Granted
Application number
JP2006024841A
Other languages
English (en)
Other versions
JP2006299234A (ja
JP5046522B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2006024841A priority Critical patent/JP5046522B2/ja
Priority claimed from JP2006024841A external-priority patent/JP5046522B2/ja
Publication of JP2006299234A publication Critical patent/JP2006299234A/ja
Publication of JP2006299234A5 publication Critical patent/JP2006299234A5/ja
Application granted granted Critical
Publication of JP5046522B2 publication Critical patent/JP5046522B2/ja
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (6)

  1. アクリル酸および/またはその塩を主成分とするモノマーを重合させて吸水性を有する重合ゲルを得る工程と、
    吸水性樹脂の製造において得られ重量平均粒子径が10〜150μmの範囲内である微粉に、熱分解型ラジカル重合開始剤、酸化剤および還元剤からなる群より選ばれる少なくとも1種の添加剤を含む水性液を添加することにより、造粒されたゲルを得る工程と、
    前記造粒されたゲルと前記重合ゲルとを共存させて乾燥する工程とを含む吸水性樹脂の製造方法。
  2. 前記水性液は、微粉に添加される前に予め加熱される請求項1に記載の吸水性樹脂の製造方法。
  3. 前記添加剤は、過硫酸塩を含む請求項1又は2に記載の吸水性樹脂の製造方法。
  4. 前記造粒されたゲルと前記重合ゲルとを共存させて乾燥する工程において、造粒されたゲルの固形分率A(%)と重合ゲルの固形分率B(%)との比(A/B)が、1/3以上3以下となっている請求項1から3のいずれかに記載の吸水性樹脂の製造方法。
  5. 前記造粒されたゲルと前記重合ゲルとを共存させて乾燥する工程において、造粒されたゲル中の固形分量が重合ゲル中の固形分量に対して40重量%以下となるようにする、請求項1から4までのいずれかに記載の吸水性樹脂の製造方法。
  6. 吸水性を有する重合ゲルと、造粒されたゲルとを含む吸水性樹脂であって、前記造粒されたゲルは、重量平均粒子径が10〜150μmの範囲内である微粉からなり、前記造粒
    されたゲルの固形分率A(%)と重合ゲルの固形分率B(%)との比(A/B)が、1/3以上3以下であり、残存モノマーが0以上500ppm以下である吸水性樹脂。
JP2006024841A 2005-02-15 2006-02-01 吸水性樹脂及びその製造方法 Active JP5046522B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2006024841A JP5046522B2 (ja) 2005-02-15 2006-02-01 吸水性樹脂及びその製造方法

Applications Claiming Priority (5)

Application Number Priority Date Filing Date Title
JP2005038123 2005-02-15
JP2005038123 2005-02-15
JP2005089307 2005-03-25
JP2005089307 2005-03-25
JP2006024841A JP5046522B2 (ja) 2005-02-15 2006-02-01 吸水性樹脂及びその製造方法

Publications (3)

Publication Number Publication Date
JP2006299234A JP2006299234A (ja) 2006-11-02
JP2006299234A5 true JP2006299234A5 (ja) 2008-12-18
JP5046522B2 JP5046522B2 (ja) 2012-10-10

Family

ID=37467903

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2006024841A Active JP5046522B2 (ja) 2005-02-15 2006-02-01 吸水性樹脂及びその製造方法

Country Status (1)

Country Link
JP (1) JP5046522B2 (ja)

Families Citing this family (13)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101605818B (zh) * 2007-02-06 2012-10-03 巴斯夫欧洲公司 通过聚合单体溶液的液滴生产吸水性聚合物颗粒的方法
EP2291416A1 (de) * 2008-06-19 2011-03-09 Basf Se Verfahren zur kontinuierlichen herstellung wasserabsorbierender polymerpartikel
US8410222B2 (en) * 2008-07-15 2013-04-02 Basf Se Method for producing water-absorbing polymer particles
US8802800B2 (en) 2009-08-28 2014-08-12 Nippon Shokubai Co., Ltd. Production method for water-absorbent resin
JP5718816B2 (ja) * 2009-09-16 2015-05-13 株式会社日本触媒 吸水性樹脂粉末の製造方法
JP6169926B2 (ja) * 2013-08-30 2017-07-26 株式会社日本触媒 吸水性樹脂の微粉砕方法及び耐塩性に優れた吸水性樹脂
EP3165558B1 (en) 2014-10-08 2019-08-14 LG Chem, Ltd. Method for preparing super absorbent polymer granules
KR101782501B1 (ko) 2014-12-10 2017-09-27 주식회사 엘지화학 고흡수성 수지의 제조 방법
CN112119114A (zh) 2018-05-16 2020-12-22 株式会社日本触媒 吸水性树脂粉末及其制造方法
KR102566285B1 (ko) * 2018-12-19 2023-08-10 주식회사 엘지화학 고흡수성 수지 섬유 제조용 방사 용액의 제조방법
JPWO2021049451A1 (ja) * 2019-09-09 2021-03-18
CN116783234A (zh) * 2021-01-29 2023-09-19 株式会社日本触媒 吸水性树脂的制造方法
WO2023139987A1 (ja) * 2022-01-18 2023-07-27 松本油脂製薬株式会社 粒子、及びその用途

Family Cites Families (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS56103207A (en) * 1980-01-22 1981-08-18 Sumitomo Chem Co Ltd Preparation of dried high-molecular weight water-soluble polymer
JPH06192319A (ja) * 1992-12-25 1994-07-12 Nippon Shokubai Co Ltd 吸水性樹脂の製造方法
JP3979724B2 (ja) * 1997-06-18 2007-09-19 株式会社日本触媒 吸水性樹脂造粒物の乾燥体の製造方法
JP2000026510A (ja) * 1998-07-06 2000-01-25 Sanyo Chem Ind Ltd 樹脂の製造法および吸水性樹脂

Similar Documents

Publication Publication Date Title
JP2006299234A5 (ja)
CA1086447A (en) Water absorbent polymers
JP2005525445A5 (ja)
JP4227650B2 (ja) 噴霧重合法
JP2013511612A5 (ja)
JP2008142714A5 (ja)
WO2008090961A1 (ja) 粒子状吸水性ポリマーおよびその製造方法
JP2009540045A5 (ja)
JP2002538275A5 (ja)
JP2010505986A5 (ja)
JP2008533288A5 (ja)
JP2006291180A5 (ja)
JPS6025045B2 (ja) 塩水吸収能のすぐれたアクリル酸重合体の製造方法
RU2008152188A (ru) Способ изготовления полимерного бисера однородного размера
JP2010508413A5 (ja)
JP2014505151A5 (ja)
JP2007121346A5 (ja)
CN105461939B (zh) 一种具有剪切增稠特性的温敏水凝胶的制备方法
JP2008102396A5 (ja)
JP2008535963A5 (ja)
JP2016537499A5 (ja)
JP2005097519A5 (ja) 吸水性樹脂組成物、その用途およびその製造方法
JP2009300719A5 (ja)
CN104693347A (zh) 金属离子交联的含两性离子结构纳米凝胶及其制备方法
JP2002520458A5 (ja)