CN1731072A - 礼花球壳、发射架及其制作方法 - Google Patents

礼花球壳、发射架及其制作方法 Download PDF

Info

Publication number
CN1731072A
CN1731072A CN 200510019309 CN200510019309A CN1731072A CN 1731072 A CN1731072 A CN 1731072A CN 200510019309 CN200510019309 CN 200510019309 CN 200510019309 A CN200510019309 A CN 200510019309A CN 1731072 A CN1731072 A CN 1731072A
Authority
CN
China
Prior art keywords
launcher
ball shell
powder
fireworks ball
waste paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 200510019309
Other languages
English (en)
Other versions
CN100370213C (zh
Inventor
徐青田
杨群
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNB2005100193096A priority Critical patent/CN100370213C/zh
Publication of CN1731072A publication Critical patent/CN1731072A/zh
Application granted granted Critical
Publication of CN100370213C publication Critical patent/CN100370213C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种礼花球壳、发射架是由以下重量百分比的原料组成:秸秆20-30%、废纸20-30%、滑石粉6-12%、轻钙粉10-18%、淀粉4-8%、双飞粉8-15%、硬脂酸4-8%。其制作方法是:将秸秆、废纸粉碎成长度3-8毫米;按上述比例将各原料一起混合搅匀,并加入70-90℃的水搅拌,水的量为料重的0.6-0.8倍;将礼花球壳及发射架的模具加热到180-240℃;用分料机分料,将搅拌好的料放入加热的模具中,加压60-120秒后出模即可。本发明的礼花球壳及发射架是以秸秆和废纸为主要原料配以辅料制成,其原料均可燃烧和降解,对环境不会产生污染,且废料可重复利用,大大减少了生产成本,生产工艺也简单。

Description

礼花球壳、发射架及其制作方法
技术领域
本发明涉及礼花,尤其是一种礼花球壳、发射架及其制作方法。
背景技术
我们国家是礼花的生产大国,每年都有大量的礼花出口到世界各地。随着全世界各个国家对环境保护的重视,那种以塑料为原料制作礼花球壳和发射架的礼花的使用已大大受到限制,有的甚至禁止使用。这就要求我们生产的礼花应具备环保、无污染等特点。
发明内容
本发明的目的就是提供一种生产成本低、环保、可降解无污染的礼花球壳、发射架及其制作方法。
本发明的礼花球壳、发射架是由以下重量百分比的原料组成:
秸杆   20-30%    废纸   20-30%    滑石粉   6-12%    轻钙粉   10-18%
淀粉   4-8%      双飞粉 8-15%     硬脂酸   4-8%。
本发明的礼花球壳、发射架制作方法是:
1、将秸杆、废纸粉碎成长度3-8毫米;
2、按上述比例将各原料一起混合搅匀,并加入70-90℃的水搅拌,水的量为料重的0.6-0.8倍;
3、将礼花球壳及发射架的模具加热到180-240℃;
4、用分料机分料,将搅拌好的料放入加热的模具中,加压60-120秒后出模即可。
在上述原料中,秸杆和废纸为主要原料,可降解、燃烧,废纸的使用能增加产品的强度和拉力;轻钙粉和双飞粉为填充料,起填充纤维空隙的作用;硬脂酸能提高产品的强度;淀粉起粘接作用;滑石粉的功能是使产品表面光滑、脱模方便。
本发明的礼花球壳及发射架是以秸杆和废纸为主要原料配以辅料制成,其原料均可燃烧和降解,对环境不会产生污染,且废料可重复利用,大大减少了生产成本,生产工艺也简单。
具体实施方式
实施例1:
一种礼花球壳、发射架是由以下重量百分比的原料组成:
秸杆   30%    废纸   25%    滑石粉   10%    轻钙粉   15%
淀粉   6%     双飞粉 10%    硬脂酸   4%。
本发明的礼花球壳、发射架制作方法是:
1、将秸杆、废纸粉碎成长度4-6毫米;
2、按上述比例将各原料一起混合搅匀,并加入80-85℃的水搅拌,水的量为料重的0.6倍;
3、将礼花球壳及发射架的模具加热到180℃;
4、用分料机分料,将搅拌好的料放入加热的模具中,加压90秒后出模即可。
实施例2:
一种礼花球壳、发射架是由以下重量百分比的原料组成:
秸杆   30%    废纸   30%    滑石粉   10%    轻钙粉   10%
淀粉   4%     双飞粉 12%    硬脂酸   4%。
其制作方法与实施例1相同。
实施例3:
一种礼花球壳、发射架是由以下重量百分比的原料组成:
秸杆   30%    废纸   20%    滑石粉   12%    轻钙粉   10%
淀粉   8%     双飞粉 15%    硬脂酸   5%。
其制作方法与实施例1相同。

Claims (5)

1、一种礼花球壳、发射架,其特征在于:它是由以下重量百分比的原料组成:
秸杆20-30%    废纸20-30%     滑石粉6-12%    轻钙粉10-18%
淀粉4-8%      双飞粉8-15%    硬脂酸4-8%。
2、如权利要求1所述的礼花球壳、发射架,其制作方法是:
a、将秸杆、废纸粉碎成长度3-8毫米;
b、按上述比例将各原料一起混合搅匀,并加入70-90℃的水搅拌,水的量为料重的0.6-0.8倍;
c、将礼花球壳、发射架的模具加热到180-240℃;
d、用分料机分料,将搅拌好的料放入加热的模具中,加压60-120秒后出模即可。
3、如权利要求1所述的礼花球壳、发射架,其特征在于:它是由以下重量百分比的原料组成:
秸杆30%    废纸25%      滑石粉10%    轻钙粉15%
淀粉6%     双飞粉10%    硬脂酸4%。
4、如权利要求1所述的礼花球壳、发射架,其特征在于:它是由以下重量百分比的原料组成:
秸杆30%    废纸30%      滑石粉10%    轻钙粉10%
淀粉4%     双飞粉12%    硬脂酸4%。
5、如权利要求1所述的礼花球壳、发射架,其特征在于:它是由以下重量百分比的原料组成:
秸杆30%    废纸20%      滑石粉12%    轻钙粉10%
淀粉8%     双飞粉15%    硬脂酸5%。
CNB2005100193096A 2005-08-15 2005-08-15 礼花球壳、发射架及其制作方法 Expired - Fee Related CN100370213C (zh)