CN202534443U - 电缆用金属线材绞制模具 - Google Patents
电缆用金属线材绞制模具 Download PDFInfo
- Publication number
- CN202534443U CN202534443U CN2012201900507U CN201220190050U CN202534443U CN 202534443 U CN202534443 U CN 202534443U CN 2012201900507 U CN2012201900507 U CN 2012201900507U CN 201220190050 U CN201220190050 U CN 201220190050U CN 202534443 U CN202534443 U CN 202534443U
- Authority
- CN
- China
- Prior art keywords
- mold
- molding
- twisting
- wire rod
- metal wires
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种电缆用金属线材绞制模具,包括固定装置和成型挤压模、固定装置安装在线材绞制成型机上,固定装置有进水口、出水口和冷却水腔,成型挤压模由一段圆锥面和一段圆柱面组成,成型挤压模的圆柱面部位的内管的横截面呈圆形。本实用新型用于生产不同直径,横截面呈圆形的金属线缆,只需要更换成型挤压模,更换方便,减少了模具的制造成本,与此同时,固定装置具有冷却水腔,在金属线材绞制过程中采用冷却水降低成型挤压模表面的温度,可以同时降低金属线材的温度,减少因为温度升高引入到金属线材内部的热应力,提高金属线材绞制的紧密程度。
Description
技术领域
本实用新型涉及电缆用金属线材绞制模具,更确切地说是涉及一种金属线材生产方面的发明。
背景技术
在电缆用金属线材绞制过程中,多股金属线材经过绞制模具的挤压、变形和绞合,形成为不同截面形状和截面积的缆用金属线材,多股线材之间绞合接触紧密,有利于导电和线材的柔韧性。在绞制过程中,在绞制模具的挤压部位,由于线材受到压力、摩擦和形变,往往温度会升高。由于存在热胀冷缩,处于高温状态的线材通过绞合在一起紧密接触,但温度降低以后,各股线材会冷却收缩,导致线材绞合紧密程度降低,影响电缆质量。为了保证绞制过程的温度升高不至于严重影响电缆质量,不得不降低绞制的速度,影响产品的交期。在另外一方面,不同规格的电缆要用不同截面形状和截面积的绞制模具,这样不但要生产大量的模具,而且占用大量的地方存放这些模具,另外也给模具的管理带来了困难。生产的时候,每更换一种规格的电缆,就必须更换一套模具,费时费力,影响生产效率。
由此可见,上述现有电缆用金属线材绞制模具仍存在有诸多的缺陷,而亟待加以改进。
有鉴于上述现有电缆用金属线材绞制模具存在的缺陷,本设计人基于从事此类产品设计制造多年,积有丰富的实务经验及专业知识,积极加以研究创新,以期创设一种改进成型结构的电缆用金属线材绞制模具,能够改进一般市面上现有电缆用金属线材绞制模具的成型结构,使其更具有竞争性。经过不断的研究、设计,并经反复试作样品及改进后,终于创设出确具实用价值的本实用新型。
发明内容
本实用新型所要解决的主要技术问题在于,克服现有的电缆用金属线材绞制模具存在的缺陷,而提供一种新型结构的电缆用金属线材绞制模具,克服了现有电缆用金属线材绞制模具在升温、低速和更换麻烦的缺陷,提高电缆用金属线材绞制模具的使用效果。
本实用新型解决其主要技术问题是采用以下技术方案来实现的。依据本实用新型提出的电缆用金属线材绞制模具,包括固定装置和成型挤压模,固定装置安装在线材绞制成型机上。
本实用新型解决其技术问题还可以采用以下技术措施来进一步实现。
前所述的固定装置有进水口、出水口和冷却水腔。
前所述的成型挤压模由一段圆锥面和一段圆柱面组成。
前所述的成型挤压模的圆柱面部位的内管的横截面呈圆形。
本实用新型与现有技术相比具有明显的优点和有益效果。由以上技术方案可知,本实用新型由于采用上述技术方案,绞制模具分为固定装置和易拆装的成型挤压模,固定装置起到固定和冷却的作用,成型挤压模起到成型和挤压的作用,这样生产出来的电缆用金属线材绞制模具就避免了现有技术成本高,温度高,速度慢,更换麻烦的缺陷,达到本实用新型的目的。
上述说明仅为本实用新型技术方案特征部份的概述,为使专业技术人员能够更清楚了解本实用新型的技术手段,并可依照说明书的内容予以实施,以下以本实用新型的较佳实施例并配合附图详细说明如后。
本实用新型的具体实施方式由以下实施例及其附图详细给出。。
附图说明
图1是本实用新型的纵截面图。
图2是本实用新型的成型挤压模的圆柱面部位的横截面图。
图中,固定装置1,成型挤压模2,冷却水腔3,出水口4,进水口5,圆柱面6,圆锥面7,螺丝孔8。
具体实施方式
以下结合附图及较佳实施例,对依据本实用新型提出的其具体实施方式、结构、特征及其功效,详细说明如后。
请参阅图1所示,本实用新型的电缆用金属线材绞制模具, 包括固定装置1和成型挤压模2,固定装置1安装在线材绞制成型机上,固定装置1有冷却水腔3、出水口4、和进水口5,成型挤压模2由一段圆柱面6和一段圆锥面7组成,固定装置1和成型挤压模2通过螺丝孔8固定,圆柱面6部位的内管的横截面呈圆形,请参阅图2所示。
在生产电缆的时候,固定装置的冷却水腔通过冷却水,起到降温的作用,根据截面为圆形的线材的尺寸选择不同尺寸的成型挤压模,使其嵌入固定装置内,这样更换方便,成本低廉,效率高。
以上所述,仅是本实用新型的较佳实施例而已,并非对本实用新型作任何形式上的限制,凡是依据本实用新型的技术实质对以上实施例所作的任何简单修改、等同变化与修饰,均仍属于本实用新型技术方案的范围内。
Claims (4)
1.电缆用金属线材绞制模具,其特征在于,包括固定装置和成型挤压模,固定装置安装在线材绞制成型机上。
2.根据权利要求1所述的电缆用金属线材绞制模具,其特征在于,其中所述的固定装置有进水口、出水口和冷却水腔。
3.根据权利要求1所述的电缆用金属线材绞制模具,其特征在于,其中所述的成型挤压模由一段圆锥面和一段圆柱面组成。
4.根据权利要求1或3所述的电缆用金属线材绞制模具,其特征在于,其中所述的成型挤压模的圆柱面部位的内管的横截面呈圆形。