CN202090075U - 电解铜箔装置 - Google Patents
电解铜箔装置 Download PDFInfo
- Publication number
- CN202090075U CN202090075U CN 201120161067 CN201120161067U CN202090075U CN 202090075 U CN202090075 U CN 202090075U CN 201120161067 CN201120161067 CN 201120161067 CN 201120161067 U CN201120161067 U CN 201120161067U CN 202090075 U CN202090075 U CN 202090075U
- Authority
- CN
- China
- Prior art keywords
- guide wheels
- guide wheel
- plate
- copper
- cathode roller
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
电解铜箔装置,包括槽体、阴极辊,在阴极辊的端面设有环板,环板上一周设有螺孔,环板与阴极辊之间设有间隙,在环板前侧对应的槽体上分别设置前水平导轮和前竖向导轮,在环板后侧对应的槽体上分别设置后水平导轮和后竖向导轮;O型密封圈依次套在前水平导轮、前竖向导轮、环板的下部、后竖向导轮、后水平导轮上设置;环板与阴极辊之间设有6mm的间隙;阴极辊端面和槽体壁之间设置有负阴极。本实用新型结构简单、功能实用,把密封圈从起箔线处剥离,不让密封圈与箔面摩擦,让箔在起箔时没有阻力。有效地密封阴极辊边部,防止边部出现铜豆、铜渣或铜条。
Description
技术领域
本实用新型涉及一种电解铜箔装置。
背景技术
在铜箔生产各个环节中,生箔***尤为重要。铜箔生产中在阴极辊两边的密封圈看似简单,但却有着十分重要的作用,它有效地密封阴极辊边部,防止边部出现铜豆、铜渣或铜条。因而在实际生产过程中,往往会因为种种原因如:密封圈本身缺陷、操作翻转不彻底、擦拭的用具不干净、密封不严、操作不认真等而造成撕边、压坑、边部氧化等铜箔生产缺陷问题,这些缺陷给企业带来了严重的经济损失,一直是铜箔生产难以解决的问题。
电解铜箔装置中的撕边、压坑、边部氧化等缺陷从产生原因上说,就是密封圈与阴极辊钛边接触密封不好,阴极辊钛边长铜较快,在起箔时箔遇到阻力,被撕裂或边部铜豆被弹到箔上,造成压坑、氧化。
如果用固定支架在阴极辊正上方边部把密封圈挂起,刚开始,能运行稳定,但是时间一长就不行了,因为密封圈长时间被挂起,弹性受到影响而变形,与钛边密封不实,产生铜杂较多,极易出现撕边现象,而且端板也会变形,漏点较多。一块端板有多处漏点,在漏点处易长铜豆,铜豆较多,对阴极辊的使用安全构成了严重的威胁,易造成阴极辊电击危险。
如果用直径4cm的圆形滚桶,安装在阴极辊进出口,用来挤压密封圈,防止边部氧化,也是开始的时候运行稳定,时间长了,出现密封圈因挤压而变形,与端板密封不好。
实用新型内容
本实用新型提供一种电解铜箔装置,有效地密封阴极辊边部,防止边部出现铜豆、铜渣或铜条,解决了撕边、压坑、边部氧化的铜箔生产缺陷。
为了解决上述技术问题,本实用新型采用如下技术方案:电解铜箔装置,包括槽体、阴极辊,在阴极辊的端面设有环板,环板上一周设有螺孔,环板与阴极辊之间设有间隙,在环板前侧对应的槽体上分别设置前水平导轮和前竖向导轮,在环板后侧对应的槽体上分别设置后水平导轮和后竖向导轮;O型密封圈依次套在前水平导轮、前竖向导轮、环板的下部、后竖向导轮、后水平导轮上设置。
所述的环板与阴极辊之间设有6mm的间隙。
所述的阴极辊端面和槽体壁之间设置有负阴极。
本实用新型结构简单、功能实用,把密封圈从起箔线处剥离,不让密封圈与箔面摩擦,让箔在起箔时没有阻力。有效地密封阴极辊边部,防止边部出现铜豆、铜渣或铜条。解决了撕边、压坑、边部氧化等铜箔生产缺陷。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
实施例:如图1所示,电解铜箔装置,包括槽体1、阴极辊2,在阴极辊2的端面设有环板3,环板3上一周设有40个均匀分布的螺孔10,环板3与阴极辊2之间设有间隙,在环板3前侧对应的槽体1上分别设置前水平导轮6和前竖向导轮7,在环板3后侧对应的槽体1上分别设置后水平导轮8和后竖向导轮9;O型密封圈5依次套在前水平导轮6、前竖向导轮7、环板3的下部、后竖向导轮9、后水平导轮8上设置。环板3与阴极辊2之间设有6mm的间隙用以安装O型密封圈5。阴极辊2端面和槽体1壁之间设置有负阴极4。
阴极辊2转动运行,下半部分浸入生箔机槽体1中溶液电解,浸入溶液的阴极辊2边部由O型密封圈2密封,断绝边部电沉积。负阴极4:用8mm铜杆做成圆形,通阴极电安装于阴极辊两侧,即环板与槽体之间,用于吸附O型密封圈5周围的铜离子,防止阴极辊2边部和O型密封圈5长铜。
本实用新型把阴极辊两边端板全部去掉,然后换成环板,把密封圈更换为R=7㎜,在阴极辊槽体前后安装导轮,把密封圈从侧面剥离出来。把端板全部换掉,可以杜绝端板变形、漏液、长铜豆等问题;采用环板,它只有端板的五分之一厚,可以把阴极辊两边全部暴露出来;然后在槽体两边部加上负阴极,它可以把阴极辊钛边的铜离子吸附,防止钛边镀铜,钛边不长铜豆就不会出现撕边;另外环形花板不易变形,不会出现漏点,且材料成本低,安装较方便。
此项技术的应用使撕边、压坑、边部氧化等铜箔生产缺陷问题迅速得到解决,降低毛箔损失、减少废箔量,在实际生产线上应用后,每月可减少撕边废箔9.96吨,压坑废箔0.3吨;每月可提高卷重1500㎏以上,减少接头直废1.6吨;边部氧化B级毛箔15吨;阴极辊复抛14次,可提高产量1.8吨;合计年增产21.6吨,减少废箔142.32吨,减少B级180吨,按每吨成品箔价值9万元,B级差价0.8万元计算,共增加产值1620万元,增加利税320余万元。
Claims (3)
1.电解铜箔装置,包括槽体、阴极辊,其特征在于:在阴极辊的端面设有环板,环板上一周设有螺孔,环板与阴极辊之间设有间隙,在环板前侧对应的槽体上分别设置前水平导轮和前竖向导轮,在环板后侧对应的槽体上分别设置后水平导轮和后竖向导轮;O型密封圈依次套在前水平导轮、前竖向导轮、环板的下部、后竖向导轮、后水平导轮上设置。
2.根据权利要求1所述的电解铜箔装置,其特征在于:所述的环板与阴极辊之间设有6mm的间隙。
3.根据权利要求1或2所述的电解铜箔装置,其特征在于:所述的阴极辊端面和槽体壁之间设置有负阴极。