JPS58120800A - 軽金属の表面処理法 - Google Patents

軽金属の表面処理法

Info

Publication number
JPS58120800A
JPS58120800A JP416082A JP416082A JPS58120800A JP S58120800 A JPS58120800 A JP S58120800A JP 416082 A JP416082 A JP 416082A JP 416082 A JP416082 A JP 416082A JP S58120800 A JPS58120800 A JP S58120800A
Authority
JP
Japan
Prior art keywords
alloy
spraying
surface treatment
aluminum
light metal
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP416082A
Other languages
English (en)
Inventor
Masakatsu Mushiro
莚 正勝
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP416082A priority Critical patent/JPS58120800A/ja
Publication of JPS58120800A publication Critical patent/JPS58120800A/ja
Pending legal-status Critical Current

Abstract

(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。

Description

【発明の詳細な説明】 アルミニウムの表面処理法として、陽極酸化法は古くよ
り広く普及している。しかし、ケイ素や銅を多く含有す
るアルミニウム合金には良質な皮膜を形成させることが
困難な現状にある。また、マグネシウムあるいはその合
金にはアルミニウムの陽極酸化皮膜に匹敵する性能を有
する表面処理d;か未だに確立されていない。
本発明はこれらの軽金属素材に、アルミニウムまたはそ
の合金を溶射することにより、陽極酸化性を昔しく向上
させることを特徴としている。
溶射は鉄鋼上への亜鉛やアルミニウムの溶射のように、
防食を目的とする利用をはしめ、ジェットエンジン部品
なとへの耐熱、耐摩耗材料による被覆、あるいは電動機
などの回転軸や印刷ローラーなどへの補修Iζ広く利用
されている。しかし、軽金属またはその合金上に、陽極
酸化性の向上を目的として、アルミニウムないしはその
合金を溶射した例は無い。
本発明によれば、従来、陽極酸化か困難であったA、D
C−IQやADC−12に代表されるアルミダイカスト
あるいはマグネシウム素材などに対して純アルミニウム
の陽極酸化皮膜に匹敵する性能を有する皮膜を容易に形
成することができる。
特にADC,−10およびADC−12は、アルミダイ
カストの生産量の90%以上を占めているにも拘らず、
その陽極酸化性の問題から、大部分が止むなく、塗装な
いしは表面処理熱して使用されるため、用途上の制約が
大きく、本発明の適用による工業的な効果は大きい。
実施例1 素材 ADC−12 溶射法ニアルミ粉末のプラズマ溶射 溶射後の処理:0.4mmφのスティールショット後、
200 メソシュのガラスピ ーズショット 陽極酸化:15%硫酸浴、20°G 、  1.5 A
/dm”、30分 染色:水溶性染料、70’C12分 封孔:沸とう水、10分 実施例2 素材:ADC−12 溶射法ニアルミ線のアーク溶射 以下、実施例1に同じ 実施例3 素材:マグネンウム合金(AZ−91C)溶射法:実施
例1に同じ 溶射後の処理二同上 陽極酸化: Na、po、浴 以下、実施例IIこ同じ

Claims (1)

    【特許請求の範囲】
  1. アルミニウムまたはマグネシウムもしくはこれらの合金
    に代表される軽金属素材表面の一部または全面に、アル
    ミニウムまたはその合金を溶射したのちに、陽極酸化処
    理を施すことを特徴とする表面処理法。
JP416082A 1982-01-14 1982-01-14 軽金属の表面処理法 Pending JPS58120800A (ja)