JPS57169096A - Protecting method of electrolytic cell - Google Patents
Protecting method of electrolytic cellInfo
- Publication number
- JPS57169096A JPS57169096A JP4291782A JP4291782A JPS57169096A JP S57169096 A JPS57169096 A JP S57169096A JP 4291782 A JP4291782 A JP 4291782A JP 4291782 A JP4291782 A JP 4291782A JP S57169096 A JPS57169096 A JP S57169096A
- Authority
- JP
- Japan
- Prior art keywords
- electrolysis
- small current
- electrolytic cell
- solution
- ion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To prevent contamination of an ion-exchange resin membrance, by supplying a very small current being less than decomposition voltage of an alkali metallic salt solution through the electrolysis stop period, into an electrolytic cell in case of electrolysis of said solution by an ion-exchange resin membrane process. CONSTITUTION:In case when an alkali metallic solution is electrolyzed by putting an electrolyte into an anode chamber and a cathode chamber of said electrolytic cell, a very small current is supplied as soon as the electrolysis is stopped, and also during the stop period. This very small current is set within the range of 10mA/m<2>- less than decomposition voltage of said alkali solution. Also, as for this current value, such a small current as 10-1,000mA/m<2> generally, preferably 5-500mA/m<2> is enough. As a result, contamination of an ion- exchange resin membrane is prevented, its resistance is maintained for a long period of time, and also even when the electrolysis is restarted, voltage and current efficiency before its stop can be maintained.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4291782A JPS5846554B2 (en) | 1982-03-19 | 1982-03-19 | How to protect an electrolytic cell |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP4291782A JPS5846554B2 (en) | 1982-03-19 | 1982-03-19 | How to protect an electrolytic cell |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6607076A Division JPS52149295A (en) | 1976-06-08 | 1976-06-08 | Protecting method for electrolytic bath |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57169096A true JPS57169096A (en) | 1982-10-18 |
JPS5846554B2 JPS5846554B2 (en) | 1983-10-17 |
Family
ID=12649365
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP4291782A Expired JPS5846554B2 (en) | 1982-03-19 | 1982-03-19 | How to protect an electrolytic cell |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5846554B2 (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4561949A (en) * | 1983-08-29 | 1985-12-31 | Olin Corporation | Apparatus and method for preventing activity loss from electrodes during shutdown |
JP2001026893A (en) * | 1999-07-14 | 2001-01-30 | Toagosei Co Ltd | Method for protecting alkali chloride electrolytic cell and protective device therefor |
-
1982
- 1982-03-19 JP JP4291782A patent/JPS5846554B2/en not_active Expired
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4561949A (en) * | 1983-08-29 | 1985-12-31 | Olin Corporation | Apparatus and method for preventing activity loss from electrodes during shutdown |
JP2001026893A (en) * | 1999-07-14 | 2001-01-30 | Toagosei Co Ltd | Method for protecting alkali chloride electrolytic cell and protective device therefor |
Also Published As
Publication number | Publication date |
---|---|
JPS5846554B2 (en) | 1983-10-17 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
FR2524814B1 (en) | PROCESS FOR THE PRODUCTION OF ION EXCHANGE MEMBRANES PROVIDED WITH A COATING FOR ELECTROLYSIS | |
MY129999A (en) | Method of copper plating. | |
JPS5579884A (en) | Preparation of glyoxylic acid | |
JPS57155390A (en) | Manufacture of organic ammonium hydroxide using ion exchange membrane | |
EP0235444A3 (en) | Metal halogen electrochemical cell | |
ES8201132A1 (en) | Process for the preparation of methionine. | |
JPS57169096A (en) | Protecting method of electrolytic cell | |
JPS56112500A (en) | Method for electroplating | |
GB1121468A (en) | Improvements relating to electrolytic production of electro-chemically active cadmium | |
JPS5475497A (en) | Electrolyzing method for aqueous solution of sodium chloride | |
JPS558413A (en) | Protecting method of stop electrolytic cell | |
JPS552765A (en) | Production of hydrogen sulfide by electrolysis | |
JPS5641392A (en) | Electrolytic method of alkali chloride aqueous solution | |
JPS61261488A (en) | Electrolyzing method for alkaline metallic salt of amino acid | |
JPS56139193A (en) | Treatment of waste copper plating solution | |
JPS5524924A (en) | Adjustment of metal ion concentration in nickel plating liquor | |
JPS5312798A (en) | Electrolyzing eqiupment for aqueous solution of alkali metal salt | |
JPS5691805A (en) | Electrochemical device with oxygen electrode | |
JPS57149498A (en) | Method of supplying zinc ion to zinc plating alkaline bath | |
JPS55129157A (en) | Electrolytic regeneration method of ion exchange resin | |
JPS52149295A (en) | Protecting method for electrolytic bath | |
EP0219968A3 (en) | Electrolytic process for producing extremely low chloride anion exchange resins | |
JPS5633488A (en) | Method for electrolysis of aqueous solution of alkali chloride | |
JPS57174477A (en) | Electrolyzing method for aqueous solution of alkali metal salt | |
JPS5735688A (en) | Method for electrolysis of potassium chloride brine |