CN101186723B - 运动鞋底用超耐磨橡胶配方 - Google Patents

运动鞋底用超耐磨橡胶配方 Download PDF

Info

Publication number
CN101186723B
CN101186723B CN2006101460934A CN200610146093A CN101186723B CN 101186723 B CN101186723 B CN 101186723B CN 2006101460934 A CN2006101460934 A CN 2006101460934A CN 200610146093 A CN200610146093 A CN 200610146093A CN 101186723 B CN101186723 B CN 101186723B
Authority
CN
China
Prior art keywords
parts
rubber
mass parts
agent
sports shoes
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2006101460934A
Other languages
English (en)
Other versions
CN101186723A (zh
Inventor
丁世忠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anta China Co Ltd
Original Assignee
Anta China Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anta China Co Ltd filed Critical Anta China Co Ltd
Priority to CN2006101460934A priority Critical patent/CN101186723B/zh
Publication of CN101186723A publication Critical patent/CN101186723A/zh
Application granted granted Critical
Publication of CN101186723B publication Critical patent/CN101186723B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种运动鞋底用超耐磨橡胶配方,其特征在于按质量份配方如下:聚丁二烯橡胶:80份,天然胶STR-5L:20份,均匀增粘树脂:1份,白炭黑:45-48份,软化油:3.5份,偶联剂:3-3.2份,活性剂:5.2-5.8份,硬脂酸锌:1份,防雾剂:1份,硫磺:1.9-2.1份,促进剂:1.65-1.95份,采用上述的运动鞋用橡胶配方后,可获得理想的原料功能组合,使这种运动鞋橡胶鞋底具有普通橡胶鞋底所无法比拟的超级耐磨性能,并具有良好的抗湿滑,抗冲击等多种性能。

Description

运动鞋底用超耐磨橡胶配方
技术领域
本发明涉及一种橡胶配方,特别是指一种运动鞋底用橡胶的配方。
背景技术
运动鞋由于其特殊的用途,要求其鞋底用橡胶应耐磨、抗湿滑,还要求有良好的抗冲击性,然而目前的运动鞋用橡胶技术中,由于配方的不合理性,出现了许多缺点:运动鞋在反复的弹跳、奔跑过程中,鞋底很快磨损,失去弹力,打滑。
发明内容
针对以上存在的不足之处,本发明提供一种耐磨性能优异,抗湿滑,具有良好抗冲击性能的运动鞋底用超耐磨橡胶配方。
为实现上述目的,本发明技术方案为:
运动鞋底用超耐磨橡胶配方,其特征在于:该配方主要由聚丁二烯橡胶80质量份,天然胶20质量份,增粘剂1质量份,补强剂45-48质量份,增塑剂3.5质量份,偶联剂3-3.2质量份,活性剂5.2-5.8质量份,硬脂酸1质量份,防老剂1质量份,硫化剂1.9-2.1质量份,促进剂1.65-1.95质量份组成。
所述的天然胶为STR-5L,增粘剂为均匀增粘树脂,补强剂为白炭黑,增塑剂为软化油,活性剂5.2-5.8质量份具体为:活性剂DEG 1.4-1.6质量份、活性剂PEG 2.4-2.6质量份、活性剂ZNO 1.4-1.6质量份,硬脂酸为硬脂酸锌,防老剂为防雾蜡,硫化剂为硫磺,促进剂1.65-1.95质量份具体为:促进剂DM 1.2-1.5质量份、促进剂M 0.3质量份、促进剂TS 0.15质量份。
上述技术方案的有益之处在于:
采用上述的运动鞋底用橡胶配方后,可获得理想的原料功能组合,该配方采用耐磨性能优异的聚丁二烯橡胶80质量份作为主体材料,为改善聚丁二烯橡胶加工性以及抗撕裂性能等综合性能,与具有良好综合性能的天然胶STR-5L 20质量份并用,从而提高橡胶大料本身的整体性能。
所述的均匀增粘树脂1质量份的加入,使丁二烯橡胶与天然胶STR-5L各自的分解更充分,更容易被搅匀、混合;
配方补强剂中使用白炭黑45-48质量份,可以提高橡胶的耐曲挠性,使之具有良好的曲挠耐疲劳性能;
针对白炭黑在加工过程中极易结团、分散不良的现象,使用环保型偶联剂3-3.2质量份对白炭黑改性,并同时使用增塑剂软化油3.5质量份,使白炭黑及粉末配合剂完全浸润、分散,以达到最佳效果;
防护体系使用具有优良抗氧、抗臭氧的防雾剂1质量份,其能在胶料表面形成一层腊膜,能够阻止臭氧的渗透,达到良好有防护作用;
硫化剂采用硫磺1.9-2.1质量份,活性剂DEG 1.4-1.6质量份、活性剂PEG 2.4-2.6质量份、活性剂ZNO 1.4-1.6质量份,及硬脂酸锌1质量份的配比,活化了整个的硫化体系,提高了硫化胶的交联密度并提高了硫化胶的耐热老化性能,使硫化胶的疲劳寿命提高,动态性能好。加之促进剂DM 1.2-1.5质量份、促进剂M 0.3质量份、促进剂TS 0.15质量份的作用,硫化过程更理想;以此技术方案制作的运动鞋用橡胶鞋底,具有普通橡胶鞋底所无法比拟的超级耐磨性能,并具有良好的抗湿滑,抗冲击等多种性能。
附图说明
具体实施方式
运动鞋底用超耐磨橡胶配方及一批料中最佳重量组合如表1:
  原材料名称   质量份   重量(kg)
  聚丁二烯橡胶   80   30.5
  天然胶STR-5L   20   7.5
  均匀增粘树脂   1   0.4
  白炭黑   45-48   18
  软化油   3.5   1.3
  偶联剂   3-3.2   1.2
  活性剂DEG   1.4-1.6   0.5
  活性剂PEG   2.4-2.6   1
  活性剂ZNO   1.4-1.6   0.6
  硬脂酸锌   1   0.4
  防雾剂   1   0.4
  硫磺   1.9-2.1   0.74
  促进剂DM   1.2-1.5   0.5
  促进剂M   0.3   0.12
  促进剂TS   0.15   0.06
实施上述配方后运动鞋用橡胶的检测结果如表2:
  硬度  邵尔A   72
  拉伸强度Mpa   13
  断裂伸长率%   580
  直角撕裂N/cm   63
  200%定伸强度Mpa   3
  扯断永久变形%   30
  密度g/cm3   1.15
  AKRON cm3   0.05

Claims (1)

1.运动鞋底用超耐磨橡胶,其特征在于,配方如下:
聚丁二烯橡胶:30.5kg,
天然胶STR-5L:7.5kg,
均匀增粘树脂:0.4kg,
白炭黑:18kg,
软化油:1.3kg,
偶联剂:1.2kg,
活性剂DEG:0.5kg,
活性剂PEG:1kg,
活性剂ZnO:0.6kg,
硬脂酸锌:0.4kg,
防雾剂:0.4kg,
硫磺:0.74kg,
促进剂DM:0.5kg,
促进剂M:0.12kg,
促进剂TS:0.06kg。
CN2006101460934A 2006-11-16 2006-11-16 运动鞋底用超耐磨橡胶配方 Active CN101186723B (zh)