JPH0924496A - Cip mold - Google Patents

Cip mold

Info

Publication number
JPH0924496A
JPH0924496A JP17343695A JP17343695A JPH0924496A JP H0924496 A JPH0924496 A JP H0924496A JP 17343695 A JP17343695 A JP 17343695A JP 17343695 A JP17343695 A JP 17343695A JP H0924496 A JPH0924496 A JP H0924496A
Authority
JP
Japan
Prior art keywords
mold
die
molding
cip
rubber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
JP17343695A
Other languages
Japanese (ja)
Inventor
Takeo Sasaki
丈夫 佐々木
Keiichi Iida
恵一 飯田
Masaharu Yamada
雅治 山田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Materials Corp
Original Assignee
Mitsubishi Materials Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Materials Corp filed Critical Mitsubishi Materials Corp
Priority to JP17343695A priority Critical patent/JPH0924496A/en
Publication of JPH0924496A publication Critical patent/JPH0924496A/en
Withdrawn legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To prevent the infiltration of a pressure medium by preventing the failure of a CIP mold at the time of pressure molding. SOLUTION: Cap-like rubber molds 1, 2 erected with wall-like parts 1A, 2A to be put on the outer peripheral surface of a rubber cylindrical mold 13 are put thereon and are provided with sealing taps 5A, 5B across the front ends of these wall-like parts 1A, 2A and the outer peripheral surface of the rubber cylindrical mold 13. As a result, the sealing tapes are protected by the wall-like parts 1A, 2A to prevent the peeling and breaking of the sealing tapes when powder S is compressed and deformed. The failure of the rubber cylindrical mold 13 is prevented as well in the parts in contact with the end edges of the metal molds and the joint parts of the molds. The infiltration of the pressure medium into the mold 10 is surely prevented and the failure of the molding by the infiltration of the pressure medium is prevented. The easy and efficient molding of the moldings having desired shapes at a good yield is possible even with the large-sized or thick-shaped parts.

Description

【発明の詳細な説明】Detailed Description of the Invention

【0001】[0001]

【発明の属する技術分野】本発明は、粉体を冷間静水圧
加圧(Cold Isostatic Press:CIP)して成形体を得るた
めのCIP成形型に係り、詳しくは、大型又は厚肉形状
の成形体であっても所期の形状に容易に成形することが
できるCIP成形型に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a CIP molding die for obtaining a compact by cold isostatic pressing (CIP) of powder, and more specifically, it has a large or thick shape. The present invention relates to a CIP mold capable of easily molding a molded body into a desired shape.

【0002】[0002]

【従来の技術】セラミックス等の各種粉体の成形方法と
してCIP成形法が知られている。CIP成形法は、成
形型内に粉体を充填し、水又は油等の加圧媒体を介して
該成形型を外方から等方的に加圧して成形する方法であ
り、使用される成形型の少なくとも一部は、ゴム等の可
撓性を有した軟質材料で構成されている。成形に使用さ
れる粉体は、通常、スプレードライ造粒粉などの流動性
の良い球状顆粒である。
CIP molding is known as a method for molding various powders such as ceramics. The CIP molding method is a method in which powder is filled in a molding die and isotropically pressurized from the outside through a pressure medium such as water or oil to mold the molding die. At least a part of the mold is made of a flexible soft material such as rubber. The powder used for molding is usually spherical granules having good fluidity such as spray-dried granulated powder.

【0003】図3,4は、肉厚円筒形状の成形体を成形
するために用いられる従来のCIP成形型の断面図であ
る。
3 and 4 are sectional views of a conventional CIP mold used for molding a thick-walled cylindrical molded body.

【0004】図3に示すCIP成形型11は、得られる
成形体の上下面の加工の手間を省くために、上面及び下
面に金型を用い、側周部のみを可撓性のあるゴム型とし
たものであり、成形型の上面を構成する蓋金型12、側
周部を構成するゴム筒型13及び中子部分及び底面を構
成するコア金型14とで構成されている。なお、蓋金型
に代えて、ゴム蓋型を用いたものもある。成形に際して
は、コア金型14にゴム筒型13を取り付け、型同士の
継目部分にシールテープ15Aを貼り、成形型11の成
形用空間内に粉体Sを充填した後、蓋金型12を装着す
る。次いで、型同士の継目部分にシールテープ15Bを
貼り、CIP装置内に装入し、加圧媒体を加圧して成形
を行う。
The CIP mold 11 shown in FIG. 3 uses a mold for the upper surface and the lower surface in order to save the labor of processing the upper and lower surfaces of the obtained molded product, and has a flexible rubber mold only in the side peripheral portion. It is composed of a lid mold 12 that constitutes the upper surface of the molding die, a rubber cylinder mold 13 that constitutes the side peripheral portion, and a core mold 14 that constitutes the core portion and the bottom surface. In addition, instead of the lid mold, there is also one using a rubber lid mold. At the time of molding, the rubber cylindrical mold 13 is attached to the core mold 14, the seal tape 15A is attached to the joint between the molds, the powder S is filled in the molding space of the mold 11, and then the lid mold 12 is attached. Installing. Next, the seal tape 15B is attached to the joint between the molds, the seal tape 15B is loaded into the CIP device, and the pressurizing medium is pressed to perform molding.

【0005】一方、図4のCIP成形型21は、得られ
る成形体の均一性を高めるために、中子のみ金型とし、
外型はすべてゴム型としたものであり、成形型の上面を
構成するゴム蓋型22と、底面及び側部を構成する容器
形状の底付ゴム型23と、芯金型24とで構成されてい
る。このCIP成形型21の場合においても、底付ゴム
型23内に芯金型24を配置して成形用空間に粉体Sを
充填した後、ゴム蓋型22を装着してシールテープ25
を貼り、上記と同様にCIP装置に装入して成形を行
う。
On the other hand, in the CIP molding die 21 of FIG. 4, in order to improve the uniformity of the molded body obtained, only the core is made into a mold,
The outer molds are all rubber molds, and are composed of a rubber lid mold 22 that constitutes the upper surface of the molding mold, a container-shaped rubber mold 23 that composes the bottom surface and side portions, and a core metal mold 24. ing. Also in the case of this CIP molding die 21, after placing the core metal die 24 in the bottomed rubber die 23 to fill the molding space with the powder S, the rubber lid die 22 is attached and the sealing tape 25 is attached.
Then, the CIP device is charged and molded in the same manner as above.

【0006】なお、成形に当り、シールテープによるシ
ール部分から成形型内に水や油等の加圧媒体が浸入する
のを防止するため、或いは、成形型が水や油等の加圧媒
体に濡れることを防止するために、成形型全体を薄手の
ビニール袋やゴム袋に入れてCIP装置に装入すること
も行われている。
[0006] In molding, in order to prevent a pressurized medium such as water or oil from entering the molding die from the sealing portion of the seal tape, or the molding die is exposed to a pressurized medium such as water or oil. In order to prevent getting wet, it is also practiced to put the entire molding die in a thin vinyl bag or rubber bag and load it in the CIP device.

【0007】[0007]

【発明が解決しようとする課題】このような従来の成形
型に粉体を充填してCIP成形を行う場合、特に、大型
形状や肉厚形状の成形体をCIP成形する場合におい
て、加圧時に粉体が大きく圧縮されるため、シールテー
プによるシール部分が剥れたり、切れたり、或いは、金
型に接触したゴム型が切れる等して加圧媒体(水や油な
ど)が成形型内に浸入し、成形体が破損することがあ
る。
When CIP molding is carried out by filling powder into such a conventional molding die, particularly in the case of CIP molding of a large-sized or thick-walled molded body, at the time of pressurization. The powder is compressed so much that the sealing tape peels off or breaks, or the rubber mold that comes into contact with the mold breaks, so that the pressure medium (water, oil, etc.) enters the mold. It may penetrate and damage the molded body.

【0008】即ち、例えば、図3に示す成形型11の場
合には、図5に示す如く、加圧時に粉体Sが径方向に圧
縮されるが、その際に、ゴム筒型13の蓋金型12及び
コア金型14の縁部に接触した部分Aに亀裂が入り、そ
こから加圧媒体が浸入することがある。
That is, for example, in the case of the molding die 11 shown in FIG. 3, as shown in FIG. 5, the powder S is compressed in the radial direction at the time of pressurization. A portion A contacting the edges of the mold 12 and the core mold 14 may be cracked, and the pressurized medium may penetrate from there.

【0009】一方、図4に示す成形型21の場合には、
図6に示す如く、加圧時に粉体Sが上下及び径方向に圧
縮される際にゴム型22と23との継目部分で破損がお
き、加圧媒体が浸入することがある。
On the other hand, in the case of the molding die 21 shown in FIG.
As shown in FIG. 6, when the powder S is compressed in the vertical and radial directions at the time of pressurization, the joint portion between the rubber molds 22 and 23 may be damaged and the pressurizing medium may infiltrate.

【0010】成形型全体を薄手のビニール袋やゴム袋に
装入してCIP成形を行った場合でも、これらの袋も実
際には局部的に引っ張られて破損するため、実用上、上
記加圧媒体の浸入防止効果は得られない。
Even when the entire molding die is put in a thin vinyl bag or a rubber bag and CIP molding is performed, these bags are actually pulled locally and damaged, so that the above-mentioned pressure is applied in practice. The effect of preventing penetration of the medium cannot be obtained.

【0011】本発明は上記従来の加圧媒体浸入の問題を
解決し、大型形状や肉厚形状の成形体でも、良好な成形
体を得ることを可能とするCIP成形型を提供すること
を目的とする。
It is an object of the present invention to provide a CIP molding die which solves the above-mentioned problem of the penetration of a pressurized medium and enables to obtain a good molded product even in a large-sized or thick-walled molded product. And

【0012】[0012]

【課題を解決するための手段】請求項1のCIP成形型
は、被成形物の側周面を囲む軟質な第1の外型と、被成
形物の上側及び/又は下側に配置される軟質な第2の外
型と、該第1の外型と第2の外型との継目部の外面に付
着されたシールテープとを備えるCIP成形型におい
て、該第2の外型は、前記第1の外型の外周面に被さる
壁状部がその外周縁に立設されており、前記シールテー
プは、該壁状部の先端縁と前記第1の外型の外周面とに
股がるように付着されていることを特徴とする。
A CIP molding die according to claim 1 is arranged on a soft first outer mold surrounding a side peripheral surface of a molding target and on an upper side and / or a lower side of the molding target. A CIP molding die including a soft second outer die and a seal tape attached to an outer surface of a joint portion between the first outer die and the second outer die, wherein the second outer die is A wall-shaped portion covering the outer peripheral surface of the first outer die is erected on the outer peripheral edge thereof, and the seal tape has a crotch between the tip edge of the wall-shaped portion and the outer peripheral surface of the first outer die. It is characterized in that it is attached as.

【0013】このCIP成形型によれば、成形型の上面
及び/又は底面を構成する第2の外型の外周縁に、成形
型の外周面を構成する第1の外型の外周面に被さる壁状
部が立設されているため、この壁状部による保護効果
で、加圧により粉体が圧縮変形した際に、シールテープ
が剥れたり、破損したりすることがなく、また、金型の
端縁部に接触した部分や継目部分において、軟質な第1
の外型が破損することも防止される。このため、水や油
などの加圧媒体の浸入が確実に防止され、加圧媒体の浸
入による成形体の破損も防止される。
According to this CIP mold, the outer peripheral edge of the second outer mold constituting the upper surface and / or the bottom surface of the mold is covered with the outer peripheral surface of the first outer mold constituting the outer peripheral surface of the mold. Since the wall-shaped part is erected, the protective effect of this wall-shaped part prevents the seal tape from peeling off or being damaged when the powder is compressed and deformed by the pressure. At the part that touches the edge of the mold and the seam, the soft first
It is also prevented that the outer mold of the is damaged. Therefore, intrusion of a pressurized medium such as water or oil is reliably prevented, and damage to the molded body due to infiltration of the pressurized medium is also prevented.

【0014】請求項2のCIP成形型は、請求項1にお
いて、前記第1の外型は筒状型であり、前記第2の外型
は、該筒状型の底部に装着された底型と、上部に装着さ
れた蓋型とからなることを特徴とする。
According to a second aspect of the present invention, in the CIP molding die according to the first aspect, the first outer die is a tubular die, and the second outer die is a bottom die mounted on a bottom portion of the tubular die. And a lid type attached to the upper part.

【0015】請求項3のCIP成形型は、請求項1にお
いて、前記第1の外型は、被成形物の側周面と底面とを
囲む容器状型であり、前記第2の外型は、該容器状型の
上面に装着された蓋型からなることを特徴とする。
According to a third aspect of the present invention, there is provided a CIP molding die according to the first aspect, wherein the first outer die is a container-shaped die that surrounds a side peripheral surface and a bottom surface of an object to be molded, and the second outer die. It is characterized by comprising a lid type mounted on the upper surface of the container type.

【0016】[0016]

【発明の実施の形態】以下に図面を参照して本発明のC
IP成形型を詳細に説明する。
BEST MODE FOR CARRYING OUT THE INVENTION C of the present invention will be described below with reference to the drawings.
The IP mold will be described in detail.

【0017】図1,2は各々本発明のCIP成形型の一
実施例を示す断面図であり、図1,2において、図3,
4に示す部材と同一機能を奏する部材には同一符号を付
してある。
FIGS. 1 and 2 are sectional views showing an embodiment of the CIP molding die of the present invention. In FIGS.
The members having the same functions as those of the member shown in FIG.

【0018】図1に示すCIP成形型10は、図3に示
す従来の成形型を改良したものであり、ゴム筒型(第1
の外型)13の外周面に被さる壁状部1A,2Aが外周
縁に立設されたキャップ形状のゴム型(以下「キャップ
状ゴム型」と称す。)1,2を、各々、蓋金型12及び
コア金型14に被せ、このキャップ状ゴム型1,2の壁
状部1A,2Aの先端縁とゴム筒型13の外周面とに股
がるようにシールテープ5B,5Aを付着させたもので
ある。
The CIP molding die 10 shown in FIG. 1 is an improved version of the conventional molding die shown in FIG.
Outer mold 13), and cap-shaped rubber molds (hereinafter, referred to as “cap-shaped rubber molds”) 1 and 2 in which wall-shaped portions 1A and 2A covering the outer peripheral surface of the outer mold 13 are erected on the outer peripheral edge, respectively. Cover the mold 12 and the core mold 14, and attach the seal tapes 5B and 5A so as to groin the tip edges of the wall-shaped portions 1A and 2A of the cap-shaped rubber molds 1 and the outer peripheral surface of the rubber cylindrical mold 13. It was made.

【0019】このような成形型10を用いてCIP成形
を行うには、コア金型14にゴム筒型13を取り付け、
型同士の継目部分にシールテープ(図示せず)を貼り、
更に、キャップ状ゴム型2を被せてシールテープ5Aを
貼った後、成形型10の成形用空間内に粉体Sを充填す
る。その後、蓋金型12を装着し、蓋金型12とゴム筒
型13との継目をシールテープ(図示せず)で止め、更
に、キャップ状ゴム型1を被せ、キャップ状ゴム型1と
ゴム筒型13との継目をシールテープ5Bで止める。そ
して、この成形型10をCIP成形装置に入れてCIP
成形する。
In order to perform CIP molding using such a molding die 10, a rubber tube mold 13 is attached to a core mold 14,
Stick a seal tape (not shown) on the seam between the molds,
Further, after covering the cap-shaped rubber die 2 and sticking the seal tape 5A, the powder S is filled in the molding space of the molding die 10. After that, the lid mold 12 is attached, the joint between the lid mold 12 and the rubber tube mold 13 is stopped with a seal tape (not shown), and the cap-shaped rubber mold 1 is covered, and the cap-shaped rubber mold 1 and the rubber The joint with the tubular mold 13 is stopped with the sealing tape 5B. Then, the molding die 10 is put into a CIP molding device to perform CIP
Molding.

【0020】このCIP成形型10によれば、キャップ
状ゴム型1,2でゴム筒型13と金型12,14との継
目が保護され、粉体Sが径方向に縮径した際にゴム筒型
13に亀裂が入ることが防止されるため、加圧媒体が浸
入して成形体が破損することなく大型、肉厚形状の成形
体であっても良好な成形を行える。
According to this CIP mold 10, the seams between the rubber tube mold 13 and the molds 12, 14 are protected by the cap-shaped rubber molds 1, 2, and the rubber is used when the powder S is reduced in diameter in the radial direction. Since the cylindrical mold 13 is prevented from being cracked, the molding medium is not damaged by the intrusion of the pressurizing medium, and good molding can be performed even with a large-sized, thick-walled molded body.

【0021】図2のCIP成形型20は、図4に示すC
IP成形型を改良したものであり、ゴム蓋型22に代え
て、底付ゴム型23の側周面に被さる壁状部3Aが外周
縁に立設されたキャップ状ゴム型3を設け、このキャッ
プ状ゴム型3の壁状部3Aの先端縁と底付ゴム型23の
側周面とに股がるようにシールテープ25を貼り付けた
ものである。
The CIP molding die 20 shown in FIG. 2 has a C shape shown in FIG.
This is an improvement of the IP mold, and instead of the rubber lid mold 22, a cap-shaped rubber mold 3 is provided in which a wall-shaped portion 3A covering the side peripheral surface of the bottomed rubber mold 23 is erected on the outer peripheral edge. A sealing tape 25 is attached to the tip end edge of the wall-shaped portion 3A of the cap-shaped rubber die 3 and the side peripheral surface of the bottomed rubber die 23 so as to groin.

【0022】このような成形型20を用いてCIP成形
を行うには、底付ゴム型23内に芯金型24を配置し、
成形用空間内に粉体Sを充填した後、キャップ状ゴム型
3を装着し、キャップ状ゴム型3と底付ゴム型23との
継目をシールテープ25で止める。これをCIP成形装
置に入れて、CIP成形する。
In order to perform CIP molding using such a molding die 20, a core metal die 24 is placed in a rubber die 23 with a bottom,
After the powder S is filled in the molding space, the cap-shaped rubber mold 3 is mounted, and the joint between the cap-shaped rubber mold 3 and the bottomed rubber mold 23 is stopped with the seal tape 25. This is put into a CIP molding device and CIP molding is performed.

【0023】このような成形型20であれば、粉体Sが
上下及び径方向に圧縮されても、キャップ状ゴム型3の
壁状部3Aによる保護効果で、キャップ状ゴム型3と底
付ゴム型23との継目部が破損することがない。このた
め、加圧媒体が浸入して成形体が破損することなく大
型、肉厚形状の成形体であっても良好な成形を行える。
With such a molding die 20, even if the powder S is compressed in the vertical and radial directions, the wall-shaped portion 3A of the cap-shaped rubber die 3 protects the cap-shaped rubber die 3 from the bottom. The joint with the rubber mold 23 is not damaged. Therefore, good molding can be performed even with a large-sized, thick-walled molded body without the pressurized medium penetrating and damaging the molded body.

【0024】なお、一般に、CIP成形型においては、
成形体が大型になる程、成形型に充填された粉体は、自
重により下部では充填密度が高く、上部になる程充填密
度が低くなる傾向がみられる。このため、成形体の上部
は圧縮変形量が大きく、時にはいびつになる等、複雑な
変形をする場合もあるが、本発明によりキャップ状ゴム
型を設けることにより、成形型の保形性が高まり、この
ような変形を防止する効果も得ることができる。
Generally, in the CIP mold,
As the size of the compact increases, the powder filled in the mold tends to have a higher packing density in the lower part due to its own weight and a lower packing density in the upper part. For this reason, the upper portion of the molded body has a large amount of compressive deformation and sometimes becomes complicated such as being distorted. However, by providing the cap-shaped rubber mold according to the present invention, the shape retention of the molding die is enhanced. The effect of preventing such deformation can also be obtained.

【0025】本発明において、成形原料として用いられ
る粉体としては、スプレードライ造粒粉など、流動性に
優れた球状造粒粉体が好適である。また、その材質とし
ては、各種セラミックス粉、金属粉やサーメット粉など
が挙げられる。
In the present invention, the powder used as a forming raw material is preferably a spherical granulated powder having excellent fluidity such as a spray-dried granulated powder. Further, examples of the material thereof include various ceramic powders, metal powders and cermet powders.

【0026】なお、図1,2に示すCIP成形型は、本
発明の一実施例であり、本発明はその要旨を超えない限
り、何ら図示のものに限定されるものではない。例え
ば、図1のCIP成形型において、キャップ状ゴム型
1,2と金型12,14とは、各々、接着により一体化
させたものであっても良い。
The CIP mold shown in FIGS. 1 and 2 is one embodiment of the present invention, and the present invention is not limited to the illustrated one as long as the gist thereof is not exceeded. For example, in the CIP mold of FIG. 1, the cap-shaped rubber molds 1 and 2 and the molds 12 and 14 may be integrated by adhesion.

【0027】本発明において、キャップ状ゴム型の壁状
部の高さは、小さ過ぎるとキャップ状のゴム型を設ける
ことによる本発明の効果が十分に得られず、大き過ぎる
と、装着し難く、また、CIP成形時の加圧力が変化し
たり、徒らに成形型の厚さが厚くなるなどして好ましく
ない。この壁状部の高さは、成形する成形体の大きさや
形状に応じ、加圧時の変形量を考慮して適宜決定される
が、通常の場合、充填された粉体Sの肉厚(図1,2の
L)に対して、該第1の外型の外周面のうち、該壁状部
で覆われた部分の長さ(図1,2のH)が50〜150
%程度となるように壁状部の高さを設定するのが好まし
い。
In the present invention, if the height of the wall portion of the cap-shaped rubber mold is too small, the effect of the present invention due to the provision of the cap-shaped rubber mold cannot be sufficiently obtained, and if it is too large, it is difficult to mount. In addition, the pressure applied during CIP molding is changed, and the thickness of the mold is undesirably increased. The height of the wall-shaped portion is appropriately determined in consideration of the amount of deformation at the time of pressurization according to the size and shape of the molded body to be molded, but in the normal case, the thickness of the filled powder S ( 1, 2), the length (H in FIGS. 1 and 2) of the portion of the outer peripheral surface of the first outer die which is covered by the wall-shaped portion is 50 to 150.
It is preferable to set the height of the wall-shaped portion so as to be about%.

【0028】[0028]

【発明の効果】以上詳述した通り、本発明のCIP成形
型によれば、外型の継目部分のシール性能が良好で、ま
た、大型又は肉厚形状の成形体を成形する場合であって
も、粉体の圧縮変形による破損のおそれがないため、加
圧媒体の浸入が確実に防止され、所期の形状の成形体を
容易かつ効率的に、歩留り良く成形することができる。
As described in detail above, according to the CIP molding die of the present invention, the sealing performance of the seam portion of the outer die is good, and in the case of molding a large or thick shaped body. However, since there is no possibility of damage due to compressive deformation of the powder, it is possible to reliably prevent the pressurizing medium from penetrating, and it is possible to easily and efficiently form a molded body having a desired shape with a good yield.

【0029】[0029]

【図面の簡単な説明】[Brief description of drawings]

【図1】本発明のCIP成形型の一実施例を示す断面図
である。
FIG. 1 is a cross-sectional view showing an embodiment of a CIP mold of the present invention.

【図2】本発明のCIP成形型の他の実施例を示す断面
図である。
FIG. 2 is a sectional view showing another embodiment of the CIP mold of the present invention.

【図3】従来のCIP成形型を示す断面図である。FIG. 3 is a sectional view showing a conventional CIP mold.

【図4】従来のCIP成形型を示す断面図である。FIG. 4 is a sectional view showing a conventional CIP mold.

【図5】図3に示すCIP成形型の破損機構を示す模式
的断面図である。
FIG. 5 is a schematic cross-sectional view showing a damage mechanism of the CIP mold shown in FIG.

【図6】図4に示すCIP成形型の破損機構を示す模式
的断面図である。
FIG. 6 is a schematic cross-sectional view showing a damage mechanism of the CIP mold shown in FIG.

【符号の説明】[Explanation of symbols]

1,2,3 キャップ状ゴム型 1A,2A,3A 壁状部 10,20 CIP成形型 12 蓋金型 13 ゴム筒型 14 コア金型 5A,5B,15A,15B,25 シールテープ 23 底付ゴム型 24 芯金型 S 粉体 1,2,3 Cap-shaped rubber mold 1A, 2A, 3A Wall-shaped part 10,20 CIP molding mold 12 Lid mold 13 Rubber cylinder mold 14 Core mold 5A, 5B, 15A, 15B, 25 Seal tape 23 Bottom rubber Mold 24 Core metal mold S Powder

Claims (3)

【特許請求の範囲】[Claims] 【請求項1】 被成形物の側周面を囲む軟質な第1の外
型と、被成形物の上側及び/又は下側に配置される軟質
な第2の外型と、該第1の外型と第2の外型との継目部
の外面に付着されたシールテープとを備えるCIP成形
型において、 該第2の外型は、前記第1の外型の外周面に被さる壁状
部がその外周縁に立設されており、 前記シールテープは、該壁状部の先端縁と前記第1の外
型の外周面とに股がるように付着されていることを特徴
とするCIP成形型。
1. A soft first outer mold surrounding a side peripheral surface of a molding target, a soft second outer mold disposed on an upper side and / or a lower side of the molding target, and the first outer mold. A CIP molding die comprising a seal tape attached to an outer surface of a joint portion between an outer die and a second outer die, wherein the second outer die is a wall-shaped portion covering an outer peripheral surface of the first outer die. Is erected on the outer peripheral edge thereof, and the seal tape is attached to the tip edge of the wall-shaped portion and the outer peripheral surface of the first outer die so as to groin. Mold.
【請求項2】 請求項1において、前記第1の外型は筒
状型であり、前記第2の外型は、該筒状型の底部に装着
された底型と、上部に装着された蓋型とからなることを
特徴とするCIP成形型。
2. The first outer die according to claim 1, wherein the first outer die is a tubular die, and the second outer die is a bottom die attached to a bottom portion of the tubular die and an upper portion thereof. A CIP molding die comprising a lid mold.
【請求項3】 請求項1において、前記第1の外型は、
被成形物の側周面と底面とを囲む容器状型であり、前記
第2の外型は、該容器状型の上面に装着された蓋型から
なることを特徴とするCIP成形型。
3. The first outer die according to claim 1, wherein
A CIP molding die, which is a container-shaped mold that surrounds a side peripheral surface and a bottom surface of an object to be molded, wherein the second outer mold is a lid mold mounted on an upper surface of the container-shaped mold.
JP17343695A 1995-07-10 1995-07-10 Cip mold Withdrawn JPH0924496A (en)