CN102601975A - 一种采用螺杆挤出机连续制备液体再生胶的方法 - Google Patents
一种采用螺杆挤出机连续制备液体再生胶的方法 Download PDFInfo
- Publication number
- CN102601975A CN102601975A CN2012100694174A CN201210069417A CN102601975A CN 102601975 A CN102601975 A CN 102601975A CN 2012100694174 A CN2012100694174 A CN 2012100694174A CN 201210069417 A CN201210069417 A CN 201210069417A CN 102601975 A CN102601975 A CN 102601975A
- Authority
- CN
- China
- Prior art keywords
- screw extruder
- rubber
- reclaimed rubber
- liquid reclaimed
- shoddy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (4)