JPS6054281A - 肉盛溶接フランジの製作方法 - Google Patents
肉盛溶接フランジの製作方法Info
- Publication number
- JPS6054281A JPS6054281A JP16043883A JP16043883A JPS6054281A JP S6054281 A JPS6054281 A JP S6054281A JP 16043883 A JP16043883 A JP 16043883A JP 16043883 A JP16043883 A JP 16043883A JP S6054281 A JPS6054281 A JP S6054281A
- Authority
- JP
- Japan
- Prior art keywords
- welding
- build
- flange
- shrinkage
- manufacture
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
【発明の詳細な説明】
〔発明の利用分野〕
本発明は管式熱交換器に係り、特に氷室につ〈肉盛溶接
式フランジの製作方法に関するものである。
式フランジの製作方法に関するものである。
従来の肉盛溶接フランジ製作方法としては、フランジ内
側に拘束リング(角形または丸棒)を取付けておき拘束
リングに沿って溶接する方法であるが、殆んどの場合溶
接熱により端部に著しい収縮及びヘアークラック等の欠
陥が発生し、その後さらに溶接補修により修正しなけれ
ば所定の形状、寸法、品質が得られないとい2大きな欠
点がある。
側に拘束リング(角形または丸棒)を取付けておき拘束
リングに沿って溶接する方法であるが、殆んどの場合溶
接熱により端部に著しい収縮及びヘアークラック等の欠
陥が発生し、その後さらに溶接補修により修正しなけれ
ば所定の形状、寸法、品質が得られないとい2大きな欠
点がある。
本発明の目的は肉盛溶接により生ずる不具合部を完全に
除去し、以後の溶接補修を要さない健全な溶接部を得る
ことにある。
除去し、以後の溶接補修を要さない健全な溶接部を得る
ことにある。
本発明は溶接熱により収縮および欠陥の発生が避けられ
ないことを考慮し、その発生位置を本来必要としない部
位に集中させ、溶接完了後機械加工により完全に除去で
きるよう素材の段階であらかじめ7う/ジ内側に突起部
を設けるようにしたものである。
ないことを考慮し、その発生位置を本来必要としない部
位に集中させ、溶接完了後機械加工により完全に除去で
きるよう素材の段階であらかじめ7う/ジ内側に突起部
を設けるようにしたものである。
以下、本発明の一実施例を第1図〜第8図により説明す
る。熱交換器1は胴体2と水室3から構成され・管板4
はパツキン5を介し氷室フランジ6と接続される。海水
冷却形熱交換器の場合管板4は通常炭素鋼にモネル、ア
ルミプラス等の耐食性合金を爆着したものを使用し、こ
れと相対するフランジ6は通常炭素鋼で海水に接触する
部分のみ管板と同材質の合金を肉盛の上側用する。
る。熱交換器1は胴体2と水室3から構成され・管板4
はパツキン5を介し氷室フランジ6と接続される。海水
冷却形熱交換器の場合管板4は通常炭素鋼にモネル、ア
ルミプラス等の耐食性合金を爆着したものを使用し、こ
れと相対するフランジ6は通常炭素鋼で海水に接触する
部分のみ管板と同材質の合金を肉盛の上側用する。
従来技術では、拘束リング7″!、たは8をあらかじめ
フランジ内面に仮付溶接しておき肉盛溶接完了後機械加
工により所定の形状、寸法に仕上げているが、異材溶接
のため殆んどの場合第5図及び第6図の如く収縮および
ヘアークラック等の溶接欠陥が拘束リングとの境界部付
近に発生し、再度溶接により補修しなければ所定の形状
、品質が得られないという大きな問題点がある。
フランジ内面に仮付溶接しておき肉盛溶接完了後機械加
工により所定の形状、寸法に仕上げているが、異材溶接
のため殆んどの場合第5図及び第6図の如く収縮および
ヘアークラック等の溶接欠陥が拘束リングとの境界部付
近に発生し、再度溶接により補修しなければ所定の形状
、品質が得られないという大きな問題点がある。
第2図及び第8図は本発明の要点を表わしたもので、素
材10の段階でフランジ内面にあらかじめ突起部9を設
けておけば肉盛溶接時生ずる収縮及び欠陥はすべてこの
突起部に集中し、本来必要とする部分には影響が及ばな
いため溶接完工後の機械加工によりこれらの不具合部は
完全に除去され、第8図の如く健全な肉盛溶接部が得ら
れることになる。
材10の段階でフランジ内面にあらかじめ突起部9を設
けておけば肉盛溶接時生ずる収縮及び欠陥はすべてこの
突起部に集中し、本来必要とする部分には影響が及ばな
いため溶接完工後の機械加工によりこれらの不具合部は
完全に除去され、第8図の如く健全な肉盛溶接部が得ら
れることになる。
本発明によれば一回の溶接及び機械加工により所定の形
状、寸法〃5得られるので、溶接補修による修正作業が
一切不要となるだけでなく、品質管理の上でも顕著な効
果がある。
状、寸法〃5得られるので、溶接補修による修正作業が
一切不要となるだけでなく、品質管理の上でも顕著な効
果がある。
第9図は本発明の他の実施例を示すもので、第7図と異
なるのは突起部が外面側に位置していることであるが、
フランジの場合と同様の効果がある。
なるのは突起部が外面側に位置していることであるが、
フランジの場合と同様の効果がある。
第1図(a)は管式熱交換器の外形図、第1図(b)は
A部の詳細図、第2図は氷室フランジの素材形状図、第
3図及び第4図は従来技術による施工要領図、第5図及
び第6図は従来技術による不具合発生状況図、第7図は
本発明による施工要領図、第8図は最終仕上り形状図、
第9図は応用施工例を示す図である。 1・・・熱交換器本体、2・・・胴体、3・・・水室、
4・・・管板、5・・・パツキン、6・・・フランジ、
7・・・角形拘束リング、8・・・丸棒拘束リング、9
・・・突起部、10第 1 図 (α) (b) 第20 第32 第40 第S図 系60 第7 図 第8 区
A部の詳細図、第2図は氷室フランジの素材形状図、第
3図及び第4図は従来技術による施工要領図、第5図及
び第6図は従来技術による不具合発生状況図、第7図は
本発明による施工要領図、第8図は最終仕上り形状図、
第9図は応用施工例を示す図である。 1・・・熱交換器本体、2・・・胴体、3・・・水室、
4・・・管板、5・・・パツキン、6・・・フランジ、
7・・・角形拘束リング、8・・・丸棒拘束リング、9
・・・突起部、10第 1 図 (α) (b) 第20 第32 第40 第S図 系60 第7 図 第8 区
Claims (1)
- 1゜溶接により生ずる収縮および欠陥を集中させること
を目的として、内面に突起部を設けたことを特徴とする
肉盛溶接フランジの製作方法。