JPS6132059A - Resin press plate - Google Patents

Resin press plate

Info

Publication number
JPS6132059A
JPS6132059A JP60046182A JP4618285A JPS6132059A JP S6132059 A JPS6132059 A JP S6132059A JP 60046182 A JP60046182 A JP 60046182A JP 4618285 A JP4618285 A JP 4618285A JP S6132059 A JPS6132059 A JP S6132059A
Authority
JP
Japan
Prior art keywords
film
mount
base
printing plate
main body
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP60046182A
Other languages
Japanese (ja)
Other versions
JPH0468618B2 (en
Inventor
Seiichi Uchida
内田 精一
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Osaka Sealing Printing Co Ltd
OSAKA SEIHAN CENTER KYOGYO KUMIAI
Original Assignee
Osaka Sealing Printing Co Ltd
OSAKA SEIHAN CENTER KYOGYO KUMIAI
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Osaka Sealing Printing Co Ltd, OSAKA SEIHAN CENTER KYOGYO KUMIAI filed Critical Osaka Sealing Printing Co Ltd
Priority to JP60046182A priority Critical patent/JPS6132059A/en
Publication of JPS6132059A publication Critical patent/JPS6132059A/en
Publication of JPH0468618B2 publication Critical patent/JPH0468618B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE:To attain welding by a high fequency welder by constituting a titled form plate so that a base part is formed in the periphery of a mount part, exposing and extending a base film in the periphery of the base part, and its outside peripheral part is deposited to a mount film. CONSTITUTION:A base part 23, a mount part 22 and a relief 21 are formed successively on a transparent base film 11 by a transparent hardening resin of an optical hardening resin, and a form plate main body 1 is formed. Subsequently, the form plate main body 1 is placed on a mount film 8 so that its matchmark 12 coindes with a matchmark on the mount film 8, the overall length of the outside peripheral edge of the base film 11 of the form plate main body 1 is deposted to the mount film 8 by a high frequency welder, and the form plate is completed. In such a way, after printing, when taking out ink by washing the surface of the form plate, and keeping it in a state that it has been installed to the mount film 8, it does not occur that washing water invades between the press plate main body 1 and the mount film 8.

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は光硬化性液体樹脂を用いて製作した刷版に関す
る。
DETAILED DESCRIPTION OF THE INVENTION [Industrial Field of Application] The present invention relates to a printing plate manufactured using a photocurable liquid resin.

〔従来の技術〕[Conventional technology]

近時、段ボール紙や新聞の印刷に際し、保存状態では液
状だが紫外線照射等の外的刺激を受けると硬化する性質
を有するウレタン系光硬化性液体樹脂(製造元:旭化成
工業株式会社)(商品名:APR)を使用した刷版が使
用されている。
Recently, when printing corrugated paper and newspapers, urethane-based photocurable liquid resin (manufacturer: Asahi Kasei Corporation) (product name: APR) printing plate is used.

斯種刷版の製作は第7図乃至第11図に示す工程を経て
行なわれている。
The production of this type of printing plate is carried out through the steps shown in FIGS. 7 to 11.

一例として第6図に示す如<rABJの標章をダンボー
ル紙に印刷するために用いる刷版主体(1)(標章は刷
版表面では裏返し標章(9)となって表われる)をマウ
ントフィルム(8)に取付けた刷版の従来の製造方法を
説明する。
As an example, as shown in Figure 6, a printing plate main body (1) used to print the <rABJ mark on cardboard paper (the mark appears as a reverse mark (9) on the surface of the printing plate) is mounted. A conventional method for manufacturing a printing plate attached to a film (8) will be explained.

第7図は刷版主体(1)の製作に用いるネガフィルム(
3)トマスキングフィルム(4)を示しており、ネガフ
ィルム(3)上に前記標章(9)に対応する透光性パタ
ーン(31)が形成され、該パターン以外の斜線で示す
部分は完全遮光面となっている。
Figure 7 shows the negative film (
3) A masking film (4) is shown, in which a transparent pattern (31) corresponding to the mark (9) is formed on the negative film (3), and the shaded area other than the pattern is completely It is a light-shielding surface.

マスキングフィルム(4)はネガフィルム(3)上の上
記透光性パターン011に対応して該パターンC11)
よりも稍大きな輪郭の透光性パターン(41)を有し、
その他の斜線で示す部分は完全遮光面となっている。
The masking film (4) has a pattern C11 corresponding to the above-mentioned translucent pattern 011 on the negative film (3).
It has a translucent pattern (41) with a slightly larger outline than the
The other shaded areas are completely light-shielding surfaces.

a工程 第8図に示す如く透明台板(5)上に樹脂に対
して剥離可能なネガフィルム(3)を置き、ネガフィル
ム(3)の上に保護用の透明フィルム(6)を被せる。
Step a: As shown in FIG. 8, a negative film (3) that can be peeled off from the resin is placed on a transparent base plate (5), and a protective transparent film (6) is placed on the negative film (3).

b工程 透明フィルム(6)の外周部に液体樹脂に対し
て堰となる様に枠体(7)を配設して、ネガフィルム(
3)の透光性パターン曲全体を取り囲み、枠体(7)に
よって囲まれた内側の透明フィルム[61上へ光硬化性
液体樹脂を流し込んで光硬化性液体樹脂層(2)を形成
する(第8図)。
Step b: A frame (7) is arranged around the outer periphery of the transparent film (6) so as to act as a dam against the liquid resin, and the negative film (
A photocurable liquid resin is poured onto the inner transparent film [61] surrounding the entire translucent pattern of 3) and surrounded by a frame (7) to form a photocurable liquid resin layer (2). Figure 8).

C工程 光硬化性液体樹脂層(2)の液面に透明ベース
フィルム(11)を載せ、該ベースフィルム+111 
上にマスキングフィルム(4)を被せる(第8図)。
Step C: Place the transparent base film (11) on the liquid surface of the photocurable liquid resin layer (2), and add the base film +111
Cover the top with masking film (4) (Figure 8).

d工程 第9図の如くマスキングフィルム(4)及び透
明台板(5)の外側から紫外線ランプ(51+ (51
+を照射して液体樹脂層を露光する。マスキングフィル
ム(4)及びネガフィルム(3)の夫々パターンC31
1F411に対応して露光部分は硬化を始め、未露光部
分は液体の侭で残り、ネガフィルム(3)側の樹脂硬化
部は前記標章(9)に一致するレリーフ部(21)とな
り、マスキングフィルム(4)側の樹脂硬化部は該レリ
ーフ部011に太(繋がって補強となるマウント部(社
)となる。
Step d: As shown in Figure 9, the ultraviolet lamp (51+ (51)
Expose the liquid resin layer by irradiating +. Each pattern C31 of masking film (4) and negative film (3)
Corresponding to 1F411, the exposed part begins to harden, the unexposed part remains as a liquid, and the cured resin part on the negative film (3) side becomes a relief part (21) that corresponds to the mark (9), and is masked. The cured resin portion on the film (4) side is connected to the relief portion 011 to form a mount portion (shape) for reinforcement.

C工程 マスキングフィルム(4)を外して第10図の
如くベースフィルム(11)の外側から再び短時間露光
し、樹脂液層の上面全体を薄く硬化させベースフィルム
(11)と一体に接合したベース部内を形成する。
Step C: The masking film (4) is removed and the base film (11) is exposed again for a short time from the outside as shown in Figure 10, and the entire upper surface of the resin liquid layer is thinly cured and the base is integrally bonded to the base film (11). Form the department.

f工程 枠体(7)及び透明フィルム(6)を外し、未
硬化の樹脂液を回収する。
Step f: Remove the frame (7) and transparent film (6) and collect the uncured resin liquid.

第11図に示す如く、レリーフ部(21)がマウント部
いによって補強され、マウント部■がベースフィルム0
1)のほぼ全面を覆うベース部(ハ)に繋がった刷版主
体(1)が形成される。
As shown in Fig. 11, the relief part (21) is reinforced by the mount part (2), and the mount part (2) is
A printing plate main body (1) is formed which is connected to a base portion (c) that covers almost the entire surface of the printing plate (1).

上記刷版主体(1)はベースフィルムαDが樹脂の接着
力に□よってベース部内に接合して一様に覆った2層構
造になっている。
The printing plate main body (1) has a two-layer structure in which the base film αD is bonded into the base portion by the adhesive force of the resin and uniformly covered.

g工程 上記刷版主体(1)を印刷機用透明マウントフ
ィルム(8)上へ位置決めして固定し刷版を形成する。
Step g: The printing plate main body (1) is positioned and fixed onto a transparent mounting film (8) for a printing press to form a printing plate.

上記刷版を印刷機の回転胴へ着脱可能に取り付けて使用
する。
The printing plate is used by being removably attached to the rotating cylinder of a printing press.

〔発明が解決しようとする問題点〕[Problem that the invention seeks to solve]

刷版主体をマウントフィルム上へ位置決めした後、取り
付ける手段として、従来は刷版主体を押えながら周囲に
粘着テープ(131を接着し、刷版主体のベース部とマ
ウントフィルムとを止めるか、或は刷版主体の裏面に予
め両面接着テープを貼り、これをマウントフィルム上へ
置いて押え、接着した。
After positioning the printing plate main body on the mount film, the conventional method for attaching it is to attach adhesive tape (131) around the printing plate main body while holding the printing plate main body, and fix the base part of the printing plate main body and the mount film, or Double-sided adhesive tape was pasted on the back side of the main printing plate in advance, and this was placed on the mounting film and pressed to adhere.

しかし何れの方法も、万一接着テープの接着力が弱って
いると高速印刷の際に刷版主体に作用する遠心力によっ
て刷版主体がマウントフィルムから剥れる危険があり、
又印刷後に刷版表面を洗浄してインキを落し、マウント
フィルムに取り付けた侭で保管する際、洗浄水が刷版主
体とマウントフィルムの間へ侵入して残恍、これが次の
印刷の際に流出して来て印刷面を汚す虞れがあった。マ
ウントフィルムと刷版主体とを高周波ウエルターによっ
て一体結合させて取り付けることも試みられたが、マウ
ントフィルムは材質はポリエステルであり、刷版主体は
表面をウレタン系樹脂のベース部が一様に覆っているた
め、高周波ウェルターは実施出来なかった。
However, with either method, if the adhesive strength of the adhesive tape is weak, there is a risk that the printing plate will peel off from the mounting film due to the centrifugal force that acts on the printing plate during high-speed printing.
Also, when the surface of the printing plate is washed to remove ink after printing and stored on the mount film, the washing water enters between the main body of the printing plate and the mount film and leaves a residue, which can be used for the next printing. There was a risk that it would leak out and stain the printed surface. Attempts have been made to attach the mount film and the main body of the printing plate by integrally bonding them together using a high-frequency welter, but the material of the mount film is polyester, and the surface of the main body of the printing plate is uniformly covered with a base of urethane resin. High frequency weltering could not be performed due to the presence of

〔問題を解決するための手段〕[Means to solve the problem]

本発明は刷版主体をベースフィルムに溶着固定して前記
問題を解決するものであり、ベース部はマウント部の周
囲に゛形成し該ベース部の周囲へベースフィルムを露出
して伸ばし、ベースフィルムの外周部をマウントフィル
ムに溶着する。
The present invention solves the above problem by welding and fixing the main body of the printing plate to the base film.The base part is formed around the mount part, and the base film is exposed and stretched around the base part. Weld the outer periphery of the mount film to the mounting film.

〔作用及び効果〕 ベース部囚)の周囲にはベースフィルムαDが露出した
状態で完成するから、これをマウントフィルムに位置決
めして置き周囲を高周波ウエルター等によって溶着すれ
ば、容易に溶着し一体結合し、しかも溶着線[株]を刷
版主体の外周に沿って一周して形成すれば、従来の如く
刷版主体とマウントフィルムとの間へ洗浄水が侵入する
問題も解決出来る。
[Operations and Effects] The base film αD is completed with exposed surroundings of the base part, so if this is positioned on the mount film and the surrounding area is welded using a high frequency welter, etc., it will be easily welded and integrally joined. However, if the welding line is formed around the outer periphery of the printing plate main body, the conventional problem of cleaning water entering between the printing plate main body and the mounting film can be solved.

〔実施例〕〔Example〕

刷  版 第1図は本発明の特徴とする刷版主体(1)をその縁部
を高周波溶着によってマウントフィルム(8)に取付け
て形成した刷版を示している。
Printing Plate FIG. 1 shows a printing plate formed by attaching a printing plate main body (1), which is a feature of the present invention, to a mounting film (8) by high-frequency welding at its edges.

刷版主体(1)は従来例で説明したものと同様にrAB
Jの標章(9)をレリーフ部(21+ (21+によっ
て浮き出している。
The printing plate main body (1) is rAB as explained in the conventional example.
The mark (9) of J is embossed by the relief part (21+ (21+).

レリーフ部(21)はそれよりも少し輪郭の大きなマウ
ント部@上に形成され、マウント部にはそれを取り囲む
広い面積のベース部内上に形成されている。
The relief part (21) is formed on a mount part @ having a slightly larger outline than the relief part (21), and the mount part is formed inside a base part with a wide area surrounding it.

ベース部(ハ)ハポリエステル製のベースフィルム1I
ll上へ樹脂自身の接着力によって、或は必要によりベ
ースフィルムに塗布した接着剤の接着力によって強く接
着しており、第5図の如くレリーフ部(21+、マウン
ト部@及びベース部器は光硬化性樹脂にて一体に形成さ
れる。段ボール紙用の刷版の場合、ベース部t2mの厚
みり、は約2. OwM、マウント部@の厚みh2は約
2.5m、レリーフ部t211の厚みh3は約2mに形
成するのが好ましい。
Base part (c) Polyester base film 1I
The relief part (21+, mount part @ and base part are not exposed to light) as shown in Figure 5. It is integrally formed with a curable resin.In the case of a printing plate for corrugated paper, the thickness of the base part t2m is approximately 2.0m, the thickness h2 of the mount part @ is approximately 2.5m, and the thickness of the relief part t211. Preferably, h3 is approximately 2 m long.

刷版主体(1)は、ベース部(2)が形成されない部分
にはベースフィルム(11)がその侭露出しており、ベ
ーフィルムの露出部には、位置決め用の合マーク(12
1がベース部22)と同じ高さに形成されている。
The printing plate main body (1) has a base film (11) exposed on the side where the base part (2) is not formed, and a positioning mark (12) is provided on the exposed part of the base film.
1 is formed at the same height as the base portion 22).

刷版主体をマウントフィルム上へ固定するには刷版主体
の合マークを利用してマウントフィルム上に位置決めし
た後、公知の携帯用高周波ウエルダー機等によって刷版
主体のベースフィルム露出部をマウントフィルムへ溶着
し、一体化させて取り付ける。
To fix the main body of the printing plate onto the mount film, use the alignment marks on the main body of the printing plate to position it on the mount film, and then use a known portable high-frequency welder or the like to fix the exposed part of the base film of the main body of the printing plate onto the mount film. Weld it to and install it as one piece.

製作工程 次に上記刷版主体(1)の製作工程を説明する。Manufacturing process Next, the manufacturing process of the printing plate main body (1) will be explained.

第1図は刷版主体゛(1)の製作に用いるネガフィルム
(3)とマスキングフィルム(4)を示している。
FIG. 1 shows a negative film (3) and a masking film (4) used in the production of the printing plate body (1).

マスキングフィルム(4)は透明フィルム(4急の一方
の面に完全遮光フィルム(49、他方の面に半遮光フィ
ルム(431を接着剤にて剥離可能に貼着したものであ
る。
The masking film (4) is a transparent film (4), with a completely light-shielding film (49) attached to one side and a semi-light-shielding film (431) removably attached to the other side with an adhesive.

ネガフィルム(3)は前記標章(9)に対応する透光性
パターン(31)の他は斜線で示す如(完全遮光面とな
っている。ここで注目すべき点はネガフィルム(3)に
は刷版主体(1)の合マーク(121に対応する透光部
は形成しておらず、マスキングフィルムの完全遮光面に
だけ適位置に合マークに対応する透光部(46a)を切
り抜いて形成したことである・。
The negative film (3) has a completely light-shielding surface as shown by diagonal lines except for the translucent pattern (31) corresponding to the mark (9).The important point to note here is that the negative film (3) The transparent part corresponding to the match mark (121) of the main body of the printing plate (1) is not formed, and the transparent part (46a) corresponding to the match mark is cut out at the appropriate position only on the completely light-shielding surface of the masking film. It was formed by

半遮光フィルム(431には前記ネガフィルム(3)の
透光性パターン(31)に対応して該パターン(31)
よりも稍大きな輪郭の透光性パターン(417を切り抜
いて形成され、完全遮光性フィルム(45)には半遮光
フィルム(4団の透光性パターン(441よりも更に大
きい輪郭の透光性パターン(46)を切り抜いて形成さ
れている。
The semi-light-shielding film (431 has a pattern (31) corresponding to the translucent pattern (31) of the negative film (3))
The completely light-shielding film (45) is formed by cutting out a light-transmitting pattern (417) with a slightly larger outline, and the semi-light-shielding film (45) is formed by cutting out a light-transmitting pattern (441) with a slightly larger outline. It is formed by cutting out (46).

上記各透光性パターン+441 (461は半遮光フィ
ルム(43)及び完全遮光フィルム(45)に透明フィ
ルム(42)に達する深さにナイフでパターン(44J
 f461に対応する切込み線を施し、切込み線の内側
を透明フィルム(421から剥き取って形成されている
Each of the above light-transmitting patterns +441 (461 is a pattern (44J) on the semi-light-shielding film (43) and the completely light-shielding film (45) with a knife to a depth that reaches the transparent film (42).
It is formed by making a cut line corresponding to f461 and peeling off the inside of the cut line from the transparent film (421).

半遮光フィルム(4!9は露光の約10〜15%を透過
せしめる。
A semi-shading film (4!9) allows about 10-15% of the exposed light to pass through.

されず、例えば透明フィルム(421の上に上記半遮光
フィルム(43)を剥離可能に貼着し、該半遮光フィル
ム(431の上に上記完全遮光フィルム(451を剥離
可能に貼着したものでも可い。
For example, the above-mentioned semi-light-shielding film (43) may be removably adhered to a transparent film (421), and the above-mentioned completely light-shielding film (451) may be removably adhered to the semi-light-shielding film (431). Yes.

第1工程 第3図に示す如く透明台板(5)上にネガフ
ィルム(3)を置き、ネガフィルム(3)の上に透明フ
ィルム(6)を被せる。更に透明フィルム(6)の外周
部に略長方形の枠体(7)を置き、枠体(7)内に光硬
化性液体樹脂を流し込み、透明フィルム(6)上に光硬
化性液体樹脂層(2)を形成する。
First step: As shown in FIG. 3, a negative film (3) is placed on a transparent base plate (5), and a transparent film (6) is placed over the negative film (3). Furthermore, a substantially rectangular frame (7) is placed around the outer periphery of the transparent film (6), a photocurable liquid resin is poured into the frame (7), and a photocurable liquid resin layer ( 2) Form.

第2工程 光硬化性液体樹脂層(2)の上面に透明ベー
スフィルム(11)を載せ、該フィルム011の上にマ
スキングフィルム+41 ヲ被−)t ル。
Second step: A transparent base film (11) is placed on the top surface of the photocurable liquid resin layer (2), and a masking film (41) is placed on top of the film (011).

透明ベースフィルム01)の下面には必要に応じて予め
光硬化性樹脂との接着性の良好な透明接着剤(図示せず
)を塗布しておく。
A transparent adhesive (not shown) having good adhesion to the photocurable resin is applied in advance to the lower surface of the transparent base film 01), if necessary.

第3工程 第4図に示す如く透明台板(5)及びマスキ
ングフィルム(4)の外から光源(51)からの光を当
て、光硬化性樹脂を380〜400秒露光オス− 露光によって樹脂層の下部はネガフィルム(3)のパタ
ーン(131+に対応する部分が硬化してレリーフ部閉
)となる。
Third step As shown in Figure 4, light from a light source (51) is applied from outside the transparent base plate (5) and masking film (4), and the photocurable resin is exposed for 380 to 400 seconds to form a resin layer. The lower part becomes a pattern of negative film (3) (the part corresponding to 131+ is cured and the relief part is closed).

他方、マスキングフィルム(4)側での液体樹脂層(2
)の硬化状態は、マスキングフィルム(4)及び半遮光
フィルム(43)の透光性パターン+44) (461
と対応した部分は、樹脂層が厚く硬化して前記レリーフ
部因)と一体に繋がったマウント部(221となり、又
半遮光フィルム(43)に掛って弱められた完全遮光面
(45a)上の透光性部分では、パターン(46)に対
応して樹脂層の上部が薄く硬化してマウント部(22)
と繋がったベース部t23+となる。
On the other hand, the liquid resin layer (2) on the masking film (4) side
) is the cured state of the masking film (4) and semi-shading film (43) +44) (461
The part corresponding to the mount part (221) where the resin layer is thick and hardened and is integrally connected with the relief part), and the part on the completely light-shielding surface (45a) weakened by covering the semi-light-shielding film (43). In the translucent part, the upper part of the resin layer is thinly hardened in correspondence with the pattern (46) to form the mount part (22).
The base part t23+ is connected to the base part t23+.

ベース部(23+は樹脂自体の接着性により、又は予め
ベースフィルム(IJ)に塗布された接着剤によってベ
ースフィルム(11)に強固に接合される。
The base portion (23+) is firmly joined to the base film (11) by the adhesive property of the resin itself or by an adhesive applied to the base film (IJ) in advance.

尚、露光の順序は先ずマスキングフィルム(4)側の露
光を開始して露光所要時間の約−が経過した時期にネガ
フィルム(3)側からの露光を開始し、夫々露光の所要
時間が経過すれば露光を別々に停止する。
The order of exposure is to first start exposing the masking film (4) side, and when the required exposure time has elapsed, start exposing the negative film (3) side, and then start exposing the negative film (3) side when the required exposure time has elapsed. Then, the exposure will be stopped separately.

上記の様にマスキングフィルム(4)側の露光をネガフ
ィルム(3)側からの露光よりも先行させることにより
、レリーフ部(21)の土台となるマウント部@、ベー
ス部(23)がレリーフ部(2υよりも先に形成され、
レリーフ部(211が該マウント部(22)に安定して
一体化形成される。
As described above, by exposing the masking film (4) side before the exposure from the negative film (3) side, the mount part @, which becomes the base of the relief part (21), and the base part (23) become the relief part. (formed before 2υ,
A relief part (211) is stably formed integrally with the mount part (22).

マスキングフィルム(4)側からの露光が終了してから
ネガフィルム(3)側からの露光を開始しても可いが、
この場合、時間的にロスが生じる。
Although it is possible to start exposure from the negative film (3) side after the exposure from the masking film (4) side is completed,
In this case, a time loss occurs.

尚、露光時間は形成すべき刷版の厚み、光の強さによっ
て最適に決めれば可いのは勿論である。
It goes without saying that the exposure time can be optimally determined depending on the thickness of the printing plate to be formed and the intensity of light.

第4工程 72スキングフイルム(4)、枠体(7)、
透明フィルム(6)を取り外し、未硬化の液体樹脂を回
収し刷版主体(1)が完成する。
4th step 72 skin film (4), frame (7),
The transparent film (6) is removed and the uncured liquid resin is collected to complete the printing plate body (1).

第5工程 刷版主体(1)をその合マーク0りをマウン
トフィルム(8)上の合マーク(図示せず)lζ合わせ
て該フィルム(8)上に置き、高周波ウェルグーニよっ
て刷版主体(1)のベースフィルム(11)の外周縁の
全長を溶着し、刷版を完成する。
Fifth step: Place the printing plate main body (1) on the film (8) with its matching mark 0 and the matching mark (not shown) lζ on the mount film (8), and use the high frequency Welgooni to ) The entire length of the outer periphery of the base film (11) is welded to complete the printing plate.

【図面の簡単な説明】[Brief explanation of the drawing]

第1図は刷版の斜面図、第2図はネガフィルム及びマス
キングフィルムの斜面図、第3図、第4図、第5図は製
造工程図、第6図は従来例の刷版の斜面図、第7図は従
来のマスキングフィルム及びネガフィルムの斜面図、第
8図、第9図、第10図、第11図は従来方法の製造工
程図である。 (1)・・・刷版主体    (11)・・・透明ベー
スフィルム(2)・・・光硬化性液体樹脂層 ■1)・・・レリーフ部   (社)・・・マウント部
(8)・・・マウントフィルム
Figure 1 is a slope view of a printing plate, Figure 2 is a slope view of a negative film and masking film, Figures 3, 4, and 5 are manufacturing process diagrams, and Figure 6 is a slope view of a conventional printing plate. 7 are oblique views of a conventional masking film and a negative film, and FIGS. 8, 9, 10, and 11 are manufacturing process diagrams of a conventional method. (1)...Printing plate main body (11)...Transparent base film (2)...Photocurable liquid resin layer ■1)...Relief part (sha)...Mount part (8)・Mount film

Claims (1)

【特許請求の範囲】[Claims] 光硬化性樹脂の透明硬化樹脂によってレリーフ部、該レ
リーフ部を補強するマウント部及び該マウント部の周囲
に拡がるベース部が形成されベース部が透明ベースフィ
ルム上に接合している刷版主体をマウントフィルムに取
り付けた樹脂刷版に於て、ベース部はマウント部の周囲
に形成され該ベース部の周囲へベースフィルムが露出し
て伸びており、ベースフィルムの外周部がマウントフィ
ルムに溶着固定されている樹脂刷版。
A relief part, a mount part for reinforcing the relief part, and a base part extending around the mount part are formed using a transparent curing photocurable resin, and the base part is attached to a transparent base film to mount the main body of the printing plate. In a resin printing plate attached to a film, the base part is formed around the mount part, the base film is exposed and extends around the base part, and the outer periphery of the base film is welded and fixed to the mount film. Resin printing plate.
JP60046182A 1985-03-07 1985-03-07 Resin press plate Granted JPS6132059A (en)