CN104831450B - 一种棉涤交织低弹牛仔面料及其制造方法 - Google Patents

一种棉涤交织低弹牛仔面料及其制造方法 Download PDF

Info

Publication number
CN104831450B
CN104831450B CN201510176110.8A CN201510176110A CN104831450B CN 104831450 B CN104831450 B CN 104831450B CN 201510176110 A CN201510176110 A CN 201510176110A CN 104831450 B CN104831450 B CN 104831450B
Authority
CN
China
Prior art keywords
jean
cotton
fabric
warp
road
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201510176110.8A
Other languages
English (en)
Other versions
CN104831450A (zh
Inventor
毛瑞元
曹浩明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangsu ERay family Industrial Co Ltd
Original Assignee
YINGRUI ENTERPRISE CORP
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YINGRUI ENTERPRISE CORP filed Critical YINGRUI ENTERPRISE CORP
Priority to CN201510176110.8A priority Critical patent/CN104831450B/zh
Publication of CN104831450A publication Critical patent/CN104831450A/zh
Application granted granted Critical
Publication of CN104831450B publication Critical patent/CN104831450B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本申请公开了一种棉涤交织低弹牛仔面料及其制造方法,该面料的经纱为全棉,该面料的纬纱为PBT长丝。本发明面料具有良好的耐久性、尺寸稳定性和较好的弹性,而且弹性不受湿度的影响,避免服装在经拉伸后形成的经向滑移,影响服装实用性。本发明面料纬向具有细而密的立体卷曲、优越的回弹性、手感柔软与皮肤摩擦无硬挺效果,提高了服装穿着舒适度。

Description

一种棉涤交织低弹牛仔面料及其制造方法
技术领域
本申请属于服装布料技术领域,特别是涉及一种棉涤交织低弹牛仔面料及其制造方法。
背景技术
随着经济的发展,生活水平的提高,人们对服装的追求不断向休闲,舒适,随意大方发展,所以牛仔面料逐渐的引领了服装的潮流,备受消费者的青睐。现在的牛仔面料已经不单单的局限于预缩整理,而是经过烧毛,退浆整理,液氨整理,树脂整理等新工艺,使面料手感更加柔软,细腻,滑爽。随着面料不断的深加工,在整理过程中容易出现不少的问题。
常规棉涤(FDY)牛仔面料一般以经向全棉纬向涤纶长丝交织而成,有优点为:布面挺括,不容易出现折皱,服装耐磨性优于全棉同规格产品;其缺点为:纬向纤维刚性较大,面料制成服装后长时间与皮肤摩擦易造成轻微过敏情况;布面纬向无弹力,纤维光滑摩擦力较小容易形成经向滑移,影响布面使用效果。
发明内容
本发明的目的在于提供一种棉涤交织低弹牛仔面料及其制造方法,以克服现有技术中的不足。
为实现上述目的,本发明提供如下技术方案:
本申请实施例公开一种棉涤交织低弹牛仔面料,该面料的经纱为全棉,该面料的纬纱为PBT长丝。
相应地,本申请还公开了一种棉涤交织低弹牛仔面料的制造方法,包括步骤:
(1)、浆染,10只经轴—润湿前处理(1道)—水洗(1道)—染色氧化(1道)—水洗(2道)—预烘—储纱—上浆—后烘—分绞排筘—织轴,
所述润湿前处理采用渗透剂Z0,包括上车工艺和水洗工艺,其中上车工艺中染槽的浓度为3g/L,上车时间30s,轧辊压力为26kN,轧余率为70%,水洗工艺中轧辊压力为35kN,轧余率为75%,
浆料的配方按重量份包括:110份的变性淀粉ZZD-LV,19份的聚丙烯SFB,以及5份的油剂301;
(2)、织造;
(3)、烧毛,车速为60m/min;
(4)、丝光,25℃下浸扎碱液-酸洗中和-温水60℃水洗4次-冷水30℃洗4次-落布,其中所述碱液包括:烧碱浓度290g/L、丝光渗透剂7g/L,所述酸洗中和中酸是指2.1g/L的冰醋酸;
(5)、预缩,采用40米/分莫里森预缩机,经向缩率5%、纬向4%。
与现有技术相比,本发明的优点在于:
1)面料具有良好的耐久性、尺寸稳定性和较好的弹性,而且弹性不受湿度的影响,避免服装在经拉伸后形成的经向滑移,影响服装实用性。
2)面料纬向具有细而密的立体卷曲、优越的回弹性、手感柔软与皮肤摩擦无硬挺效果,提高了服装穿着舒适度。
具体实施方式
新型涤纶长丝(PBT)品种特点:大分子基本链节上的柔性部分较长,具有良好的弹性和柔性可替代解决常规涤纶长丝硬挺无弹力缺点,提升面料服装舒适性和实用性。
本发明通过下列实施例作进一步说明:根据下述实施例,可以更好地理解本发明。然而,本领域的技术人员容易理解,实施例所描述的具体的物料比、工艺条件及其结果仅用于说明本发明,而不应当也不会限制权利要求书中所详细描述的本发明。
棉涤交织低弹牛仔面料的制造方法,包括步骤:
(1)、浆染,10只经轴—润湿前处理(1道)—水洗(1道)—染色氧化(1道)—水洗(2道)—预烘—储纱—上浆—后烘—分绞排筘—织轴,
所述润湿前处理采用渗透剂Z0,包括上车工艺和水洗工艺,其中上车工艺中染槽的浓度为3g/L,上车时间30s,轧辊压力为26kN,轧余率为70%,水洗工艺中轧辊压力为35kN,轧余率为75%,
浆料的配方按重量份包括:110份的变性淀粉ZZD-LV,19份的聚丙烯SFB,以及5份的油剂301;
(2)、织造;
(3)、烧毛,车速为60m/min;
(4)、丝光,25℃下浸扎碱液-酸洗中和-温水60℃水洗4次-冷水30℃洗4次-落布,其中所述碱液包括:烧碱浓度290g/L、丝光渗透剂7g/L,所述酸洗中和中酸是指2.1g/L的冰醋酸;
(5)、预缩,采用40米/分莫里森预缩机,经向缩率5%、纬向4%。
本发明实施例中,经向全棉、纬向PBT长丝交织面料:成分为C 60%T 38%与常规棉涤交织面料成分一致保持原有品种生产优点;经向全棉、纬向PBT长丝交织面料:经向水洗在缩率3%和普通棉涤弹一致,纬向水洗再缩率6-7%纬向回弹力明显提高。
最后,还需要说明的是,术语“包括”、“包含”或者其任何其他变体意在涵盖非排他性的包含,从而使得包括一系列要素的过程、方法、物品或者设备不仅包括那些要素,而且还包括没有明确列出的其他要素,或者是还包括为这种过程、方法、物品或者设备所固有的要素。

Claims (1)

1.一种棉涤交织低弹牛仔面料的制造方法,其特征在于,所述棉涤交织低弹牛仔面料的经纱为全棉,纬纱为PBT长丝,包括步骤:
(1)、浆染,10只经轴—润湿前处理1道—水洗1道—染色氧化1道—水洗2道—预烘—储纱—上浆—后烘—分绞排筘—织轴,
所述润湿前处理采用渗透剂,包括上车工艺和水洗工艺,其中上车工艺中染槽的浓度为3g/L,上车时间30s,轧辊压力为26kN,轧余率为70%,水洗工艺中轧辊压力为35kN,轧余率为75%,
浆料的配方按重量份包括:110份的变性淀粉,19份的聚丙烯SFB,以及5份的油剂301;
(2)、织造;
(3)、烧毛,车速为60m/min;
(4)、丝光,25℃下浸轧碱液-酸洗中和-温水60℃水洗4次-冷水30℃洗4次-落布,其中所述碱液包括:烧碱浓度290g/L、丝光渗透剂7g/L,所述酸洗中和中酸是指2.1g/L的冰醋酸;
(5)、预缩,采用40米/分莫里森预缩机,经向缩率3%、纬向缩率7%。
CN201510176110.8A 2015-04-15 2015-04-15 一种棉涤交织低弹牛仔面料及其制造方法 Active CN104831450B (zh)