WO2012131902A1 - シガレット巻紙の製造方法、その製造機及びシガレット巻紙 - Google Patents

シガレット巻紙の製造方法、その製造機及びシガレット巻紙 Download PDF

Info

Publication number
WO2012131902A1
WO2012131902A1 PCT/JP2011/057808 JP2011057808W WO2012131902A1 WO 2012131902 A1 WO2012131902 A1 WO 2012131902A1 JP 2011057808 W JP2011057808 W JP 2011057808W WO 2012131902 A1 WO2012131902 A1 WO 2012131902A1
Authority
WO
WIPO (PCT)
Prior art keywords
web
combustion
paper
auxiliary
cigarette
Prior art date
Application number
PCT/JP2011/057808
Other languages
English (en)
French (fr)
Inventor
圭祐 戸渡
貴文 泉屋
Original Assignee
日本たばこ産業株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 日本たばこ産業株式会社 filed Critical 日本たばこ産業株式会社
Priority to PCT/JP2011/057808 priority Critical patent/WO2012131902A1/ja
Publication of WO2012131902A1 publication Critical patent/WO2012131902A1/ja

Abstract

 紙製のウエブ(W)が走行する走行経路(2)と、該走行経路(2)上に位置し、前記ウエブ(W)の燃焼を抑制するための燃焼抑制剤を塗布するための第1の塗布装置(3)と、該第1の塗布装置(3)の下流に位置し、前記ウエブ(W)の燃焼を促進するための助燃剤(26)を塗布するための第2の塗布装置(5)と、該第2の塗布装置(5)の上流又は下流に位置し、前記燃焼抑制剤及び前記助燃剤(26)が塗布された前記ウエブ(W)を乾燥する乾燥装置(4)とを備えた。

Description

シガレット巻紙の製造方法、その製造機及びシガレット巻紙
 本発明は、低延焼性が付与されたシガレット巻紙の製造方法、その製造機及びシガレット巻紙に関する。
 近年、シガレットに使用される低延焼性巻紙が知られており、巻紙の所定領域に燃焼抑制剤が塗布されている。一般に、たばこの紙(巻紙)には抄紙工程で助燃剤が加えられている。助燃剤としては、クエン酸ナトリウムやクエン酸カリウム等の有機酸塩が付与され、これら助燃剤は燃焼を促進するため、燃焼速度の調節剤として用いられている。
 抄紙工程で助燃剤が加えられたウエブは、その後所定領域に燃焼抑制剤が帯状に塗布される。この場合、助燃剤はウエブ全域に亘って添加されているため、多くの燃焼抑制剤が必要である。また、このように抄紙工程で予め助燃剤を添加する方法は、後工程で燃焼抑制剤を添加するため、両者の量を同時に調整することはできない。
 一方、燃焼抑制剤と助燃剤とを適切な割合で巻紙に付加する方法として、燃焼抑制剤と燃焼促進剤とを混合したものを付加する技術が開示されている(例えば特許文献1参照)。詳しくは、特許文献1は、通気度減少物質(でんぷん、セルロース)、燃焼遅延物質(リン酸アンモニウム)、燃焼加速物質(カルボン酸のアルカリ金属塩又はアルカリ土類金属塩)による処理がされ、全体の喫煙間隔を一定にしようとするものである。
米国特許出願公開第2002/179105号明細書
 本発明は、紙製のウエブに対し、シガレットの品種等に応じて適切な量の助燃剤と燃焼抑制剤とをそれぞれ塗布することができるシガレット巻紙の製造方法、その製造機及びシガレット巻紙を提供することを目的とする。
 本発明では、走行経路に沿って紙製のウエブを走行させ、前記ウエブの燃焼を抑制するための燃焼抑制剤を塗布する第1の塗布工程と、前記ウエブを加熱して乾燥させるための乾燥工程とを備えたシガレット巻紙の製造方法において、前記ウエブの燃焼を促進するための助燃剤を塗布する第2の塗布工程を備えたことを特徴とするシガレット巻紙の製造方法を提供する。
 好ましくは、前記第2の塗布工程は、前記第1の塗布工程の後であって、前記乾燥工程の前又は後に行われる。
 好ましくは、前記第2の塗布工程にて、前記助燃剤は、前記ウエブの前記燃焼抑制剤が塗布された側に対して反対側に塗布される。
 好ましくは、前記第2の塗布工程にて、前記助燃剤を前記ウエブを搬送するためのロールに一旦塗布し、該ロールを介して前記助燃剤を前記ウエブに塗布する。
 好ましくは、前記第2の塗布工程にて、前記助燃剤の塗布量を監視する。
 好ましくは、前記ウエブの全面あるいは一部の領域に対して前記助燃剤を選択的に塗布する。
 好ましくは、前記ウエブの長手方向に対して一定間隔を存して前記ウエブの幅方向に横断するように前記燃焼抑制剤を複数箇所に塗布する。
 また、本発明では、紙製のウエブが走行する走行経路と、該走行経路上に位置し、前記ウエブの燃焼を抑制するための燃焼抑制剤を塗布するための第1の塗布装置と、該第1の塗布装置の下流に位置し、前記ウエブの燃焼を促進するための助燃剤を塗布するための第2の塗布装置と、該第2の塗布装置の上流又は下流に位置し、前記燃焼抑制剤及び前記助燃剤が塗布された前記ウエブを乾燥する乾燥装置とを備えたことを特徴とするシガレット巻紙の製造機を提供する。
 また、本発明では、紙製のウエブの一方の面に塗布された燃焼抑制剤と、前記ウエブの他方の面に塗布された助燃剤とを備え、前記助燃剤中に含まれる成分の濃度が前記ウエブの長手方向に沿って異なっていることを特徴とするシガレット巻紙を提供する。
 さらに、紙製のウエブの一方の面に部分的に塗布された燃焼抑制剤と、前記ウエブの他方の面であって、前記燃焼抑制剤が塗布された領域以外の領域に対応する領域に塗布された助燃剤とを備えたことを特徴とするシガレット巻紙も提供する。
 本発明によれば、助燃剤を塗布する工程を有している。したがって、助燃剤と燃焼抑制剤との塗布量、塗布する位置等を調整しながら両者を塗布することができ、必要に応じた量の助燃剤及び燃焼抑制剤をウエブに対して塗布することができる。これを用いて、ウエブに対する塗布量に濃度勾配を設けて塗布することもできる。これにより、少量多品種ロットのシガレットの生産に有効となる。
 また、第2の塗布工程にて、助燃剤は、ウエブの燃焼抑制剤が塗布された側に対して反対側に塗布されるため、助燃剤が燃焼抑制剤に対して影響を与えることはない。
 また、ロールを介して間接的に助燃剤を塗布するので、ウエブを搬送するための搬送ロールを利用して効率的に助燃剤を塗布することができる。
 また、本発明によれば、第2の塗布工程にて助燃剤の塗布量を監視するため、この監視による結果を利用して、ウエブに対する助燃剤塗布の制御を行うことができる。これを用いてウエブの全面あるいは一部の領域に対して選択的に塗布することも可能である。適切な量又は位置で助燃剤を塗布できることにより、従来の抄紙工程で添加する際の使用量よりも低減させることができる。
 また、本発明では上述した製造方法でシガレットの巻紙を製造するので、品質の安定した低延焼性の巻紙を製造することができる。
本発明に係るシガレット巻紙の製造機の概略図である。 燃焼抑制剤及び助燃剤を塗布したウエブWの概略図である。 燃焼抑制剤及び助燃剤を塗布した別のウエブWの概略図である。 本発明に係る別のシガレット巻紙の製造機の概略図である。
 図1に示すように、本発明に係るシガレット巻紙の製造機1は、図1中の矢印に沿って紙製のウエブWを走行させる走行経路2を備えている。走行経路2には、その上流側から順に、第1の塗布装置3と、第2の塗布装置5と、乾燥装置4とが配設されている。
 第1の塗布装置3は、ウエブWに燃焼抑制剤6(図2、図3参照)を部分的に塗布するためのものである。具体的には、燃焼抑制剤6は、ウエブWの長手方向に対して一定間隔を存してウエブWの幅方向に横断するように複数箇所に塗布される。すなわち、燃焼抑制剤6はウエブWに対してバンド状に塗布される。この塗布は、第1の塗布装置3に含まれるプレスロール7やグラビアロール8等を用いて公知の方法で行われる。
 第2の塗布装置5は、第1の塗布装置3の下流に位置し、第1の塗布装置3を通過したウエブWに助燃剤26(図2、図3参照)を塗布するためのものである。この助燃剤26は、従来と同様、クエン酸カリウム等の有機酸塩、あるいはその他の燃焼を促進させる物質を含むものを用いることができる。図2及び図3に示すように、助燃剤26は、燃焼抑制剤6が塗布された面とは反対側の面に塗布される。このため、助燃剤26が燃焼抑制剤6に対して影響を与えることはない。すなわち、燃焼抑制剤6は水溶性であるため、助燃剤26によって燃焼抑制剤6が溶解することを防止できる。なお、助燃剤26として粉末状の助燃剤を使用した場合には、燃焼抑制剤6が塗布された面と同じ面に塗布してもよい。
 助燃剤26の塗布は、具体的には、第2の塗布装置5は、第1の塗布装置3と同様に、プレスロール9やグラビアロール10、さらにはノズル11から供給される助燃剤26をグラビアロール10との間で受けるため、グラビアロール10に転接されたファニッシャロール12とを有している。ノズル11から供給された助燃剤26は、グラビアロール10の外周面に塗布され、そしてグラビアロール10とプレスロール9との間を走行するウエブWに対して塗布(転写)される。このように、グラビアロール10を介して間接的に助燃剤を塗布するので、ウエブWを搬送するための搬送ロールを利用して効率的に助燃剤を塗布することができる。グラビアロール10にて助燃剤26を塗布する際、余剰の助燃剤26はドクタブレード27によって掻き取られ、グラビアロール10から除去される。除去された助燃剤26は、グラビアロール10からファニッシャロール12に至る領域を下方から覆う回収シュート28に回収され、後述するタンク14に戻される(図1の矢印F)。
 乾燥装置4は、第2の塗布装置5の下流に位置し、燃焼抑制剤及び助燃剤が塗布されたウエブWを乾燥するためのものである。具体的には、乾燥装置4には乾燥炉(不図示)が複数備わっていて、この乾燥炉内を通過することでウエブWは加熱され、乾燥される。なお、図4に示すように、乾燥装置4は、第2の塗布装置5の上流に位置していてもよい。このように乾燥装置4が第2の塗布装置5の上流又は下流のいずれの位置に配されていても、適切な量の助燃剤26を塗布するという目的は達成できる。
 上述したような製造機1を用いてシガレット巻紙を製造する場合について、図1を例にして説明する。まず、紙製のウエブWが巻かれた原反13から、走行経路2を矢印A方向に走行するようにウエブWが送り出される。そして、第1の塗布装置3にて燃焼抑制剤6が所定間隔ごとに塗布される。このような第1の塗布工程を経て、ウエブWはさらに矢印B方向に走行し、第2の塗布装置5を通過する。第2の塗布装置では、燃焼抑制剤6が塗布されたウエブWの反対側の面に対し、助燃剤26が塗布される。このように、第2の塗布工程にて、助燃剤26は、ウエブWの燃焼抑制剤6が塗布された側に対して反対側に塗布されるため、助燃剤26が燃焼抑制剤6に対して影響を与えることはない。そして、ウエブWはさらに矢印C方向に走行し、乾燥装置4内を通過する。乾燥装置4ではウエブWが加熱され、乾燥される。このような乾燥工程を経て、ウエブWは走行経路2を矢印D方向に進み、後述する皺伸ばし装置17を通過する。
 このように、本発明に係るシガレット巻紙の製造方法では、乾燥工程を行うための乾燥装置4を通過する前のウエブWに対し、第2の塗布装置5を用いて塗布工程を行い、助燃剤26を塗布する。すなわち、乾燥工程の前に置いて、ウエブWには助燃剤26及び燃焼抑制剤6の双方が塗布されていることになる。
 第2の塗布工程で塗布される助燃剤26、すなわち第2の塗布装置5に供給されるべき助燃剤26は、実際には水溶液としてタンク14に充填されている。このタンク14と第2の塗布装置5との間には、助燃剤をタンク14から第2の塗布装置5に送り出すためのポンプ15が配設されている。タンク14内の助燃剤26の残量、すなわち消費量は、その監視機能を含む制御装置16によって計測される。また、ポンプ15による送り出し量は、ポンプ15の調節機能を含む制御装置16によって調節される。なお、これら監視機能や調節機能を有する装置を別体として備えてもよい。
 ウエブWに対する単位面積当たりの助燃剤の塗布量を監視する機能を制御装置16に設け、これを利用してウエブWの全面あるいは一部の領域に対して助燃剤を選択的に塗布してもよい。この場合は、例えば上述したグラビアロール10のセル形状(周面の凹凸形状)を変更したり、あるいは上述したプレスロール9を上下に移動させたりして助燃剤の塗布量を変更する。プレスロール9の移動は、例えばアクチュエータ29を用いて行うことができる。このアクチュエータ29を制御装置16と接続すれば、制御装置を用いて助燃剤26の塗布量を変更できる。
 このように制御装置を用いれば、例えば図2に示すように助燃剤26に濃度勾配(濃淡)を設けて塗布することができる。すなわち、図2の例では、紙製のウエブWの一方の面に塗布された燃焼抑制剤6と、ウエブWの他方の面に厚さが異なって塗布された助燃剤26とが備わっている。あるいは、助燃剤26中に含まれる成分(例えば上述したクエン酸ナトリウムやクエン酸カリウム等)の濃度がウエブWの長手方向に沿って異なるように塗布されている。
 あるいは、図3に示すように、燃焼抑制剤6が塗布された箇所の裏面には助燃剤26を塗布しないようにすることもできる。すなわち、図3の例では、紙製のウエブWの一方の面に部分的に塗布された燃焼抑制剤6と、ウエブWの他方の面であって、燃焼抑制剤6が塗布された領域以外の領域に対応する領域に塗布された助燃剤26とを備えている。上述した本発明に係る製造方法は、図2や図3で示すような様々な助燃剤26の塗布形態にも対応できる。このため、ウエブWの材質や通気度に応じて適切な助燃剤26の塗布を行うことができる。
 乾燥装置4を通過したウエブWは、上述したように、走行経路2を矢印D方向に走行し、皺伸ばし装置17を通過する。皺伸ばし装置17はダンピング部18と皺伸ばし部19と乾燥部20とを有している。ダンピング部18はグラビアロール21とピンチロール22からなり、グラビアロール21がウエブWに対し水を塗布する。そして、皺伸ばし部19では、皺伸ばしロール23がロールに係る張力によりウエブWを横方向に拡張させる。そして、ウエブWは拡張された状態で、乾燥部20を用いて乾燥される。乾燥部20は加熱されたヒータロール24と、これに転接されたプレスロール25とを有している。このロール24、25の間を通過する際、ウエブWはプレスロール25により確実に平坦化されながら、ヒータロール24で加熱されて乾燥される。
 本発明は、従来抄紙工程で添加されていた助燃剤をあえて塗布装置を用い、ウエブWの燃焼抑制剤とともに塗布するものである。こうすることで、種々のウエブWの材質等に合わせて適切量の助燃剤を塗布することができ、燃焼抑制剤との塗布量との兼ね合いも考慮しながら塗布することができる。塗布量を適切にすることで、従来よりも塗布量の低減を実現できる。
 一方で、皺伸ばし工程を経たウエブWは、走行経路2を矢印E方向に走行し、ウエブWにスリットを形成して所定幅に切断するスリット形成工程とを経て、シガレットの巻紙として製造される。このように、上述したウエブWを用いれば、品質の安定した低延焼性の巻紙を製造することができる。また、本発明の製造方法は特に、少量多品種ロットの生産に有効である。
1 シガレット巻紙の製造機
2 走行経路
3 第1の塗布装置
4 乾燥装置
5 第2の塗布装置
6 燃焼抑制剤
7 プレスロール
8 グラビアロール
9 プレスロール
10 グラビアロール
11 ノズル
12 ファニッシャロール
13 原反
14 タンク
15 ポンプ
16 制御装置
17 皺伸ばし装置
18 ダンピング部
19 皺伸ばし部
20 乾燥部
21 グラビアロール
22 ピンチロール
23 皺伸ばしロール
24 ヒータロール
25 プレスロール
26 助燃剤
27 ドクタブレード
28 回収シュート
29 アクチュエータ

Claims (10)

  1.  走行経路に沿って紙製のウエブを走行させ、
     前記ウエブの燃焼を抑制するための燃焼抑制剤を塗布する第1の塗布工程と、
     前記ウエブを加熱して乾燥させるための乾燥工程とを備えたシガレット巻紙の製造方法において、
     前記ウエブの燃焼を促進するための助燃剤を塗布する第2の塗布工程を備えたことを特徴とするシガレット巻紙の製造方法。
  2.  前記第2の塗布工程は、前記第1の塗布工程の後であって、前記乾燥工程の前又は後に行われることを特徴とする請求項1に記載のシガレット巻紙の製造方法。
  3.  前記第2の塗布工程にて、前記助燃剤は、前記ウエブの前記燃焼抑制剤が塗布された側に対して反対側に塗布されることを特徴とする請求項1に記載のシガレット巻紙の製造方法。
  4.  前記第2の塗布工程にて、前記助燃剤を前記ウエブを搬送するためのロールに一旦塗布し、該ロールを介して前記助燃剤を前記ウエブに塗布することを特徴とする請求項1に記載のシガレット巻紙の製造方法。
  5.  前記第2の塗布工程にて、前記助燃剤の塗布量を監視することを特徴とする請求項1に記載のシガレット巻紙の製造方法。
  6.  前記ウエブの全面あるいは一部の領域に対して前記助燃剤を選択的に塗布することを特徴とする請求項1に記載のシガレット巻紙の製造方法。
  7.  前記ウエブの長手方向に対して一定間隔を存して前記ウエブの幅方向に横断するように前記燃焼抑制剤を複数箇所に塗布することを特徴とする請求項1に記載のシガレット巻紙の製造方法。
  8.  紙製のウエブが走行する走行経路と、
     該走行経路上に位置し、前記ウエブの燃焼を抑制するための燃焼抑制剤を塗布するための第1の塗布装置と、
     該第1の塗布装置の下流に位置し、前記ウエブの燃焼を促進するための助燃剤を塗布するための第2の塗布装置と、
     該第2の塗布装置の上流又は下流に位置し、前記燃焼抑制剤及び前記助燃剤が塗布された前記ウエブを乾燥する乾燥装置と
    を備えたことを特徴とするシガレット巻紙の製造機。
  9.  紙製のウエブの一方の面に塗布された燃焼抑制剤と、
     前記ウエブの他方の面に塗布された助燃剤と
    を備え、
     前記助燃剤中に含まれる成分の濃度が前記ウエブの長手方向に沿って異なっていることを特徴とするシガレット巻紙。
  10.  紙製のウエブの一方の面に部分的に塗布された燃焼抑制剤と、
     前記ウエブの他方の面であって、前記燃焼抑制剤が塗布された領域以外の領域に対応する領域に塗布された助燃剤とを備えたことを特徴とするシガレット巻紙。
PCT/JP2011/057808 2011-03-29 2011-03-29 シガレット巻紙の製造方法、その製造機及びシガレット巻紙 WO2012131902A1 (ja)