CN104626540B - 一种用于分油管焊接机的红外加热装置 - Google Patents

一种用于分油管焊接机的红外加热装置 Download PDF

Info

Publication number
CN104626540B
CN104626540B CN201510021277.7A CN201510021277A CN104626540B CN 104626540 B CN104626540 B CN 104626540B CN 201510021277 A CN201510021277 A CN 201510021277A CN 104626540 B CN104626540 B CN 104626540B
Authority
CN
China
Prior art keywords
infrared
heater
heating
heating device
welding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201510021277.7A
Other languages
English (en)
Other versions
CN104626540A (zh
Inventor
苏伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Suzhou Kaierbo Technology Co ltd
Original Assignee
Suzhou Keber Precision Machinery Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Keber Precision Machinery Co Ltd filed Critical Suzhou Keber Precision Machinery Co Ltd
Priority to CN201510021277.7A priority Critical patent/CN104626540B/zh
Publication of CN104626540A publication Critical patent/CN104626540A/zh
Application granted granted Critical
Publication of CN104626540B publication Critical patent/CN104626540B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种用于分油管焊接机的红外加热装置,包括加热装置移动驱动器、加热装置导轨,红外加热器和红外温度检测仪;所述红外加热器有左右2个,一个对应端盖固定装置,一个对应管体固定装置,所述红外温度检测仪有左右2个,一个对应端盖固定装置,一个对应管体固定装置;所述红外加热器设置在加热装置导轨上,红外加热器的前端设置有红外温度检测仪。本发明使用红外加热期间进行加热焊接,焊接部位与加热板不粘连,加热均匀,所用时间较短,焊缝翻遍小,焊接强度高,可以检测焊接温度,提高焊接质量。

Description

一种用于分油管焊接机的红外加热装置
技术领域
本发明涉及一种用于分油管焊接机的,加热效率高还可以检测温度的红外加热装置。
背景技术
分油管是由端盖和管体组成,需要将端盖和管体利用焊接技术将其焊接在一起,常用的加工方式是自熔焊接,但是目前的自熔焊接技术需要针对焊接面的形状制作相应的模具,模具通过加热板加热后与零件接触使其表面熔化,再将零件对接施压使其焊接,这种加工方式的针对性差,对于加工不同的零件需要加工不同的模具,消耗成本大,且加热时通过加热模具后再加热焊接面,这种间接的加热方式加热时间较长,且损耗的热量大,致使生产效率低,能源消耗大。
发明内容
针对上述存在的技术问题,本发明的目的是:提出了一种用于分油管焊接机的,加热效率高还可以检测温度的红外加热装置。
为达到上述目的,本发明采用的技术方案是:一种用于分油管焊接机的红外加热装置,包括加热装置移动驱动器、加热装置导轨,红外加热器和红外温度检测仪;所述红外加热器有左右2个,一个对应端盖固定装置,一个对应管体固定装置,所述红外温度检测仪有左右2个,一个对应端盖固定装置,一个对应管体固定装置;所述红外加热器设置在加热装置导轨上,红外加热器的前端设置有红外温度检测仪。
优选的,红外加热器均包括红外加热体、聚光板和遮光罩,所述聚光板上设置有排气孔,红外加热体设置在聚光板和遮光罩之间,所述遮光罩上设置有通光孔,所述聚光板为圆弧形抛光面,所述通光孔内壁也为抛光面。
优选的,所述红外温度检测仪包括上下左右4个温度检测器。
由于上述技术方案的运用,本发明与现有技术相比具有下列优点:
本发明方案的一种用于分油管焊接机的红外加热装置,使用红外加热期间进行加热焊接,焊接部位与加热板不粘连,加热均匀,所用时间较短,焊缝翻遍小,焊接强度高,可以检测焊接温度,提高焊接质量。
附图说明
下面结合附图对本发明技术方案作进一步说明:
附图1为本发明的一种用于分油管焊接机的红外加热装置的示意图;
附图2为本发明的一种用于分油管焊接机的红外加热装置的红外加热器和红外温度检测仪的俯视示意图;
附图3为附图1中A-A面的剖视图;
其中:31加热装置移动驱动器、32加热装置导轨、33红外加热器、34红外温度检测仪、331红外加热体、332聚光板、333遮光罩、334排气孔、335通光孔、341温度检测器。
具体实施方式
下面结合附图及具体实施例对本发明作进一步的详细说明。
附图1-3为本发明所述的一种用于分油管焊接机的红外加热装置,包括加热装置移动驱动器31、加热装置导轨32,红外加热器33和红外温度检测仪34;所述红外加热器33有2个,一个与端盖固定装置1对应,一个与管体固定装置2对应,所述红外温度检测仪34有2个,一个与端盖固定装置1对应,一个与管体固定装置2对应;所述红加热器33包括红外加热体331、聚光板332和遮光罩333,所述聚光板332上设置有排气孔334,红外加热体331设置在聚光板332和遮光罩333之间,所述遮光罩333上设置有通光孔335,所述聚光板332为圆弧形抛光面,所述通光孔335内壁也为抛光面;所述红外温度检测仪34包括上下左右4个温度检测器341,所述红外温度检测仪34可以检测被加热零件上下左右四个角的温度;所述加热装置移动驱动器31设置在加热装置导轨32的后端,所述红外加热器33设置在加热装置导轨32上,所述红外加热器33的前端设置有红外温度检测仪34;
当所述端盖固定装置1和管体固定装置2预对接后各自退回,这时所述红外加热装置33由加热装置移动驱动器31驱动在加热装置导轨32上向前移动,使通光孔335对准焊接零件表面,红外加热体331的红外光被聚光板332聚光反射后,由通光孔335处照射在焊接零件表面使其熔化,同时所述排气孔334向红外加热器33内通气,气体再从通光孔335排出,这样可以防止加热零件的过程中产生的污浊气从通光孔335进入红外加热器33影响红外加热体331的发光度,也可以使加热零件受热更均匀,加热完毕红外加热器33后退使红外温度检测仪34对准焊接零件熔化表面进行温度检测,当检测温度达到预定温度后,红外加热器33由加热装置驱动器31驱动退回到初始位置,完成加热动作,这时端盖固定装置1和管体固定装置2对接进行焊接动作;当检测温度没有达到预定温度,红外加热器33由加热装置驱动器31驱动回到加热的位置继续加热,然后再由红外温度检测仪34进行温度检测,直到检测温度达到预定温度后红外加热器33退回,再进行焊接动作。
以上仅是本发明的具体应用范例,对本发明的保护范围不构成任何限制。凡采用等同变换或者等效替换而形成的技术方案,均落在本发明权利保护范围之内。

Claims (2)

1.一种用于分油管焊接机的红外加热装置,包括加热装置移动驱动器(31)、加热装置导轨(32),红外加热器(33)和红外温度检测仪(34);所述红外加热器(33)有左右2个,一个对应端盖固定装置(1),一个对应管体固定装置(2),所述红外温度检测仪(34)有左右2个,一个对应端盖固定装置(1),一个对应管体固定装置(2);所述红外加热器(33)设置在加热装置导轨(32)上,红外加热器(33)的前端设置有红外温度检测仪(34);红外加热器(33)均包括红外加热体(331)、聚光板(332)和遮光罩(333),所述聚光板(332)上设置有排气孔(334),红外加热体(331)设置在聚光板(332)和遮光罩(333)之间,所述遮光罩(333)上设置有通光孔(335),所述聚光板(332)为圆弧形抛光面,所述通光孔(335)内壁也为抛光面。
2.根据权利要求1所述的用于分油管焊接机的红外加热装置,其特征在于:所述红外温度检测仪(34)包括上下左右4个温度检测器(341)。
CN201510021277.7A 2015-01-16 2015-01-16 一种用于分油管焊接机的红外加热装置 Active CN104626540B (zh)