JP4540035B2 - 電池及び電池の製造方法 - Google Patents
電池及び電池の製造方法 Download PDFInfo
- Publication number
- JP4540035B2 JP4540035B2 JP2003301287A JP2003301287A JP4540035B2 JP 4540035 B2 JP4540035 B2 JP 4540035B2 JP 2003301287 A JP2003301287 A JP 2003301287A JP 2003301287 A JP2003301287 A JP 2003301287A JP 4540035 B2 JP4540035 B2 JP 4540035B2
- Authority
- JP
- Japan
- Prior art keywords
- terminal
- battery
- battery case
- nut
- screw portion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
(1)体積及び重量当たりのエネルギー密度が高く、軽量化及び大容量化が図れる。
(2)高出力密度であるため、大電流を取り出すことができる。
(3)充放電サイクル性能に優れ寿命が長い。
(4)動作温度範囲が広い。
(5)急速充電が可能である。
(6)自己放電が少ない。
れ、その上にワッシャ8を介してナット10が配置されている。端子3のロッド部32は、フランジ部31の段部31aの上側に連なる大径部32aと、大径部32aの上側に連なるネジ部32bと、ネジ部32bの上側に連なる小径部32cとからなる。大径部32aは、押さえ板7の筒部7aの内周に挿通されている。そして、押さえ板7及びワッシャ8の上から、ナット10を端子3のネジ部32bに螺合して締め込むことにより、端子キャップ5と端子3の段部31aとの間に介在されたガスケット6が圧縮変形され、これにより端子3と端子キャップ5の端子孔5aとの隙間がシールされている。
H 8603−1995 「アルミニウム及びアルミニウム合金の工業用硬質陽極酸化皮膜」に規定されている。
した保持力でガスケットを保持して気密性を高めることができる。
2 電槽
3 端子(正極端子)
32 ロッド部(先端側)
32b ネジ部
5 端子キャップ(電槽側の部材)
5a 端子孔
6 ガスケット
10 ナット
Claims (4)
- 発電要素を収納した電槽と、前記電槽に形成された開口に配置された純アルミニウム製の端子と、前記電槽と前記端子との間に介在されたガスケットと、を有し、
前記端子は、電槽内部において前記発電要素に接続される基端部と、ネジ部を有しかつ前記電槽の外部に突出する先端部とを備え、
前記先端部の前記ネジ部に螺合されるナットを締め込むことにより、前記ナットと前記端子の基端部とで前記ガスケットを圧縮変形させて前記端子と前記電槽との隙間をシールする電池において、
前記端子の前記ネジ部の表面に硬質アルマイト処理による硬化膜が形成されていることを特徴とする電池。 - 前記硬化膜の厚さが10〜100μmの範囲に設定されていることを特徴とする請求項1記載の電池。
- 前記ネジ部の表面のビッカース硬さがHV350〜500であることを特徴とする請求項1または2記載の電池。
- 140〜200N・mの締め付けトルクで前記ネジ部に螺合されるナットが締め込まれたことを特徴とする請求項1から3のいずれかに記載の電池の製造方法。