CN102248490A - 一种汽车地毯的生产方法 - Google Patents

一种汽车地毯的生产方法 Download PDF

Info

Publication number
CN102248490A
CN102248490A CN2011101405321A CN201110140532A CN102248490A CN 102248490 A CN102248490 A CN 102248490A CN 2011101405321 A CN2011101405321 A CN 2011101405321A CN 201110140532 A CN201110140532 A CN 201110140532A CN 102248490 A CN102248490 A CN 102248490A
Authority
CN
China
Prior art keywords
carpet
water cutter
cutting
pvc
car carpeting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011101405321A
Other languages
English (en)
Inventor
叶佳乐
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuxi Jixing Auto Acoustic Parts Technology Co Ltd
Original Assignee
Wuxi Jixing Auto Acoustic Parts Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuxi Jixing Auto Acoustic Parts Technology Co Ltd filed Critical Wuxi Jixing Auto Acoustic Parts Technology Co Ltd
Priority to CN2011101405321A priority Critical patent/CN102248490A/zh
Publication of CN102248490A publication Critical patent/CN102248490A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种汽车地毯的生产方法,属于汽车内饰件加工技术领域。本发明选用PVC与XPE发泡复合型材料为基材,根据水刀切割治具上限位装置,将基材平铺在水刀切割治具上;将基材进行定位后用水刀切割,得到所需汽车地毯;检验所得汽车地毯后,装箱入库。本发明的方法解决了地毯总成的吸音、隔音、环保、轻量化等性能指标;大大降低了地毯重量,满足了整车轻量化设计的要求;选用PVC与XPE发泡复合型材料使原材料成本减低,并具有选择性;在材料加工过程中,采用双刀头水刀进行切割,工艺稳定,确保了操作的安全性和准确度,同时提升了作业效率;产品不会折断;途中没有半成品堆积,节约了制造成本;产品整个生产过程没有有害物质产生。

Description

一种汽车地毯的生产方法
技术领域
本发明涉及一种汽车地毯的生产方法,具体地说是用于安装在汽车底盘上方且具有隔音、吸音作用的汽车地毯的生产方法,属于汽车内饰件加工技术领域。 
背景技术
汽车地毯安装在汽车底盘上方,起到隔音与吸音作用。在越来越追求高性能、环保型、节能型、轻量化、个性化的时代,汽车的内饰与汽车的外形一样,成为人们选购汽车的一个重要因素。因此对汽车内饰件的要求也越来越高。在现有技术中,地毯的高吸音、高隔音、低克重、环保等性能指标成为瓶颈,制约着汽车地毯的发展。现有地毯主要存在着以下问题:1、吸音指标达不到要求;2、隔音指标达不到要求;3、产品材料不环保;5、产品重量大,不利于整车轻量化,节能。 
发明内容
本发明的目的是克服现有技术中存在的不足,从而提供一种能降低产品重量、节能环保,强度高、能大大降低生产过程中工人的劳动强度、没有有害物质产生,并能提高生产效率的汽车地毯的生产方法。 
按照本发明提供的技术方案,所述汽车地毯的生产方法包括如下步骤: 
(a)、原材料铺放:选用PVC与XPE发泡复合型材料为基材,根据水刀切割治具的上限位装置,平铺在水刀切割治具上;
(b)、水刀切割:将原材料进行定位,按所需尺寸进行水刀切割,得到所需汽车地毯;切割水压为40000~50000psi,切割气压为0.6~0.8MPa;
(c)、检验:检验确保汽车地毯表面平整,无损伤、破裂、皱折等缺陷;经检验过的地毯依包装技术标准准确装箱。
所述PVC与XPE发泡复合型材料购自江阴市海江高分子材料有限公司,每块基材密度240-250㎏/m3,按重量百分比计算,PVC材料含量为70%-90%,XPE发泡材料含量为10%-30%。 
所述水刀为双刀头水刀。 
本发明与现有技术相比具有如下优点:本发明的方法解决了地毯总成的吸音、隔音、环保、轻量化等性能指标;大大降低了地毯重量,满足了整车轻量化设计的要求;选用PVC与XPE发泡复合型材料使原材料成本减低,并具有选择性;在材料加工过程中,采用双刀头水刀进行切割,工艺稳定,确保了操作的安全性和准确度,同时提升了作业效率;产品不会折断;途中没有半成品堆积,节约了制造成本;产品整个生产过程没有有害物质产生。 
具体实施方式
下面结合具体实施例对本发明作进一步说明。 
实施例1 
生产郑州日产C16A后地毯,其规格为:L1600×W1400mm。
所述地毯的生产工艺步骤如下: 
所述PVC与XPE发泡复合型材料购自常州市中复丽宝第复合材料有限公司,每块基材密度246㎏/m3,按重量百分比计算,PVC材料含量为90%,XPE发泡材料含量为10%。
(a)、原材料铺放:选用PVC与XPE发泡复合型材料为基材,根据水刀切割治具的上限位装置,平铺在水刀切割治具上; 
(b)、水刀切割:将原材料进行定位,按所需尺寸进行水刀切割,得到所需汽车地毯;切割水压为40000~50000psi,切割气压为0.6~0.8MPa;
(c)、检验:检验确保汽车地毯表面平整,无损伤、破裂、皱折等缺陷;经检验过的地毯依包装技术标准准确装箱,按60套/箱入库。
实施例2 
生产东风股份中宽车前地毯,其规格为:L1650×W800mm。
所述地毯的生产工艺步骤如下: 
所述PVC与XPE发泡复合型材料购自江阴市海江高分子材料有限公司,每块基材密度246㎏/m3,按重量百分比计算,PVC材料含量为80%,XPE发泡材料含量为20%。
(a)、原材料铺放:选用PVC与XPE发泡复合型材料为基材,根据水刀切割治具的上限位装置,平铺在水刀切割治具上; 
(b)、水刀切割:将原材料进行定位,按所需尺寸进行水刀切割,得到所需汽车地毯;切割水压为40000~50000psi,切割气压为0.6~0.8MPa;
(c)、检验:检验确保汽车地毯表面平整,无损伤、破裂、皱折等缺陷;经检验过的地毯依包装技术标准准确装箱,按50套/箱入库。
实施例3 
生产东风股份中宽车后地毯,其规格为:L1650×W1100mm。
所述PVC与XPE发泡复合型材料购自江阴市海江高分子材料有限公司,每块基材密度246㎏/m3,按重量百分比计算,PVC材料含量为80%,XPE发泡材料含量为20%。 
(a)、原材料铺放:选用PVC与XPE发泡复合型材料为基材,根据水刀切割治具的上限位装置,平铺在水刀切割治具上; 
(b)、水刀切割:将原材料进行定位,按所需尺寸进行水刀切割,得到所需汽车地毯;切割水压为40000~50000psi,切割气压为0.6~0.8MPa;
(c)、检验:检验确保汽车地毯表面平整,无损伤、破裂、皱折等缺陷;经检验过的地毯依包装技术标准准确装箱,按50套/箱入库。

Claims (3)

1. 一种汽车地毯的生产方法,其特征在于所述生产方法包括如下步骤:
(a)、原材料铺放:选用PVC与XPE发泡复合型材料为基材,平铺在水刀切割治具上;
(b)、水刀切割:将原材料进行定位,按所需尺寸进行水刀切割,得到所需汽车地毯;切割水压为40000-50000psi,切割气压为0.6-0.8MPa;
(c)、检验:检验确保汽车地毯表面平整,无损伤、破裂、皱折等缺陷;经检验合格装箱。
2.根据权利要求1所述的汽车地毯的生产方法,其特征在于所述PVC与XPE发泡复合型材料每块基材密度240-250㎏/m3
3.根据权利要求1所述的汽车地毯的生产方法,其特征在于所述水刀为双刀头水刀。
CN2011101405321A 2011-05-28 2011-05-28 一种汽车地毯的生产方法 Pending CN102248490A (zh)