CN101985544A - 一种丁基橡胶密封胶带及其制备方法 - Google Patents

一种丁基橡胶密封胶带及其制备方法 Download PDF

Info

Publication number
CN101985544A
CN101985544A CN2010105420951A CN201010542095A CN101985544A CN 101985544 A CN101985544 A CN 101985544A CN 2010105420951 A CN2010105420951 A CN 2010105420951A CN 201010542095 A CN201010542095 A CN 201010542095A CN 101985544 A CN101985544 A CN 101985544A
Authority
CN
China
Prior art keywords
butyl rubber
preparation
rubber sealant
sealant band
sealing adhesive
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2010105420951A
Other languages
English (en)
Other versions
CN101985544B (zh
Inventor
邵双喜
杨建平
周国权
蒋岚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Ningbo University of Technology
Original Assignee
Ningbo University of Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ningbo University of Technology filed Critical Ningbo University of Technology
Priority to CN 201010542095 priority Critical patent/CN101985544B/zh
Publication of CN101985544A publication Critical patent/CN101985544A/zh
Application granted granted Critical
Publication of CN101985544B publication Critical patent/CN101985544B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供一种丁基橡胶密封胶带及其制备方法,属于密封胶带及其制备技术领域。其特点是以丁基橡胶等为基本原料,添加废弃皮革粉为填充增强剂,通过反复混炼、捏合、挤出成型、切割成条块状、隔离纸包装成品。该产品原料易得,成本较低,制造工艺简单,性能指标达到和超过现有同类产品指标;不仅如此,产品应用废弃皮革粉为原料,属于废弃物资源化再利用,其环境生态及社会效益明显。

Description

一种丁基橡胶密封胶带及其制备方法
技术领域
本发明属于密封胶带及其制备技术领域,同时涉及废弃皮革粉的再生资源化利用的技术方法。
背景技术
丁基橡胶具有优良的气密性和良好的粘接性、耐低温、耐老化等特性,而广泛应用于防水气密、减震粘接密封等方面。如文化用品粘接、建筑材料粘接密封防水、机器设备减震粘接密封、材料接缝气密粘接等等,普遍认为是一类使用方便、用途广泛、安全可靠、经济实用的粘接密封材料。
通常,以丁基橡胶为主制备非硫化密封胶带,需要添加补强剂炭黑和大量有机溶剂,使用过程中环境污染不容忽视。为此,中国发明专利ZL00123581.8提供了一种彩色、高性能、压敏型丁基橡胶密封粘接胶带,采用纳米及准纳米二氧化硅做补强剂的方案。
另外,我国的制革产量已占全球的23%左右,皮革又是轻工业出口的主要行业。在皮革制造中,动物皮的制革利用率不到90%,多于10%的皮胶原作为边角下脚料废弃。不计废弃的破旧损坏的皮革制品,仅制革生产过程中每年约有20万吨(干基)废弃的动物皮胶原资源尚待利用,废弃物总量非常可观。然而,围绕废弃皮革的再生资源化利用技术,仍处于初级阶段;人们追求资源与环境的和谐,实现循环经济模式的资源节约型社会目标任重而道远。
发明内容
本发明主要目的是提供一种丁基橡胶密封胶带及其制备方法。
为实现本发明主要目的的技术方案:以废弃皮革粉为填充增强剂,马来酸酐为助剂,制备高强度非硫化型丁基橡胶密封胶带。
本发明丁基橡胶密封胶带,由以下原料组成及其份量(按重量计)组成:丁基橡胶10-15份、皮革粉2-10份、聚异丁烯10-18份、轻质碳酸钙45-60份、沉淀法二氧化硅3-8份、增塑剂3-8份、着色剂3-8份、马来酸酐0.1-3份和防老剂1-3份。
本发明所采用的皮革粉来自制革厂的铬鞣猪牛羊皮下脚废料,含铬量小于5%,粉碎成粒度为40-400目的粉末。
本发明所采用的增塑剂包括古马隆树脂、环烷油、邻苯二甲酸二辛酯其中的一种或者一种以上物质。
本发明所采用的着色剂包括炭黑、氰兰、铁红、永固黄、塑料红其中的一种或者一种以上物质。
本发明所采用的防老剂包括防老剂MB,化学名为二巯基苯并咪唑;或防老剂RD,化学名为2,2,4三甲基1,2二氢化喹啉聚合物;或两者的混合物。
本发明丁基橡胶密封胶带的制备方法如下:所述的丁基橡胶密封胶带经过所述份量各组成的混炼、捏合、挤出成型、切割成条块状、隔离纸包装成品。
本发明的积极效果在于:利用制革厂铬鞣革屑、边角废料等,将其粉碎成粒度为40-400目的皮革粉,作为丁基橡胶密封胶带组成的填充增强剂,并获得强度较高、成本较低的密封胶带产品。不仅产品性能指标达到和超过现有同类产品指标,且应用废弃皮革粉为原料,属于废弃物资源化的再生利用,其环境生态及社会效益明显。
具体实施方式
以下实施例是对本发明的进一步的说明,但是并不限制本发明的范围。
实施例1
取3.0Kg素炼后的丁基橡胶,加人1.6Kg皮革粉和0.02Kg马来酸酐混合均匀20分钟后,加入2.0Kg聚异丁烯、15.0Kg轻质碳酸钙、1.8Kg沉淀法二氧化硅、0.5Kg古马隆树脂、0.6Kg环烷油、1.2Kg炭黑和0.6Kg防老剂RD的混合物,使物料充分混合,控制开炼机辊温80℃,再捏合30分钟后出料。
捏合完毕,将炼好的胶割成30×300mm左右的条状,摊晾至室温。
将晾至室温的胶条送进挤出机,按要求挤出成型,切割成规整条块,隔离纸包装或打卷成品。
实施例2
取5.0Kg素炼后的丁基橡胶,加入2.8Kg皮革粉和0.8Kg马来酸酐混合均匀20分钟后,加入5.0Kg聚异丁烯、20.0Kg轻质碳酸钙、2.8Kg沉淀法二氧化硅、2.6Kg环烷油、1.2Kg氰兰、1.4Kg铁红和1.0Kg防老剂MB的混合物,使物料充分混合,控制开炼机辊温80℃,再捏合30分钟后出料。
捏合完毕,将炼好的胶割成30×300mm左右的条状,摊晾至室温。
将晾至室温的胶条送进挤出机,按要求挤出成型,切割成规整条块,隔离纸包装或打卷成品。
实施例3
取4.0Kg素炼后的丁基橡胶,加人0.8Kg皮革粉和0.03Kg马来酸酐混合均匀20分钟后,加入4.0Kg聚异丁烯、18.0Kg轻质碳酸钙、1.0Kg沉淀法二氧化硅、0.8Kg古马隆树脂、1.0Kg邻苯二甲酸二辛酯、0.6Kg永固黄、1.2Kg塑料红和0.8Kg防老剂RD的混合物,使物料充分混合,控制开炼机辊温80℃,再捏合30分钟后出料。
捏合完毕,将炼好的胶割成30×300mm左右的条状,摊晾至室温。
将晾至室温的胶条送进挤出机,按要求挤出成型,切割成规整条块,隔离纸包装或打卷成品。
实施例4
取3.5Kg素炼后的丁基橡胶,加人2.0Kg皮革粉和0.05Kg马来酸酐混合均匀20分钟后,加入3.0Kg聚异丁烯、15.0Kg轻质碳酸钙、2.2Kg沉淀法二氧化硅、1.5Kg古马隆树脂、0.4Kg氰兰1.0Kg、永固黄、0.4Kg防老剂MB和0.6Kg防老剂RD的混合物,使物料充分混合,控制开炼机辊温80℃,再捏合30分钟后出料。
捏合完毕,将炼好的胶割成30×300mm左右的条状,摊晾至室温。
将晾至室温的胶条送进挤出机,按要求挤出成型,切割成规整条块,隔离纸包装或打卷成品。

Claims (6)

1.一种丁基橡胶密封胶带及其制备方法,其特征在于所述密封胶带原料组成及其份量(按重量计)如下:丁基橡胶10-15份、皮革粉2-10份、聚异丁烯10-18份、轻质碳酸钙45-60份、沉淀法二氧化硅3-8份、增塑剂3-8份、着色剂3-8份、马来酸酐0.1-3份和防老剂1-3份。
2.根据权利要求1所述丁基橡胶密封胶带,其特征在于:所述的皮革粉来自制革厂的铬鞣猪牛羊皮下脚废料,含铬量小于5%,粉碎成粒度为40-400目的粉术。
3.根据权利要求1所述丁基橡胶密封胶带,其特征在于:所述的增塑剂包括古马隆树脂、环烷油、邻苯二甲酸二辛酯其中的一种或者一种以上物质。
4.根据权利要求1所述丁基橡胶密封胶带,其特征在于:所述的着色剂包括炭黑、氰兰、铁红、永固黄、塑料红其中的一种或者一种以上物质。
5.根据权利要求1所述丁基橡胶密封胶带,其特征在于:所述的防老剂包括防老剂MB或RD或两者的混合物。
6.根据权利要求1所述丁基橡胶密封胶带的制备方法,其特征在于:所述的丁基橡胶密封胶带经过所述份量各组成的混炼、捏合、挤出成型、切割成条块状、隔离纸包装成品。
CN 201010542095 2010-11-03 2010-11-03 一种丁基橡胶密封胶带及其制备方法 Expired - Fee Related CN101985544B (zh)