Prior art keywords
mold
cooler
water
steel ingot
ingot
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2009200901623U
Other languages
English (en)
Inventor
朱书成
王希彬
曹国超
赵家亮
吕艳伍
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanyang Hanye Special Steel Co Ltd
Original Assignee
Nanyang Hanye Special Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanyang Hanye Special Steel Co Ltd filed Critical Nanyang Hanye Special Steel Co Ltd
Priority to CN2009200901623U priority Critical patent/CN201423430Y/zh
Application granted granted Critical
Publication of CN201423430Y publication Critical patent/CN201423430Y/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Landscapes

  • Continuous Casting (AREA)

Abstract

本实用新型属于冶金铸造技术领域的一种由水冷结晶器冷却的锭模装置,具有铸模和位于铸模底部的冷却器,所述铸模由支架固定,所述冷却器设置在底板上,其特征在于:所述冷却器为水冷结晶器,所述铸模内腔竖直截面形状为倒置的锥台形,在冷却器与底板之间设有可带动冷却器上下移动的升降装置。与现有相比,在铸造过程使钢锭始终与铸模处于紧贴状态,有效地解决了冷凝过程中气隙现象的产生,使钢锭通过正常的热传导进行散热,保障了钢锭心部晶粒冷凝后内部组织的机械性能,使用寿命长。

Description

一种由水冷结晶器冷却的锭模装置
技术领域
本实用新型属于冶金铸造技术领域,具体涉及一种由水冷结晶器冷却的锭模装置。
背景技术
在公知的铸造技术中,铸造钢锭所用模具通常均为铸铁整体铸模,这种铸模的存在以下缺点:第一、钢液在锭模中冷凝的中后阶段,锭模吸收大量的热并上升很高温度,而锭模向外散热主要靠向外辐射,散热的速度很慢,于是钢液冷凝的速度逐渐降低。第二、钢锭在整个冷凝的过程中,由于热胀冷缩的原因,钢锭与铸模间便形成气隙,气隙的存在使钢锭与铸模间热传导性能下降,钢锭结晶的速度更受影响,这样的结果使得钢锭心部晶粒粗大,且成分偏析现象明显,结果造成铸出的钢锭心部组织机械性能差。第三、原锭模的使用寿命低,一般仅能铸造30多个钢锭,铸锭平摊模具费用较高。
实用新型内容
为解决现有技术存在的上述缺陷,本实用新型的目的在于提供一种能够消除在铸造中钢锭与铸模间形成的气隙,可以使钢锭快速均匀冷凝,保证了钢锭的结晶速度,提高钢锭整体机械性能的由水冷结晶器冷却的锭模装置。
为实现上述目的,本实用新型采用的技术方案是:该由水冷结晶器冷却的锭模装置,具有铸模和位于铸模底部的冷却器,所述铸模由支架固定,所述冷却器设置在底板上,其特征在于:所述冷却器为水冷结晶器,所述铸模内腔竖直截面形状为倒置的锥台形,在冷却器与底板之间设有可带动冷却器上下移动的升降装置。
所述升降装置为多个液压油缸,液压油缸连接液压站。
所述升降装置具有导向柱、丝母和丝杠构成。
所述铸模的顶部设置有保温帽。
采用上述技术方案的有益效果是:该由水冷结晶器冷却的锭模装置,具有铸模和位于铸模底部的冷却器,冷却器为水冷结晶器,锭模及钢锭本身的热量可以迅速地通过流动的水带走,改变了原有锭模仅由辐射向外散热的方式,大大加快钢锭冷凝的速度,铸模内腔形状为倒置的锥台形或圆锥台形,在冷却器与底板之间设有升降装置,水冷结晶器在升降装置的作用下可上下移动,在钢锭冷凝的过程中,由于热胀冷缩的原因,钢锭与铸模间便形成气隙,通过实时调节升降装置的下降,带动水冷结晶器的下移,由于钢锭是靠水冷结晶器来支撑的,当水冷结晶器的移时钢锭也会随着下移,由于铸模具有上宽下窄的锥度,使钢锭始终与铸模处于紧贴状态,有效地解决了冷凝过程中气隙现象的产生,使钢锭通过正常的热传导进行散热,保障了钢锭心部晶粒冷凝后内部组织的机械性能;在铸模的顶部设置有保温帽的结构,使钢锭处于相对封密的空间中,从而使整个钢锭热胀冷缩均匀,分离干净,在生产过程中不易出现损坏,使用寿命长。
附图说明
下面结合附图对本实用新型的具体实施例作进一步详细的说明。
图1是本实用新型的结构示意图。
图1是本实用新型的升降装置的另一结构示意图。
具体实施方式
如图1所示的一种由水冷结晶器冷却的锭模装置,具有铸模1,铸模1由由支架2固定,铸模的顶部设置有保温帽9。铸模1的内腔竖直截面形状为倒置的锥台形或圆锥台形,冷却器3构成锭模的底部,冷却器采用水冷结晶器。水冷结晶器的下部设有多个液压油缸4,液压油缸4连接液压站,由液压站为液压油缸4提供动力,水冷结晶器为可移动,由液压油缸4带动其上下移动,液压油缸4设置在底板5上。作为水冷结晶器的移动结构的另一实施方式为:水冷结晶器的下部设有具有导向柱6、丝母7和丝杠8,导向柱6对水冷结晶器的上下移动起导向作用,丝母7由减速器和电机驱动。
工作时,降起水冷结晶器下部的升降机构,使水冷结晶器贴位铸模的底部,由水冷结晶器构成铸模的底,开始浇注,待钢液在铸模内坯壳凝结一定厚度时,通过升降机构动作带动水冷结晶器下移,铸模内坯壳在重力作用下下移,从而填充由坯壳的冷却收缩在坯壳与铸模之间产生的气隙,使钢锭始终与铸模的内壁紧贴在一起,充分利用热传导作用使钢锭快速冷凝。待铸锭凝固基本完成时,将保温帽移开,利用升降机构将钢锭顶出铸锭,再将钢锭吊出即可。
由于在冷却器与底板之间设有升降装置,水冷结晶器在升降装置的作用下可上下移动,在钢锭冷凝的过程中,由于热胀冷缩的原因,钢锭与铸模间便形成气隙,通过实时调节升降装置的下降,带动水冷结晶器的下移,由于钢锭是靠水冷结晶器来支撑的,当水冷结晶器的移时钢锭也会随着下移,由于铸模具有上宽下窄的锥度,使钢锭始终与铸模处于紧贴状态,有效地解决了冷凝过程中气隙现象的产生,使钢锭通过正常的热传导进行散热,保障了钢锭心部晶粒冷凝后内部组织的机械性能;在铸模的顶部设置有保温帽的结构,使钢锭处于相对封密的空间中,从而使整个钢锭热胀冷缩均匀,分离开净,在生产过程中不易出现损坏,使用寿命长。

Claims (4)

1、一种由水冷结晶器冷却的锭模装置,具有铸模和位于铸模底部的冷却器,所述铸模由支架固定,所述冷却器设置在底板上,其特征在于:所述冷却器为水冷结晶器,所述铸模内腔竖直截面形状为倒置的锥台形,在冷却器与底板之间设有可带动冷却器上下移动的升降装置。
2、根据权利要求1所述的一种由水冷结晶器冷却的锭模装置,其特征在于:所述升降装置为多个液压油缸,液压油缸连接液压站。
3、根据权利要求1所述的一种由水冷结晶器冷却的锭模装置,其特征在于:所述升降装置具有导向柱、丝母和丝杠构成。
4、根据权利要求1至3任一权利要求所述的一种由水冷结晶器冷却的锭模装置,其特征在于:所述铸模的顶部设置有保温帽。
CN2009200901623U 2009-05-11 2009-05-11 一种由水冷结晶器冷却的锭模装置 Expired - Lifetime CN201423430Y (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2009200901623U CN201423430Y (zh) 2009-05-11 2009-05-11 一种由水冷结晶器冷却的锭模装置

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2009200901623U CN201423430Y (zh) 2009-05-11 2009-05-11 一种由水冷结晶器冷却的锭模装置

Publications (1)

Publication Number Publication Date
CN201423430Y true CN201423430Y (zh) 2010-03-17

Family

ID=42022866

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2009200901623U Expired - Lifetime CN201423430Y (zh) 2009-05-11 2009-05-11 一种由水冷结晶器冷却的锭模装置

Country Status (1)

Country Link
CN (1) CN201423430Y (zh)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101982256A (zh) * 2010-09-30 2011-03-02 西峡龙成特种材料有限公司 洁净金属锭模
CN102019379A (zh) * 2010-10-26 2011-04-20 西峡龙成特种材料有限公司 环境伺服式洁净金属铸模
CN103212674A (zh) * 2013-03-16 2013-07-24 南阳汉冶特钢有限公司 一种钢板铸锭装置及用该装置生产特厚钢板铸锭的方法
CN103611893A (zh) * 2013-11-26 2014-03-05 辽宁科技大学 一种填充钢锭模气隙的方法及其装置
CN106001521A (zh) * 2016-06-01 2016-10-12 安庆石化联盟铸管厂 一种金属管节能式水冷设备

Cited By (11)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101982256A (zh) * 2010-09-30 2011-03-02 西峡龙成特种材料有限公司 洁净金属锭模
WO2012040963A1 (zh) * 2010-09-30 2012-04-05 西峡龙成特种材料有限公司 洁净金属锭模
CN101982256B (zh) * 2010-09-30 2013-06-12 西峡龙成特种材料有限公司 洁净金属锭模
US9016350B2 (en) 2010-09-30 2015-04-28 Nanyang Xingzhi Patent Technology Service Co., Ltd. Clean metal ingot mold
CN102019379A (zh) * 2010-10-26 2011-04-20 西峡龙成特种材料有限公司 环境伺服式洁净金属铸模
CN102019379B (zh) * 2010-10-26 2012-08-08 西峡龙成特种材料有限公司 环境伺服式洁净金属铸模
CN103212674A (zh) * 2013-03-16 2013-07-24 南阳汉冶特钢有限公司 一种钢板铸锭装置及用该装置生产特厚钢板铸锭的方法
CN103212674B (zh) * 2013-03-16 2015-09-09 南阳汉冶特钢有限公司 一种钢板铸锭装置及用该装置生产特厚钢板铸锭的方法
CN103611893A (zh) * 2013-11-26 2014-03-05 辽宁科技大学 一种填充钢锭模气隙的方法及其装置
CN103611893B (zh) * 2013-11-26 2015-08-19 辽宁科技大学 一种填充钢锭模气隙的方法及其装置
CN106001521A (zh) * 2016-06-01 2016-10-12 安庆石化联盟铸管厂 一种金属管节能式水冷设备

Similar Documents

Publication Publication Date Title
CN103212674B (zh) 一种钢板铸锭装置及用该装置生产特厚钢板铸锭的方法
CN201423430Y (zh) 一种由水冷结晶器冷却的锭模装置
CN101543877B (zh) 用水冷结晶器作为锭模的装置
CN108723324B (zh) 一种多工位自动压电机铸铝转子装置
CN208303840U (zh) 一种高压轮毂铸造模具
CN109732023B (zh) 一种控制铝合金壳体等温精锻过程尺寸回弹的方法
CN202398784U (zh) 一种铸造砂型
CN211191981U (zh) 一种合金精密铸造模具
CN202779688U (zh) 一种金属半固态浆料制备的装置
CN208357776U (zh) 一种电机转子铝低压浇注模
CN107685142A (zh) 一种热平衡法半固态加工自动生产线
CN209223158U (zh) 一种阳极铜板生产加工***
CN201997669U (zh) 耐磨铸球水冷金属型模
CN208357774U (zh) 一种自动化低压铸造轮毂生产装置
CN207508245U (zh) 一种热平衡法半固态加工自动生产线
CN110899659A (zh) 一种模具生产用压铸装置
CN215468025U (zh) 一种汽车电机壳低压铸造模具
CN201862748U (zh) 一种立式分段半连铸装置
KR101030168B1 (ko) 저압 주조기
CN202683971U (zh) 高强度铝合金轮毂模具
CN211679901U (zh) 连铸圆钢锭模的高效保温冒口
CN204747433U (zh) 圆钢锭模
CN205020772U (zh) 外开槽圆钢锭模
CN209174852U (zh) 一种金属铸锭模具
CN206009789U (zh) 一种车轮铸造模具边模

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
CX01 Expiry of patent term

Granted publication date: 20100317

CX01 Expiry of patent term