JPS57137077A - Submerged arc welding by one side penetration of butt joint - Google Patents
Submerged arc welding by one side penetration of butt jointInfo
- Publication number
- JPS57137077A JPS57137077A JP2144181A JP2144181A JPS57137077A JP S57137077 A JPS57137077 A JP S57137077A JP 2144181 A JP2144181 A JP 2144181A JP 2144181 A JP2144181 A JP 2144181A JP S57137077 A JPS57137077 A JP S57137077A
- Authority
- JP
- Japan
- Prior art keywords
- groove
- tack
- welding
- recess
- joint part
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To prevent the cracking of tack welding beads completely and eliminate the weld defects of a joint part by performing tack welding by utilizing the recess formed in a groove by gouging. CONSTITUTION:A root face 4 of a sufficient size is beforehand formed in the welded joint part of a single Vee groove of plate-like base materials 1. Next, the part to be tack welded in a groove 2 of the butt welded joint part is chipped off discontinuously by gouging, whereby a recess 3 is formed. After tack welding 5 for burying only the recess 3 is executed, the upper part of the tack weld beads is finished with a grinder to the same shape as that of the other groove face, thence continuous welding by perfect penetration is accomplished as regular welding to the single Vee groove.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2144181A JPS5947629B2 (en) | 1981-02-18 | 1981-02-18 | One side back wave submerged arc welding method of butt joint |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2144181A JPS5947629B2 (en) | 1981-02-18 | 1981-02-18 | One side back wave submerged arc welding method of butt joint |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS57137077A true JPS57137077A (en) | 1982-08-24 |
JPS5947629B2 JPS5947629B2 (en) | 1984-11-20 |
Family
ID=12055046
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2144181A Expired JPS5947629B2 (en) | 1981-02-18 | 1981-02-18 | One side back wave submerged arc welding method of butt joint |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5947629B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103737162A (en) * | 2013-12-20 | 2014-04-23 | 南车长江车辆有限公司 | Compound welding method |
-
1981
- 1981-02-18 JP JP2144181A patent/JPS5947629B2/en not_active Expired
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103737162A (en) * | 2013-12-20 | 2014-04-23 | 南车长江车辆有限公司 | Compound welding method |
Also Published As
Publication number | Publication date |
---|---|
JPS5947629B2 (en) | 1984-11-20 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS57137077A (en) | Submerged arc welding by one side penetration of butt joint | |
JPS5775283A (en) | Method and device for welding of metallic plate material | |
JPS53113734A (en) | One-side arc welding method for 9% ni steel | |
JPS5725288A (en) | Method for welding thick copper plate | |
GB1445429A (en) | Welding method employing inclined parallel sided groove | |
JPS56102433A (en) | Wire cut discharge machining method | |
JPS5545506A (en) | One side welding method | |
JPS5770085A (en) | Plasma arc welding method | |
Orlov et al. | Effects of the Ductility of Weld Metal and the Weld Gap on Strength of Welds in Biaxial Loading | |
JPS55139194A (en) | Automatic one side welding method of pipeline girth joint | |
JPS56163087A (en) | Laser welding method | |
JPS61206565A (en) | Simultaneous both sides welding method | |
JPS551953A (en) | Arc welding method | |
JPS54101737A (en) | Welding method by high output high density electron beam | |
Klein | Know How--Some Rules on Electro-Gas Welding | |
JPS56126092A (en) | Butt welding method | |
JPS5630089A (en) | Welding emthod for slender tube and tube plate of heat exchanger and the like | |
Aravin et al. | Residual Weld Stresses in Aluminum Bronzes | |
JPS57100891A (en) | Method for edge preparation in gradually changing welding part | |
JPS5736080A (en) | Electron beam welding method | |
JPS5768289A (en) | Arc welding method | |
JPS5570472A (en) | Welding method of fillet joint part of tank | |
Nikov | Steel Welding on Reinforced-Glass Backing With One-Side Weld Formation | |
JPS56163092A (en) | Welding method for stainless clad steel plate | |
JPS54102437A (en) | Manufacturing method of speed ring for hydraulic machinery |