CN102515839B - 一种石材仿古做旧方法 - Google Patents

一种石材仿古做旧方法 Download PDF

Info

Publication number
CN102515839B
CN102515839B CN201110411040.1A CN201110411040A CN102515839B CN 102515839 B CN102515839 B CN 102515839B CN 201110411040 A CN201110411040 A CN 201110411040A CN 102515839 B CN102515839 B CN 102515839B
Authority
CN
China
Prior art keywords
stone
antique
paint
finish method
weight ratio
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201110411040.1A
Other languages
English (en)
Other versions
CN102515839A (zh
Inventor
李寿仁
陈伟江
边华锋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HANGZHOU LANDSCAPING Inc
Original Assignee
HANGZHOU LANDSCAPING Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HANGZHOU LANDSCAPING Inc filed Critical HANGZHOU LANDSCAPING Inc
Priority to CN201110411040.1A priority Critical patent/CN102515839B/zh
Publication of CN102515839A publication Critical patent/CN102515839A/zh
Application granted granted Critical
Publication of CN102515839B publication Critical patent/CN102515839B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明属于石材铺设施工工艺技术领域,具体涉及一种石材仿古做旧方法,其步骤为:1)将已铺装的石材清洁干燥;2)将液体石蜡、黑色油漆和红色油漆按80-120:3-7:0.7-1.3的重量比配制呈着色剂;3)选择天晴,将着色剂均匀涂抹在清洁干燥后的石材上,2分钟后将多余涂料擦干净;4)日晒2-3天即得到仿古做旧后的石材。本发明是在对天然石材的物理结构的分析,为板材着色提供了理论依据,并通过有机物着色做旧仿古处理,使石材符合一定的景观氛围,同时可以修复工程的材质与原留有的材料相协调。

Description

一种石材仿古做旧方法
技术领域
本发明属于石材铺设施工工艺技术领域,具体涉及一种石材仿古做旧方法。
背景技术
新开采的石材,加工而成的板材或其它工艺品,在某些特定的景观氛围中或修复工程中,显得唐突不协调。仿古做旧工艺是运用一系列工艺手法和色调的变换将新的板材或工艺品模仿成很久以前的材料产品,在新的材料产品上赋予漫长的历史印记。
天然石材结晶相对较粗,存在许多肉眼看不到的毛细管,花岗岩细孔率为0.5~1.5%,大理石细孔率为0.5~2.0%。天然石材的这种特性及毛细孔的存在,为有机着色物质的渗入提供了环境条件。有机着色物质的渗入天然石材、砖体后,经日晒封皮,达到保持色彩的目的。
发明内容
本发明为了解决上述现有技术存在的缺陷和不足,提供了一种为石材着色,使石材符合一定的景观氛围,同时可以修复工程的材质与原留有的材料相协调的石材仿古做旧方法。
本发明的技术方案:一种石材仿古做旧方法,其步骤为:
1)将已铺装的石材清洁干燥;
2)将液体石蜡、黑色油漆和红色油漆按80-120:3-7:0.7-1.3的重量比配制呈着色剂;
3)选择天晴,将着色剂均匀涂抹在清洁干燥后的石材上,2分钟后将多余涂料擦干净;
4)日晒2-3天即得到仿古做旧后的石材。
优选地,步骤1)中铺装好的石材可以为花岗岩板材、台阶或者清水墙体中的一种。
优选地,步骤2)中的用于配制着色剂的液体石蜡、黑色油漆和红色油漆的重量比为100:5:1。
优选地,步骤2)中的用于配制着色剂的液体石蜡、黑色油漆和红色油漆的重量比为90:4:0.9。
优选地,步骤2)中的用于配制着色剂的液体石蜡、黑色油漆和红色油漆的重量比为110:6:1.1。
本发明是在对天然石材的物理结构的分析,为板材着色提供了理论依据,并通过有机物着色做旧仿古处理,使石材符合一定的景观氛围,同时可以修复工程的材质与原留有的材料相协调。
具体实施方式
下面结合实施例对本发明作进一步详细的说明,但并不是对本发明保护范围的限制。
实施例1
因景观氛围需要,对河埠头踏步、铺地及压顶、塔身进行了做旧处理。芝麻灰花岗铺地板材及压顶材料,铺贴安装后清洁干燥,将液体石蜡、黑色油漆、红色油漆按100:5:1的配合比例制作着色剂,均匀涂抹2分钟后擦干净多余涂料,日晒封皮二天并做好成品保护。祭塔完工后,对塔身清水墙体进行清洁,再用着色剂均匀涂抹,2分钟后将多余涂料擦干净。经做旧处理,达到了预期的景观效果。
实施例2
在古石桥修复时,换补上桥面花岗岩板材后,新花岗岩材料与原有桥体的颜色、质感格格不入。在清洁新换补上桥面花岗岩板材后,将液体石蜡、黑色油漆、红色油漆按90:4:0.9的配合比例制作着色剂,均匀涂抹2分钟后擦干净多余涂料,使新用材料的材质与原留有的材料相协调。
实施例3
明清古建筑的石器构件、附属物摆设,由新矿石料雕刻而成的,质感轻新,与建筑的历史年代感不相协调。在新雕刻的石器构件、附属物摆设表面,经清洁处理后,将液体石蜡、黑色油漆、红色油漆按110:6:1.1的配合比例制作着色剂,均匀涂抹2分钟后擦干净多余涂料,使新的石器上赋予漫长的历史印记。 

Claims (6)

1.一种石材仿古做旧方法,其特征在于:其步骤为:
1)将已铺装的石材清洁干燥;
2)将液体石蜡、黑色油漆和红色油漆按80-120:3-7:0.7-1.3的重量比配制成着色剂;
3)选择天晴,将着色剂均匀涂抹在清洁干燥后的石材上,2分钟后将多余涂料擦干净;
4)日晒2-3天即得到仿古做旧后的石材。
2.根据权利要求1所述的一种石材仿古做旧方法,其特征在于:步骤1)中铺装好的石材可以为花岗岩板材、台阶或者清水墙体中的一种。
3.根据权利要求1所述的一种石材仿古做旧方法,其特征在于:步骤1)中铺装好的石材可以为大理石板材、台阶或者清水墙体中的一种。
4.根据权利要求1所述的一种石材仿古做旧方法,其特征在于:步骤2)中的用于配制着色剂的液体石蜡、黑色油漆和红色油漆的重量比为100:5:1。
5.根据权利要求1所述的一种石材仿古做旧方法,其特征在于:步骤2)中的用于配制着色剂的液体石蜡、黑色油漆和红色油漆的重量比为90:4:0.9。
6.根据权利要求1所述的一种石材仿古做旧方法,其特征在于:步骤2)中的用于配制着色剂的液体石蜡、黑色油漆和红色油漆的重量比为110:6:1.1。
CN201110411040.1A 2011-12-12 2011-12-12 一种石材仿古做旧方法 Active CN102515839B (zh)