SU1106382A1 - METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT - Google Patents

METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT

Info

Publication number
SU1106382A1
SU1106382A1 SU3505560/07A SU3505560A SU1106382A1 SU 1106382 A1 SU1106382 A1 SU 1106382A1 SU 3505560/07 A SU3505560/07 A SU 3505560/07A SU 3505560 A SU3505560 A SU 3505560A SU 1106382 A1 SU1106382 A1 SU 1106382A1
Authority
SU
USSR - Soviet Union
Prior art keywords
electrodes
manufacturing
current
burning
chemical source
Prior art date
Application number
SU3505560/07A
Other languages
Russian (ru)
Inventor
В.А. Аржанников
А.А. Аржанников
А.Д. Неуймин
Original Assignee
Институт электрохимии Уральского научного центра АН СССР
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Институт электрохимии Уральского научного центра АН СССР filed Critical Институт электрохимии Уральского научного центра АН СССР
Priority to SU3505560/07A priority Critical patent/SU1106382A1/en
Application granted granted Critical
Publication of SU1106382A1 publication Critical patent/SU1106382A1/en

Abstract

Способ изготовления химического источника тока путем нанесения на обе стороны твердого электролита слоев активной массы электродов разной полярности с последующим обжигом, отличающийся тем, что, с целью уменьшения брака и повышения удельных электрических характеристик, обжиг проводят при температуре на 100 - 400 К ниже температуры плавления активной массы электродов и одновременно пропускают через электроды электрический ток плотностью 0,2 - 2,0 А/смв течение 5 - 20 мин при поляризации на электродах, не превышающей напряжения разложения электролита.A method of manufacturing a chemical current source by applying on both sides of a solid electrolyte layers of an active mass of electrodes of different polarity with subsequent burning, characterized in that, in order to reduce scrap and improve specific electrical characteristics, the burning is carried out at a temperature of 100 - 400 K below the melting temperature of the active the masses of the electrodes and at the same time pass through the electrodes an electric current with a density of 0.2 - 2.0 A / cm for 5 to 20 minutes with polarization on the electrodes not exceeding the decomposition voltage of the electric Olita.

SU3505560/07A 1982-10-29 1982-10-29 METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT SU1106382A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU3505560/07A SU1106382A1 (en) 1982-10-29 1982-10-29 METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU3505560/07A SU1106382A1 (en) 1982-10-29 1982-10-29 METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT

Publications (1)

Publication Number Publication Date
SU1106382A1 true SU1106382A1 (en) 1999-10-10

Family

ID=60524467

Family Applications (1)

Application Number Title Priority Date Filing Date
SU3505560/07A SU1106382A1 (en) 1982-10-29 1982-10-29 METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT

Country Status (1)

Country Link
SU (1) SU1106382A1 (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2006112757A1 (en) * 2005-04-21 2006-10-26 The Potanin Institute Limited Method for producing a solid-state power supply

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2006112757A1 (en) * 2005-04-21 2006-10-26 The Potanin Institute Limited Method for producing a solid-state power supply
US7806942B2 (en) 2005-04-21 2010-10-05 The Potanin Institute Limited Method for production of secondary solid state current source

Similar Documents

Publication Publication Date Title
MX9504546A (en) Electrical energy storage device and method of charging and discharging same.
JPS52131991A (en) High destruction and high voltage electrodes for bromideecontaining electrolyte electrolysis
JPS5596568A (en) Novel ion conductivity lithium compound*solid ion conductive material made of same* process for producing same compound and battery containing same ion conductive material
BR7906061A (en) CATHOD FOR AN ELECTROCHEMICAL BATTERY, ELECTROCHEMICAL BATTERY, PROCESS TO FORM A CATHOD, AND ACTIVE CATHODIC CURRENT COLLECTOR
JPS55161341A (en) Microwave ion source
SE8402437L (en) END BLYCELL WITH GAS RECOVERY
MX143481A (en) METHOD OF FORMING AN INTERCELLULAR CONNECTION IN AN ELECTRICAL BATTERY AND RESULTING ELECTRIC BATTERY
JPS55130075A (en) Active electroce* electrochemical battery having same and method of forming active electrode
BR8702942A (en) ELECTROCHEMICAL BATTERY AND PROCESS TO MAKE ELECTRICAL CONTACT WITH PLATE ELECTRODE OF AN ELECTROCHEMICAL BATTERY
SU1106382A1 (en) METHOD OF MANUFACTURING A CHEMICAL SOURCE OF CURRENT
ES456295A1 (en) High energy density electric cells
ATE179796T1 (en) REFERENCE ELECTRODES
FR2314589A1 (en) SOLID ELECTROLYTE CONDUCTING IONS, AND SOLID BATTERY ELEMENT
EP0093539A3 (en) Improved double layer energy storage device
SE8005528L (en) ELECTRICAL BLYACK CUMULATOR WITH THIN ELECTRODES
JPS5288733A (en) Method of producing lithium ion conductive solid electrolyte
BR8402571A (en) POSITIVE ACTIVE MATERIA FOR SPECIFIC LARGE SPECIFIC ELECTRIC CHEMICAL GENERATOR, WELL AS A GENERATOR USING THE SAME
SE8007781L (en) lead acid battery
ES2111540T3 (en) METHOD FOR THE PRODUCTION OF A MICROPARTICLE ELECTROSUSPENSION.
JPS5249490A (en) Production method of lithium ion conductive solid state electrolyte
JPS5326774A (en) Construction of electrode in electroysis cell
JPH0755817Y2 (en) Thermal battery
ES449812A1 (en) Rechargeable electrical accumulator cell
JPS51145279A (en) Manufacture of electric charge combination cells
JPS5798978A (en) Chargeable organic electrolytic battery