CN103666068B - A kind of energy-conserving and environment-protective UV curing inks and preparation method thereof - Google Patents

A kind of energy-conserving and environment-protective UV curing inks and preparation method thereof Download PDF

Info

Publication number
CN103666068B
CN103666068B CN201310602412.8A CN201310602412A CN103666068B CN 103666068 B CN103666068 B CN 103666068B CN 201310602412 A CN201310602412 A CN 201310602412A CN 103666068 B CN103666068 B CN 103666068B
Authority
CN
China
Prior art keywords
energy
conserving
protective
environment
curing inks
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310602412.8A
Other languages
Chinese (zh)
Other versions
CN103666068A (en
Inventor
陈可亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dongguan Haocai Ink Technology Co ltd
Original Assignee
Tongling Founder Plastics Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tongling Founder Plastics Technology Co Ltd filed Critical Tongling Founder Plastics Technology Co Ltd
Priority to CN201310602412.8A priority Critical patent/CN103666068B/en
Publication of CN103666068A publication Critical patent/CN103666068A/en
Application granted granted Critical
Publication of CN103666068B publication Critical patent/CN103666068B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of energy-conserving and environment-protective UV curing inks, it is characterized in that, be made up of the raw material of following weight part: pigment dyestuff 1-3, aminoresin 20-23, bicarbonate of ammonia 1-2, zeolite 1-2, ethylene glycol ether acetate 13-15, isoamyl butyrate 11-13, Viscoat 295 12-14, cobalt naphthenate 1-1.1, dibutyl tin laurate 1-2, tri (propylene glycol) diacrylate 10-12, ethyl acetate 5-8, UV epoxy acrylate 10-12, 1173 light trigger 4-8, trifluoroacetylacetone europium 4-5, vulcabond 5-6, auxiliary agent 4-5, it once can be imprinted in gold and silver paperboard or PVC card by screen painting mode by ink of the present invention, improves production efficiency, has saved the energy, and not containing solvent, alleviates the infringement to human body and environmental pollution.

Description

A kind of energy-conserving and environment-protective UV curing inks and preparation method thereof
Technical field
The present invention relates to a kind of ink and preparation method thereof, particularly a kind of energy-conserving and environment-protective UV curing inks and preparation method thereof.
Background technology
Ultraviolet light polymerization (UV) ink refers under uviolizing, utilizes the UV-light of different wave length and energy to make ink film forming and dry ink.Utilize different UV spectrum, can different-energy be produced, the monomer polymerization in different ink vehicle is become polymkeric substance, so the look film of UV ink has good machinery and chemical property.The major advantage of UV ink has: (1) is without solvent; (2) rate of drying is fast, and power consumption is few; (3) good luster, bright in luster; (4) water-fast, solvent resistant, wear resisting property is good.In UV ink, light trigger is that one is subject to light activated compound, after absorb light is shone, be excited into free radical, and energy trasfer, to photosensitivity molecule or photocrosslinking agent, makes UV ink that photocuring reaction occur.Current UV ink has become a kind of more ripe ink technology, and its pollutant emission is almost nil.UV curable ink due in system not containing solvent, there is efficient, wide adaptability, economy, energy-conservation, environmental friendliness, become tool novel ink with broad prospects for development.
Summary of the invention
The object of this invention is to provide a kind of energy-conserving and environment-protective UV curing inks and preparation method thereof.
In order to realize object of the present invention, the present invention is by following scheme implementation:
A kind of energy-conserving and environment-protective UV curing inks, is made up of the raw material of following weight part: pigment dyestuff 1-3, aminoresin 20-23, bicarbonate of ammonia 1-2, zeolite 1-2, ethylene glycol ether acetate 13-15, isoamyl butyrate 11-13, Viscoat 295 12-14, cobalt naphthenate 1-1.1, dibutyl tin laurate 1-2, tri (propylene glycol) diacrylate 10-12, ethyl acetate 5-8, UV epoxy acrylate 10-12,1173 light trigger 4-8, trifluoroacetylacetone europium 4-5, vulcabond 5-6, auxiliary agent 4-5;
Described auxiliary agent is prepared from by the raw material of following weight part: nano diatomite powder 0.2-0.3, nano mica powder 0.2-0.3, double pentaerythritol methacrylate 10-12, neopentyl glycol 5-7, p-tert-butyl benzoic acid 1-2, linking agent TAC2-3, polyisobutene 2-3, silane coupling agent KH5601-2, Tenox PG 2-3, coix seed oil 1-2; Its preparation method is by each mixing of materials, is heated to 60-70 DEG C, and stirring reaction 30-40 minute, to obtain final product.
Energy-conserving and environment-protective UV curing inks of the present invention, be made up of following concrete steps: first add pigment dyestuff, aminoresin, bicarbonate of ammonia, zeolite, ethylene glycol ether acetate, isoamyl butyrate, Viscoat 295, cobalt naphthenate, dibutyl tin laurate stirring and evenly mixing, be heated to 80-90 DEG C, stir 25-35 minute; Then all the other remaining components except 1173 light triggers are added, stirring reaction 3-5 hour; Finally be cooled to 60-70 DEG C, add 1173 light triggers, stirring reaction 40-50 minute, after cooling, grinding obtains 20-40 μm of slurry, to obtain final product.
The invention has the beneficial effects as follows: it once can be imprinted in gold and silver paperboard or PVC card by screen painting mode by ink of the present invention, improves production efficiency, has saved the energy, and not containing solvent, alleviate the infringement to human body and environmental pollution.
Specific embodiments
Below by specific examples, the present invention is described in detail.
A kind of energy-conserving and environment-protective UV curing inks, is made up of the raw material of following weight part (kilogram): pigment dyestuff 1, aminoresin 20, bicarbonate of ammonia 1, zeolite 1, ethylene glycol ether acetate 13, isoamyl butyrate 11, Viscoat 295 12, cobalt naphthenate 1, dibutyl tin laurate 1, tri (propylene glycol) diacrylate 10, ethyl acetate 5, UV epoxy acrylate 10,1173 light trigger 4, trifluoroacetylacetone europium 4, vulcabond 5, auxiliary agent 4;
Described auxiliary agent is prepared from by the raw material of following weight part (kilogram): nano diatomite powder 0.2, nano mica powder 0.2, double pentaerythritol methacrylate 10, neopentyl glycol 5, p-tert-butyl benzoic acid 1, linking agent TAC2, polyisobutene 2, silane coupling agent KH5601, Tenox PG 2, coix seed oil 1; Its preparation method is by each mixing of materials, is heated to 60-70 DEG C, and stirring reaction 30-40 minute, to obtain final product.
Energy-conserving and environment-protective UV curing inks of the present invention, be made up of following concrete steps: first add pigment dyestuff, aminoresin, bicarbonate of ammonia, zeolite, ethylene glycol ether acetate, isoamyl butyrate, Viscoat 295, cobalt naphthenate, dibutyl tin laurate stirring and evenly mixing, be heated to 80-90 DEG C, stir 25-35 minute; Then all the other remaining components except 1173 light triggers are added, stirring reaction 3-5 hour; Finally be cooled to 60-70 DEG C, add 1173 light triggers, stirring reaction 40-50 minute, after cooling, grinding obtains 20-40 μm of slurry, to obtain final product.
The ink of gained, uses cross-hatching ox-hide tape stripping, draws compartment apart from 1mm, 100% attachment; Use the spirituous cotton balls of leaching, 300 grams of pressure wipings 50 times, are as good as shape; To be soaked in salad oil (normal temperature) 8 hours, to be as good as shape; Use and be soaked with the cotton balls of salt solution, 300 grams of pressure wipings 50 times, are as good as shape.

Claims (2)

1. an energy-conserving and environment-protective UV curing inks, it is characterized in that, be prepared from by the raw material of following weight part: pigment dyestuff 1-3, aminoresin 20-23, bicarbonate of ammonia 1-2, zeolite 1-2, ethylene glycol ether acetate 13-15, isoamyl butyrate 11-13, Viscoat 295 12-14, cobalt naphthenate 1-1.1, dibutyl tin laurate 1-2, tri (propylene glycol) diacrylate 10-12, ethyl acetate 5-8, UV epoxy acrylate 10-12,1173 light trigger 4-8, trifluoroacetylacetone europium 4-5, vulcabond 5-6, auxiliary agent 4-5;
Described auxiliary agent is prepared from by the raw material of following weight part: nano diatomite powder 0.2-0.3, nano mica powder 0.2-0.3, double pentaerythritol methacrylate 10-12, neopentyl glycol 5-7, p-tert-butyl benzoic acid 1-2, linking agent TAC2-3, polyisobutene 2-3, silane coupling agent KH5601-2, Tenox PG 2-3, coix seed oil 1-2; Its preparation method is by each mixing of materials, is heated to 60-70 DEG C, and stirring reaction 30-40 minute, to obtain final product.
2. energy-conserving and environment-protective UV curing inks according to claim 1, it is characterized in that, be made up of following concrete steps: first add pigment dyestuff, aminoresin, bicarbonate of ammonia, zeolite, ethylene glycol ether acetate, isoamyl butyrate, Viscoat 295, cobalt naphthenate, dibutyl tin laurate stirring and evenly mixing, be heated to 80-90 DEG C, stir 25-35 minute; Then all the other remaining components except 1173 light triggers are added, stirring reaction 3-5 hour; Finally be cooled to 60-70 DEG C, add 1173 light triggers, stirring reaction 40-50 minute, after cooling, grinding obtains 20-40 μm of slurry, to obtain final product.
CN201310602412.8A 2013-11-25 2013-11-25 A kind of energy-conserving and environment-protective UV curing inks and preparation method thereof Active CN103666068B (en)