CN106734896A - 一种叉车驱动桥桥壳的铸造方法 - Google Patents
一种叉车驱动桥桥壳的铸造方法 Download PDFInfo
- Publication number
- CN106734896A CN106734896A CN201611214604.1A CN201611214604A CN106734896A CN 106734896 A CN106734896 A CN 106734896A CN 201611214604 A CN201611214604 A CN 201611214604A CN 106734896 A CN106734896 A CN 106734896A
- Authority
- CN
- China
- Prior art keywords
- mould
- casting
- axle housing
- potting syrup
- resin bonded
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供一种叉车驱动桥桥壳的铸造方法,所述方法包括以下步骤:(1)采用两箱分模造型,(2)使用所述的树脂砂制作砂型,(3)浇注液的制作,(4)将上述原料在电炉内加热至熔炼温度,形成浇注液;(5)向所述的树脂砂型中浇注所述的浇注液,凝固后形成铸件。本发明该铸造方法不仅很好的克服了桥壳在铸造过程中容易产生锁孔、裂纹等缺陷的产生,同时还提高了钢水利用率;可直接铸造出桥壳铸件,铸件成品高度精确,加工制作工艺简单。
Description
技术领域
本发明涉及叉车部件制造技术领域,具体涉及一种叉车驱动桥桥壳的铸造方法。
背景技术
由于后桥壳结构复杂壁厚不均,公知的铸造方法存在很多不足,如:因为铸件的结构工艺性不好,导致非常容易产生裂纹,且不易解决表面褶皱及补缩问题,制成的成品铸件硬度不够,不仅铸造工序较多,影响产能,同时铸件的精度无法得到有效保证,废品率较高。
发明内容
针对现有技术不足,本发明提供一种叉车驱动桥桥壳的铸造方法,该铸造方法不仅很好的克服了桥壳在铸造过程中容易产生锁孔、裂纹等缺陷的产生,同时还提高了钢水利用率;可直接铸造出桥壳铸件,铸件成品高度精确,加工制作工艺简单。
为实现以上目的,本发明的技术方案通过以下技术方案予以实现:
一种叉车驱动桥桥壳的铸造方法,所述方法包括以下步骤:
(1)采用两箱分模造型,分型面选择在后桥壳两耳孔水平中心线处,根据不同位置的热节大小,分别设置相应的冒口,以满足补缩要求;
(2)使用所述的树脂砂制作砂型,配模合箱后形成树脂砂型,树脂砂型的轴心线与水平面相垂直,两个摸合箱上分别设有直浇口,两个直浇口通过横跑道相连接;
(3)浇注液的制作,其原料化学成分的百分比含量如下:C:2.4-3.2%;Si:0.5-1.5%;Mn:0.3-1.2%;P:0.01%;S:0.02%;Mg:0.04-0.05%;RE:0.01-0.015%;Cu:0.2-0.4%和Cr:0.3-1.5%;其余为Fe;
(4)将上述原料在电炉内加热至熔炼温度,使合金充分熔化形成铁水,在铁水包内筑有的坑穴内放入球化剂,并覆盖孕育剂,将铁水倒入铁水包进行球化、孕育处理,形成浇注液;
(5)向所述的树脂砂型中浇注所述的浇注液,凝固后形成曲轴铸件,后桥壳上使用的外冷铁均为随行外冷铁,以增强冷铁的激冷作用,然后向所述的树脂砂型中浇注所述的浇注液,凝固后形成铸件。
本发明提供一种叉车驱动桥桥壳的铸造方法,与现有技术相比优点在于:
本发明该铸造方法不仅很好的克服了桥壳在铸造过程中容易产生锁孔、裂纹等缺陷的产生,同时还提高了钢水利用率;可直接铸造出桥壳铸件,铸件成品高度精确,加工制作工艺简单。
具体实施方式
为使本发明实施例的目的、技术方案和优点更加清楚,下面结合本发明实施例对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有作出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
一种叉车驱动桥桥壳的铸造方法,所述方法包括以下步骤:
(1)采用两箱分模造型,分型面选择在后桥壳两耳孔水平中心线处,根据不同位置的热节大小,分别设置相应的冒口,以满足补缩要求;
(2)使用所述的树脂砂制作砂型,配模合箱后形成树脂砂型,树脂砂型的轴心线与水平面相垂直,两个摸合箱上分别设有直浇口,两个直浇口通过横跑道相连接;
(3)浇注液的制作,其原料化学成分的百分比含量如下:C:2.4-3.2%;Si:0.5-1.5%;Mn:0.3-1.2%;P:0.01%;S:0.02%;Mg:0.04-0.05%;RE:0.01-0.015%;Cu:0.2-0.4%和Cr:0.3-1.5%;其余为Fe;
(4)将上述原料在电炉内加热至熔炼温度,使合金充分熔化形成铁水,在铁水包内筑有的坑穴内放入球化剂,并覆盖孕育剂,将铁水倒入铁水包进行球化、孕育处理,形成浇注液;
(5)向所述的树脂砂型中浇注所述的浇注液,凝固后形成曲轴铸件,后桥壳上使用的外冷铁均为随行外冷铁,以增强冷铁的激冷作用,然后向所述的树脂砂型中浇注所述的浇注液,凝固后形成铸件。
本发明该铸造方法不仅很好的克服了桥壳在铸造过程中容易产生锁孔、裂纹等缺陷的产生,同时还提高了钢水利用率;可直接铸造出桥壳铸件,铸件成品高度精确,加工制作工艺简单。
需要说明的是,以上实施例仅用以说明本发明的技术方案,而非对其限制;尽管参照前述实施例对本发明进行了详细的说明,本领域的普通技术人员应当理解:其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换;而这些修改或者替换,并不使相应技术方案的本质脱离本发明各实施例技术方案的精神和范围。
Claims (1)
1.一种叉车驱动桥桥壳的铸造方法,其特征在于:所述方法包括以下步骤:
(1)采用两箱分模造型,分型面选择在后桥壳两耳孔水平中心线处,根据不同位置的热节大小,分别设置相应的冒口,以满足补缩要求;
(2)使用所述的树脂砂制作砂型,配模合箱后形成树脂砂型,树脂砂型的轴心线与水平面相垂直,两个摸合箱上分别设有直浇口,两个直浇口通过横跑道相连接;
(3)浇注液的制作,其原料化学成分的百分比含量如下:C:2.4-3.2%;Si:0.5-1.5%;Mn:0.3-1.2%;P:0.01%;S:0.02%;Mg:0.04-0.05%;RE:0.01-0.015%;Cu:0.2-0.4%和Cr:0.3-1.5%;其余为Fe;
(4)将上述原料在电炉内加热至熔炼温度,使合金充分熔化形成铁水,在铁水包内筑有的坑穴内放入球化剂,并覆盖孕育剂,将铁水倒入铁水包进行球化、孕育处理,形成浇注液;
(5)向所述的树脂砂型中浇注所述的浇注液,凝固后形成曲轴铸件,后桥壳上使用的外冷铁均为随行外冷铁,以增强冷铁的激冷作用,然后向所述的树脂砂型中浇注所述的浇注液,凝固后形成铸件。