JPH01134760U - - Google Patents
Info
- Publication number
- JPH01134760U JPH01134760U JP3175388U JP3175388U JPH01134760U JP H01134760 U JPH01134760 U JP H01134760U JP 3175388 U JP3175388 U JP 3175388U JP 3175388 U JP3175388 U JP 3175388U JP H01134760 U JPH01134760 U JP H01134760U
- Authority
- JP
- Japan
- Prior art keywords
- bead
- metal gasket
- periphery
- metal
- laminated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
第1図は本考案の実施例に係る金属ガスケツト
の平面図、第2図は第1図のA―A線における一
部省略の拡大端面図、第3図は本考案の金属ガス
ケツトを使用した積層型金属ガスケツトであつて
、第1図のA―A線部分に相当する位置における
一部省略の拡大端面図、第4図はデインプルの実
施例を示す説明図である。
1……合成樹脂皮膜、2……弾性金属板、3…
…シリンダーボアー、4……ボルト穴、5……冷
却水通路穴、6……冷却水通路穴、7……ビード
、8……デインプル、9……調整板。
Fig. 1 is a plan view of a metal gasket according to an embodiment of the present invention, Fig. 2 is an enlarged end view taken along line AA in Fig. 1, and Fig. 3 is an enlarged end view of a metal gasket according to an embodiment of the present invention. FIG. 4 is an explanatory diagram showing an example of a dimple, which is a partially omitted enlarged end view of the laminated metal gasket at a position corresponding to the line AA in FIG. 1. 1...Synthetic resin film, 2...Elastic metal plate, 3...
... Cylinder bore, 4 ... Bolt hole, 5 ... Cooling water passage hole, 6 ... Cooling water passage hole, 7 ... Bead, 8 ... Dimple, 9 ... Adjustment plate.
Claims (1)
設するとともに、該穴の周縁及び弾性金属薄板の
周縁に断面視波形状のビードを形成し、かつ両面
にゴム等の合成樹脂皮膜を施して、該皮膜と前記
ビードの弾性によりシールの維持を果すようにし
た金属ガスケツトにおいて、前記ビードの膨出高
さよりも低い高さのデインプルの多数を、ビード
の周囲に沿う一部若しくは全周に形成したことを
特徴とする金属ガスケツト。 2 請求項1記載の金属ガスケツトを調整板の両
面に積層しこれらを一体化してなる積層型金属ガ
スケツト。[Scope of Claim for Utility Model Registration] 1. A hole such as a cylinder bore is formed in an elastic thin metal plate, and a bead with a visible wave shape in cross section is formed on the periphery of the hole and on the periphery of the elastic metal thin plate, and rubber, etc. are formed on both sides. In a metal gasket that is coated with a synthetic resin film and whose seal is maintained by the elasticity of the film and the bead, a large number of dimples having a height lower than the bulging height of the bead are formed along the periphery of the bead. A metal gasket characterized in that it is formed around the entire circumference. 2. A laminated metal gasket comprising the metal gasket according to claim 1 laminated on both sides of an adjustment plate and integrated.