstarrungszeit von Aufschlämmungen aus Braunkohlenfilterasche oder hydraulischen Zementen durch Zugabe von 0,5 his 40/0 Di- oder Trinatriumphosphat.
- 2. Verfahren nach Anspruch i, dadurch gekennzeichnet, daß der Braunkohlenfilterasclie 10 bis 4o0/0 Sand, Kalk, Zement, Traß oder Tuff zugesetzt werden.