JP4389659B2 - メタクリル樹脂製導光体の製造法 - Google Patents
メタクリル樹脂製導光体の製造法 Download PDFInfo
- Publication number
- JP4389659B2 JP4389659B2 JP2004143344A JP2004143344A JP4389659B2 JP 4389659 B2 JP4389659 B2 JP 4389659B2 JP 2004143344 A JP2004143344 A JP 2004143344A JP 2004143344 A JP2004143344 A JP 2004143344A JP 4389659 B2 JP4389659 B2 JP 4389659B2
- Authority
- JP
- Japan
- Prior art keywords
- methacrylic resin
- group
- light guide
- molding
- disulfide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
R1−S−S−R2 (1)
〔式中、R1およびR2はそれぞれ独立に、炭素数1〜12のアルキル基または炭素数1〜12のアルコキシル基で置換されていてもよい炭素数3〜12のシクロアルキル基を示す。〕
で示されるジスルフィド類を配合することにより、メタクリル樹脂の熱分解が防止できるばかりでなく、より着色の少ない導光体が得られることを見出し、本発明に至った。
アクリル酸メチル、アクリル酸エチル、アクリル酸プロピル、アクリル酸ブチル、アクリル酸ベンジル、アクリル酸2−エチルヘキシル、アクリル酸シクロヘキシル、アクリル酸ボルニル、アクリル酸アダマンチル、アクリル酸シクロペンタジエニルなどのアクリル酸エステル類、
アクリル酸、メタクリル酸、マレイン酸、イタコン酸、無水マレイン酸、無水イタコン酸などの不飽和カルボン酸およびその酸無水物、アクリル酸2−ヒドロキシエチル、アクリル酸2−ヒドロキシプロピル、アクリル酸2−ヒドロキシプロピル、アクリル酸モノグリセロール、メタクリル酸2−ヒドロキシエチル、メタクリル酸2−ヒドロキシプロピル、メタクリル酸モノグリセロールなどのヒドロキシル基含有単量体、アクリルアミド、メタクリルアミド、アクリロニトリル、メタクリロニトリル、ジアセトンアクリルアミド、メタクリル酸ジメチルアミノエチルなどの窒素含有単量体、アリルグリシジルエーテル、アクリル酸グリシジル、メタクリル酸グリシジルなどのエポキシ基含有単量体、スチレン、α−メチルスチレンなどのスチレン系単量体などが挙げられる。
(1)熱安定性
TG−DTA装置〔「TG/DTA6300」、セイコーインスツルメンツ社製〕を用いて昇温速度2℃/分で50℃から430℃までペレットを昇温しながら重量損失を測定し、ペレットの重量が2%減少したときの温度を読み取った。この温度が高いほど熱安定性に優れ、熱分解しにくいことを示す。
(2)単量体含有量
各実施例で得たペレットおよび成形体からそれぞれ0.1gの試験片を採取し、20cm3のジクロロメタンに溶解して溶液とし、ガスクロマトグラフ装置〔「GC−14B型」、島津製作所製〕を用いて単量体含有量(質量%)を測定した。
(3)成形着色性
各実施例で得た試験片の端面を研磨機〔「プラビューティー PB−100」、旭メガロ社製〕で研磨してから、分光光度計〔「U−4000」、日立製作所製〕にて波長380〜780nmの範囲で150mmパス透過率を測定し、得られた透過率からJIS Z−8722記載の方法に従ってXYZ値を求め、JIS K−7105記載の方法に従って黄色度を求めた。2個の試験片について求めた黄色度の平均値(YIavr)を成形着色性とした。黄色度の平均値(YIavr)が小さいほど、成形時の着色が少ないことを示す。
メタクリル酸メチル98.8質量部およびアクリル酸メチル0.8質量部を混合し、ジシクロヘキシルジスルフィド0.1質量部、連鎖移動剤〔オクチルメルカプタン〕0.17質量部および離型剤〔ステアリルアルコール〕0.1質量部を加えて単量体混合液を得た。また、メタクリル酸メチル100質量部に重合開始剤〔1,1−ジ(t−ブチルパーオキシ)3,3,5−トリメチルシクロヘキサン〕0.036質量部を加えて開始剤混合液を得た。単量体混合液と開始剤混合液とを流量比が8.8:1になるように完全混合型重合反応器へ連続して供給し、平均滞留時間20分、温度175℃で平均重合率54%まで重合して部分重合物を得た。得られた部分重合物を200℃に加熱してベント付き脱揮押出機へ導き、240℃で未反応の単量体をベントから脱揮すると共に、脱揮後の重合体は溶融状態で押出し、水冷後、裁断してペレットとした。このペレットの熱安定性および単量体含有量を第1表に示す。
単量体混合液におけるメタクリル酸メチルの使用量を98.7質量部とし、ジシクロヘキシルジスルフィドの使用量を0.18質量部とした以外は実施例1と同様に操作してペレットを得た。このペレットの熱安定性および単量体含有量を第1表に示す。
ジシクロヘキシルジスルフィドに代えて、ジ−tert−ドデシルジスルフィド0.01質量部を用いた以外は実施例1と同様に操作して、ペレットを得た。このペレットの熱安定性および単量体含有量を第1表に示す。
ジシクロヘキシルジスルフィドを用いなかった以外は実施例1と同様に操作して、ペレットを得た。このペレットの熱安定性および単量体含有量を第1表に示す。
━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━
ペレット 成形体
熱安定性 単量体含有量 単量体含有量 成形着色性
(℃) (質量%) (質量%) (YIavr)
280℃ 290℃ 280℃ 290℃
━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━
実施例1 298 0.18 0.51 0.82 7.2 −
実施例2 302 0.17 − 0.73 − 8.5
比較例1 297 0.18 0.46 0.73 14.8 17.1
比較例2 269 0.23 1.54 − 5.6 −
━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━━
2:バックライト 3:光源
4:フラットパネルディスプレイ
Claims (4)
- メタクリル樹脂にジシクロヘキシルジスルフィドが配合され、該ジシクロヘキシルジスルフィドの配合量がメタクリル樹脂に対して10ppm〜5000ppmであるメタクリル樹脂組成物を加熱溶融で成形することを特徴とするメタクリル樹脂製導光体の製造方法。
- 射出成形法または押出成形法により成形する請求項1に記載の製造方法。
- 230℃以上で成形する請求項1に記載の製造方法。
- メタクリル樹脂にジシクロヘキシルジスルフィドが配合され、該ジシクロヘキシルジスルフィドの配合量がメタクリル樹脂に対して10ppm〜5000ppmであるメタクリル樹脂組成物であって、請求項1〜3のいずれかに記載のメタクリル樹脂製導光体の製造方法に使用されるメタクリル樹脂組成物。