Prior art keywords
cotton denim
cashmere
finishing process
fabric
denim fabric
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN 201310119585
Other languages
English (en)
Inventor
蒋岑章
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TAICANG QIDE GARMENT CO Ltd
Original Assignee
TAICANG QIDE GARMENT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TAICANG QIDE GARMENT CO Ltd filed Critical TAICANG QIDE GARMENT CO Ltd
Priority to CN 201310119585 priority Critical patent/CN103194906A/zh
Publication of CN103194906A publication Critical patent/CN103194906A/zh
Withdrawn legal-status Critical Current

Links

Landscapes

  • Treatments For Attaching Organic Compounds To Fibrous Goods (AREA)
  • Coloring (AREA)

Abstract

本发明公开了一种羊绒棉牛仔布的有机硅柔软整理工艺,浴液中加入3owf%-6owf%有机硅油和0.5g/L-2g/L的渗透剂,调节pH值到5.0-6.0,放入羊绒棉牛仔布,在温度30℃-50℃、浴比1:20-1:30的条件下处理30min-60min,冲洗,烘干。本发明的工艺对羊绒棉牛仔布有着良好的处理效果,织物风格改善明显,织物档次大大提高,工艺简单,符合环保要求。

Description

羊绒棉牛仔布的有机硅柔软整理工艺
技术领域
本发明属于纺织染整技术领域,涉及牛仔布柔软整理技术,具体涉及一种羊绒棉牛仔布的有机硅柔软整理工艺。
背景技术
羊绒棉牛仔布兼具羊绒纤维和棉纤维的优点,其制品质地优良、高雅华贵,风格独特,具有轻、柔、软、滑、爽等优良特点,作为高档服装面料越来越受到消费者的欢迎。为了弥补牛仔坯布的弹性、柔软性稍差,手感偏粗和容易起皱等缺陷,避免影响织物的外观和穿着舒适性,必须对其进行后整理。在后整理过程中,合理采用生态工艺,最大限度地减少对其风格的破坏,提高产品的附加值,成为了开发此类高档面料的关键。
目前牛仔布柔软整理多采取机械柔软整理和化学柔软整理的方法。机械整理柔软作用不持久,效果不明显;化学整理效果好,克服了传统牛仔布布坯僵直,柔软性差等缺陷。有机硅是一种半无机半有机的高分子聚合物,附着固化于纤维表面,其具有独特的表面性能和优异的柔软性能,可以修饰、修复和美化纤维感观,改善织物功能,而且对环境无毒害和污染,是一种优良的生态型纺织品整理剂,在纺织领域里起着越来越重要的作用。
发明内容
本发明提供了一种新的羊绒棉牛仔布的有机硅柔软整理工艺,保证羊绒棉牛仔布的柔软性。
本发明的羊绒棉牛仔布的有机硅柔软整理工艺,包括下述步骤:
浴液中加入3owf%-6owf%有机硅油和0.5g/L-2g/L的渗透剂,调节pH值到5.0-6.0,放入羊绒棉牛仔布,在温度30℃-50℃、浴比1:20-1:30的条件下处理30min-60min,冲洗,烘干。
优选的,浴液中加入5owf%有机硅油和1g/L的渗透剂。
优选的,放入羊绒棉牛仔布,在温度40℃、浴比1:25的条件下处理50min。
本发明的工艺对羊绒棉牛仔布有着良好的处理效果,织物风格改善明显,织物档次大大提高,工艺简单,符合环保要求。
具体实施方式
下面结合实施例对本发明的羊绒棉牛仔布的有机硅柔软整理工艺进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
实施例1
浴液中加入3owf%有机硅油和0.5g/L的渗透剂,调节pH值到5.0,放入羊绒棉牛仔布,在温度30℃、浴比1:20的条件下处理60min,冲洗,烘干。
实施例2
浴液中加入6owf%有机硅油和2g/L的渗透剂,调节pH值到6.0,放入羊绒棉牛仔布,在温度50℃、浴比1:30的条件下处理30min,冲洗,烘干。
实施例3
浴液中加入4owf%有机硅油和1g/L的渗透剂,调节pH值到5.5,放入羊绒棉牛仔布,在温度40℃、浴比1:25的条件下处理40min,冲洗,烘干。
实施例4
浴液中加入4owf%有机硅油和1.5g/L的渗透剂,调节pH值到5.5,放入羊绒棉牛仔布,在温度40℃、浴比1:25的条件下处理50min,冲洗,烘干。
实施例5
浴液中加入5owf%有机硅油和1g/L的渗透剂,调节pH值到5.5,放入羊绒棉牛仔布,在温度40℃、浴比1:25的条件下处理50min,冲洗,烘干。

Claims (3)

1.一种羊绒棉牛仔布的有机硅柔软整理工艺,其特征在于,包括以下步骤:
浴液中加入3owf%-6owf%有机硅油和0.5g/L-2g/L的渗透剂,调节pH值到5.0-6.0,放入羊绒棉牛仔布,在温度30℃-50℃、浴比1:20-1:30的条件下处理30min-60min,冲洗,烘干。
2.根据权利要求1所述的羊绒棉牛仔布的有机硅柔软整理工艺,其特征在于:浴液中加入5owf%有机硅油和1g/L的渗透剂。
3.根据权利要求1所述的羊绒棉牛仔布的有机硅柔软整理工艺,其特征在于:放入羊绒棉牛仔布,在温度40℃、浴比1:25的条件下处理50min。
CN 201310119585 2013-04-08 2013-04-08 羊绒棉牛仔布的有机硅柔软整理工艺 Withdrawn CN103194906A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201310119585 CN103194906A (zh) 2013-04-08 2013-04-08 羊绒棉牛仔布的有机硅柔软整理工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201310119585 CN103194906A (zh) 2013-04-08 2013-04-08 羊绒棉牛仔布的有机硅柔软整理工艺

Publications (1)

Publication Number Publication Date
CN103194906A true CN103194906A (zh) 2013-07-10

Family

ID=48717713

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201310119585 Withdrawn CN103194906A (zh) 2013-04-08 2013-04-08 羊绒棉牛仔布的有机硅柔软整理工艺

Country Status (1)

Country Link
CN (1) CN103194906A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107385640A (zh) * 2017-08-23 2017-11-24 山东万泰创业投资有限公司 一种山羊绒/莫代尔/棉/氨纶纤维生产牛仔面料的方法

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107385640A (zh) * 2017-08-23 2017-11-24 山东万泰创业投资有限公司 一种山羊绒/莫代尔/棉/氨纶纤维生产牛仔面料的方法

Similar Documents

Publication Publication Date Title
CN102505404B (zh) 一种双丝光棉针织布仿丝绸整理工艺
CN101338502B (zh) 全棉织物仿天丝处理工艺
CN101368340B (zh) 一种超细纤维合成革的后整饰工艺
CN100358950C (zh) 茜草染料的提取法及其染丝光羊毛或丝光毛织物的方法
CN104313898B (zh) 一种超仿棉改性聚酯纤维功能性印花毛毯的制备方法
CN102587147B (zh) 一种无氟防水透气针织面料的生产工艺
CN105350286A (zh) 一种天然免烫纯棉面料的加工方法
CN101285267B (zh) 一种天然彩棉针织品的防污整理方法
CN104762821A (zh) 一种蚕丝织物的免烫整理方法
CN102965964A (zh) 一种超柔软耐磨仿真皮聚氨酯鞋里革的制造方法
CN103526603A (zh) 羊毛纤维活性染料低温染色工艺
CN111394992A (zh) 一种抗菌防紫外线面料的制备方法
CN105862387A (zh) 一种抗菌防皱莱赛尔棉混纺织物的染整加工方法
CN102418249B (zh) 一种铜氨亚麻交织布的染色整理工艺及铜氨亚麻交织面料
CN102787458B (zh) 一种具有拒水拒油多功能的涂料染色牛仔面料的生产方法
CN104120606A (zh) 一种生态环保型桃皮绒家纺面料的生产工艺
CN104594020A (zh) 一种山羊绒纱线防缩工艺
CN103469540B (zh) 纯棉织物耐久免烫整理方法
CN103194906A (zh) 羊绒棉牛仔布的有机硅柔软整理工艺
CN102995444B (zh) 一种棉针织织物仿真丝绸风格的加工方法
CN107938318A (zh) 一种羊毛织物的环保印花工艺
CN103276587A (zh) 一种羊毛织物的防缩抗静电整理工艺
CN103938396B (zh) 服装免熨烫整理工艺
CN102978863A (zh) 薄型弹力面料的前处理工艺
CN103741424B (zh) 一种高档仿毛料棉布的加工工艺

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C04 Withdrawal of patent application after publication (patent law 2001)
WW01 Invention patent application withdrawn after publication

Application publication date: 20130710