CN105295376A - 一种自粘性纳米pet胶带 - Google Patents
一种自粘性纳米pet胶带 Download PDFInfo
- Publication number
- CN105295376A CN105295376A CN201510765150.6A CN201510765150A CN105295376A CN 105295376 A CN105295376 A CN 105295376A CN 201510765150 A CN201510765150 A CN 201510765150A CN 105295376 A CN105295376 A CN 105295376A
- Authority
- CN
- China
- Prior art keywords
- adhesive tape
- parts
- nanometer
- rubber
- nano
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种自粘性纳米PET胶带,其按质量份数计,其包括以下配比的成分:基础橡胶:100;纳米银:30-50;增粘橡胶:20-40;微粉二氧化硅:50-200;增强树脂:10-20;硫化剂:0.5-1.5;纳米二氧化钛:4-6;纳米钛白粉:3-50。本发明中添加的二氧化硅和硅的微粒的粒径等级不同,容纳的空气量多,防粘连效果好,制成的PET胶带省去了表面涂布的工序,减少胶带因涂布而产生的污染,增加胶带的环保质量水平和使用范围。通过添加纳米材料,解决了现有技术中PET胶带柔韧性差的问题。同时纳米二氧化钛不容易迁移,大大的延长功能的时效性。
Description
技术领域
本发明涉及一种自粘性纳米PET胶带。
背景技术
纳米颗粒提供令人感兴趣的并且常常预料不到的性质,因为它们的性质是颗粒表面的而不是本体体积的结果。例如,纳米颗粒可显示出令人惊讶的机械、光学和电性质,即使在低的浓度下。在聚合物科学中,特别是对于聚合物增强,纳米颗粒的性质已经吸引了关注。特别的注意力已经集中于碳纳米管(CNT)。
目前,电力、通信***使用的国产密封绝缘材料,耐水、碱、酸性、电气性能较差,适用性不强,自粘性工艺性差,目前大部分使用进口3M等公司的材料,价格较高。
当前我国已经具备了制造各类自粘带的技术和能力,为使产品能够在更多领域使用,片材的透明性极高,故在生产成型时,表面常常贴粘在一起,不容易分离,或者分离时经常形成划伤,摩擦等质量问题,通常客户会使用涂布技术,但在表面会形成花斑,而且在食品、医疗等领域使用存在环保卫生等问题,制约了PET胶带的广泛应用。现有的PET胶带在柔韧性效果还欠佳,这样大大降低了产品的使用寿命。因此,为解决上述问题,特提供一种新的技术方案来满足需求。
发明内容
本发明要解决的技术问题是克服现有技术的缺陷,提供一种自粘性纳米PET胶带。
为了解决上述技术问题,本发明提供了如下的技术方案:
本发明一种自粘性纳米PET胶带,其按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:30-50;
增粘橡胶:20-40;
微粉二氧化硅:50-200;
增强树脂:10-20;
硫化剂:0.5-1.5;
纳米二氧化钛:4-6;
纳米钛白粉:3-50。
进一步地,所述的基础橡胶为丁基橡胶。
进一步地,所述的基础橡胶为乙丙橡胶。
进一步地,所述的基础橡胶为硅橡胶。
进一步地,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:30;
增粘橡胶:20;
微粉二氧化硅:50;
增强树脂:10;
硫化剂:0.5;
纳米二氧化钛:4;
纳米钛白粉:3。
进一步地,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:50;
增粘橡胶:40;
微粉二氧化硅:200;
增强树脂:20;
硫化剂:1.5;
纳米二氧化钛:4-6;
纳米钛白粉:50。
本发明所达到的有益效果是:
本发明通过在PET胶带的功能层中添加二氧化硅和硅的复合微粉颗粒,增加胶带表面微观上的粗糙度,使收卷时胶带之间可以容纳少量的空气,以防止胶带粘连,达到易分离的效果;并且本发明中添加的二氧化硅和硅的微粒的粒径等级不同,容纳的空气量多,防粘连效果好,制成的PET胶带省去了表面涂布的工序,减少胶带因涂布而产生的污染,增加胶带的环保质量水平和使用范围。通过添加纳米材料,解决了现有技术中PET胶带柔韧性差的问题。同时纳米二氧化钛不容易迁移,大大的延长功能的时效性。
具体实施方式
以下对本发明的优选实施例进行说明,应当理解,此处所描述的优选实施例仅用于说明和解释本发明,并不用于限定本发明。
本发明一种自粘性纳米PET胶带,其按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:30-50;
增粘橡胶:20-40;
微粉二氧化硅:50-200;
增强树脂:10-20;
硫化剂:0.5-1.5;
纳米二氧化钛:4-6;
纳米钛白粉:3-50。
进一步地,所述的基础橡胶为丁基橡胶。
进一步地,所述的基础橡胶为乙丙橡胶。
进一步地,所述的基础橡胶为硅橡胶。
进一步地,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:30;
增粘橡胶:20;
微粉二氧化硅:50;
增强树脂:10;
硫化剂:0.5;
纳米二氧化钛:4;
纳米钛白粉:3。
进一步地,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:50;
增粘橡胶:40;
微粉二氧化硅:200;
增强树脂:20;
硫化剂:1.5;
纳米二氧化钛:4-6;
纳米钛白粉:50。
本发明所达到的有益效果是:
本发明通过在PET胶带的功能层中添加二氧化硅和硅的复合微粉颗粒,增加胶带表面微观上的粗糙度,使收卷时胶带之间可以容纳少量的空气,以防止胶带粘连,达到易分离的效果;并且本发明中添加的二氧化硅和硅的微粒的粒径等级不同,容纳的空气量多,防粘连效果好,制成的PET胶带省去了表面涂布的工序,减少胶带因涂布而产生的污染,增加胶带的环保质量水平和使用范围。通过添加纳米材料,解决了现有技术中PET胶带柔韧性差的问题。同时纳米二氧化钛不容易迁移,大大的延长功能的时效性。
最后应说明的是:以上所述仅为本发明的优选实施例而已,并不用于限制本发明,尽管参照前述实施例对本发明进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。
Claims (6)
1.一种自粘性纳米PET胶带,其特征在于,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:30-50;
增粘橡胶:20-40;
微粉二氧化硅:50-200;
增强树脂:10-20;
硫化剂:0.5-1.5;
纳米二氧化钛:4-6;
纳米钛白粉:3-50。
2.根据权利要求1所述的一种自粘性纳米PET胶带,其特征在于,所述的基础橡胶为丁基橡胶。
3.根据权利要求1所述的一种自粘性纳米PET胶带,其特征在于,所述的基础橡胶为乙丙橡胶。
4.根据权利要求1所述的一种自粘性纳米PET胶带,其特征在于,所述的基础橡胶为硅橡胶。
5.根据权利要求1所述的一种自粘性纳米PET胶带,其特征在于,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:30;
增粘橡胶:20;
微粉二氧化硅:50;
增强树脂:10;
硫化剂:0.5;
纳米二氧化钛:4;
纳米钛白粉:3。
6.根据权利要求1所述的一种自粘性纳米PET胶带,其特征在于,按质量份数计,其包括以下配比的成分:
基础橡胶:100;
纳米银:50;
增粘橡胶:40;
微粉二氧化硅:200;
增强树脂:20;
硫化剂:1.5;
纳米二氧化钛:4-6;
纳米钛白粉:50。