KR20060054498A - Method for removal shock tube inside of the nuclear reactor cold tube safety injection nozzle - Google Patents

Method for removal shock tube inside of the nuclear reactor cold tube safety injection nozzle Download PDF

Info

Publication number
KR20060054498A
KR20060054498A KR1020040093554A KR20040093554A KR20060054498A KR 20060054498 A KR20060054498 A KR 20060054498A KR 1020040093554 A KR1020040093554 A KR 1020040093554A KR 20040093554 A KR20040093554 A KR 20040093554A KR 20060054498 A KR20060054498 A KR 20060054498A
Authority
KR
South Korea
Prior art keywords
plate
injection nozzle
safety injection
buffer
buffer plate
Prior art date
Application number
KR1020040093554A
Other languages
Korean (ko)
Other versions
KR100598352B1 (en
Inventor
김원옥
방상혁
Original Assignee
두산중공업 주식회사
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 두산중공업 주식회사 filed Critical 두산중공업 주식회사
Priority to KR1020040093554A priority Critical patent/KR100598352B1/en
Publication of KR20060054498A publication Critical patent/KR20060054498A/en
Application granted granted Critical
Publication of KR100598352B1 publication Critical patent/KR100598352B1/en

Abstract

본 발명은 원자로 저온관의 안전주입노즐 내부에 삽입되어진 열전달 완충판의 제거방법에 관한 것으로, 안전주입노즐을 통하여 주입되는 일차 계통수의 온도보다 더 낮은 온도의 유체가 유입될 때, 계통수와 유입되는 유체간에 급격한 온도차이로 인한 열충격을 완화하는 완충판을 제거시, 우선 안전주입노즐의 내면에 대하여 파손과 손상을 전혀 주지 않으면서도 신속 간편하게 제거할 수 있도록 한 것이다.The present invention relates to a method of removing a heat transfer buffer plate inserted into a safety injection nozzle of a nuclear reactor cold tube. When a fluid having a temperature lower than the temperature of a primary system introduced through the safety injection nozzle is introduced, the system water and the fluid introduced therein When removing the shock absorbing plate to alleviate the thermal shock caused by the sudden temperature difference between the first and the first, the inner surface of the safety injection nozzle can be quickly and easily removed without any damage or damage.

본 발명은, 완충판의 이탈을 방지하기 위하여 안전주입노즐의 내면에 용접된 방지턱을 절단 제거하는 단계와; 이 단계 이후 완충판이 상층판, 중층판, 하층판으로 나뉘어지도록 등분 절단하는 단계와; 이 단계 이후 하층판을 안전주입노즐의 내부로부터 빼내어 제거하는 단계와; 이 단계 이후 중층판을 제거하는 단계와; 이 단계 이후 상층판을 제거하는 단계와; 이 단계 이후 안전주입노즐의 내면에 형성된 스크래치를 제거하는 단계;로 이루어진 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법이 제시된다.The present invention includes the steps of cutting off the jaw welded to the inner surface of the safety injection nozzle to prevent the separation of the buffer plate; After this step, the buffer plate is divided into equal parts so that the upper plate, the middle plate, the lower plate; Removing the lower layer plate from the inside of the safety injection nozzle after the step; Removing the laminate after this step; Removing the upper plate after this step; After the step of removing the scratch formed on the inner surface of the safety injection nozzle; buffer plate removal method provided in the safety injection nozzle of the reactor low-temperature tube is presented.

또한, 상기 중층판를 제거하는 단계는, 중층판의 길이방향을 따라 소정깊이 만큼 절개홈이 형성되도록 절개하는 단계와; 이 단계 이후 절개홈을 따라 소정의 온도로 가열시키는 단계와; 이 단계 이후 중층판과 안전주입노즐 사이에 알루미늄 테이프와 쐐기를 고정시켜 중층판의 제거를 도모하면서 안전주입노즐의 내면을 보호하는 단계와; 이 단계 이후 중층판의 내경이 작아도록 절개홈을 따라 절단하는 단계;로 이루어진 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법이 제시된다.In addition, the step of removing the interlayer plate, the step of cutting so that the incision groove is formed by a predetermined depth in the longitudinal direction of the interlayer plate; Heating to a predetermined temperature along the incision after this step; Protecting the inner surface of the safety injection nozzle while fixing the aluminum tape and the wedge between the middle plate and the safety injection nozzle after the step; After the step is cut along the incision groove so that the inner diameter of the middle plate; a buffer plate removal method provided in the safety injection nozzle of the reactor cold tube consisting of.

원자로, 저온관, 안전주입노즐, 완충, 판Reactor, low temperature pipe, safety injection nozzle, buffer, plate

Description

원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법{Method for Removal Shock Tube Inside of The Nuclear Reactor Cold Tube Safety Injection Nozzle} Method for Removal Shock Tube Inside of The Nuclear Reactor Cold Tube Safety Injection Nozzle}             

도 1는 일반적으로 원자로 저온관의 안전주입노즐에 완충판이 설치된 상태를 보여주는 단면도이다.1 is a cross-sectional view showing a state in which a buffer plate is generally installed in the safety injection nozzle of the reactor cold tube.

도 2는 본 발명의 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법을 나타낸 순서도이다.Figure 2 is a flow chart showing a method of removing the buffer plate provided in the safety injection nozzle of the reactor cold tube of the present invention.

도 3a~3c는 도 1에서 중층판의 제거과정을 개략적으로 보여주는 것으로, 도 3a는 도 1의 A"부의 확대도이다.3A to 3C schematically show a process of removing the middle plate in FIG. 1, and FIG. 3A is an enlarged view of the portion A ″ of FIG. 1.

도 3b는 도 3a의 중층판이 일정깊이 만큼 절개된 상태를 보여주는 사시도이다. 3B is a perspective view illustrating a state in which the middle plate of FIG. 3A is cut by a predetermined depth.

도 3c는 중층판이 완전히 절개된 상태를 보여주는 사시도이다. Figure 3c is a perspective view showing a state in which the middle plate is completely cut.

* 도면의 주요부분에 대한 부호설명 * * Explanation of Signs of Major Parts of Drawings *

10 : 안전주입노즐 12 : 완충판10: safety injection nozzle 12: buffer plate

14 : 방지턱 20,22 : 절단선14: jaw 20,22: cutting line

24 : 상층판 26 : 중층판24: upper layer 26: middle layer

28 : 하층판 30 : 앵글 그라인더28: lower plate 30: angle grinder

32 : 절개홈 34 : 테이프32: incision groove 34: tape

36 : 쐐기36: wedge

본 발명은 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법에 관한 것으로, 더욱 상세하게는 안전주입노즐의 내부에 설치된 완충판을 제거시, 안전주입노즐의 내면에 대하여 파손 혹은 손상을 전혀 주지 않고 안전하게 제거하면서, 아울러 제거 작업이 신속 간편하게 이루어지도록 한 것이다.The present invention relates to a method for removing a buffer plate provided in a safety injection nozzle of a nuclear reactor low temperature pipe, and more particularly, when removing a buffer plate installed inside a safety injection nozzle, without damaging or damaging the inner surface of the safety injection nozzle. It is safe to remove and the removal is quick and easy.

일반적으로 원자로의 저온관에는 첨부된 예시도면 도 1에 도시된 바와 같이 안전주입노즐(10)이 구비되며, 그 내부에는 열전달을 완화시키기 위한 완충판(12)이 삽입고정되는데, 이러한 완충판(12)은 폭발 확관방법을 이용하여 안전주입노즐(10)에 확관 걸림된다.상기 완충판(12)은, 안전주입노즐(10)을 통하여 일차 유입되는 계통수의 온도보다 낮은 온도의 유체(예를들어 냉각수)가 유입될 때, 계통수와 저온의 유체간에 급격한 온도차이로 인하여 안전주입노즐(10)에 미치는 열충격을 완화시킴으로써, 안전주입노즐(10)에 대하여 손상이 발생되지 않도록 하기 위한 기능을 가지고 있다. 그런데, 원자로가 가동되면, 그 유동에 의하여 완충판(12)이 화살표방향으로 조금씩 위치 이동을 하게 되고, 그에 따라 완충판(12)이 안전주입노즐(10)로부터 이탈되어 저온관을 통해 원자로 유입된다. 특히 원자로의 가동중에 완충판(12)이 유입되면, 막대한 비용으로 제작된 원자로의 파손은 물론, 엄청난 비용과 복구시간이 요구되는 치명적인 문제점이 발생된다.In general, the cold tube of the reactor is provided with a safety injection nozzle 10, as shown in the accompanying drawings, Figure 1, therein is inserted into the buffer plate 12 to mitigate heat transfer, the buffer plate 12 Is expanded to the safety injection nozzle 10 using an explosion expansion method. The buffer plate 12 is a fluid (for example, coolant) having a temperature lower than the temperature of the system water introduced through the safety injection nozzle 10. When is introduced, by reducing the thermal shock on the safety injection nozzle 10 due to the rapid temperature difference between the system water and the low temperature fluid, it has a function to prevent damage to the safety injection nozzle (10). However, when the reactor is operated, the buffer plate 12 is moved little by little in the direction of the arrow by the flow, and thus the buffer plate 12 is separated from the safety injection nozzle 10 and introduced into the reactor through the low temperature pipe. In particular, if the buffer plate 12 is introduced during the operation of the reactor, a fatal problem that requires a huge cost and recovery time, as well as damage to the reactor produced at a huge cost.

따라서, 위와 같은 사고를 사전에 방지하기 위하여 안전주입노즐(10)의 내면에 여러개의 방지턱(14)을 용접으로 고정하여 완충판(12)을 지지고정하는 방법도 사용하였으나, 시간이 지나감에 따라 방지턱(14)의 용접부가 탈락되면서, 방지턱(14)과 완충판(12)이 함께 원자로로 유입되어져 앞서 제기되었던 문제점이 재차 발생하였다.Therefore, in order to prevent such an accident in advance, a method of fixing the support plate 12 by fixing a plurality of preventive jaws 14 on the inner surface of the safety injection nozzle 10 by welding is also used. As the welded portion of (14) was dropped, the bumps 14 and the buffer plate 12 were introduced into the reactor together, which caused the above-mentioned problems.

이에 따라, 가장 중요한 원자로의 파손을 막기 위해서는 안전주입노즐의 손상은 어느 정도 감수하더라도, 현실적으로 완충판의 제거가 절실히 요구되며, 그에 따라 안전주입노즐의 손상없이 완충판을 신속 간편하게 제거하기 위한 방법들이 지속적으로 연구되어 왔다. Accordingly, in order to prevent the damage of the most important reactor, even if the safety injection nozzle is damaged to some extent, it is urgently required to remove the buffer plate. Accordingly, methods for quickly and easily removing the buffer plate without damaging the safety injection nozzle are continuously performed. Has been studied.

이에 본 발명은 상기와 같은 종래의 문제점을 해소하기 위해 발명된 것으로, 안전주입노즐의 내부에 설치된 완충판을 제거시, 안전주입노즐의 내면에 대하여 파손 혹은 손상을 전혀 주지 않고 안전하게 제거하면서, 아울러 제거 작업이 신속 간편하도록 하는 점에 목적이 있다.Accordingly, the present invention has been invented to solve the above conventional problems, and when removing the buffer plate installed inside the safety injection nozzle, while safely removing without damaging or damaging the inner surface of the safety injection nozzle, and also removed The purpose is to make the work quick and easy.

상기와 같은 목적을 달성하기 위한 본 발명은, 완충판의 이탈을 방지하기 위하여 안전주입노즐의 내면에 용접된 방지턱을 절단 제거하는 단계와; 이 단계 이후 완충판이 상층판, 중층판, 하층판으로 나뉘어지도록 등분 절단하는 단계와; 이 단계 이후 하층판을 안전주입노즐의 내부로부터 빼내어 제거하는 단계와; 이 단계 이후 중층판을 제거하는 단계와; 이 단계 이후 상층판을 제거하는 단계와; 이 단계 이후 안전주입노즐의 내면에 형성된 스크래치를 제거하는 단계;로 이루어진 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법에 기술적 특징이 있다.The present invention for achieving the above object, the step of removing and removing the jaw welded to the inner surface of the safety injection nozzle to prevent the separation of the buffer plate; After this step, the buffer plate is divided into equal parts so that the upper plate, the middle plate, the lower plate; Removing the lower layer plate from the inside of the safety injection nozzle after the step; Removing the laminate after this step; Removing the upper plate after this step; Removing the scratch formed on the inner surface of the safety injection nozzle after this step; there is a technical feature in the method of removing the buffer plate provided in the safety injection nozzle of the reactor cold tube.

또한, 상기 중층판를 제거하는 단계는, 중층판의 길이방향을 따라 소정깊이 만큼 절개홈이 형성되도록 절개하는 단계와; 이 단계 이후 절개홈을 따라 소정의 온도로 가열시키는 단계와; 이 단계 이후 중층판과 안전주입노즐 사이에 알루미늄 테이프와 쐐기를 고정시켜 중층판의 제거를 도모하면서 안전주입노즐의 내면을 보호하는 단계와; 이 단계 이후 중층판의 내경이 작아도록 절개홈을 따라 절단하는 단계;로 이루어진 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법에 기술적 특징이 있다.In addition, the step of removing the interlayer plate, the step of cutting so that the incision groove is formed by a predetermined depth in the longitudinal direction of the interlayer plate; Heating to a predetermined temperature along the incision after this step; Protecting the inner surface of the safety injection nozzle while fixing the aluminum tape and the wedge between the middle plate and the safety injection nozzle after the step; Thereafter, the step of cutting along the incision groove so that the inner diameter of the middle plate is small; there is a technical feature in the buffer plate removal method provided in the safety injection nozzle of the reactor low-temperature tube.

이하 본 발명의 실시예를 첨부된 예시도면에 의거 상세히 설명하기로 한다. Hereinafter, the embodiments of the present invention will be described in detail with reference to the accompanying drawings.

첨부된 예시도면 도 1은 일반적으로 안전주입노즐의 내부에 완충판이 설치된 상태를 보여주는 단면도이고, 도 2는 본 발명의 원자로 안전주입노즐의 완충판 제거방법을 나타낸 순서도이다.1 is a cross-sectional view illustrating a state in which a buffer plate is installed in a safety injection nozzle, and FIG. 2 is a flowchart illustrating a method of removing a buffer plate of a nuclear reactor safety injection nozzle of the present invention.

첨부된 예시도면에 도시된 바와 같이, 완충판의 이탈을 방지하기 위한 방지턱을 제거하는 단계와(a); 이 단계 이후 완충판을 등분으로 절단하는 단계(b)와; 이 단계 이후 하층판을 제거하는 단계(c)와; 이 단계 이후 중층판(d)을 제거하는 단계와; 이 단계 이후 상층판(e)를 제거하는 단계와; 이 단계 이후 안전주입노즐의 내면에 발생된 스크래치를 제거하는 단계(f)로; 요약될 수 있다.여기서, 상기 중층판를 제거하는 단계(d)는, 먼저 중층판의 종방향을 따라 소정깊이 만큼 절개하는 단계(d1)와; 이 단계 이후 절개라인을 따라 가열하는 단계(d2)와; 이 단계 이후 알루미늄 테이프 및 쐐기를 이용하여 안전주입노즐을 보호하는 단계(d3)와; 이 단계 이후 절개라인을 따라 절단하는 단계(d4)로; 이루어진다.As shown in the accompanying drawings, the step of removing the jaws for preventing the separation of the buffer plate (a); (B) cutting the buffer plate into equal parts after this step; (C) removing the lower plate after this step; Removing the middle layer d after this step; Removing the upper plate (e) after this step; (F) removing the scratches generated on the inner surface of the safety injection nozzle after this step; Here, the step (d) of removing the interlayer plate may include: first, cutting (d1) a predetermined depth along the longitudinal direction of the interlayer plate; (D2) heating along the incision line after this step; Protecting the safety injection nozzle using the aluminum tape and the wedge after the step (d3); To step d4 along the incision line after this step; Is done.

아래에서는 상기 안전주입노즐로부터 완충판의 제거방법을 보다 구체적으로 설명하기로 한다.Hereinafter, a method of removing the buffer plate from the safety injection nozzle will be described in more detail.

상기 안전주입노즐(10)에 삽입 고정된 완충판(12)을 제거하기 위해서는 첨부된 예시도면 도 1 및 도 2에 도시된 바와 같이 우선 작업자가 안전주입노즐(10)의 내부로 들어가서 완충판(12)을 지지하는 방지턱(14)을 탈락 혹은 절단시켜 완전히 제거한다. 이와 같이 방지턱(14)이 전부 제거되더라도 완충판(12)은 안전주입노즐(10)에 폭발 확관방식으로 결합되어 있어 하부방향으로 빠져나오지 않는다.In order to remove the buffer plate 12 inserted and fixed to the safety injection nozzle 10, as shown in FIGS. 1 and 2, first, an operator enters the interior of the safety injection nozzle 10 and the buffer plate 12. Dropping or cutting the jaw 14 for supporting the complete removal. In this way, even if the stopper 14 is completely removed, the shock absorbing plate 12 is coupled to the safety injection nozzle 10 in an explosion expanding manner and thus does not escape downward.

그 다음, 상기 완충판(12)의 내부에는 중심을 기준으로 하여 회전반경을 따라 회전가능한 절단공구를 삽입 위치시키고, 이 절단공구가 완충판(12)의 내주면을 따라 회전하면서 절단하게 된다. 이때 서로 소정간격을 갖는 각각의 절단선(20,22)을 따라 절단되어 상층판(24), 중층판(26), 하층판(28)으로 나뉘어지게 된다. Then, the cutting tool which is rotatable along the rotation radius is inserted into the buffer plate 12, and the cutting tool rotates along the inner circumferential surface of the buffer plate 12 to cut it. At this time, it is cut along each cutting line (20, 22) having a predetermined distance from each other is divided into an upper plate 24, a middle layer 26, a lower layer 28.

그리고, 상기와 같이 절단되면, 상기 하층판(28)은 방지턱(14)의 제거로 인하여 화살표방향으로 먼저 빠져나오게 되며, 상기 중층판(26)은 안전주입노즐(10) 에 결합되는 상태를 그대로 유지하게 된다.Then, when the cut as described above, the lower layer plate 28 is first exited in the direction of the arrow due to the removal of the blocking jaw (14), the middle layer plate 26 is left as it is coupled to the safety injection nozzle (10) Will be maintained.

그 다음, 상기 중층판(26)을 제거하고자 할 경우, 첨부된 예시도면 도 3a, 도 3b, 도 3c에 도시된 바와 같이 중층판(26)을 안전주입노즐(10)의 내면으로부터 이격시켜 제거하게 된다.Next, when the middle plate 26 is to be removed, the middle plate 26 is removed from the inner surface of the safety injection nozzle 10 as shown in the accompanying drawings (FIGS. 3A, 3B and 3C). Done.

위와 같은 작업을 수행하기 위해서는, 우선 앵글그라인더(30)와 같은 절단장비를 이용하여 중층판(26)의 길이방향인 종방향으로 소정깊이 만큼 절개홈(32)이 형성되도록 절개한다. 이때 중층판(26)의 두께가 예를들어 4.5mm인 경우에는 3.5mm ~ 4.0mm 깊이만큼 절개하게 된다. 이러한 절개홈(32)의 깊이는 하나의 예를 제시한 것일 뿐, 이로 한정되거나 국한될 필요는 없다. 예컨데 상기 중층판(26)의 두께가 달라지게 되면 절개홈(32)의 깊이도 달라지게 된다.In order to perform the above operation, first, a cutting device such as an angle grinder 30 is cut to form a cut groove 32 in a longitudinal direction in a longitudinal direction of the middle layer 26 in a longitudinal direction. At this time, in the case where the thickness of the middle layer 26 is, for example, 4.5mm, it is cut by a depth of 3.5mm to 4.0mm. The depth of the cutout 32 is only one example, and need not be limited thereto. For example, when the thickness of the middle plate 26 is changed, the depth of the cut groove 32 is also changed.

그리고, 상기와 같은 상태에서 토치와 같은 가열장비를 이용하여 절개홈(32)을 따라 그 주위를 높은 온도로 가열시켜 중층판(26)이 쉽게 변형될 수 있도록 하게 되는데, 이때 안전주입노즐(10)의 내면의 손상과 자칫 중층판(26)의 변형에 의하여 갑작스런 이탈됨을 방지하고자, 중층판(26)의 하단부와 대응하는 안전주입노즐(10)의 내면에 알루미늄재질로 이루어진 테이프(34)가 부착되어 고정되고, 아울러 테이프(34)와 중층판(26) 사이에는 쐐기(36)가 삽입되어 고정된다.Then, in the above state by using a heating device such as a torch to heat the circumference along the cutting groove 32 to a high temperature so that the middle plate 26 can be easily deformed, in this case the safety injection nozzle (10) In order to prevent sudden departure due to damage of the inner surface of the) and the deformation of the middle layer plate 26, the tape 34 made of an aluminum material on the inner surface of the safety injection nozzle 10 corresponding to the lower end of the middle layer plate 26 The wedge 36 is inserted and fixed between the tape 34 and the middle plate 26.

그리고, 이러한 상태에서 상기 쐐기(36)를 화살표와 같은 방향으로 힘을 가하여 절개홈(32)을 안쪽으로 밀어서 중층판(26)이 안전주입노즐(10)의 내면으로부터 이격되도록 한다. 동시에 앞서 언급된 앵글라인더(30)를 이용하여 절개홈(32)을 따라 완전히 절단시킨다. 이와 같이 절개홈(32)이 완전히 절단되면, 중층판(26)의 내경이 작아지도록 오므린 후 안전주입노즐(10)로부터 빠지도록 하여 제거한다.In this state, the wedge 36 is applied in the same direction as the arrow to push the incision groove 32 inward so that the middle plate 26 is spaced apart from the inner surface of the safety injection nozzle 10. At the same time, the above-mentioned angle grinder 30 is used to completely cut along the cutout groove 32. When the cutting groove 32 is completely cut in this manner, the inner diameter of the middle layer plate 26 is retracted to be smaller, and then removed from the safety injection nozzle 10.

그 다음, 상층판(24)을 하부방향으로 끌어 내리기 위하여 상층판(24)이 상단을 걸수 있는 걸림장비가 투입되어, 이 걸림장비에 구비된 걸림구를 상층판(24)의 상단에 걸고 하부방향으로 끌어내려 안전주입노즐(10)로부터 상층판(24)을 제거하게 된다. 그러나 이러한 방법은 하나의 예일 뿐이며, 상기 상층판(24)을 하부방향으로 끌어 내릴 수 있다면, 어떠 방법 및 장비가 사용되어도 무방할 것이다. 마지막으로, 상기 상층판(24), 중층판(26), 하층판(28)을 제거시, 안전주입노즐(10)의 내면에 발생된 스크래치 및 방지턱(14)의 용접부위는 사포 또는 샌드페이퍼등과 같은 연마장비을 이용하여 깨끗하게 제거시킨다.Then, in order to pull down the upper plate 24 in the downward direction, a locking device to which the upper plate 24 can be hooked up is inserted, and the locking mechanism provided in the locking device is hooked to the upper end of the upper plate 24 and the lower portion thereof is lowered. The upper plate 24 is removed from the safety injection nozzle 10 by pulling down in the direction. However, this method is only one example, and any method and equipment may be used as long as the upper plate 24 can be lowered downward. Finally, when the upper plate 24, the middle plate 26, the lower plate 28 is removed, the welding portion of the scratch and the prevention jaw 14 generated on the inner surface of the safety injection nozzle 10 is sandpaper or sandpaper, etc. Remove it cleanly using a polishing machine such as this.

본 발명은 안전주입노즐 내부에 삽입되어진 열전달 완충판의 제거방법에 의하여 안전주입노즐의 내면에 파손과 손상을 전혀 주지 않으면서도 신속 간편하게 제거할 수 있도록 하고, 나아가 작업자의 작업 편의를 도모할 수 있는 효과가 있다.The present invention provides a quick and easy removal without damaging or damaging the inner surface of the safety injection nozzle by the method of removing the heat transfer buffer plate inserted into the safety injection nozzle, and furthermore, to facilitate the operation of the operator. There is.

Claims (2)

완충판의 이탈을 방지하기 위하여 안전주입노즐의 내면에 용접된 방지턱을 절단 제거하는 단계(a)와;(A) cutting and removing the jaw welded to the inner surface of the safety injection nozzle to prevent the buffer plate from being separated; 이 단계 이후 완충판을 상층판, 중층판, 하층판으로 나뉘어지도록 등분 절단하는 단계(b)와;(B) dividing the buffer plate into the upper plate, the middle plate, and the lower plate after this step; 이 단계 이후 하층판을 안전주입노즐의 내부로부터 빼내어 제거하는 단계(c)와;(C) removing the lower layer plate from the inside of the safety injection nozzle after the step; 이 단계 이후 중층판을 제거하는 단계(d)와;(D) removing the interlayer plate after this step; 이 단계 이후 상층판을 제거하는 단계(e)와;(E) removing the upper plate after this step; 이 단계 이후 안전주입노즐의 내면에 형성된 스크래치를 제거하는 단계(f);로 이루어진 것을 특징으로 하는 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법.Removing the scratch formed on the inner surface of the safety injection nozzle after this step (f); Method of removing the buffer plate provided in the safety injection nozzle of the reactor low-temperature tube. 제 1항에 있어서,The method of claim 1, 상기 중층판를 제거하는 단계(d)는,Removing the middle layer plate (d), 중층판의 길이방향을 따라 소정깊이 만큼 절개홈이 형성되도록 절개하는 단계(d1)와;이 단계 이후 절개홈을 따라 소정의 온도로 가열시키는 단계(d2)와;Cutting (d1) the cutting groove so that a cutout groove is formed to a predetermined depth along the longitudinal direction of the middle lamination plate; and heating (d2) the cutout groove to a predetermined temperature along the cutting groove; 이 단계 이후 중층판과 안전주입노즐 사이에 알루미늄 테이프와 쐐기를 고정 시켜 중층판의 제거를 도모하면서 안전주입노즐의 내면을 보호하는 단계(d3)와;Securing the inner surface of the safety injection nozzle while fixing the aluminum tape and the wedge between the middle plate and the safety injection nozzle after the step (d3); 이 단계 이후 중층판의 내경이 작아도록 절개홈을 따라 절단하는 단계(d4);로 이루어진 것을 특징으로 하는 원자로 저온관의 안전주입노즐에 구비된 완충판 제거방법이 제시된다.After the step (d4) is cut along the cutting groove so that the inner diameter of the middle plate is small; buffer buffer removal method provided in the safety injection nozzle of the reactor low-temperature tube is characterized in that it consists of.
KR1020040093554A 2004-11-16 2004-11-16 Removal Method of Thermal Sleeve from Safety Injection Nozzle KR100598352B1 (en)