JP2017502175A - 陽極酸化処理された材料の腐食を防止するための組成物及び方法 - Google Patents
陽極酸化処理された材料の腐食を防止するための組成物及び方法 Download PDFInfo
- Publication number
- JP2017502175A JP2017502175A JP2016562454A JP2016562454A JP2017502175A JP 2017502175 A JP2017502175 A JP 2017502175A JP 2016562454 A JP2016562454 A JP 2016562454A JP 2016562454 A JP2016562454 A JP 2016562454A JP 2017502175 A JP2017502175 A JP 2017502175A
- Authority
- JP
- Japan
- Prior art keywords
- composition
- corrosion
- conductive nanomaterial
- anodized
- panels
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
実施例1:
(腐食防止組成物)
第1の腐食防止組成物は、脱イオン水のリットル毎に5グラムのグラフェンナノプレートレットの濃度で、脱イオン水と産業品質のグラフェンナノプレートレット(2から10nmの厚み)を組み合わせる(例えば、混合する)ことによって調製された。混合物は、絶えず撹拌された(例えば、かき混ぜられた)。
(腐食防止組成物)
第2の腐食防止組成物は、60:1(浸透溶液対グラフェンナノプレートレット)の重量比で、HM−707蛍光性浸透溶液(Sherwin, Inc.)と産業品質のグラフェンナノプレートレット(2から10nmの厚み)を組み合わせることによって調製された。混合物は、絶えず撹拌された。
(塩霧試験)
15枚の同一の陽極酸化処理された2024−T3ベアアルミニウムのテストパネルが試験用に入手された。すべてのパネルは、最初にアルカリ洗浄されて還元された。水洗いした後、パネルは、陽極酸化処理タンク内に配置され、電流が、19ボルトに達するまで毎分4ボルトの速度で上昇した。電圧は、35分間19ボルトで維持された。次いで、パネルが取り外されて水洗いされた。本明細書で以下でより詳しく説明されるように、3つのパネルが、それぞれのポスト陽極酸化密封処理(post−anodized seal treatment)に対して使用された。
Claims (20)
- 陽極酸化処理された材料の腐食を防止するための方法であって、
液体キャリア、及び
前記キャリア内で分散された導電性ナノ材料(22)
を含む腐食防止組成物を前記陽極酸化処理された材料に適用すること(ブロック104)を含む方法。 - 前記陽極酸化処理された材料が酸化層(14)を有する基板(12)を含み、前記適用するステップが、前記腐食防止組成物を前記酸化層(14)に適用することを含む、請求項1に記載の方法。
- 前記酸化層が孔(20)を含み、前記適用するステップの間に前記導電性ナノ材料が前記孔内に堆積される、請求項2に記載の方法。
- 前記基板がアルミニウムを含む、請求項2に記載の方法。
- 前記酸化層が酸化アルミニウムを含む、請求項4に記載の方法。
- 前記適用するステップが、前記腐食防止組成物を前記陽極酸化処理された材料上へとブラッシングすることを含む、請求項1に記載の方法。
- 前記陽極酸化処理された材料から前記腐食防止組成物の余分な分量を除去することを更に含む、請求項1に記載の方法。
- 前記除去するステップが、ワイピング及び洗浄のうちの少なくとも1つを含む、請求項7に記載の方法。
- 前記除去するステップが、少なくとも30分間の滞留時間の終了の後に行われる、請求項7に記載の方法。
- 前記滞留時間が少なくとも60分間である、請求項9に記載の方法。
- 前記適用するステップが、前記陽極酸化処理された材料を前記腐食防止組成物内に浸すことを含む、請求項1に記載の方法。
- 前記腐食防止組成物を乾燥させること(ブロック108)を更に含む、請求項1に記載の方法。
- 前記適用するステップに先立って、前記腐食防止組成物を190°F及び200°Fの間の温度に加熱することを更に含む、請求項1に記載の方法。
- 前記腐食防止組成物が、前記適用するステップの間に絶えず撹拌される、請求項1に記載の方法。
- 液体キャリア、及び
前記キャリア内で分散された導電性ナノ材料(22)
を含む腐食防止組成物。 - 前記液体キャリアが、最大で72ダイン/センチメートルの表面張力を含む、請求項15に記載の腐食防止組成物。
- 前記液体キャリアが脱イオン水を含み、前記脱イオン水内の前記導電性ナノ材料(22)の濃度が、約1グラム毎リットルから約10グラム毎リットルの範囲である、請求項15に記載の腐食防止組成物。
- 前記液体キャリアが浸透溶液を含み、前記浸透溶液と前記導電性ナノ材料との重量比が、約120:1から約30:1の範囲である、請求項15に記載の腐食防止組成物。
- 前記導電性ナノ材料(22)が、ナノプレートレット、ナノチューブ、及びナノロッドのうちの少なくとも1つを含む、請求項15に記載の腐食防止組成物。
- 前記導電性ナノ材料(22)が、グラフェンナノプレートレットを含む、請求項15に記載の腐食防止組成物。