CN104291747A - 一种高强度节能保温墙板及其制备方法 - Google Patents
一种高强度节能保温墙板及其制备方法 Download PDFInfo
- Publication number
- CN104291747A CN104291747A CN201410460011.8A CN201410460011A CN104291747A CN 104291747 A CN104291747 A CN 104291747A CN 201410460011 A CN201410460011 A CN 201410460011A CN 104291747 A CN104291747 A CN 104291747A
- Authority
- CN
- China
- Prior art keywords
- parts
- stir
- slurry
- activated carbon
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种高强度节能保温墙板,由下列重量份的原料制成:橡胶颗粒2-3、聚羧酸减水剂1-2、过碳酸钠1-2、氢化蓖麻油酸0.5-0.8、二烷基二硫代磷酸锌0.8-1.2、煤灰5-8、聚苯乙烯微球4-6、铁矿渣3-5、粉煤灰15-20、碳酸钠1-1.3、贝壳粉1-1.3、十二烷基硫酸钠1-2、高粘凹凸棒石粘土粉5-7、聚萘甲醛磺酸钠盐1-1.3、耐碱玻璃纤维网格布适量、改性活性炭25-30、水适量;本发明保温墙板通过使用铁矿渣、煤灰制作多孔的填料,配合使用聚氯乙烯微球,不仅减轻了墙体的重量,结合紧密,还能增加墙板的韧性,提高消音降噪功能,还减少了环境污染,节约了能源。
Description
技术领域
本发明属于建筑材料领域,尤其涉及一种高强度节能保温墙板及其制备方法。
背景技术
随着建筑业的蓬勃发展,能源的不断枯竭,还有全球变暖的影响,降低建筑能耗,提高能源利用率,已受到全社会的关注和重视。目前建筑用的保温材料性能良莠不齐,存在强度低、保温性不够好、价格高、耐久性差、耐水和耐腐蚀性不好、对环境有污染、阻燃性不好等缺点,需要进行改进。
活性炭具有质量轻,孔隙发达,吸附性好的特点,如果加入保温材料中,不仅具有良好的保温性能。活性炭具有良好的吸附性能,能够吸附有益的物质、气味,再缓慢释放,起到有益于健康的作用。
发明内容
本发明的目的在于提供一种高强度节能保温墙板及其制备方法,该保温墙板不仅减轻了墙体的重量,还能增加墙板的韧性,提高消音降噪功能,还减少了环境污染,节约了能源。
本发明的技术方案如下:
一种高强度节能保温墙板,其特征在于由下列重量份的原料制成:橡胶颗粒2-3、聚羧酸减水剂1-2、过碳酸钠1-2、氢化蓖麻油酸0.5-0.8、二烷基二硫代磷酸锌0.8-1.2、煤灰5-8、聚苯乙烯微球4-6、铁矿渣3-5、粉煤灰15-20、碳酸钠1-1.3、贝壳粉1-1.3、十二烷基硫酸钠1-2、高粘凹凸棒石粘土粉5-7、聚萘甲醛磺酸钠盐1-1.3、耐碱玻璃纤维网格布适量、改性活性炭25-30、水适量;
所述改性活性炭由下列重量份的原料制成:艾叶2-3、茶树叶2-3、樟树皮2-3、硅藻土2-3、檀木碎屑3-5、50-60%乙醇水溶液适量、活性炭20-25、硅烷偶联剂KH-550 0.5-0.7;制备方法为:将艾叶、茶树叶、樟树皮、檀木碎屑粉碎,加入25-30倍重量的50-60%乙醇水溶液,加热至70-80℃,搅拌30-40分钟,过滤得浆料,加入硅藻土,搅拌均匀;将活性炭粉碎成1-5mm的颗粒,加入所述浆料中,浸泡6-8个小时,烘干备用;将硅烷偶联剂KH-550加入5-6倍重量的50-60%乙醇水溶液,搅拌均匀,再均匀地喷洒在活性炭颗粒表面,边烘干边不停翻动活性炭颗粒,防止粘连,烘干至绝干,即得。
所述的高强度节能保温墙板的制备方法,其特征在于包括以下步骤:
(1)将煤灰、铁矿渣、高粘凹凸棒石粘土粉、贝壳粉混合,粉碎成100-200目颗粒,加入7-9%重量份的水,造粒,粒径在3-9mm,送入煅烧炉中,在300-400℃下预烧10-20分钟,在800-1000℃下烧结,取出得到颗粒;
(2)将水泥、橡胶颗粒、聚羧酸减水剂、聚苯乙烯微球、活性硅酸钙、改性活性炭、第(1)步得到的颗粒混合,送入砂浆搅拌机中搅拌均匀,按照水料比为0.3-0.5加入水,搅拌均匀得到浆料;
(3)将除碳酸钠、过碳酸钠、十二烷基硫酸钠以外的其他剩余成分混合,加入第(2)步得到的浆料中搅拌均匀,加入碳酸钠、过碳酸钠、十二烷基硫酸钠,搅拌均匀,得到保温芯材浆料;
(4)将墙板模具底层涂布一层耐碱玻璃纤维网格布,将保温芯材浆料浇筑到模具中,校平,再在上面涂布一层耐碱玻璃纤维网格布,经振捣成型、发泡、脱模、养护,即得。
本发明的有益效果
本发明保温墙板通过使用铁矿渣、煤灰制作多孔的填料,配合使用聚氯乙烯微球,不仅减轻了墙体的重量,结合紧密,还能增加墙板的韧性,提高消音降噪功能,还减少了环境污染,节约了能源;通过使用改性活性炭,增加了保温性能,还具有持久抗菌、释放香气、有益人体健康的效果。
具体实施方式
一种高强度节能保温墙板,由下列重量份(公斤)的原料制成:橡胶颗粒2.5、聚羧酸减水剂1.5、过碳酸钠1.5、氢化蓖麻油酸0.6、二烷基二硫代磷酸锌1、煤灰6、聚苯乙烯微球5、铁矿渣4、粉煤灰17、碳酸钠1.2、贝壳粉1.2、十二烷基硫酸钠1.5、高粘凹凸棒石粘土粉6、聚萘甲醛磺酸钠盐1.2、耐碱玻璃纤维网格布适量、改性活性炭28、水适量;
所述改性活性炭由下列重量份(公斤)的原料制成:艾叶2.5、茶树叶2.5、樟树皮2.5、硅藻土2.5、檀木碎屑4、55%乙醇水溶液适量、活性炭23、硅烷偶联剂KH-550 0.6;制备方法为:将艾叶、茶树叶、樟树皮、檀木碎屑粉碎,加入28倍重量的55%乙醇水溶液,加热至75℃,搅拌35分钟,过滤得浆料,加入硅藻土,搅拌均匀;将活性炭粉碎成1-5mm的颗粒,加入所述浆料中,浸泡7个小时,烘干备用;将硅烷偶联剂KH-550加入5.5倍重量的55%乙醇水溶液,搅拌均匀,再均匀地喷洒在活性炭颗粒表面,边烘干边不停翻动活性炭颗粒,防止粘连,烘干至绝干,即得。
所述的高强度节能保温墙板的制备方法,包括以下步骤:
(1)将煤灰、铁矿渣、高粘凹凸棒石粘土粉、贝壳粉混合,粉碎成100-200目颗粒,加入8%重量份的水,造粒,粒径在3-9mm,送入煅烧炉中,在350℃下预烧15分钟,在900℃下烧结,取出得到颗粒;
(2)将水泥、橡胶颗粒、聚羧酸减水剂、聚苯乙烯微球、活性硅酸钙、改性活性炭、第(1)步得到的颗粒混合,送入砂浆搅拌机中搅拌均匀,按照水料比为0.4加入水,搅拌均匀得到浆料;
(3)将除碳酸钠、过碳酸钠、十二烷基硫酸钠以外的其他剩余成分混合,加入第(2)步得到的浆料中搅拌均匀,加入碳酸钠、过碳酸钠、十二烷基硫酸钠,搅拌均匀,得到保温芯材浆料;
(4)将墙板模具底层涂布一层耐碱玻璃纤维网格布,将保温芯材浆料浇筑到模具中,校平,再在上面涂布一层耐碱玻璃纤维网格布,经振捣成型、发泡、脱模、养护,即得。
实验数据:
测得厚度为120mm的保温墙板的性能如下:抗冲击性能(次)为17,抗弯破坏载荷(自重倍数)≥5,吊挂力(N)为1697,传热系数为0.49b/w/m.k,空气声隔声量(dB)为63,抗压强度(MPa)为6.4。
Claims (2)
1.一种高强度节能保温墙板,其特征在于由下列重量份的原料制成:橡胶颗粒2-3、聚羧酸减水剂1-2、过碳酸钠1-2、氢化蓖麻油酸0.5-0.8、二烷基二硫代磷酸锌0.8-1.2、煤灰5-8、聚苯乙烯微球4-6、铁矿渣3-5、粉煤灰15-20、碳酸钠1-1.3、贝壳粉1-1.3、十二烷基硫酸钠1-2、高粘凹凸棒石粘土粉5-7、聚萘甲醛磺酸钠盐1-1.3、耐碱玻璃纤维网格布适量、改性活性炭25-30、水适量;
所述改性活性炭由下列重量份的原料制成:艾叶2-3、茶树叶2-3、樟树皮2-3、硅藻土2-3、檀木碎屑3-5、50-60%乙醇水溶液适量、活性炭20-25、硅烷偶联剂KH-550 0.5-0.7;制备方法为:将艾叶、茶树叶、樟树皮、檀木碎屑粉碎,加入25-30倍重量的50-60%乙醇水溶液,加热至70-80℃,搅拌30-40分钟,过滤得浆料,加入硅藻土,搅拌均匀;将活性炭粉碎成1-5mm的颗粒,加入所述浆料中,浸泡6-8个小时,烘干备用;将硅烷偶联剂KH-550加入5-6倍重量的50-60%乙醇水溶液,搅拌均匀,再均匀地喷洒在活性炭颗粒表面,边烘干边不停翻动活性炭颗粒,防止粘连,烘干至绝干,即得。
2.根据权利要求1所述的高强度节能保温墙板的制备方法,其特征在于包括以下步骤:
(1)将煤灰、铁矿渣、高粘凹凸棒石粘土粉、贝壳粉混合,粉碎成100-200目颗粒,加入7-9%重量份的水,造粒,粒径在3-9mm,送入煅烧炉中,在300-400℃下预烧10-20分钟,在800-1000℃下烧结,取出得到颗粒;
(2)将水泥、橡胶颗粒、聚羧酸减水剂、聚苯乙烯微球、活性硅酸钙、改性活性炭、第(1)步得到的颗粒混合,送入砂浆搅拌机中搅拌均匀,按照水料比为0.3-0.5加入水,搅拌均匀得到浆料;
(3)将除碳酸钠、过碳酸钠、十二烷基硫酸钠以外的其他剩余成分混合,加入第(2)步得到的浆料中搅拌均匀,加入碳酸钠、过碳酸钠、十二烷基硫酸钠,搅拌均匀,得到保温芯材浆料;
(4)将墙板模具底层涂布一层耐碱玻璃纤维网格布,将保温芯材浆料浇筑到模具中,校平,再在上面涂布一层耐碱玻璃纤维网格布,经振捣成型、发泡、脱模、养护,即得。