JPS5569252A - Carburizing method for steel - Google Patents

Carburizing method for steel

Info

Publication number
JPS5569252A
JPS5569252A JP14218078A JP14218078A JPS5569252A JP S5569252 A JPS5569252 A JP S5569252A JP 14218078 A JP14218078 A JP 14218078A JP 14218078 A JP14218078 A JP 14218078A JP S5569252 A JPS5569252 A JP S5569252A
Authority
JP
Japan
Prior art keywords
steel
carbon
carbide
spheroidal
point
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP14218078A
Other languages
Japanese (ja)
Other versions
JPS6224499B2 (en
Inventor
Takeshi Naito
Yasutada Kobayashi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Komatsu Ltd
Original Assignee
Komatsu Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Komatsu Ltd filed Critical Komatsu Ltd
Priority to JP14218078A priority Critical patent/JPS5569252A/en
Publication of JPS5569252A publication Critical patent/JPS5569252A/en
Publication of JPS6224499B2 publication Critical patent/JPS6224499B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE:To increase the thermal resistance, wear resistance, and pitting resistance of steel, by carburizing low alloy steel of low- or medium-carbon contg. <0.5% C, <2.4% Cr to form pseudospheroidal or spheroidal carbide of a volume ratio not smaller than 30% in the range of 0.4mm from the surface. CONSTITUTION:Low alloy steel of low- or medium-carbon contg., 0.05-0.50% C, 0.10-0.35% Si, 0.30-2.00% Mn, <5.5% Ni, <2.4% Cr, <0.7% Mo is preliminarily carburized at a carbon potential not higher than Acm point to a carbon quantity on the surface not lower than that of eutectoid, then it is air-cooled or hardened. The steel is heated from Ac1 point to 750-950 deg., the temp. at which carbide is formed, at a heating rate of steel surface not higher than 20 deg.C/min. While maintaining the carbon potential exceeding the Acm point. Then the steel is carburized at the carbide-forming temp. while maintaining the carbon potential exceeding the Acm point to the depth 0.1-0.4mm from the surface, hereby pseudo- spheroidal or spheroidal carbide of volume ratio not smaller than 30% is formed.
JP14218078A 1978-11-20 1978-11-20 Carburizing method for steel Granted JPS5569252A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP14218078A JPS5569252A (en) 1978-11-20 1978-11-20 Carburizing method for steel

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP14218078A JPS5569252A (en) 1978-11-20 1978-11-20 Carburizing method for steel

Publications (2)

Publication Number Publication Date
JPS5569252A true JPS5569252A (en) 1980-05-24
JPS6224499B2 JPS6224499B2 (en) 1987-05-28

Family

ID=15309223

Family Applications (1)

Application Number Title Priority Date Filing Date
JP14218078A Granted JPS5569252A (en) 1978-11-20 1978-11-20 Carburizing method for steel

Country Status (1)

Country Link
JP (1) JPS5569252A (en)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61104065A (en) * 1984-10-26 1986-05-22 Daido Steel Co Ltd Carburized part
JPH05263130A (en) * 1992-03-19 1993-10-12 Sumitomo Metal Ind Ltd Heat treatment for steel material
WO2008056552A1 (en) * 2006-11-06 2008-05-15 Honda Motor Co., Ltd. Process for producing high-concentration carburized steel
CN111549314A (en) * 2020-05-21 2020-08-18 湖南特科能热处理有限公司 Carburizing process for low-carbon steel thin-wall part
CN112313350A (en) * 2018-06-18 2021-02-02 株式会社小松制作所 Method for manufacturing machine component

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101115859B (en) 2005-02-08 2011-05-18 帕卡热处理工业株式会社 High-concentration carburized/low-strain quenched member and process for producing the same
JP5408465B2 (en) * 2008-07-24 2014-02-05 アイシン精機株式会社 Method of carburizing steel
JP2022108676A (en) 2021-01-13 2022-07-26 日本精工株式会社 Linear motion guide device

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5541908A (en) * 1978-09-14 1980-03-25 Hinode Kinzoku Netsuren Kk Surface hardening method of steel

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5541908A (en) * 1978-09-14 1980-03-25 Hinode Kinzoku Netsuren Kk Surface hardening method of steel

Cited By (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61104065A (en) * 1984-10-26 1986-05-22 Daido Steel Co Ltd Carburized part
JPH07828B2 (en) * 1984-10-26 1995-01-11 大同特殊鋼株式会社 Carburized parts
JPH05263130A (en) * 1992-03-19 1993-10-12 Sumitomo Metal Ind Ltd Heat treatment for steel material
WO2008056552A1 (en) * 2006-11-06 2008-05-15 Honda Motor Co., Ltd. Process for producing high-concentration carburized steel
JP2008115427A (en) * 2006-11-06 2008-05-22 Daido Steel Co Ltd Method for manufacturing steel carburized into high carbon concentration
EP2085493A1 (en) * 2006-11-06 2009-08-05 Honda Motor Co., Ltd Process for producing high-concentration carburized steel
EP2085493A4 (en) * 2006-11-06 2009-11-25 Honda Motor Co Ltd Process for producing high-concentration carburized steel
CN112313350A (en) * 2018-06-18 2021-02-02 株式会社小松制作所 Method for manufacturing machine component
CN111549314A (en) * 2020-05-21 2020-08-18 湖南特科能热处理有限公司 Carburizing process for low-carbon steel thin-wall part

Also Published As

Publication number Publication date
JPS6224499B2 (en) 1987-05-28

Similar Documents

Publication Publication Date Title
JPS5569252A (en) Carburizing method for steel
JPS5524932A (en) Manufacture of bainite tough hardening steel
JPS5496418A (en) Heat resistant cast steel
JPS56130422A (en) Heat treatment of spheroidal graphite cast iron roll for hot rolling
KR910016565A (en) Manufacturing method of tracked bushing of vehicle
JPS5794516A (en) Method for heat treatment on low-carbon boron steel
JPS552789A (en) Touch, wear resistant steel
JPS5534687A (en) Precipitation hardening type hot working tool steel
JPS54104425A (en) Heat treating method for high chromium white cast iron
JPS57110621A (en) Heat treatment of uoe steel pipe capable of obtaining high-toughness welded metal
JPS5613466A (en) Heat resistant steel
JPS5444122A (en) Manufacturing method of welded valve
JPS5465116A (en) Wear resistant cast iron
Krejcik Special Heat Treatment Processes for Improved Performance and Anisotropy in Tool Steels
JPS56116870A (en) Ring for spinning machine
JPS565952A (en) Carbonitriding steel
FR2442281A1 (en) Cementation process for low alloy steels - with a pre-cementation step in an atmos. for forming a hypereutectoid hardening, then cementation of nuclei formed
Ionica et al. Aspects of the Effect of Retained Austenite on Service Behavior of Carburized 18 MoCN 13 Steel Gears
Lysak et al. Effect of Preliminary Heating of Austenite on the Martensite Transformation in a Nickel Steel
Lunika Effect of Alloying on the Hardenability and Tempering Characteristics of Graphitized Steels
JPS5472712A (en) Wear resistant cast steel for low temperature use
JPS5747847A (en) Pump lever for pile hammer and its heat treatment
Spies Optimization of Part Properties in Heat Treatment
Ognevskii Use of Steel 45 for Induction Hardening of an Automobile Differential Cross-Piece
JPS54124816A (en) Highly tough and wear resistant steel