CN201064917Y - 表面粘接有耐磨纸的染色木板 - Google Patents
表面粘接有耐磨纸的染色木板 Download PDFInfo
- Publication number
- CN201064917Y CN201064917Y CNU2007200790960U CN200720079096U CN201064917Y CN 201064917 Y CN201064917 Y CN 201064917Y CN U2007200790960 U CNU2007200790960 U CN U2007200790960U CN 200720079096 U CN200720079096 U CN 200720079096U CN 201064917 Y CN201064917 Y CN 201064917Y
- Authority
- CN
- China
- Prior art keywords
- abrasion
- board
- dyeing
- proof paper
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型表面粘接有耐磨纸的染色木板属于板材装饰技术领域,特别是表面耐磨的木材装饰板材。为使板材表面性能耐磨耐划伤,且表面装饰效果为木材天然装饰,本板由三层组成,即在耐磨纸和基层之间粘有染色薄木皮层。而且可在背面粘一防止张力和热涨冷缩应力不平衡的平衡层。本实用新型的优点:可按家具用、地板用或其他装饰板材用对板材表面性能要求的不同,制成表面不同性能的板材。由于中层粘有染色薄木皮层3,使得表面美术效果自然。表层贴有耐磨纸1,使得板材表面具有很好的耐磨、耐划伤性能。在木材装饰方面节约了木材,减少了油漆的使用,降低了生产成本。
Description
技术领域
本实用新型属于板材表面装饰技术领域,特别是表面耐磨的木质板材。
背景技术
当前用于地板、家具以及用于室内装饰的板材中,主要有两种,一种是浸渍纸层压木质板材,一种是在人造板板材表面贴装饰木材,然后再在装饰木材表面涂饰油漆的板材。这两种装饰板材各有优点和缺点。浸渍纸层压木质板材具有很高的耐磨、耐划伤性能,但其装饰层为纸质印刷图案;用珍贵木材作为装饰层并做油漆涂饰的板材,其装饰效果自然美观,但耐磨、耐划痕性能较浸渍纸层压木质板表面差很多,而且生产成本高。
发明内容
本实用新型的目的是提供一种性能适合地板、家具以及装饰用要求,表面美术效果体现木材自然美观的人造板材。
本实用新型表面粘接有耐磨纸的染色木板,包括耐磨纸1和基层2,其特征在于:耐磨纸1和基层2之间粘有染色薄木皮层3。根据需要染色薄木皮层3厚度为0.15-6.00mm。所以粘接有耐磨纸的染色木板的使用面为三层,从里向外依次是基层2、染色薄木皮层3、耐磨纸1。
由于基层2的一面贴有染色薄木皮层3和耐磨纸1这两层,而另一面没粘任何材料层,常常产生基层2两面张力和热涨冷缩应力不平衡。因而本实用新型在没有粘染色薄木皮层3和耐磨纸1的那一面即背面粘平衡层4。粘平衡层4的目的一是平衡基层2两面的张力和热涨冷缩应力,使表面粘接有耐磨纸的染色木板不发生大的弯曲变形;二是对基层2的另一面起装饰作用。
耐磨纸1是浸渍纸。浸渍纸的浸渍液是:三聚氰胺甲醛树脂、尿醛树脂、酚醛树脂等树脂中的某一种。
基层2是创花板、纤维板、胶合板等人造板中的某一种。
平衡层4是浸渍纸或木材层。为达到基层2两面张力和热涨冷缩应力的平衡,还可用其它材料作为平衡层4粘在基层2背面。
本实用新型的优点:可按家具用、地板用或其他装饰板材用对板材表面性能要求的不同,制成表面不同性能的板材。由于中层粘有染色薄木皮层3,使得表面美术效果自然。表层贴有耐磨纸1,使得板材表面具有很好的耐磨、耐划伤性能。在木材装饰方面节约了木材,减少了油漆的使用,降低了生产成本。
附图说明
图1是一面粘贴耐磨纸的染色木板各层结构示意图;
图2是一面粘贴耐磨纸另一面粘有平衡层的染色木板各层结构示意图;
图中1是耐磨纸、2是基层、3是薄木皮层、4是平衡层。
具体实施例
实施例1、三层结构的表面粘接有耐磨纸的染色木板
用15mm厚的纤维板作为基层2,在基层2的一面涂上三聚氰胺甲醛树脂,用已染色薄木皮层3粘在涂有三聚氰胺甲醛树脂的基层2上。再在已染色薄木皮层3表面用三聚氰胺甲醛树脂的浸渍纸作为耐磨纸1粘贴在已染色薄木皮层3表面,经热压机压贴加工,三层结构的表面粘接有耐磨纸的染色木板制成。
实施例2、四层结构的表面粘接有耐磨纸的染色木板
在实施例1用耐磨纸1粘在已染色薄木皮层3表面后,又在基层2没粘已染色薄木皮层3的表面,即背面再粘一层尿醛树脂浸渍纸作为平衡层4。
实施例3、另一种四层结构的表面粘接有耐磨纸的染色木板
所粘层数和层间秩序同于实施例2,不同于实施例2的是用的粘接剂和平衡层。本实施例在基层2的一面涂上酚醛树脂,耐磨纸1都用三聚氰胺甲醛树脂浸渍。三聚氰胺甲醛树脂耐磨纸1粘在已染色薄木皮层3上,基层2背面用三聚氰胺甲醛树脂粘上薄木皮层作为平衡层4。
Claims (6)
1.表面粘接有耐磨纸的染色木板,包括耐磨纸(1)和基层(2),其特征在于:耐磨纸(1)和基层(2)之间粘有染色薄木皮层(3)。
2.根据权利要求1所述的表面粘接有耐磨纸的染色木板,其特征在于:基层(2)面依秩向外粘有染色薄木皮层(3)、耐磨纸(1);基层(2)另一面粘有平衡层(4)。
3.根据权利要求1或2所述的表面粘接有耐磨纸的染色木板,其特征在于:耐磨纸(1)是浸渍纸。
4.根据权利要求1或2所述的表面粘接有耐磨纸的染色木板,其特征在于:基层(2)是创花板、纤维板、胶合板等人造板中的某一种。
5.根据权利要求1或2所述的表面粘接有耐磨纸的染色木板,其特征在于:染色薄木皮层(3)是厚度为0.15-6.00mm厚的实木皮。
6.根据权利要求2所述的表面粘接有耐磨纸的染色木板,其特征在于:平衡层(4)是浸渍纸或木材层等其他可用的平衡材料。