CN106283314A - The pulp yarn that the twisting method of pulp yarn and the method are twisted - Google Patents

The pulp yarn that the twisting method of pulp yarn and the method are twisted Download PDF

Info

Publication number
CN106283314A
CN106283314A CN201510247308.0A CN201510247308A CN106283314A CN 106283314 A CN106283314 A CN 106283314A CN 201510247308 A CN201510247308 A CN 201510247308A CN 106283314 A CN106283314 A CN 106283314A
Authority
CN
China
Prior art keywords
paper
paper roll
vexed
twisting
softener
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510247308.0A
Other languages
Chinese (zh)
Inventor
唐文华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510247308.0A priority Critical patent/CN106283314A/en
Publication of CN106283314A publication Critical patent/CN106283314A/en
Pending legal-status Critical Current

Abstract

The invention provides a kind of twisting method of pulp yarn and pulp yarn that the method is twisted, belong to textile technology field.The twisting method of this pulp yarn includes: 1), tubular paper roll is carried out separation, obtains treating vexed paper roll;2), treat that vexed paper roll is dipped in paper softener by described, and make paper softener do not had described in treat vexed paper roll, further take out and treat vexed paper roll after soaking, be placed in confined space placing;Obtain vexed rear paper roll;3), described vexed rear paper roll is carried out twisting, obtain circular pulp yarn.The little paper roll (treating vexed paper roll) obtained after tubular paper roll (the biggest paper disc or paper roll) separation is dipped in paper softener by this twisting method, and is placed in confined space, to realize vexed paper effect.Obtain after vexed paper vexed after paper roll, its pliability and resistance to draw performance to be substantially improved so that it is be difficult to that during coil paper yarn phenomenon of rupture occurs, thus improve production efficiency and the yields of pulp yarn.

Description

The pulp yarn that the twisting method of pulp yarn and the method are twisted
Technical field
The present invention relates to textile technology field, in particular to the twisting of a kind of pulp yarn The pulp yarn that method and the method are twisted.
Background technology
Pulp yarn refers to be divided into paper roll fillet dish, upper spinning machine, makes certain diameter circular Weaving fine rule, pulp yarn can be weaved, and does cloth, clothes, artware, braiding etc..
In the related, pulp yarn is during preparation (i.e. during coil paper yarn) Mainly include separation and coil paper yarn.Wherein, in the operation of separation, big paper disc is divided into There is the little paper disc of one fixed width;And during coil paper yarn, use traditional textile industry spinning set Rolling of paper is become cord by road.
Owing to paper toughness and the Nai La degree of little paper disc are very limited, therefore, this little paper disc During using traditional textile mode to be rolled into cord, it is very easy to fracture, has a strong impact on Production efficiency and yields, efficiency is low.
In view of this, the special proposition present invention.
Summary of the invention
It is an object of the invention to provide a kind of twisting method of pulp yarn, this twisting method will Little paper roll (the treating vexed paper roll) leaching obtained after tubular paper roll (the biggest paper disc or paper roll) separation In or directly spray paper softener, and placed in confined space, to realize Vexed paper effect.Obtain after vexed paper vexed after paper roll, its pliability and resistance to draw performance big Width promotes so that it is is difficult to phenomenon of rupture occur during coil paper yarn, thus improves paper The production efficiency of yarn and yields.
Another object of the present invention is to provide the pulp yarn that above-mentioned twisting method is made, with Realize its application at field of textiles.
This pulp yarn that the present invention provides, compared with traditional terylene or nylon wire, one Aspect, its waste products is prone to be decomposed, thus has preferable environmental-protecting performance;On the other hand, This pulp yarn waste product is also very easy to realize recycling, has the effect economized on resources.
In order to realize the above-mentioned purpose of the present invention, spy by the following technical solutions:
The invention provides a kind of twisting method of pulp yarn, including: will obtain after separation The paper disc arrived soaks through paper softener or sprays, after standing in airtight space Directly weave, obtain circular pulp yarn.
In paper fiber molecule chain, typically can contain multiple hydroxyls, and be straight chain type macromole, Having the strongest molecular separating force and hydrogen bond between its chain, degree of crystallinity is higher, for being rigidly connected, Therefore it is highly susceptible to being pulled off.But after being soaked by paper softener, softening agent adheres to In the surface of paper roll, stand at closed environment and (prevent softening agent generation qualitative change, and lose Go ins and outs) during, softening agent is fully infiltrated into inside paper roll, and paper softener exists Nonpolar isolating membrane is formed, so that strand occurs mutually the most under stress between fiber Sliding and motion, and add pliability and the Nai La performance of paper so that it is it is difficult to be pulled off, During coil paper yarn (by circular for the rolls of paper sheets of strip cord), it is difficult to that fracture occurs Phenomenon, thus improve production efficiency and the yields of pulp yarn.
Preferably, in order to reach superior technique effect, above-mentioned twisting method, specifically may be used Comprise the following steps:
1), tubular paper roll is carried out separation, obtain treating vexed paper roll;
2), treat that vexed paper roll is dipped in paper softener by described, and make paper softener not have Described treat vexed paper roll, further take out and treat vexed paper roll after soaking, be placed in confined space Place so that paper softener permeates, and obtains vexed rear paper roll;
It is said that in general, (make paper softener fully soak to realize preferable osmotic effect Enter in paper roll), preferred standing time is 2-12 hour.
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2-4 part and fatty alcohol-polyoxyethylene ether 1-2 part;
3), described vexed rear paper roll is carried out twisting, obtain circular pulp yarn.
Preferably, in step 2) in, the composition of paper softener used has been carried out spy Fixed selection, by dimethyl siloxane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyl Methyl dimethoxysilane is mixed into silicon crude oil complex 2-4 part and fatty alcohol-polyoxyethylene ether 1-2 part.
Dimethyl siloxane mixed methylcyclosiloxane is from one or more line styles, ring-type and chain siloxanes Set out, under catalyst action, made by reactions such as balance, addition or condensations, its property Matter is relatively stable, it is easy to N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane Mixture, and N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane is difunctional idol Connection agent, after its functional group is bonded on silicone oil skeleton, can improve organosilicon (molecule) and exist The degree of orientation on fiber, adds the affinity to fiber, gives the super softness of fiber, cunning Refreshing, pendency, antistatic, the washable effect such as wrinkle resistant;Fatty alcohol-polyoxyethylene ether as auxiliary agent, There is emulsifying and osmosis, so that paper softener permeates the most comprehensive in paper.
Optionally, in step 2) in, in described silicon crude oil complex, dimethyl siloxane Mixed methylcyclosiloxane and the volume ratio of N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane It is 1: (1-4).
When dimethyl siloxane mixed methylcyclosiloxane and N-β-(aminoethyl)-γ-aminopropyltriethoxy two The volume ratio of methoxy silane is 1: time (1-4), and each component of softening agent is more easy to realize mixing Effect, and due to N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane content More, therefore there is preferably softening and increasing and rub effect.
Optionally, in step 2) in, in terms of volume parts, in described paper softener also Including water 3-54 part.
For the most narrower little paper roll, its softening agent that need not the biggest concentration can realize Increase soft increasing and slide effect, therefore to cost-effective, by its dilute.
Optionally, in step 2) in, in described silicon crude oil complex, dimethyl siloxane Mixed methylcyclosiloxane and the volume ratio of N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane It is 1: 1;And described standing time is 2 hours.
When dimethyl siloxane mixed methylcyclosiloxane and N-β-(aminoethyl)-γ-aminopropyltriethoxy two When the volume ratio of methoxy silane is 1: 1, more meet the increasing of the less paper roll of some width Soft, and after soaking, it is not necessary to stand the too long of time (about 2 hours), Realize the effect being impregnated with completely, further increasing the twisting efficiency of pulp yarn.
Optionally, in step 2) in, the time of described immersion is the 1-20 second.
Owing to paper softener is organic materials, it has certain viscosity;In the mistake soaked Cheng Zhong, will treat that vexed paper roll should not immerse the time oversize, to prevent paper softener infiltration capacity mistake Big thus can not be absorbed by paper roll completely.Therefore, the time of immersion is preferably the 1-20 second.
Optionally, in step 3) in, specifically include: described vexed rear paper roll is sheathed on again In the rotating shaft of twister, and after making paper inside described vexed rear paper roll wind described rotating shaft, Pass sequentially through after multiple feeding roller guides and fix with Wound-up roller;Make Wound-up roller and described Axis of rotation, obtains circular pulp yarn.
In traditional technology, during twisting, spindle is pyramidal structure, and in the mistake of twisting Cheng Zhong, carries out twisting from the outside of spindle, owing to the radius of gyration is big, is highly susceptible to so that paper Bar ruptures, thus affects twisting efficiency;Secondly, during twisting, paper slip consumes one After the space that after part, paper roll is middle has become big, paper slip will not even be difficult to be wound on again In rotating shaft, therefore, production efficiency is the lowest.
In the present invention, in order to improve twisting effect, prevent paper slip from rupturing when twisting, excellent After choosing uses the paper inside paper roll by winding described rotating shaft, and pass sequentially through multiple feeding Mode fixing with Wound-up roller after the guiding of roller.So, when two-for-one twister runs, turn Axle rotates (bottom is provided with round turntable, for placing the paper roll of flat), and in paper roll With winding after the paper in portion is wrapped in rotating shaft and after the guiding of the drive mechanisms such as feeding roller Roller (coil of wire).Rotating shaft paper slip during rotating is rolled into cord, and spiral roller turns The winding that can realize circular cord after Dong is collected, and which is possible to prevent paper slip during twisting It is prone to be pulled off, thus improves twisting efficiency.
Optionally, in step 1) in, described in treat that the width of vexed paper roll is 2-10 millimeter.
Treat that the width of vexed paper roll selects according to the required specification of pulp yarn, it is however generally that, Treat that vexed paper roll is set between 2-10 millimeter, if width is too big, then can affect bating effect, Make to soften insufficient, it is impossible to effectively realize strengthening the effect of vexed rear paper roll pulling force, and Do not meet pulp yarn size requirements.If width is the least, during twisting, paper slip is weak to Draw, be easily pulled off.
Optionally, in step 1) in, the operation of described separation uses separation machine to carry out.
By separation machine, quickly and efficiently parent roll official form for filing a lawsuit volume can be cut into and multiple have The little paper roll of given dimensional, facilitates the operation of follow-up vexed paper to carry out in order.
The pulp yarn that twisting method described in any one of claim 1-9 is twisted.
Compared with prior art, the invention have the benefit that
(1), the little paper roll (treating vexed paper roll) obtained after separation is dipped in paper softener, And it is interior to realize vexed paper effect to be placed on confined space.Obtain after vexed paper vexed after paper roll, Its pliability and resistance to draw performance to be substantially improved, and become a softer and smoother touch, it is easy to change shape Shape so that it is during twisting, is difficult to phenomenon of rupture occur, thus improves pulp yarn Production efficiency and yields.
(2), paper softener formed by specific material combination, organosilicon can be effectively improved (molecule) degree of orientation on fiber, adds the affinity to fiber, gives paper fiber Super softness, smooth, pendency, antistatic, the washable effect such as wrinkle resistant.
(3), during vexed rear paper roll is carried out twisting, paper roll is set as flat, and Inside it, paper carries out coil paper, thus effectively prevent in conventional art from the outside of paper roll Paper twisting (during rotation, radius is big) is prone to the phenomenon that paper slip ruptures occur.
Accompanying drawing explanation
In order to be illustrated more clearly that the embodiment of the present invention or technical scheme of the prior art, with Lower the accompanying drawing used required in embodiment or description of the prior art will be briefly described.
The twisting method flow diagram of the pulp yarn that Fig. 1 provides for the present invention;
Fig. 2 shows the present invention vexed rear paper roll schematic diagram in twisting process.
Detailed description of the invention
Below in conjunction with embodiment, embodiment of the present invention are described in detail, but this Skilled person is it will be appreciated that the following example is merely to illustrate the present invention, and should not regard For limiting the scope of the present invention.Unreceipted actual conditions person in embodiment, according to normal condition Or the condition of manufacturer's suggestion is carried out.Agents useful for same or instrument unreceipted production firm person, all For the conventional products that can be obtained by commercially available purchase.
Refer to Fig. 1, the twisting method of the pulp yarn that the present invention provides, comprise the following steps:
Step 101: tubular paper roll is carried out separation, obtains treating vexed paper roll;
Preferably, in this step, in order to improve the efficiency of separation operation, separation machine is used Carry out separation, and the most specific restriction of specification of tubular paper roll, after separation, obtain Treat that the width general control of vexed paper roll is between 2-10 millimeter.And for its basic weight also without specific Limit.
Step 102: treat that vexed paper roll is dipped in paper softener by described, and make paper soft Agent treated vexed paper roll described in not having, further take out through immersion after treat vexed paper roll, be placed in airtight Place in space so that paper softener permeates, and obtains vexed rear paper roll;
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2-4 part and fatty alcohol-polyoxyethylene ether 1-2 part;
It is furthermore preferred that in described silicon crude oil complex, dimethyl siloxane mixed methylcyclosiloxane and N- The volume ratio of β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane is 1: 1-4;Have The silicon crude oil complex of this proportioning, each component of softening agent is more easy to realize Blending Efficiency of Blending, and Owing to N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane content is more, therefore There is preferably softening and increasing and rub effect.
For some large-sized paper rolls, softening agent can be with water mixture, as in said ratio On the basis of, water 3-54 part can be added.
Additionally, it is preferred that, in described silicon crude oil complex, dimethyl siloxane mixed methylcyclosiloxane It is 1: 1 with the volume ratio of N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane; And described standing time is 2 hours.The softening agent with this proportioning more meets some width Less paper roll increases soft, and after soaking, it is not necessary to (2 is little to stand the too long of time Time) effect that is impregnated with completely can be realized, improve the production efficiency of pulp yarn.
Additionally, due to paper softener is organic materials, it has certain viscosity, adheres to Power is stronger;Therefore, during soaking, treat that vexed paper roll should not immerse the long time, with Prevent paper softener infiltration capacity excessive thus can not be absorbed by paper roll completely.The time soaked It is preferably the 1-20 second;And less for width, and the more loose paper roll of ratio, directly use paper Open softening agent to spray.
Step 103: described vexed rear paper roll is carried out twisting, obtains circular pulp yarn.
Preferably, during twisting, refer to Fig. 2, particularly as follows: by described vexed after Paper roll is sheathed in the rotating shaft 2 of two-for-one twister, and the paper inside described vexed rear paper roll is rolled up After described rotating shaft 2, pass sequentially through and (scheme with Wound-up roller after multiple feeding roller 1 guides Not shown in) fixing;Make Wound-up roller and described rotating shaft 2 rotate, obtain circular pulp yarn.
Owing to vexed rear paper roll is set as flat, and paper carries out coil paper inside it, thus has When can imitate outside paper twisting (during rotation, radius is big) preventing paper roll in conventional art, It is prone to that the phenomenon that paper slip ruptures occurs.
It follows that combine above content, the twisting method of the pulp yarn of the present invention is enumerated Embodiment in detail below.
Embodiment 1
S11: utilize separation machine to carry out separation tubular paper roll, obtaining width is 4 millimeters Treat vexed paper roll;
S12: will treat that vexed paper roll is dipped in paper softener, and make paper softener not have institute State and treat vexed paper roll 2 seconds, further take out through immersion after treat vexed paper roll, be placed in confined space Interior placement 2 hours;Obtain vexed rear paper roll;
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2 parts and fatty alcohol-polyoxyethylene ether 1 part;Described silicon crude oil complex In, dimethyl siloxane mixed methylcyclosiloxane and N-β-(aminoethyl)-γ-aminopropyltriethoxy diformazan The volume ratio of TMOS is 1: 1.
S13: the rotating shaft that described vexed rear paper roll carries out being sheathed on two-for-one twister (is specially twisted Dish) on, and after making paper inside described vexed rear paper roll wind described rotating shaft, lead to successively Cross after multiple feeding roller guides and fix with Wound-up roller;Wound-up roller and described rotating shaft is made to turn Dynamic, obtain circular pulp yarn.
Embodiment 2
S21: utilize separation machine to carry out separation tubular paper roll, obtaining width is 5 millimeters Treat vexed paper roll;
S22: will treat that vexed paper roll is dipped in paper softener, and make paper softener not have institute State and treat vexed paper roll 5 seconds, further take out through immersion after treat vexed paper roll, be placed in confined space Interior placement 3 hours;Obtain vexed rear paper roll;
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2 parts, fatty alcohol-polyoxyethylene ether 1 part and 15 parts of water;Described silicon is former In oil complex, dimethyl siloxane mixed methylcyclosiloxane and N-β-(aminoethyl)-γ-aminopropyl The volume ratio of methyl dimethoxysilane is 1: 2.
S23: consistent with step S13.
Embodiment 3
S31: utilize separation machine to carry out separation tubular paper roll, obtaining width is 3 millimeters Treat vexed paper roll;
S32: will treat that vexed paper roll is dipped in paper softener, and make paper softener not have institute State and treat vexed paper roll 1 second, further take out through immersion after treat vexed paper roll, be placed in confined space Interior placement 1 hour;Obtain vexed rear paper roll;
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2 parts, fatty alcohol-polyoxyethylene ether 1 part and 7 parts of water;Described silicon is former In oil complex, dimethyl siloxane mixed methylcyclosiloxane and N-β-(aminoethyl)-γ-aminopropyl The volume ratio of methyl dimethoxysilane is 1: 1.
S33: consistent with step S13.
Embodiment 4
S41: utilize separation machine to carry out separation tubular paper roll, obtaining width is 8 millimeters Treat vexed paper roll;
S42: will treat that vexed paper roll is dipped in paper softener, and make paper softener not have institute State and treat vexed paper roll 5 seconds, further take out through immersion after treat vexed paper roll, be placed in confined space Interior placement 6 hours;Obtain vexed rear paper roll;
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2 parts, fatty alcohol-polyoxyethylene ether 1 part and 3 parts of water;Described silicon is former In oil complex, dimethyl siloxane mixed methylcyclosiloxane and N-β-(aminoethyl)-γ-aminopropyl The volume ratio of methyl dimethoxysilane is 1: 3.
S43: consistent with step S13.
The twisting method of the pulp yarn that various embodiments of the present invention provide, the vexed rear paper of different in width The tensile strength of volume all significantly improves, and becomes a softer and smoother touch, it is easy to change shape, because of This is during twisting, paper slip not easy fracture, thus improves the production efficiency of pulp yarn.
Additionally, during twisting, the paper disc of employing flat pattern or paper roll are (through vexed After paper);By guiding and the cord being twisted being rolled up online after paper winding rotating shaft inside it On volume.Rotating shaft is during rotating, due to the paper slip being pulled and the angle of rotating shaft formation Less, therefore it is difficult to be pulled off, further improves the production efficiency of pulp yarn and good Product rate.
Although illustrate and describing the present invention with specific embodiment, but it will be appreciated that May be made that without departing from the spirit and scope of the present invention many other change and Amendment.It is, therefore, intended that include in the following claims belonging in the scope of the invention All such changes and modifications.

Claims (10)

1. the twisting method of pulp yarn, it is characterised in that include to obtain after separation Paper roll soaks through paper softener or sprays, after standing in airtight space directly Carry out twisting, obtain circular pulp yarn.
The twisting method of pulp yarn the most according to claim 1, it is characterised in that tool Body comprises the following steps:
1), tubular paper roll is carried out separation, obtain treating vexed paper roll;
2), treat that vexed paper roll is dipped in paper softener by described, and make paper softener not have Described treat vexed paper roll, further take out and treat vexed paper roll after soaking, be placed in confined space Place so that paper softener permeates, and obtains vexed rear paper roll;
Wherein, in described paper softener, in terms of volume parts, including by dimethyl-silicon Oxygen alkane mixed methylcyclosiloxane, N-β-(aminoethyl)-γ-aminopropyltriethoxy dimethoxysilane mixing Become silicon crude oil complex 2-4 part and fatty alcohol-polyoxyethylene ether 1-2 part;
3), described vexed rear paper roll is carried out twisting, obtain circular pulp yarn.
Twisting method the most according to claim 2, it is characterised in that in step 2) In, in described silicon crude oil complex, dimethyl siloxane mixed methylcyclosiloxane and N-β-(ammonia second Base) volume ratio of-γ-aminopropyltriethoxy dimethoxysilane is 1: (1-4).
Twisting method the most according to claim 3, it is characterised in that in step 2) In, in terms of volume parts, described paper softener also includes water 3-54 part.
Twisting method the most according to claim 3, it is characterised in that in step 2) In,
In described silicon crude oil complex, dimethyl siloxane mixed methylcyclosiloxane and N-β-(ammonia second Base) volume ratio of-γ-aminopropyltriethoxy dimethoxysilane is 1: 1;And described standing time It it is 2 hours.
Twisting method the most according to claim 4, it is characterised in that in step 2) In, the time of described immersion is the 1-20 second.
7. according to the twisting method described in any one of claim 1-6, it is characterised in that Step 3) in, specifically include:
Described vexed rear paper roll is sheathed in the rotating shaft of two-for-one twister, and makes described vexed rear paper roll The paper of inner side winds after described rotating shaft, pass sequentially through after multiple feeding roller guides with winding Roller is fixed;Make Wound-up roller and described axis of rotation, obtain circular pulp yarn.
Twisting method the most according to claim 7, it is characterised in that in step 1) In, described in treat that the width of vexed paper roll is 2-10 millimeter.
Twisting method the most according to claim 8, it is characterised in that in step 1) In, the operation of described separation uses separation machine to carry out.
10. the pulp yarn that the twisting method described in any one of claim 1-9 is twisted.
CN201510247308.0A 2015-05-15 2015-05-15 The pulp yarn that the twisting method of pulp yarn and the method are twisted Pending CN106283314A (en)