JPS55167127A - Continuously converting method for anhydrous gypsum into gypsum - Google Patents
Continuously converting method for anhydrous gypsum into gypsumInfo
- Publication number
- JPS55167127A JPS55167127A JP7451479A JP7451479A JPS55167127A JP S55167127 A JPS55167127 A JP S55167127A JP 7451479 A JP7451479 A JP 7451479A JP 7451479 A JP7451479 A JP 7451479A JP S55167127 A JPS55167127 A JP S55167127A
- Authority
- JP
- Japan
- Prior art keywords
- gypsum
- vessel
- slurry
- hydration
- hydrated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To obtain coarse gypsum crystals, which were difficult to obtain formerly, by maintaining a slurry of by-product anhydrous gypsum and an aqueous soln. of a specified hydration accelerator at a specified temp., agitating the slurry to hydrate it, pH-adjusting the hydrated slurry with a Ca compound, and separating gypsum.
CONSTITUTION: Slurry 5 of by-product anhydrous sypsum 4 of a hydrofluoric acid manufacturing process and an aqueous soln. of a hydration accelerator consisting of sodium sulfate or potassium sulfate 1 and sodium chloride 2 is passed through primary hydration vessel 6 and secondary hydration vessel 7, maintained at 30°C or below with refrigerator 8, and hydrated by agitation. Part of the hydrate is recycled to vessel 6 as seed crystals, and the remaining hydrated slurry is adjusted to pH 6.5W8 with quick lime or the like in vessel 10 and passed through vessel 11 and dehydrator 12 to separate gypsum 16. Soln. 14 and part of washing liq. 15 are recycled. Gypsum 16 thus obtd. is coarse crystals and can be utilized as starting material gypsum for gypsum plaster board, plaster, etc.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7451479A JPS603007B2 (en) | 1979-06-13 | 1979-06-13 | Method for continuously converting anhydrite to dihydrate |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7451479A JPS603007B2 (en) | 1979-06-13 | 1979-06-13 | Method for continuously converting anhydrite to dihydrate |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS55167127A true JPS55167127A (en) | 1980-12-26 |
JPS603007B2 JPS603007B2 (en) | 1985-01-25 |
Family
ID=13549509
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7451479A Expired JPS603007B2 (en) | 1979-06-13 | 1979-06-13 | Method for continuously converting anhydrite to dihydrate |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS603007B2 (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2009040638A (en) * | 2007-08-09 | 2009-02-26 | Tokuyama Corp | Manufacture method of gypsum dihydrate |
JP2010013304A (en) * | 2008-07-02 | 2010-01-21 | Tokuyama Corp | Method for regenerating gypsum from gypsum board waste material |
CN109305791A (en) * | 2018-10-31 | 2019-02-05 | 曲靖师范学院 | A kind of hydration curing coagulant of β semi-hydrated gypsum phenolphthalein class acceleration |
CN110589869A (en) * | 2019-09-09 | 2019-12-20 | 湖北工业大学 | Method for preparing alpha high-strength gypsum by using chlor-alkali byproduct salt gypsum and chemical waste salt in normal-pressure salt solution method |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS61201272U (en) * | 1985-06-05 | 1986-12-17 |
-
1979
- 1979-06-13 JP JP7451479A patent/JPS603007B2/en not_active Expired
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2009040638A (en) * | 2007-08-09 | 2009-02-26 | Tokuyama Corp | Manufacture method of gypsum dihydrate |
JP2010013304A (en) * | 2008-07-02 | 2010-01-21 | Tokuyama Corp | Method for regenerating gypsum from gypsum board waste material |
CN109305791A (en) * | 2018-10-31 | 2019-02-05 | 曲靖师范学院 | A kind of hydration curing coagulant of β semi-hydrated gypsum phenolphthalein class acceleration |
CN110589869A (en) * | 2019-09-09 | 2019-12-20 | 湖北工业大学 | Method for preparing alpha high-strength gypsum by using chlor-alkali byproduct salt gypsum and chemical waste salt in normal-pressure salt solution method |
Also Published As
Publication number | Publication date |
---|---|
JPS603007B2 (en) | 1985-01-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4120737A (en) | Manufacture of calcium sulphate alpha hemihydrate | |
GB1016007A (en) | Improvements in or relating to the production of phosphoric acid and calcium sulphate | |
JPS5370097A (en) | Purifying method for crude sodium silicofluoride | |
GB1025236A (en) | Process for the manufacture of dicalcium phosphate | |
JPS55167127A (en) | Continuously converting method for anhydrous gypsum into gypsum | |
ES8603210A1 (en) | Process of producing manganese sulfate solutions | |
GB1505146A (en) | Recovery of fluorine and phosphate values from waste wate | |
GB1103206A (en) | Process for the purification of residual gypsum arising in the manufacture of phosphoric acid by sulphuric reaction of natural phosphates | |
DE3161703D1 (en) | Process for the preparation of phosphoric acid and calcium sulphate anhydrite | |
TW201540668A (en) | Method for recycling ammonium sulfate to manufacture dihydrate gypsum | |
EP0096063B1 (en) | Process for rapid conversion of fluoroanhydrite to gypsum | |
US3615186A (en) | Process of making hydrates of potassium-magnesium phosphates | |
US4379776A (en) | Process for reducing aluminum and fluorine in phosphoric acids | |
US3489510A (en) | Treatment of phosphate rock with acidic substances and to the resulting superphosphate products | |
JPS5299992A (en) | Production of alpha-type hemihydrate gypsum of prismatic crystal from phosphoric acid by-product dihydrate gypsum | |
JPS5527877A (en) | Production of high purity calcium secondary phosphate and ammonium chloride | |
CA1206980A (en) | Conversion of fluoroanhydrite to plaster | |
JPS57129823A (en) | Manufacture of magnesium potassium sulfate by simultaneous chemical reaction of magnesium hydroxide, potassium chloride and sulfuric acid, and manufacture of potassium sulfate | |
JPH08225320A (en) | Modification of alpha-hemihydrate gypsum obtained as by-product of wet-process for producing phosphoric acid | |
GB848617A (en) | Improvements in or relating to the preparation of anhydrite | |
SU948895A1 (en) | Method for processing waste liquors from iodine and bromine production | |
JPS55162427A (en) | Manufacture of alpha-type hemihydrate gypsum | |
JPS5641815A (en) | Purifying method for wet process phosphoric acid solution | |
JPS5299993A (en) | Production of 2-type alpha hemihydrate gypsum of needle-like crystal from phosphoric acid by-product dihydrate gypsum | |
SU1323532A1 (en) | Method of producing phosphoric acid |