CN204771160U - Mipor preparation facilities of high aspect ratio - Google Patents

Mipor preparation facilities of high aspect ratio Download PDF

Info

Publication number
CN204771160U
CN204771160U CN201520446654.7U CN201520446654U CN204771160U CN 204771160 U CN204771160 U CN 204771160U CN 201520446654 U CN201520446654 U CN 201520446654U CN 204771160 U CN204771160 U CN 204771160U
Authority
CN
China
Prior art keywords
laser
aspect ratio
reflecting mirror
sample
completely reflecting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201520446654.7U
Other languages
Chinese (zh)
Inventor
单炯
饶大幸
崔勇
李小莉
周士安
马伟新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI LASER PLASMA INSTITUTE OF CHINA ACADEMY OF ENGINEERING PHYSICS
Original Assignee
SHANGHAI LASER PLASMA INSTITUTE OF CHINA ACADEMY OF ENGINEERING PHYSICS
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI LASER PLASMA INSTITUTE OF CHINA ACADEMY OF ENGINEERING PHYSICS filed Critical SHANGHAI LASER PLASMA INSTITUTE OF CHINA ACADEMY OF ENGINEERING PHYSICS
Priority to CN201520446654.7U priority Critical patent/CN204771160U/en
Application granted granted Critical
Publication of CN204771160U publication Critical patent/CN204771160U/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The utility model relates to a mipor preparation facilities of high aspect ratio for high aspect ratio micropore. The utility model discloses a preparation facilities is that high aspect ratio micropore is prepared to the mode of utilizing dipulse combination, has contained two kinds of laser combinations that the pulse width is different in laser lamp -house, utilizes data signal time delay generator to control the time that the dipulse combination reaches the sample respectively, and the laser pulse of two kinds of laser instruments passes through the combination of optics components and parts and focuses on to the sample on, directly carries out laser ablation to the sample, including femto second laser ware, nanosecond laser instrument, data signal time delay generator, half -wave plate, the optics polarizer, beam splitter, holophote, white light light source, charge coupled cell, three -dimensional moving platform and computer in the preparation facilities. The utility model discloses the technique can directly break through the biggest micropore aspect ratio limit that the pulse can be prepared, solve well present micropore prepare in the not high technological problem of aspect ratio.

Description

A kind of preparation facilities of high aspect ratio micropore
Technical field
The utility model patent relates to laser technology application, and particularly a kind of method and device preparing superelevation aspect ratio micropore, to be applied to the high-accuracy opto-electronic device high aspect ratio micropore being had to very big demand.
Background technology
Integrated and microminiaturized in recent years along with opto-electronic device, day by day increases the small form factor requirements of unit element.Micropore is as one of the basic configuration of unit element, and its many core component requires that micropore size is little, aspect ratio large, thus effectively improves device performance and even have breakthrough development.
Utilizing single femtosecond pulse to prepare micropore is the technological means generally adopted at present, but along with the increase of the micropore degree of depth, the residue produced in preparation method and preparation process in prior art is more and more difficult to discharge, and the micropore degree of depth making pulse system standby is restricted.The limited situation of these micropore degree of depth causes this technology cannot obtain extensive use in Aero-Space, the energy, biomedicine, photoelectron microfluidic device, national defence etc. field.These defect an urgent demands of prior art we develop processing technology and the construction equipment of more direct convenience.
Summary of the invention
The purpose of this utility model is to overcome above-mentioned the deficiencies in the prior art, provides a kind of new preparation method for high aspect ratio micropore and preparation facilities.Preparation technology of the present utility model and preparation facilities directly will can break through the maximum micropore aspect ratio limit that pulse can be prepared, and solve the technical barrier that in the preparation of current micropore, aspect ratio is not high.
In order to reach foregoing invention object, the technical scheme that the utility model patent provides is as follows:
A kind of preparation method of high aspect ratio micropore, it is characterized in that, this preparation method be utilize dipulse to combine mode to prepare high aspect ratio micropore, in LASER Light Source, contain the laser in combination that two kinds of pulsewidths are different, its combination includes femtosecond-ps pulsed laser and ns pulsed laser combination, psec-Nanosecond Pulses laser in combination and the combination of femtosecond-picosecond double-pulse laser; Utilize data signal delay time generator to control dipulse respectively and combine the time reaching sample, the laser pulse of two kinds of laser instruments on sample, directly carries out laser ablation to sample, to prepare high aspect ratio micropore by optical component combined focus.
In the preparation method of the utility model height aspect ratio micropore, this preparation method specifically includes following steps:
The first step, femto-second laser is adopted to produce femto-second laser pulse, adopt nanosecond laser to produce nanosecond laser pulses simultaneously, utilize data signal delay time generator connection control femto-second laser and nanosecond laser respectively, strictly to control the time delay of femto-second laser pulse and nanosecond laser pulses arrival sample;
Second step, one group of half-wave plate and optical polariser combination is utilized to control power and the polarization of femto-second laser pulse, utilize another group half-wave plate and optical polariser combination to control power and the polarization of nanosecond laser pulses, recycling completely reflecting mirror and beam splitter are by nanosecond laser pulses and femto-second laser pulse space coincidence;
3rd step, nanosecond laser pulses and femto-second laser pulse are irradiated on sample through completely reflecting mirror and focusing objective len and carry out Laser Processing, and this sample is placed in a three-dimensional mobile platform, and this three-dimensional mobile platform is connected on computer to be moved by conputer controlled position;
4th step, design a white light source through beam splitter and completely reflecting mirror, be irradiated to sample by focusing objective len to throw light on, white light line focus object lens, completely reflecting mirror, beam splitter and completely reflecting mirror again after sample reflection, finally received by charge coupled cell, this charge coupled cell connects computer input signal with imaging on computers.
In the preparation method of high aspect ratio micropore of the present utility model, described data signal delay time generator controls the time delay of femto-second laser pulse and nanosecond laser pulses arrival sample, by nanosecond laser pulses, secondary operations is carried out to the plasma irradiating sample generation through femto-second laser pulse, suppress the accumulation of residue in micropore.
A kind of preparation facilities of high aspect ratio micropore, it is characterized in that, this preparation facilities includes femto-second laser, nanosecond laser, data signal delay time generator, half-wave plate, optical polariser, beam splitter, completely reflecting mirror, white light source, charge coupled cell, three-dimensional mobile platform and computer;
Described data signal delay time generator connect respectively and output electric pulse signal to femto-second laser and nanosecond laser, the output light path of described nanosecond laser is provided with half-wave plate, the light polarizer, first beam splitter and the second completely reflecting mirror, the output light path that described femto-second laser is stated is provided with half-wave plate, the light polarizer, first completely reflecting mirror, the femtosecond laser space coincidence that the nanosecond laser that nanosecond laser exports exports through the first completely reflecting mirror and the first beam splitter and femto-second laser, two bundle laser expose to sample through the second completely reflecting mirror and focusing objective len and carry out Laser Processing, this sample is positioned in described three-dimensional mobile platform, described computer connects and three-dimensional mobile platform described in controlling,
Described white light source, through the second beam splitter and the second completely reflecting mirror, is irradiated to sample by focusing objective len and throws light on; White light is again through focusing objective len, the second completely reflecting mirror, the second beam splitter and the 3rd completely reflecting mirror after sample reflection, and finally received by charge coupled cell, this charge coupled cell connects and transfers data to imaging on computer.
In the preparation facilities of the utility model height aspect ratio micropore, as an embody rule, described femto-second laser is the 780nm femto-second laser of pulsewidth 200fs, described nanosecond laser is the adjustable 1064nm nanosecond laser of pulsewidth 5ns to 200ns, described data signal delay time generator adopts the product of stanfordresearchsystem company, model is DG535, described charge coupled cell adopts the product of alliedvisiontechnologies company, model is StingrayF-504, described white light source is optical fiber Halogen lamp LED, described focusing objective len is the object lens of multiplication factor 10x.
Based on technique scheme, the preparation facilities of the utility model height aspect ratio micropore compared with prior art has following technological merit:
1, high aspect ratio preparation facilities of the present utility model utilize dipulse to combine mode to prepare high aspect ratio micropore, adopt a branch of nanosecond laser of extra introducing as the method for fill-in light, effectively prepared by the plasma produced in micropore process to femtosecond laser and carry out post bake, more strong discharge effect is produced to residue simultaneously, thus realize the further increase of the micropore degree of depth, and keep the aperture of micropore substantially unchanged.
2, device of the present utility model utilizes nanosecond laser to carry out post bake to irradiating via femtosecond laser the plasma generated, considerably increase the injection intensity of plasma, thus effectively inhibit the accumulation of residue in micropore, and by data signal delay time generator, can optimization nanosecond laser to the booster action of capillary processing.
3, the preparation facilities single unit system structure of high aspect ratio micropore of the present utility model is simple and clear, and topology layout is compact, is easy to adjustment.
Accompanying drawing explanation
Fig. 1 is the structure composition schematic diagram of the preparation facilities of the utility model height aspect ratio micropore.
Detailed description of the invention
We are described further the utility model with accompanying drawing in conjunction with the embodiments below, understand its structure composition and the course of work, but should not limit protection domain of the present utility model with this in the hope of more cheer and bright.
The utility model indicated a kind of preparation method of high aspect ratio micropore before this, this preparation method be utilize dipulse to combine mode to prepare high aspect ratio micropore, the laser in combination that two kinds of pulsewidths are different is contained in LASER Light Source, utilize data signal delay time generator to control dipulse respectively and combine the time reaching sample, the laser pulse of two kinds of laser instruments passes through optical component combined focus on sample, directly laser ablation is carried out to sample, to prepare high aspect ratio micropore.
In the preparation method of the utility model height aspect ratio micropore, the laser in combination that two kinds of pulsewidths are different is contained in LASER Light Source, its combination includes femtosecond-ps pulsed laser and ns pulsed laser combination, psec-Nanosecond Pulses laser in combination and the combination of femtosecond-picosecond double-pulse laser, and this preparation method specifically includes following steps:
The first step, the different laser in combination of femtosecond-nanosecond two kinds of pulsewidths is contained in LASER Light Source, femto-second laser is adopted to produce femto-second laser pulse, adopt nanosecond laser to produce nanosecond laser pulses simultaneously, utilize data signal delay time generator connection control femto-second laser and nanosecond laser respectively, strictly to control the time delay of femto-second laser pulse and nanosecond laser pulses arrival sample;
Second step, one group of half-wave plate and optical polariser combination is utilized to control power and the polarization of femto-second laser pulse, utilize another group half-wave plate and optical polariser combination to control power and the polarization of nanosecond laser pulses, recycling completely reflecting mirror and beam splitter are by nanosecond laser pulses and femto-second laser pulse space coincidence;
3rd step, nanosecond laser pulses and femto-second laser pulse are irradiated on sample through completely reflecting mirror and focusing objective len and carry out Laser Processing, and this sample is placed in a three-dimensional mobile platform, and this three-dimensional mobile platform is connected on computer to be moved by conputer controlled position;
4th step, design a white light source through beam splitter and completely reflecting mirror, be irradiated to sample by focusing objective len to throw light on, white light line focus object lens, completely reflecting mirror, beam splitter and completely reflecting mirror again after sample reflection, finally received by charge coupled cell, this charge coupled cell connects computer input signal with imaging on computers.
In the preparation method of high aspect ratio micropore of the present utility model, main laser is femtosecond laser, directly carries out laser ablation to sample, prepares micropore; Auxiliary laser is nanosecond laser, and its effect breaks through the single femtosecond pulse micropore aspect ratio numerical limitations that can obtain, thus obtains the superelevation aspect ratio micropore that single femtosecond pulse cannot be prepared.This technology can expand to multiple laser in combination such as psec-nanosecond, femtosecond-picosecond etc. equally.Described data signal delay time generator controls the time delay of femto-second laser pulse and nanosecond laser pulses arrival sample, by nanosecond laser pulses, secondary operations is carried out to the plasma irradiating sample generation through femto-second laser pulse, suppress the accumulation of residue in micropore.
The utility model also designs and produces out a kind of preparation facilities of high aspect ratio micropore based on said method.First refer to Fig. 1, Fig. 1 is the overall structure schematic diagram that the utility model prepares the device of superelevation aspect ratio micropore.As seen from the figure, the formation that the utility model prepares superelevation aspect ratio nanopore device comprises: femto-second laser 1, nanosecond laser 2, data signal delay time generator 3, half-wave plate 4, half-wave plate 5, optical polariser 6, optical polariser 7, first beam splitter 8, first completely reflecting mirror 9, second completely reflecting mirror 10, second beam splitter 11, the 3rd completely reflecting mirror 12, charge coupled cell 13, white light source 14, focusing objective len 15, sample 16, three-dimensional mobile platform 17 and computer 18.The annexation of above-mentioned component is as follows:
Described data signal delay time generator 3 output electric pulse signal controls femto-second laser 1 and nanosecond laser 2, strictly to control the time delay that two kinds of laser reach sample, specifically controls the relative time delay between nanosecond laser and femtosecond laser.
Being in half-wave plate 4 on described femto-second laser 1 output light path and optical polariser 6 for controlling power and the polarization of femtosecond laser, being in half-wave plate 5 on described nanosecond laser 2 output light path and optical polariser 7 in order to control power and the polarization of nanosecond laser.Specifically, half-wave plate is for regulating the polarization direction of laser, and optical polariser is used for the polarization direction of fixed laser.
The nanosecond laser that nanosecond laser 2 sends is through the first completely reflecting mirror 9 and the first beam splitter 8, make nanosecond laser and femtosecond laser space coincidence, two bundle laser after coincidence irradiate on sample 16 through the second completely reflecting mirror 10 and focusing objective len 15, carry out the Laser Processing of high aspect ratio micropore at sample 16.
The white light that described white light source 14 sends is successively through the second beam splitter 11 and the second completely reflecting mirror 10, be irradiated to sample 16 via focusing objective len 15 again to throw light on, white light through sample 16 reflect after again through focusing objective len 15, second completely reflecting mirror 10, second beam splitter 11 and the 3rd completely reflecting mirror 12, finally received by charge coupled cell 13, this charge coupled cell by receive Signal transmissions to computer 18 with imaging on computer 18.
Described charge coupled cell 13 and three-dimensional mobile platform 17 all with being connected of described computer 18.Described charge coupled cell 13 is for receiving the white light of sample surfaces reflection, three-dimensional mobile platform 17 is for controlling the zone of action of laser and sample, and computer 18 carries out imaging for the signal controlling three-dimensional mobile platform 17 and reception charge coupled cell 13 to the surface of sample 16.
In an embodiment: described femto-second laser 1 is the 780nm femto-second laser of pulsewidth 200fs, described nanosecond laser 2 is the adjustable 1064nm nanosecond laser of pulsewidth 5ns to 200ns, described data signal delay time generator 3 adopts the product of stanfordresearchsystem company, model is DG535, described charge coupled cell 13 adopts the product of alliedvisiontechnologies company, model is StingrayF-504, described white light source 14 is optical fiber Halogen lamp LED, and described focusing objective len is the object lens of multiplication factor 10x.
The course of work of the preparation facilities of the utility model height aspect ratio micropore is as follows:
Data signal delay time generator 3 first output electric pulse signal controls femto-second laser 1 and nanosecond laser 2, and strict adjustment two kinds of laser reach the time delay of sample; Half-wave plate 4 and optical polariser 6 control power and the polarization of femtosecond laser; Described half-wave plate 5 and optical polariser 7 control power and the polarization of nanosecond laser; Nanosecond laser is through the first completely reflecting mirror 9 and the first beam splitter 8 and femtosecond laser space coincidence; Two bundle laser irradiate sample 16 through the second completely reflecting mirror 10 and focusing objective len 15 and carry out Laser Processing.
Described white light source 14 through the second beam splitter 11 and the second completely reflecting mirror 10, then is irradiated to sample 16 by focusing objective len 15 and throws light on; White light again through focusing objective len 15, second completely reflecting mirror 10, second beam splitter 11 and the 3rd completely reflecting mirror 12, is finally received and imaging on computer 18 by charge coupled cell 13 after sample 16 reflects.
The Preparation equipment of the utility model height aspect ratio micropore has the field of very big demand to have wide practical use in Aero-Space, the energy, biomedicine, photoelectron microfluidic device, national defence etc. to superelevation aspect ratio micropore, is also that preparation superelevation aspect ratio micropore is to break through the feasible method of some core component technical functionality bottleneck simultaneously.

Claims (4)

1. the preparation facilities of one kind high aspect ratio micropore, it is characterized in that, this preparation facilities includes femto-second laser, nanosecond laser, data signal delay time generator, half-wave plate, optical polariser, beam splitter, completely reflecting mirror, white light source, charge coupled cell, three-dimensional mobile platform and computer;
Described data signal delay time generator connect respectively and output electric pulse signal to femto-second laser and nanosecond laser, the output light path of described nanosecond laser is provided with half-wave plate, the light polarizer, first beam splitter and the second completely reflecting mirror, the output light path of described femto-second laser is provided with half-wave plate, the light polarizer, first completely reflecting mirror, the femtosecond laser space coincidence that the nanosecond laser that nanosecond laser exports exports through the first completely reflecting mirror and the first beam splitter and femto-second laser, two bundle laser expose to sample through the second completely reflecting mirror and focusing objective len and carry out Laser Processing, this sample is positioned in described three-dimensional mobile platform, described computer connects and three-dimensional mobile platform described in controlling,
Described white light source, through the second beam splitter and the second completely reflecting mirror, is irradiated to sample by focusing objective len and throws light on; White light is again through focusing objective len, the second completely reflecting mirror, the second beam splitter and the 3rd completely reflecting mirror after sample reflection, and finally received by charge coupled cell, this charge coupled cell connects and transfers data to imaging on computer.
2. the preparation facilities of a kind of high aspect ratio micropore according to claim 1, it is characterized in that, described femto-second laser is the 780nm femto-second laser of pulsewidth 200fs, and described nanosecond laser is the adjustable 1064nm nanosecond laser of pulsewidth 5ns to 200ns.
3. the preparation facilities of a kind of high aspect ratio micropore according to claim 1, it is characterized in that, described data signal delay time generator adopts the product of stanfordresearchsystem company, model is DG535, described charge coupled cell adopts the product of alliedvisiontechnologies company, and model is StingrayF-504.
4. the preparation facilities of a kind of high aspect ratio micropore according to claim 1, it is characterized in that, described white light source is optical fiber Halogen lamp LED, and described focusing objective len is the object lens of multiplication factor 10x.
CN201520446654.7U 2015-06-26 2015-06-26 Mipor preparation facilities of high aspect ratio Active CN204771160U (en)