DE2354640A1 - Verfahren zur korrosionsinhibierung unter anwendung von glycinverbindungen - Google Patents
Verfahren zur korrosionsinhibierung unter anwendung von glycinverbindungenInfo
- Publication number
- DE2354640A1 DE2354640A1 DE19732354640 DE2354640A DE2354640A1 DE 2354640 A1 DE2354640 A1 DE 2354640A1 DE 19732354640 DE19732354640 DE 19732354640 DE 2354640 A DE2354640 A DE 2354640A DE 2354640 A1 DE2354640 A1 DE 2354640A1
- Authority
- DE
- Germany
- Prior art keywords
- aqueous medium
- parts
- glycine
- corrosion
- alkyl
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/10—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using organic inhibitors
- C23F11/16—Sulfur-containing compounds
- C23F11/164—Sulfur-containing compounds containing a -SO2-N group
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US37539573A | 1973-07-02 | 1973-07-02 |
Publications (1)
Publication Number | Publication Date |
---|---|
DE2354640A1 true DE2354640A1 (de) | 1975-01-30 |
Family
ID=23480724
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DE19732354640 Pending DE2354640A1 (de) | 1973-07-02 | 1973-10-31 | Verfahren zur korrosionsinhibierung unter anwendung von glycinverbindungen |
Country Status (5)
Country | Link |
---|---|
BE (1) | BE806270A (nl) |
DE (1) | DE2354640A1 (nl) |
FR (1) | FR2236018A1 (nl) |
IT (1) | IT996257B (nl) |
NL (1) | NL7313387A (nl) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0048429A1 (de) * | 1980-09-19 | 1982-03-31 | Hoechst Aktiengesellschaft | Korrosionsinhibierende und kavitationsinhibierende Kühlflüssigkeit |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2479844A1 (fr) * | 1980-04-04 | 1981-10-09 | Martin Philippe | Agent anticorrosion des metaux ferreux et non ferreux, utilisable notamment pour la protection des vehicules automobiles |
FR2481308A1 (fr) * | 1980-04-29 | 1981-10-30 | Labo Ind | Composition inhibitrice de la corrosion |
DE19757302A1 (de) | 1997-12-22 | 1999-07-01 | Siemens Ag | Beschichtung von Metalloberflächen insbesondere für die Mikroelektronik |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2602760A (en) * | 1950-07-18 | 1952-07-08 | Josef M Michel | Process of protecting metals against corrosion |
DE1259175B (de) * | 1961-12-22 | 1968-01-18 | Hoechst Ag | Verfahren zum Korrosionsschutz fuer Wasserbehaelter und wasserfuehrende Bauteile von technischen Apparaturen |
-
1973
- 1973-09-28 NL NL7313387A patent/NL7313387A/nl unknown
- 1973-10-03 IT IT5290573A patent/IT996257B/it active
- 1973-10-19 BE BE136857A patent/BE806270A/xx unknown
- 1973-10-24 FR FR7337832A patent/FR2236018A1/fr active Granted
- 1973-10-31 DE DE19732354640 patent/DE2354640A1/de active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0048429A1 (de) * | 1980-09-19 | 1982-03-31 | Hoechst Aktiengesellschaft | Korrosionsinhibierende und kavitationsinhibierende Kühlflüssigkeit |
Also Published As
Publication number | Publication date |
---|---|
IT996257B (it) | 1975-12-10 |
NL7313387A (nl) | 1975-01-06 |
FR2236018A1 (en) | 1975-01-31 |
BE806270A (fr) | 1974-02-15 |
FR2236018B1 (nl) | 1976-06-18 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE2505435C3 (de) | Verwendung von Carboxy-alkan-Verbindungen des Phosphors als Korrosionsinhibitoren | |
DE1517399A1 (de) | Verfahren zur Verhuetung der Kesselsteinbildung | |
DE69636451T2 (de) | Verfahren zur korrosionsinhibierung unter verwendung von n-halo-azolen | |
DE2055779B2 (de) | Korrosionsschutzmittel für Metalloberflächen und Verfahren zum Schutz von Metalloberflachen unter Verwendung desselben | |
DE2242473A1 (de) | Behandlungsverfahren einer verbrauchten, stromlosen bearbeitungs- oder abbeizloesung | |
DE2934461A1 (de) | Korrosionsinhibitoren fuer buntmetalle | |
DE2354640A1 (de) | Verfahren zur korrosionsinhibierung unter anwendung von glycinverbindungen | |
DE2233312A1 (de) | Polyalkylenpolyamin-korrosionsinhibitoren | |
DE3509250A1 (de) | Verfahren zum behandeln von eisenmetallwerkstuecken | |
DE2016686A1 (de) | Korrosionsschutzmittel | |
DE2240736C3 (de) | Mittel zur Inhibierung der Metallkorrosion und Verfahren zu seiner Herstellung | |
DE2344498A1 (de) | Verfahren zur verhuetung der korrosion in kuehlwasserkreislaeufen | |
EP0218798A2 (de) | Verfahren und Zusammensetzung zur Verhinderung von Korrosionen und Steinbildungen in Brauchwassersystemen | |
DE1546213A1 (de) | Verfahren zur Reinigung metallischer Vorrichtungen | |
DE10021915C2 (de) | Inhibierung von Loch- und Spaltkorrosion | |
DE69307846T2 (de) | Mikrobiologisch stabiler Buntmetall-Korrosionsinhibitor | |
EP0482614B1 (de) | Verfahren zur kontrollierten Passivierung der Innenwände eines Kühlkreislaufsystems aus Kohlenstoffstahl und Anwendung des Verfahrens zur Bestimmung des Passivierungszustandes und zur Prüfung der Qualität der Kühlflüssigkeit | |
DE597365C (nl) | ||
EP0674021B1 (de) | Verfahren zur Verhinderung der Korrosion von Metallen in wässrigen Systemen | |
AT262722B (de) | Verfahren zur Reinigung von wenigstens teilweise aus Metall bestehenden Vorrichtungen | |
DE1796321C (de) | Verfahren zum Herstellen einer Schutzschicht auf Stahl durch Eintau chen in eine Losung und Erhitzen unter Druck Ausscheidung aus 1621499 | |
DD227733B1 (de) | Verfahren zum innenkorrosionsschutz von warm- und heisswasserfuehrenden systemen aus eisenwerkstoffen | |
DE1810451A1 (de) | Korrosionsschutzmittel | |
DE2637048A1 (de) | Verfahren zur entfernung von fluorionen aus wasser | |
DE2165715A1 (de) | Verfahren zum Freihalten von Speichertanks für Petroleumölprodukte von Verunreinigungen durch Mikroorganismen |