JP2013063910A - 太陽電池用ガラス基板 - Google Patents
太陽電池用ガラス基板 Download PDFInfo
- Publication number
- JP2013063910A JP2013063910A JP2012280431A JP2012280431A JP2013063910A JP 2013063910 A JP2013063910 A JP 2013063910A JP 2012280431 A JP2012280431 A JP 2012280431A JP 2012280431 A JP2012280431 A JP 2012280431A JP 2013063910 A JP2013063910 A JP 2013063910A
- Authority
- JP
- Japan
- Prior art keywords
- glass
- glass substrate
- solar cell
- viscosity
- less
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
【解決手段】本発明の太陽電池用ガラス基板は、ガラス組成として、質量%でSiO2 30〜70%、Al2O3 3〜20%、B2O3 0〜10%、MgO 0〜10%、CaO 0〜10%、SrO 0〜25%、BaO 0〜25%、Na2O 0〜10%、K2O 0〜10%、ZrO2 0〜8%を含有し、且つ30〜380℃における熱膨張係数が50〜95×10−7/℃であることを特徴とする。
【選択図】なし
Description
(1)ガラス基板上に形成される薄膜化合物との熱膨張差による膜の剥離などを防ぐために、周辺部材と適合する熱膨張係数を有すること
(2)薄膜化合物形成時の熱処理工程では、高温で処理することにより高品位の膜が形成できるため、このような熱処理に耐える高い耐熱性を有すること。より具体的には耐熱性の指標となるガラスの歪点が高いこと
(3)光電変換効率に悪影響を及ぼすような内部欠陥が存在しないこと、特に泡欠陥が存在しないこと
(4)太陽電池全体の重量を軽減するために、低密度であること
Claims (10)
- ガラス組成として、質量%でSiO2 30〜70%、Al2O3 3〜20%、B2O3 0〜10%、MgO 0〜10%、CaO 0〜10%、SrO 0〜25%、BaO 0〜25%、Na2O 0〜10%、K2O 0〜10%、ZrO2 0〜8%を含有し、且つ30〜380℃における熱膨張係数が50〜95×10−7/℃であることを特徴とする太陽電池用ガラス基板。
- ガラス組成として、質量%でZrO2を0.01〜8%含有することを特徴とする請求項1に記載の太陽電池用ガラス基板。
- ガラス組成として、質量%でB2O3を0.1〜8%含有することを特徴とする請求項1または2に記載の太陽電池用ガラス基板。
- モル分率でAl2O3/BaOの値が0.1〜2であることを特徴とする請求項1〜3のいずれかに記載の太陽電池用ガラス基板。
- モル分率でNa2O/K2Oの値が0〜2であることを特徴とする請求項1〜4のいずれかに記載の太陽電池用ガラス基板。
- 液相温度が1200℃以下および/または液相粘度が104.5dPa・s以上であることを特徴とする請求項1〜5のいずれかに記載の太陽電池用ガラス基板。
- 密度が3.7g/cm3以下であることを特徴とする請求項1〜6のいずれかに記載の太陽電池用ガラス基板。
- 歪点が590℃以上であることを特徴とする請求項1〜7のいずれかに記載の太陽電池用ガラス基板。
- 高温粘度102.5dPa・sにおける温度が1650℃以下であることを特徴とする請求項1〜8のいずれかに記載の太陽電池用ガラス基板。
- 請求項1〜9のいずれかに記載の太陽電池用ガラス基板の製造方法であって、
ガラス基板の成形方法がオーバーフローダウンドロー法であることを特徴する太陽電池用ガラス基板の製造方法。