- Prior art keywords
- nozzle
- continuous casting
- graphite
- alumina
- wall
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B22—CASTING; POWDER METALLURGY
- B22D—CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
- B22D41/00—Casting melt-holding vessels, e.g. ladles, tundishes, cups or the like
- B22D41/50—Pouring-nozzles
- B22D41/52—Manufacturing or repairing thereof
- B22D41/54—Manufacturing or repairing thereof characterised by the materials used therefor
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Mechanical Engineering (AREA)
- Casting Support Devices, Ladles, And Melt Control Thereby (AREA)
- Continuous Casting (AREA)
Abstract
PURPOSE:To prevent sticking of an adhesive material to inner wall by using the specific composition of calcium zirconate and the specific quantity of graphite to a nozzle for continuous casting. CONSTITUTION:The nozzle for continuous casting is formed by composition containing 60-90wt.% calcium zirconate, in which contains 40-55% CaO by mol. ratio, and 10-40wt.% graphite. By this method, for example, in the continuous casting for aluminum killed steel, calcia contained in the nozzle is reacted with the alumina, and changed into the compound having melting point lower than the cast molten steel temp. and comes to melt. By this method, the sticking of the alumina to the inner wall of the nozzle is prevented.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19862987A JPS6440154A (en) | 1987-08-07 | 1987-08-07 | Nozzle for continuous casting |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP19862987A JPS6440154A (en) | 1987-08-07 | 1987-08-07 | Nozzle for continuous casting |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS6440154A true JPS6440154A (en) | 1989-02-10 |
Family
ID=16394378
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP19862987A Pending JPS6440154A (en) | 1987-08-07 | 1987-08-07 | Nozzle for continuous casting |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6440154A (en) |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0347671A (en) * | 1989-07-14 | 1991-02-28 | Harima Ceramic Co Ltd | Refractory for flow rate control device for molten metal |
JPH03138054A (en) * | 1989-07-14 | 1991-06-12 | Harima Ceramic Co Ltd | Submerged nozzle for continuous casting |
FR2657279A1 (en) * | 1990-01-23 | 1991-07-26 | Akechi Ceramics Kk | CASTING BUSH OF STEEL FADE. |
FR2686534A1 (en) * | 1992-01-27 | 1993-07-30 | Tokyo Yogyo Kk | CASTING NOZZLE OF THE MOLTEN STEEL. |
EP0664174A1 (en) * | 1994-01-25 | 1995-07-26 | Akechi Ceramics Co. Ltd. | Molten steel pouring nozzle |
KR100380755B1 (en) * | 2002-04-30 | 2003-04-18 | 주식회사 포스코 | Refractory with high quality |
CN107073565A (en) * | 2014-10-31 | 2017-08-18 | 株式会社Posco | Immersion nozzle for continuous casting |
-
1987
- 1987-08-07 JP JP19862987A patent/JPS6440154A/en active Pending
Cited By (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0347671A (en) * | 1989-07-14 | 1991-02-28 | Harima Ceramic Co Ltd | Refractory for flow rate control device for molten metal |
JPH03138054A (en) * | 1989-07-14 | 1991-06-12 | Harima Ceramic Co Ltd | Submerged nozzle for continuous casting |
FR2657279A1 (en) * | 1990-01-23 | 1991-07-26 | Akechi Ceramics Kk | CASTING BUSH OF STEEL FADE. |
US5086957A (en) * | 1990-01-23 | 1992-02-11 | Akechi Ceramics Co., Ltd. | Molten steel pouring nozzle |
FR2686534A1 (en) * | 1992-01-27 | 1993-07-30 | Tokyo Yogyo Kk | CASTING NOZZLE OF THE MOLTEN STEEL. |
EP0664174A1 (en) * | 1994-01-25 | 1995-07-26 | Akechi Ceramics Co. Ltd. | Molten steel pouring nozzle |
KR100380755B1 (en) * | 2002-04-30 | 2003-04-18 | 주식회사 포스코 | Refractory with high quality |
CN107073565A (en) * | 2014-10-31 | 2017-08-18 | 株式会社Posco | Immersion nozzle for continuous casting |
CN107073565B (en) * | 2014-10-31 | 2019-05-10 | 株式会社Posco | Immersion nozzle for continuous casting |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES8800245A1 (en) | and processes for producing the compounds. | |
JPS6440154A (en) | Nozzle for continuous casting | |
EP0309225A3 (en) | Prevention of al2o3 formation in pouring nozzles and the like | |
BR8702712A (en) | PROCESS FOR THE MANUFACTURE OF LOW CARBON LEVEL STEEL WITH A DESIRELY LOW TOTAL OXYGEN CONTENT AND COMPOSITION FOR USE AS A SYNTHETIC SLAG | |
CA2031378A1 (en) | Molten steel pouring nozzle | |
ATE89336T1 (en) | COMPOSITE CELL BOTTOM FOR ALUMINUM ELECTROMAGNE. | |
CA2139372A1 (en) | Molten Steel Pouring Nozzle | |
FR2572724B1 (en) | REFRACTORY WEAR FOR CASTING LIQUID MOLTEN MASSES | |
CA2086392A1 (en) | Molten steel pouring nozzle | |
ATE39865T1 (en) | CONTAINERS FOR HOLDING BULK AT HIGH TEMPERATURE. | |
SE7902804L (en) | FOR USE IN REFINING AN IRON MELT DEPOSITED CONTAINER CONTAINING CALCIUM OXIDE | |
ES8101123A1 (en) | Method for treating boron-containing steel. | |
GB2000198A (en) | Flux for use in continuous casting of steel | |
JPS5365212A (en) | Ingot case additive for continuous casting of steel | |
JPS55122837A (en) | Preventing method for slag adhesion to furnace wall | |
ATE48831T1 (en) | THIXOTROPIC VIBRATION REFRACTORY MASS AND METHOD FOR VIBRATION LINER OF METALLURGICAL VESSELS WITH THIS MASS. | |
FR2395089A1 (en) | Mould flux for continuously casting steel - to absorb alumina inclusions and provide controlled viscosity | |
BE874664A (en) | PROCESS FOR INFLUENCING THE HARDENING OF A MELT METAL MASS DURING THE CONTINUOUS CASTING | |
GB1504280A (en) | Methods of reducing inclusions in castings | |
JPS53120618A (en) | Fusion loss preventing method for ladle brick | |
GB1472400A (en) | Casting of ingots | |
JPS5325210A (en) | Steel refining method | |
JPS57137410A (en) | Production of gray cast iron | |
JPS5589412A (en) | Preventing method of collapse of converter slag and electric furnace slag | |
JPS5524983A (en) | Melt use desulfurizer and producing the same |