JP2007232911A - Method of manufacturing liquid crystal display panel - Google Patents

Method of manufacturing liquid crystal display panel Download PDF

Info

Publication number
JP2007232911A
JP2007232911A JP2006052740A JP2006052740A JP2007232911A JP 2007232911 A JP2007232911 A JP 2007232911A JP 2006052740 A JP2006052740 A JP 2006052740A JP 2006052740 A JP2006052740 A JP 2006052740A JP 2007232911 A JP2007232911 A JP 2007232911A
Authority
JP
Japan
Prior art keywords
substrate
liquid crystal
crystal display
display panel
polarizing plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
JP2006052740A
Other languages
Japanese (ja)
Inventor
Koji Yamabuchi
浩二 山渕
Manabu Abiru
学 阿比留
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sharp Corp
Original Assignee
Sharp Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sharp Corp filed Critical Sharp Corp
Priority to JP2006052740A priority Critical patent/JP2007232911A/en
Publication of JP2007232911A publication Critical patent/JP2007232911A/en
Withdrawn legal-status Critical Current

Abstract

<P>PROBLEM TO BE SOLVED: To provide a method of manufacturing a liquid crystal display panel capable of suppressing contamination of foreign matters and occurrence of flaws. <P>SOLUTION: The method of manufacturing the liquid crystal display panel includes a sealing material disposing step of disposing a sealing material 4 in a frame shape on the surface of a TFT substrate 3, a step of disposing a liquid crystal in a region on the inner side of the frame shape, a step of sticking the TFT substrate 3 and a CF substrate 2 to each other in a pressure reduced atmosphere to form a stuck substrate 1, a step of washing the stuck substrate 1, a first sticking step of sticking a polarizing plate 8 on a surface to be the front of the liquid crystal display panel of the stuck substrate 1 and a second sticking step of sticking a polarizing plate 9 on a surface to be the backside of the liquid crystal display panel of the stuck substrate 1 after the first sticking step. <P>COPYRIGHT: (C)2007,JPO&INPIT

Description

本発明は、液晶表示パネルの製造方法に関する。   The present invention relates to a method for manufacturing a liquid crystal display panel.

液晶表示パネルの製造においては、透明電極や薄膜トランジスタアレイなどが表面に形成された2枚の基板を、たとえば数μm程度という極めて狭い間隙を保つように貼合せる。基板の貼合せにおいては、主表面が互いに対向するように、シール材を用いて貼り合せる。シール材をほぼ枠形になるように配置して、2枚の基板とシール材とで囲まれる空間に液晶を封入する。   In the manufacture of a liquid crystal display panel, two substrates on which transparent electrodes, thin film transistor arrays, and the like are formed are bonded so as to maintain an extremely narrow gap of, for example, about several μm. In the bonding of the substrates, bonding is performed using a sealing material so that the main surfaces face each other. The sealing material is arranged so as to have a substantially frame shape, and the liquid crystal is sealed in a space surrounded by the two substrates and the sealing material.

液晶を2枚の基板同士の間に封入する方法には、いわゆるディップ方式がある。ディップ方式においては、大気圧の雰囲気下において、基板に対してシール材を配置する。シール材は、一方の基板の液晶表示素子となるべき領域の外周に沿って配置する。シール材の配置においては、ディスペンサなどを用いる。この際、シール材は、完全な閉じた枠形ではなく、シール材に囲まれる空間に液晶を注入するための切れ目(液晶の注入口)が形成されたパターンで配置する。   There is a so-called dip method as a method of sealing liquid crystal between two substrates. In the dip method, a sealing material is disposed on the substrate in an atmosphere of atmospheric pressure. The sealing material is disposed along the outer periphery of the region to be the liquid crystal display element of one substrate. For the arrangement of the sealing material, a dispenser or the like is used. At this time, the sealing material is not a completely closed frame shape, but is arranged in a pattern in which a cut (liquid crystal injection port) for injecting liquid crystal is formed in a space surrounded by the sealing material.

次に、2枚の基板を貼り合せて圧縮およびシール材の硬化を行なう。この貼り合せた基板をそれぞれのシール材の注入口が端部に配置されるように所定の大きさに分断する。基板の分断においては、単一の液晶表示素子毎に分断する。または、複数の液晶表示素子が含まれるように短冊状に切断を行なう。   Next, the two substrates are bonded together to compress and harden the sealing material. The bonded substrates are divided into predetermined sizes so that the inlets of the respective sealing materials are arranged at the ends. The substrate is divided for each single liquid crystal display element. Alternatively, it is cut into strips so as to include a plurality of liquid crystal display elements.

次に、減圧雰囲気中において、液晶表示素子の注入口に液晶を接触させる。この状態で大気開放を行なう。注入口からシール材と2枚の基板とに囲まれる空間に液晶が注入される。この後に液晶の注入口を封止する。   Next, the liquid crystal is brought into contact with the inlet of the liquid crystal display element in a reduced pressure atmosphere. In this state, the atmosphere is released. Liquid crystal is injected into a space surrounded by the sealing material and the two substrates from the inlet. Thereafter, the liquid crystal inlet is sealed.

ディップ法においては、2枚の基板を互いに貼り合せる工程と液晶を封入する工程とを別々に行なう必要がある。これに対し、2つの工程を同時に行なうことができる方法として滴下貼り合せ法が提案されている。   In the dip method, it is necessary to separately perform a process of bonding two substrates together and a process of encapsulating liquid crystals. On the other hand, a drop bonding method has been proposed as a method capable of performing two steps simultaneously.

滴下貼り合せ法においては、閉じた枠形のシール材を基板の表面に配置して、枠形の内側になるべき領域に液晶を滴下する。この後に、真空雰囲気中で2枚の基板を貼り合せてシール材を硬化させる。滴下貼り合せ法においては、基板の貼合せと液晶の封入とを同時に行なうことができ、基板同士の貼り合せおよび液晶の封入の作業時間を短くできる。   In the drop bonding method, a closed frame-shaped sealing material is placed on the surface of the substrate, and the liquid crystal is dropped onto the region that should be inside the frame. Thereafter, the two substrates are bonded together in a vacuum atmosphere to cure the sealing material. In the drop bonding method, the substrates can be bonded and the liquid crystal sealed at the same time, and the working time for bonding the substrates and sealing the liquid crystal can be shortened.

液晶表示パネルには、主表面に偏光板等の光学フィルムが貼り付けられる。たとえば、表側の主表面および裏側の主表面に偏光板が貼付けられている液晶表示パネルがある。光学フィルムの貼り付けは、基板同士の貼り合せの後に行なわれる。光学フィルムの貼付けにおいては、たとえば、光学フィルム貼付け装置のステージに基板の貼り合せが完了した液晶表示素子を載置して片面ずつ光学フィルムを表面に貼り付ける。   An optical film such as a polarizing plate is attached to the main surface of the liquid crystal display panel. For example, there is a liquid crystal display panel in which polarizing plates are attached to the main surface on the front side and the main surface on the back side. The optical film is attached after the substrates are attached to each other. In pasting the optical film, for example, a liquid crystal display element that has been bonded to the substrate is placed on the stage of the optical film pasting apparatus, and the optical film is pasted to the surface one by one.

特開平5−313113号公報においては、ポリマーフィルム基板に対してパターンを形成する前から保護フィルムを貼付けて、偏光板を貼付ける直前に、この保護フィルムを剥離することにより、異物付着や汚れ転移を防止する液晶表示セルの製造方法が開示されている。この液晶セルの製造方法によれば、ポリマーフィルムを基板とする液晶表示素子用電極基板の製造、加工処理工程における傷付き、異物付着、汚れ転移を防止することができると開示されている。   In JP-A-5-313113, a protective film is applied before forming a pattern on a polymer film substrate, and the protective film is peeled off immediately before applying a polarizing plate, thereby adhering foreign matter and transferring dirt. A method of manufacturing a liquid crystal display cell for preventing the above is disclosed. According to this method for producing a liquid crystal cell, it is disclosed that the production of an electrode substrate for a liquid crystal display element using a polymer film as a substrate and the prevention of scratches, foreign matter adhesion, and dirt transfer in processing steps can be prevented.

また、特開平10−197853号公報においては、液晶基板を接触ローラに向けて搬送して、接触ローラの周面下側に存在するテープを液晶基板の表面に接触させる液晶表示装置の製造方法が開示されている。テープの粘着面は押圧ロッドの下方への押圧力により液晶基板の表面に押し付けられる。液晶基板の移動量とテープの送り量とがほぼ一致するようにして液晶基板をさらに移動させていくと、テープは一旦液晶基板の表面に接着されてから引き剥がされるようになる。このため、液晶基板の表面上に付着していた塵埃をテープの粘着面に接着させて除去することができる。この製造方法によれば、液晶表示装置の製造工程において、洗浄液を用いることなく、液晶基板の表面に付着している塵埃を確実に除去し、しかも塵埃の再付着を防止することができると開示されている。
特開平5−313113号公報 特開平10−197853号公報
Japanese Patent Application Laid-Open No. 10-197853 discloses a method of manufacturing a liquid crystal display device in which a liquid crystal substrate is conveyed toward a contact roller, and a tape existing below the peripheral surface of the contact roller is brought into contact with the surface of the liquid crystal substrate. It is disclosed. The adhesive surface of the tape is pressed against the surface of the liquid crystal substrate by a pressing force below the pressing rod. When the liquid crystal substrate is further moved so that the moving amount of the liquid crystal substrate and the feeding amount of the tape substantially coincide with each other, the tape is once adhered to the surface of the liquid crystal substrate and then peeled off. For this reason, the dust adhering to the surface of the liquid crystal substrate can be removed by adhering to the adhesive surface of the tape. According to this manufacturing method, it is disclosed that in the manufacturing process of the liquid crystal display device, dust attached to the surface of the liquid crystal substrate can be surely removed and the reattachment of dust can be prevented without using a cleaning liquid. Has been.
JP-A-5-313113 JP-A-10-197853

液晶表示素子(液晶表示セル)の表面に偏光板などの光学フィルムを貼付ける工程および搬送工程は、大気中で行なわれるため、大気中の埃などが液晶表示パネルと光学フィルムとの間に混入してしまう場合がある。このような場合には、後に表示欠陥が生じる場合がある。   Since the process of attaching an optical film such as a polarizing plate to the surface of a liquid crystal display element (liquid crystal display cell) and the transport process are performed in the atmosphere, dust in the atmosphere is mixed between the liquid crystal display panel and the optical film. May end up. In such a case, a display defect may occur later.

また、液晶表示素子に対して、光学フィルムを貼付けるためには、光学フィルム貼付け装置が用いられる。この装置においては、たとえば、液晶表示素子をステージの表面に固定した状態で、固定面と反対側の面に光学フィルムが貼付けられる。このときに、貼付け装置のステージに密着させた固定面に、塵が付着したり傷が生じたりする場合があった。   Moreover, in order to stick an optical film with respect to a liquid crystal display element, an optical film sticking apparatus is used. In this apparatus, for example, an optical film is attached to a surface opposite to the fixed surface in a state where the liquid crystal display element is fixed to the surface of the stage. At this time, there are cases where dust adheres to the fixed surface that is in close contact with the stage of the sticking device or scratches occur.

上記の特開平5−313113号公報に開示された方法においては、異物の混入や汚れなどを防止するために、液晶表示素子に保護フィルムを貼付ける必要があり、生産性が悪くなるとともに液晶表示パネルが高価になるという問題がある。   In the method disclosed in the above Japanese Patent Laid-Open No. 5-313113, it is necessary to affix a protective film to the liquid crystal display element in order to prevent foreign matters from being mixed in, dirt, and the like. There is a problem that the panel becomes expensive.

上記の特開平10−197853号公報に開示された方法においては、塵の付着を抑制できるものの液晶表示素子に傷がつくことを抑制できないという問題がある。また、粘着テープおよび粘着テープを駆動する装置が必要であり、液晶表示パネルが高価になるという問題がある。さらに、粘着テープを粘着および剥離させる工程が必要であり、生産性が悪くなるという問題がある。   The method disclosed in the above Japanese Patent Application Laid-Open No. 10-197853 has a problem that although the adhesion of dust can be suppressed, the liquid crystal display element cannot be prevented from being damaged. Further, there is a problem that an adhesive tape and a device for driving the adhesive tape are required, and the liquid crystal display panel becomes expensive. Furthermore, there is a problem that the process of sticking and peeling the pressure-sensitive adhesive tape is required, and the productivity is deteriorated.

本発明は、異物が混入したり傷が付いたりすることを抑制した液晶表示パネルの製造方法を提供することを目的とする。   An object of this invention is to provide the manufacturing method of the liquid crystal display panel which suppressed that a foreign material mixes or a damage | wound is attached.

本発明に基づく液晶表示パネルの製造方法は、2枚の基板のうち少なくともいずれか一方の基板の表面に枠形にシール材を配置するシール材配置工程を含む。上記枠形の内側となる領域に液晶を配置する工程を含む。上記一方の基板と他方の基板とを減圧雰囲気中で互いに貼り合せて貼り合せ基板を形成する工程を含む。上記貼り合せ基板を洗浄する工程を含む。液晶表示パネルの表側となるべき上記貼り合せ基板の表面に光学フィルムを貼り付ける第1貼付け工程と、上記第1貼付け工程の後に、上記液晶表示パネルの裏側となるべき上記貼り合せ基板の表面に光学フィルムを貼り付ける第2貼付け工程とを含む。   The manufacturing method of the liquid crystal display panel based on this invention includes the sealing material arrangement | positioning process which arrange | positions a sealing material in frame shape on the surface of at least any one board | substrate among two board | substrates. A step of disposing a liquid crystal in a region inside the frame shape. The method includes a step of bonding the one substrate and the other substrate to each other in a reduced-pressure atmosphere to form a bonded substrate. And a step of cleaning the bonded substrate. A first pasting step of pasting an optical film on the surface of the bonded substrate to be the front side of the liquid crystal display panel, and a surface of the bonded substrate to be the back side of the liquid crystal display panel after the first pasting step A second pasting step for pasting the optical film.

上記発明において好ましくは、上記一方の基板および上記他方の基板として、複数の液晶表示パネルの製造が可能な基板を用いる。上記シール材配置工程は、枠形状に複数のシール材を配置する工程を含む。上記第2貼付け工程の後に、上記貼り合せ基板を分断する工程を含む。   In the above invention, preferably, a substrate capable of manufacturing a plurality of liquid crystal display panels is used as the one substrate and the other substrate. The sealing material arranging step includes a step of arranging a plurality of sealing materials in a frame shape. After the second pasting step, a step of cutting the bonded substrate is included.

本発明によれば、異物が混入したり傷が付いたりすることを抑制した液晶表示パネルの製造方法を提供することができる。   ADVANTAGE OF THE INVENTION According to this invention, the manufacturing method of the liquid crystal display panel which suppressed that a foreign material mixes or a damage | wound can be provided can be provided.

図1から図7を参照して、本発明に基づく実施の形態における液晶表示パネルの製造方法について説明する。   With reference to FIG. 1 to FIG. 7, a method for manufacturing a liquid crystal display panel according to an embodiment of the present invention will be described.

図1に、本実施の形態において製造する液晶表示パネルの概略断面図を示す。本実施の形態においては、液晶表示パネルのうちカラー液晶表示パネルを例に採り上げて説明する。液晶表示パネルは、互いに対向する2枚の基板同士の間に液晶が封入された構成を備える。   FIG. 1 is a schematic cross-sectional view of a liquid crystal display panel manufactured in the present embodiment. In the present embodiment, a color liquid crystal display panel among liquid crystal display panels will be described as an example. The liquid crystal display panel has a configuration in which liquid crystal is sealed between two substrates facing each other.

液晶表示パネル22は、駆動素子としてのTFT(Thin Film Transistor)が形成されたTFT基板3と、CF(Color Filter)が形成されたCF基板2とを備える。液晶5は、TFT基板3、CF基板2およびシール材4に囲まれる空間に封入されている。2枚の基板は、図示しないスペーサによって所定の間隔に離れて固定されている。   The liquid crystal display panel 22 includes a TFT substrate 3 on which a TFT (Thin Film Transistor) as a drive element is formed, and a CF substrate 2 on which a CF (Color Filter) is formed. The liquid crystal 5 is sealed in a space surrounded by the TFT substrate 3, the CF substrate 2, and the sealing material 4. The two substrates are fixed at a predetermined interval by a spacer (not shown).

TFT基板3は、一方の方向に延びる複数のゲートバスラインと、このゲートバスラインと交差して延在する複数のソースバスラインと、ゲートバスラインおよびソースバスラインの交差部分の近傍に形成されたTFTとを表面に備える。TFT基板3は、これらの素子の表面に配置された画素電極7を備える。画素電極7は、ソースバスラインに接続されている。画素電極7は、それぞれの画素ごとに形成されている。   The TFT substrate 3 is formed in the vicinity of a plurality of gate bus lines extending in one direction, a plurality of source bus lines extending across the gate bus lines, and an intersection of the gate bus lines and the source bus lines. A TFT is provided on the surface. The TFT substrate 3 includes pixel electrodes 7 disposed on the surfaces of these elements. The pixel electrode 7 is connected to the source bus line. The pixel electrode 7 is formed for each pixel.

画素電極7としては、透過型の液晶表示パネルの場合には透明電極が形成され、反射型の液晶表示パネルの場合には反射電極が形成されている。画素電極7の主表面には、液晶を適切な方向に配向させるための図示しない配向膜が形成されている。   As the pixel electrode 7, a transparent electrode is formed in the case of a transmissive liquid crystal display panel, and a reflective electrode is formed in the case of a reflective liquid crystal display panel. An alignment film (not shown) for aligning the liquid crystal in an appropriate direction is formed on the main surface of the pixel electrode 7.

TFT基板3と反対側に配置されるCF基板2の主表面には、カラーフィルタが配置されている。カラーフィルタは、たとえば、赤、緑および青の3色の色相を有する。カラーフィルタの表面には、たとえば、対向電極6が形成されている。対向電極6としては、たとえばITO(インジウム錫酸化物)から形成された透明電極が形成されている。さらに対向電極6の表面には、図示しない配向膜が配置されている。   A color filter is disposed on the main surface of the CF substrate 2 disposed on the side opposite to the TFT substrate 3. The color filter has, for example, three hues of red, green, and blue. For example, the counter electrode 6 is formed on the surface of the color filter. As the counter electrode 6, a transparent electrode made of, for example, ITO (indium tin oxide) is formed. Further, an alignment film (not shown) is disposed on the surface of the counter electrode 6.

TFT基板3およびCF基板2の外側の表面には、光学フィルムとしての偏光板8,9がそれぞれ貼り付けられている。本実施の形態においては、CF基板2が、液晶表示パネルの表側になる基板である。TFT基板3が、裏側になる基板である。使用者は、CF基板2の側から液晶表示パネル22に表示される映像などを見る。透過型の液晶表示パネルや半透過型の液晶表示パネルにおいては、TFT基板3に対向するようにバックライトが配置される。   Polarizing plates 8 and 9 as optical films are respectively attached to the outer surfaces of the TFT substrate 3 and the CF substrate 2. In the present embodiment, the CF substrate 2 is a substrate that becomes the front side of the liquid crystal display panel. The TFT substrate 3 is a substrate on the back side. The user views an image displayed on the liquid crystal display panel 22 from the CF substrate 2 side. In a transmissive liquid crystal display panel or a transflective liquid crystal display panel, a backlight is disposed so as to face the TFT substrate 3.

本実施の形態における液晶表示パネルの製造方法においては、大型の基板に対して複数の液晶表示素子を形成して、後に個々の単一の液晶表示素子に分断する、いわゆる多面取りによる製造方法を例に採り上げて説明する。   In the manufacturing method of the liquid crystal display panel in the present embodiment, a manufacturing method by so-called multi-planaring, in which a plurality of liquid crystal display elements are formed on a large substrate and then divided into individual single liquid crystal display elements. Take this as an example.

多面取りによる製造方法においては、大型の基板である多面取り基板の主表面に、複数のシール材を配置して、多面取り基板同士を貼り合せる。基板としては、たとえばガラス基板を用いる。この後に、カッタなどの切断手段により多面取り基板を切断して、個々の液晶表示素子を製造する。   In the manufacturing method by multi-cavity, a plurality of sealing materials are arranged on the main surface of the multi-cavity substrate which is a large substrate, and the multi-cavity substrates are bonded to each other. For example, a glass substrate is used as the substrate. Thereafter, the multi-sided substrate is cut by a cutting means such as a cutter to manufacture individual liquid crystal display elements.

図2に、本実施の形態において、貼り合せ基板を製造する工程の概略断面図を示す。本実施の形態においては、TFT基板3およびCF基板2として、表面に複数の液晶表示素子を形成することができる大型の基板をそれぞれ用いている。   FIG. 2 shows a schematic cross-sectional view of a process for manufacturing a bonded substrate in the present embodiment. In the present embodiment, large substrates capable of forming a plurality of liquid crystal display elements on the surface are used as the TFT substrate 3 and the CF substrate 2, respectively.

CF基板2の表面には、対向電極6の他に、図示しないカラーフィルタや配向膜などを形成する。また、TFT基板3の表面には、画素電極7の他に、ゲートバスラインなどの電気回路、TFTの表面の凹凸を平坦にするための平坦化絶縁膜および配向膜などを形成する。   On the surface of the CF substrate 2, a color filter and an alignment film (not shown) are formed in addition to the counter electrode 6. Further, on the surface of the TFT substrate 3, in addition to the pixel electrode 7, an electric circuit such as a gate bus line, a planarization insulating film and an alignment film for flattening the unevenness of the surface of the TFT are formed.

次に、互いに対向する2枚の基板のうち、少なくとも一方の基板にシール材を配置するシール材配置工程を行なう。本実施の形態においては、TFT基板3の主表面に、シール材4を配置する。本実施の形態においては、シール材4を閉じた枠形状に配置する。本実施の形態においては、平面形状が四角形になるようにシール材4を配置する。シール材4を、表示領域に形成された画素電極7を取り囲むように配置する。シール材4が取り囲む領域の内側にスペーサを散布する。   Next, a sealing material arrangement step is performed in which a sealing material is arranged on at least one of the two substrates facing each other. In the present embodiment, the sealing material 4 is disposed on the main surface of the TFT substrate 3. In the present embodiment, the sealing material 4 is arranged in a closed frame shape. In the present embodiment, the sealing material 4 is arranged so that the planar shape is a square. The sealing material 4 is disposed so as to surround the pixel electrode 7 formed in the display area. Spacers are dispersed inside the area surrounded by the sealing material 4.

次に、互いに対向する2枚の基板同士のうち、少なくとも一方の基板に液晶5を滴下する液晶滴下工程を行なう。本実施の形態においては、TFT基板3に液晶5を滴下する。液晶5は、シール材4に囲まれる領域の内側となるべき領域に滴下する。液晶5の滴下においては、1滴の液晶5を滴下してもよいし複数滴の液晶5を滴下しても構わない。   Next, a liquid crystal dropping step of dropping the liquid crystal 5 on at least one of the two substrates facing each other is performed. In the present embodiment, the liquid crystal 5 is dropped on the TFT substrate 3. The liquid crystal 5 is dropped on a region to be inside the region surrounded by the seal material 4. In dropping the liquid crystal 5, one drop of the liquid crystal 5 may be dropped or a plurality of drops of the liquid crystal 5 may be dropped.

次に、TFT基板3およびCF基板2を減圧雰囲気中に配置する。矢印31に示すように、TFT基板3とCF基板2とを貼り合せる。TFT基板3とCF基板2との間隔は、スペーサによって定められる。シール材4が、CF基板2に接触して、貼り合せ基板が形成される。   Next, the TFT substrate 3 and the CF substrate 2 are placed in a reduced pressure atmosphere. As indicated by an arrow 31, the TFT substrate 3 and the CF substrate 2 are bonded together. The distance between the TFT substrate 3 and the CF substrate 2 is determined by a spacer. The sealing material 4 comes into contact with the CF substrate 2 to form a bonded substrate.

図3に、本実施の形態における貼り合せ基板の概略断面図を示す。TFT基板3とCF基板2とは互いに一定の間隔を空けて結合される。貼り合せ基板1は、大気開放を行なうことにより、または、互いに圧縮されることにより、TFT基板3とCF基板2との間隔が調整される。この後に、紫外線を照射したり加熱したりすることによりシール材4を硬化させる。   FIG. 3 is a schematic cross-sectional view of the bonded substrate in this embodiment. The TFT substrate 3 and the CF substrate 2 are coupled to each other with a certain distance. The distance between the TFT substrate 3 and the CF substrate 2 is adjusted by opening the bonded substrate 1 to the atmosphere or compressing each other. Thereafter, the sealing material 4 is cured by irradiating with ultraviolet rays or heating.

液晶5は、TFT基板3、CF基板2およびシール材4に囲まれる領域に封入される。本実施の形態における貼り合せ基板1は、大型の貼り合せ基板である。貼り合せ基板1は、複数の液晶表示素子21を含む。   The liquid crystal 5 is sealed in a region surrounded by the TFT substrate 3, the CF substrate 2, and the sealing material 4. The bonded substrate 1 in the present embodiment is a large bonded substrate. The bonded substrate 1 includes a plurality of liquid crystal display elements 21.

図4に、本実施の形態における洗浄工程の概略斜視図を示す。2枚の基板同士の貼合せが完了したら、貼り合せ基板の洗浄を行なう。本実施の形態における洗浄装置は、ロールブラシ12a,12bを備える。ロールブラシ12a,12bは、互いに対向するように配置されている。ロールブラシ12a,12bは、延在する方向が互いに平行になるように配置されている。   FIG. 4 shows a schematic perspective view of the cleaning process in the present embodiment. When the bonding of the two substrates is completed, the bonded substrate is cleaned. The cleaning device in the present embodiment includes roll brushes 12a and 12b. The roll brushes 12a and 12b are arranged to face each other. The roll brushes 12a and 12b are arranged so that the extending directions are parallel to each other.

本実施の形態における洗浄工程においては、貼り合せ基板1をロールブラシ12aとロールブラシ12bとの間を通すことにより行なう。ロールブラシ12a,12bを回転させながら、矢印32に示すように貼り合せ基板1を移動させることにより、貼り合せ基板1の洗浄を行なう。本実施の形態においては、貼り合せ基板1の表側の表面および裏側の表面の洗浄を行なう。   In the cleaning process in the present embodiment, the bonded substrate 1 is passed between the roll brush 12a and the roll brush 12b. The bonded substrate 1 is cleaned by moving the bonded substrate 1 as indicated by an arrow 32 while rotating the roll brushes 12a and 12b. In the present embodiment, the front surface and the back surface of the bonded substrate 1 are cleaned.

貼り合せ基板の洗浄工程においては、この形態に限られず、任意の洗浄方法を採用することができる。たとえば、ウェブクリーナなどを用いることにより、液体が不要な洗浄を行なっても構わない。   The cleaning process for the bonded substrate is not limited to this mode, and any cleaning method can be employed. For example, cleaning that does not require liquid may be performed by using a web cleaner or the like.

図5に、本実施の形態における第1貼付け工程の概略斜視図を示す。第1貼付け工程においては、CF基板の表面に偏光板を貼付ける。本実施の形態においては、矢印33に示すように、大型の偏光板8を貼付ける。偏光板8は、貼り合せ基板1の主表面に対応する大きさを有する。偏光板8は、複数の液晶表示素子21を覆うように形成されている。   In FIG. 5, the schematic perspective view of the 1st sticking process in this Embodiment is shown. In the first attaching step, a polarizing plate is attached to the surface of the CF substrate. In the present embodiment, a large polarizing plate 8 is attached as indicated by an arrow 33. The polarizing plate 8 has a size corresponding to the main surface of the bonded substrate 1. The polarizing plate 8 is formed so as to cover the plurality of liquid crystal display elements 21.

本実施の形態においては、貼り合せ基板1のうち先にCF基板2の主表面に、偏光板8を貼付ける。すなわち、液晶表示パネルになったときに表側となるべき貼り合せ基板1の表面に偏光板8を貼付ける。   In the present embodiment, the polarizing plate 8 is pasted to the main surface of the CF substrate 2 in the bonded substrate 1 first. That is, the polarizing plate 8 is attached to the surface of the bonded substrate 1 that should be the front side when the liquid crystal display panel is formed.

図6に、本実施の形態における偏光板貼付け装置の概略側面図を示す。本実施の形態における偏光板貼付け装置は、パネルステージ23と偏光板コレット24と貼付けローラ25とを備える。パネルステージ23は、板状に形成されている。パネルステージ23は、図示しない真空装置に接続されている。パネルステージ23は、吸着により液晶表示素子を主表面に保持したり、保持を解除したりできるように形成されている。   In FIG. 6, the schematic side view of the polarizing plate sticking apparatus in this Embodiment is shown. The polarizing plate attaching apparatus in the present embodiment includes a panel stage 23, a polarizing plate collet 24, and an attaching roller 25. The panel stage 23 is formed in a plate shape. The panel stage 23 is connected to a vacuum device (not shown). The panel stage 23 is formed so that the liquid crystal display element can be held on the main surface by suction or released.

偏光板コレット24は、偏光板を保持できるように形成されている。偏光板コレット24は、板状に形成されている。偏光板コレット24は、主表面がパネルステージ23の貼り合せ基板1の載置面に対して傾斜するように配置されている。偏光板コレット24は、図示しない真空装置に接続されている。偏光板コレット24は、吸着により主表面に偏光板8を保持したり保持を解除したりすることができるように形成されている。   The polarizing plate collet 24 is formed so as to hold the polarizing plate. The polarizing plate collet 24 is formed in a plate shape. The polarizing plate collet 24 is disposed such that the main surface is inclined with respect to the mounting surface of the bonded substrate 1 of the panel stage 23. The polarizing plate collet 24 is connected to a vacuum device (not shown). The polarizing plate collet 24 is formed so that the polarizing plate 8 can be held or released from the main surface by adsorption.

貼付けローラ25は、偏光板コレット24の端部のうちパネルステージ23の側の端部に対向するように配置されている。貼付けローラ25は、回転可能なように形成されている。貼付けローラ25は、矢印35に示すように、偏光板8を貼り合せ基板1に向かって押圧することができるように形成されている。偏光板コレット24および貼付けローラ25は、矢印34に示すように、水平方向に移動可能に形成されている。   The affixing roller 25 is disposed so as to face the end portion of the polarizing plate collet 24 on the panel stage 23 side. The affixing roller 25 is formed to be rotatable. The affixing roller 25 is formed so that the polarizing plate 8 can be pressed toward the bonded substrate 1 as indicated by an arrow 35. The polarizing plate collet 24 and the pasting roller 25 are formed so as to be movable in the horizontal direction as indicated by an arrow 34.

偏光板の貼付けにおいては、貼り合せ基板1をパネルステージ23に載置する。このときに、貼り合せ基板1の主表面のうち、完成時に表側となるべき基板を上側に載置する。すなわち、完成時に裏側となるべき基板をパネルステージ23に接触させる。本実施の形態においては、TFT基板3をパネルステージ23に載置する。本実施の形態においては、CF基板2が上側を向くように配置する。貼り合せ基板1は、パネルステージ23における位置合せが行なわれた後に吸着により固定される。   In pasting the polarizing plate, the bonded substrate 1 is placed on the panel stage 23. At this time, among the main surfaces of the bonded substrate 1, the substrate that should be the front side when completed is placed on the upper side. That is, the substrate to be the back side when completed is brought into contact with the panel stage 23. In the present embodiment, the TFT substrate 3 is placed on the panel stage 23. In the present embodiment, the CF substrate 2 is disposed so as to face upward. The bonded substrate 1 is fixed by suction after being aligned on the panel stage 23.

次に、CF基板2の表面に偏光板8を貼り付ける。偏光板8は、水平方向のうち、一方の端部から他方の端部に向かって貼り合せ基板1に貼り付けられる。偏光板8は、偏光板コレット24から離れた後に、貼付けローラ25によって貼り合せ基板1に向かって押圧されながら貼り付けられる。貼付けローラ25は、偏光板8を貼り合せ基板1に向かって押圧しながら、偏光板コレット24とともに移動する。このように、偏光板8が貼り合せ基板1の一方の端部から他方の端部に向けて貼付けられる。   Next, a polarizing plate 8 is attached to the surface of the CF substrate 2. The polarizing plate 8 is attached to the laminated substrate 1 from one end portion to the other end portion in the horizontal direction. The polarizing plate 8 is pasted while being pressed toward the bonded substrate 1 by the pasting roller 25 after being separated from the polarizing plate collet 24. The pasting roller 25 moves together with the polarizing plate collet 24 while pressing the polarizing plate 8 toward the bonded substrate 1. Thus, the polarizing plate 8 is bonded from one end portion of the bonded substrate board 1 toward the other end portion.

図7に、本実施の形態における第2貼付け工程の概略斜視図を示す。第2貼付け工程においては、TFT基板3の表面に偏光板9を貼り付ける。CF基板2の表面に偏光板8の貼付けが完了したら、TFT基板3の表面に、矢印36に示すように、偏光板9を貼付ける。偏光板9の貼付けにおいては、偏光板8の貼付けと同様に偏光板貼付け装置を用いて貼付けを行なう。   In FIG. 7, the schematic perspective view of the 2nd sticking process in this Embodiment is shown. In the second attaching step, the polarizing plate 9 is attached to the surface of the TFT substrate 3. When the application of the polarizing plate 8 to the surface of the CF substrate 2 is completed, the polarizing plate 9 is applied to the surface of the TFT substrate 3 as indicated by an arrow 36. In the pasting of the polarizing plate 9, the pasting is performed using the polarizing plate pasting apparatus in the same manner as the pasting of the polarizing plate 8.

図8に、本実施の形態における偏光板の一部を切断および剥離する工程の概略側面図を示す。液晶表示素子同士の間の領域において、偏光板の切断および剥離を行なう。さらに、剥離した部分に貼り合せ基板を分断するためのスクライブ線を形成する。   In FIG. 8, the schematic side view of the process of cut | disconnecting and peeling a part of polarizing plate in this Embodiment is shown. In the region between the liquid crystal display elements, the polarizing plate is cut and peeled off. Further, a scribe line for dividing the bonded substrate is formed in the peeled portion.

本実施の形態における偏光板剥離装置は、刃物10を備える。刃物10は、偏光板を帯状に切断するとともに剥離できるように形成されている。刃物10は、断面形状がコの字形に形成されている。   The polarizing plate peeling apparatus in the present embodiment includes a blade 10. The blade 10 is formed so that the polarizing plate can be cut and stripped. The blade 10 has a U-shaped cross section.

本実施の形態における偏光板剥離装置は、ホイル11を備える。ホイル11は、円盤状に形成されている。ホイル11は、偏光板剥離装置が進行する向きにおいて、刃物10の後側に配置されている。ホイル11は、貼り合せ基板1に対して圧接するように形成されている。   The polarizing plate peeling apparatus in the present embodiment includes a foil 11. The foil 11 is formed in a disc shape. The foil 11 is disposed on the rear side of the blade 10 in the direction in which the polarizing plate peeling apparatus proceeds. The foil 11 is formed in pressure contact with the bonded substrate 1.

本実施の形態においては、貼り合せ基板のうち、CF基板2の表面に貼付けられた偏光板8の除去を行なう。偏光板剥離装置を矢印37に示す向きに移動させる。偏光板剥離装置は、貼り合せ基板1の主表面に沿って移動する。ホイル11は、貼り合せ基板1の表面に圧接するとともに矢印38に示す向きに回転する。   In the present embodiment, the polarizing plate 8 attached to the surface of the CF substrate 2 is removed from the bonded substrate. The polarizing plate peeling apparatus is moved in the direction indicated by the arrow 37. The polarizing plate peeling apparatus moves along the main surface of the bonded substrate 1. The foil 11 is pressed against the surface of the bonded substrate 1 and rotates in the direction indicated by the arrow 38.

刃物10により、液晶表示素子21(図7参照)同士の間の領域において、偏光板が帯状に切断されるとともに剥離される。次に、剥離された領域にホイル11が圧接する。ホイル11が、CF基板2の表面に圧接することにより、CF基板2の表面に傷が付いてスクライブ線が形成される。   In the region between the liquid crystal display elements 21 (see FIG. 7), the polarizing plate is cut into a strip shape and peeled off by the blade 10. Next, the foil 11 is pressed against the peeled area. When the foil 11 is pressed against the surface of the CF substrate 2, the surface of the CF substrate 2 is scratched to form a scribe line.

このような偏光板の一部の切断および剥離を、偏光板8および偏光板9に対して行なう。偏光板の剥離は、液晶表示素子の周りにスクライブ線を形成するように行なう。次に、形成されたスクライブ線に沿って、貼り合せ基板1を分断することにより単一の液晶表示素子が得られる。   The polarizing plate 8 and the polarizing plate 9 are partly cut and peeled off. The polarizing plate is peeled off so as to form a scribe line around the liquid crystal display element. Next, a single liquid crystal display element is obtained by dividing the laminated substrate 1 along the formed scribe line.

本実施の形態における液晶表示パネルの製造方法は、表側となるべき貼り合せ基板の表面に光学フィルムを貼付ける第1貼付け工程と、第1貼付け工程の後に裏側となるべき貼り合せ基板の表面に光学フィルムを貼付ける第2貼付け工程とを含む。貼り合せ基板と偏光板との間に混入する異物や貼り合せ基板の傷は、液晶表示パネルの裏側よりも表側に配置される方が表示不良となりやすい。すなわち、液晶表示パネルの裏側よりも表側に異物が混入したり傷が付いたりする方が、目立ちやすく不良になりやすい。本実施の形態においては、貼り合せ基板を洗浄した直後の表側の主表面に偏光板を貼付けている。このため、表側の主表面に、埃などの異物が配置されたり傷が付いたりすることを抑制することができ、表示不良を抑制することができる。たとえば、偏光板貼付け装置のパネルステージと擦れることにより貼り合せ基板の表側の表面に傷が付くことを抑制できる。   The manufacturing method of the liquid crystal display panel in the present embodiment includes a first pasting step of pasting the optical film on the surface of the bonded substrate to be the front side, and a surface of the bonded substrate to be the back side after the first pasting step. A second pasting step for pasting the optical film. A foreign matter mixed between the bonded substrate and the polarizing plate or a scratch on the bonded substrate is likely to cause a display defect when arranged on the front side rather than the back side of the liquid crystal display panel. That is, it is more conspicuous and defective when foreign matter is mixed or scratched on the front side than the back side of the liquid crystal display panel. In the present embodiment, a polarizing plate is attached to the front main surface immediately after cleaning the bonded substrate. For this reason, it can suppress that foreign materials, such as dust, are arrange | positioned and a damage | wound is attached to the front main surface, and a display defect can be suppressed. For example, it is possible to suppress the surface of the bonded substrate from being scratched by rubbing against the panel stage of the polarizing plate applying apparatus.

本実施の形態においては、一方の基板および他方の基板として、複数の液晶表示パネルが製造可能な大型の基板を用いている。また、第2貼付け工程の後に、貼り合せ基板を分断する工程を含む。このような、多面取りによる製造方法においては、大型の基板に対して大型の偏光板を貼付ける一括偏光板の貼付けを行なう。この製造方法においては、偏光板貼付け装置のステージに貼り合せ基板を配置したときに、ステージに密着させた側の基板の表面に塵の付着や傷の発生が起こり易いため、本発明の効果が顕著になる。   In this embodiment, large substrates on which a plurality of liquid crystal display panels can be manufactured are used as one substrate and the other substrate. Moreover, the process of parting a bonding board | substrate is included after a 2nd bonding process. In such a manufacturing method by multi-chamfering, a collective polarizing plate for attaching a large polarizing plate to a large substrate is attached. In this manufacturing method, when the bonded substrate is disposed on the stage of the polarizing plate bonding apparatus, the surface of the substrate that is in close contact with the stage is liable to cause dust adhesion and scratches. Become prominent.

本実施の形態においては、光学フィルムとして偏光板を貼付けたが、この形態に限られず、他の光学フィルムを貼付けてもよい。たとえば、位相差板や、偏光板および位相差板等を含む多層の光学フィルムを貼付けても構わない。   In this Embodiment, although the polarizing plate was affixed as an optical film, it is not restricted to this form, You may affix another optical film. For example, a multilayer optical film including a retardation plate, a polarizing plate, a retardation plate, and the like may be attached.

本実施の形態においては、多面取りによる製造方法を例に採り上げて説明を行なったが、この形態に限られず、たとえば単一の液晶表示素子を有する貼り合せ基板を形成した後に光学フィルムを貼り付けても構わない。   In the present embodiment, the description has been made by taking the manufacturing method by multi-cavity as an example. However, the present invention is not limited to this embodiment. For example, an optical film is pasted after a bonded substrate having a single liquid crystal display element is formed. It doesn't matter.

上記の実施の形態に係るそれぞれの図面において、同一または相当する部分には、同一の符号を付している。   In each drawing according to the above embodiment, the same or corresponding parts are denoted by the same reference numerals.

なお、今回開示した上記実施の形態はすべての点で例示であって制限的なものではない。本発明の範囲は上記した説明ではなくて特許請求の範囲によって示され、特許請求の範囲と均等の意味および範囲内でのすべての変更を含むものである。   In addition, the said embodiment disclosed this time is an illustration in all the points, Comprising: It is not restrictive. The scope of the present invention is defined by the terms of the claims, rather than the description above, and includes all modifications within the scope and meaning equivalent to the terms of the claims.

実施の形態における液晶表示パネルの概略断面図である。It is a schematic sectional drawing of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法の第1工程を説明する概略断面図である。It is a schematic sectional drawing explaining the 1st process of the manufacturing method of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法の第2工程を説明する概略断面図である。It is a schematic sectional drawing explaining the 2nd process of the manufacturing method of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法の第3工程を説明する概略斜視図である。It is a schematic perspective view explaining the 3rd process of the manufacturing method of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法の第4工程を説明する概略斜視図である。It is a schematic perspective view explaining the 4th process of the manufacturing method of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法において用いる偏光板貼付け装置の概略側面図である。It is a schematic side view of the polarizing plate sticking apparatus used in the manufacturing method of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法の第5工程を説明する概略斜視図である。It is a schematic perspective view explaining the 5th process of the manufacturing method of the liquid crystal display panel in embodiment. 実施の形態における液晶表示パネルの製造方法の偏光板剥離装置の概略側面図である。It is a schematic side view of the polarizing plate peeling apparatus of the manufacturing method of the liquid crystal display panel in embodiment.

符号の説明Explanation of symbols

1 貼り合せ基板、2 CF基板、3 TFT基板、4 シール材、5 液晶、6 対向電極、7 画素電極、8,9 偏光板、10 刃物、11 ホイル、12a,12b ロールブラシ、21 液晶表示素子、22 液晶表示パネル、23 パネルステージ、24 偏光板コレット、25 貼付けローラ、31〜38 矢印。   DESCRIPTION OF SYMBOLS 1 Bonding substrate, 2 CF substrate, 3 TFT substrate, 4 Sealing material, 5 Liquid crystal, 6 Counter electrode, 7 Pixel electrode, 8, 9 Polarizing plate, 10 Cutlery, 11 Foil, 12a, 12b Roll brush, 21 Liquid crystal display element , 22 liquid crystal display panel, 23 panel stage, 24 polarizing plate collet, 25 sticking roller, 31-38 arrows.

Claims (2)

2枚の基板のうち少なくともいずれか一方の基板の表面に枠形にシール材を配置するシール材配置工程と、
前記枠形の内側となる領域に液晶を配置する工程と、
前記一方の基板と他方の基板とを減圧雰囲気中で互いに貼り合せて貼り合せ基板を形成する工程と、
前記貼り合せ基板を洗浄する工程と、
液晶表示パネルの表側となるべき前記貼り合せ基板の表面に光学フィルムを貼り付ける第1貼付け工程と、
前記第1貼付け工程の後に、前記液晶表示パネルの裏側となるべき前記貼り合せ基板の表面に光学フィルムを貼り付ける第2貼付け工程と
を含む、液晶表示パネルの製造方法。
A sealing material arrangement step of arranging a sealing material in a frame shape on the surface of at least one of the two substrates;
Disposing a liquid crystal in a region inside the frame;
Bonding the one substrate and the other substrate together in a reduced pressure atmosphere to form a bonded substrate;
Cleaning the bonded substrate;
A first pasting step of pasting an optical film on the surface of the bonded substrate to be the front side of the liquid crystal display panel;
The manufacturing method of a liquid crystal display panel including the 2nd affixing process which affixes an optical film on the surface of the said bonding substrate which should become the back side of the said liquid crystal display panel after a said 1st affixing process.
前記一方の基板および前記他方の基板として、複数の液晶表示パネルの製造が可能な基板を用い、
前記シール材配置工程は、枠形状に複数のシール材を配置する工程を含み、
前記第2貼付け工程の後に、前記貼り合せ基板を分断する工程を含む、請求項1に記載の液晶表示パネルの製造方法。
As the one substrate and the other substrate, a substrate capable of manufacturing a plurality of liquid crystal display panels is used.
The sealing material arranging step includes a step of arranging a plurality of sealing materials in a frame shape,
The manufacturing method of the liquid crystal display panel of Claim 1 including the process of parting the said bonding substrate after a said 2nd bonding process.
JP2006052740A 2006-02-28 2006-02-28 Method of manufacturing liquid crystal display panel Withdrawn JP2007232911A (en)