Japan
Prior art keywords
chitin
water
alkali
under pressure
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP6166079A
Other languages
Japanese (ja)
Other versions
JPS6121242B2 (en
Inventor
Junzo Noguchi
Akio Tateishi
Takeji Otani
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Rayon Co Ltd
Original Assignee
Mitsubishi Rayon Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Rayon Co Ltd filed Critical Mitsubishi Rayon Co Ltd
Priority to JP6166079A priority Critical patent/JPS55152703A/en
Publication of JPS55152703A publication Critical patent/JPS55152703A/en
Publication of JPS6121242B2 publication Critical patent/JPS6121242B2/ja
Granted legal-status Critical Current

Links

Abstract

PURPOSE: To obtain an alkali chitin, completely soluble in ice water, which is under consideration as a replacement for the biological membrane, by boiling chitin under pressure at a high temperature with addition of water, and then treating it with an aqueous alkali solution.
CONSTITUTION: Chitin is mixed with water and the mixture is boiled at 0.1W 5kg/cm2, preferably 1W25kg/cm2, at 103W160°C, preferably 110W140°C. The obtained gruel-like substance is filtered, and the resulting bean curd refuse-like chitin powder is loosened and impregnated with an alkali under pressure after addition of an aqueous alkali solution at 15°C. It is then frozen, thawed and impregnated again with the alkali under pressure, to obtain an alkali chitin, which is homogeneously soluble in ice water. 0.1W1,000pts.wt., preferably 1W100pts.wt. of water is added to 1pts.wt. of chitin, and the period of time for the treatment is preferably 30minW10hr.
COPYRIGHT: (C)1980,JPO&Japio
JP6166079A 1979-05-18 1979-05-18 Preparation of water-soluble alkali chitin Granted JPS55152703A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6166079A JPS55152703A (en) 1979-05-18 1979-05-18 Preparation of water-soluble alkali chitin

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6166079A JPS55152703A (en) 1979-05-18 1979-05-18 Preparation of water-soluble alkali chitin

Publications (2)

Publication Number Publication Date
JPS55152703A true JPS55152703A (en) 1980-11-28
JPS6121242B2 JPS6121242B2 (en) 1986-05-26

Family

ID=13177592

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6166079A Granted JPS55152703A (en) 1979-05-18 1979-05-18 Preparation of water-soluble alkali chitin

Country Status (1)

Country Link
JP (1) JPS55152703A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61255902A (en) * 1985-05-09 1986-11-13 Lion Corp Production of activated chitin and chitosan
CN110128567A (en) * 2019-05-13 2019-08-16 金陵科技学院 The method for preparing environmentally friendly reinforcing steel bar corrosion inhibitor using natural biomass chitin high polymer

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61255902A (en) * 1985-05-09 1986-11-13 Lion Corp Production of activated chitin and chitosan
CN110128567A (en) * 2019-05-13 2019-08-16 金陵科技学院 The method for preparing environmentally friendly reinforcing steel bar corrosion inhibitor using natural biomass chitin high polymer
CN110128567B (en) * 2019-05-13 2021-03-16 金陵科技学院 Method for preparing environment-friendly type reinforcement corrosion inhibitor by using natural biomass chitin high polymer

Also Published As

Publication number Publication date
JPS6121242B2 (en) 1986-05-26

Similar Documents

Publication Publication Date Title
JPS55152705A (en) Preparation of water-soluble alkali chitin
JPS55152703A (en) Preparation of water-soluble alkali chitin
JPS55152704A (en) Preparation of alkali chitin
JPS5420196A (en) Preparation of anticarcinogen
JPS5675078A (en) Preparation of snapping turtle powder
JPS57125676A (en) Preparation of powdered calcium compound used as a food additive
JPS5458245A (en) Freezing liquid for wet freezing
JPS565056A (en) Feed additive for cultured aquatic life
JPS5739733A (en) Preparation of molded dried vegetable
JPS5548372A (en) Preparation of heat-resistant agar noodles
JPS5716670A (en) Preparation of frozen "tofu"
JPS57152882A (en) Method for killing living general chlorella
JPS5521713A (en) Food composition preservable for long time
JP3058895B2 (en) Oil temperature dehydration method for starfish
JPS5733568A (en) Preparation of "konjak" (devil's-tongue jelly) containing tea made from mugwort
JPS5554033A (en) Disoxidant
JPS5736958A (en) Deodorizing, processing and preparing technique for making krill into food
JPS5635948A (en) Preparing method of solid food containing flesh extract from ume as main constituent
JPS5537119A (en) Preparation of instant creaming powder
JPS5399317A (en) Method for preparing solid compositions
JPS5750858A (en) Preparation of raw material for salt-free food with high proteinic content
JPS55138371A (en) Preparation of flavor formulation
JPS5774063A (en) Preparation of aquatic paste product
JPS5515728A (en) Food antiseptic
JPS55120766A (en) Prparation of powdered fermented soybean