DK141143B - Method of manufacturing a separator for an electric accumulator. - Google Patents

Method of manufacturing a separator for an electric accumulator. Download PDF

Info

Publication number
DK141143B
DK141143B DK603374AA DK603374A DK141143B DK 141143 B DK141143 B DK 141143B DK 603374A A DK603374A A DK 603374AA DK 603374 A DK603374 A DK 603374A DK 141143 B DK141143 B DK 141143B
Authority
DK
Denmark
Prior art keywords
plates
accumulator
separator
edges
electrolyte
Prior art date
Application number
DK603374AA
Other languages
Danish (da)
Other versions
DK141143C (en
DK603374A (en
Inventor
Jean Bonnefont
Original Assignee
Europ Accumulateurs
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Europ Accumulateurs filed Critical Europ Accumulateurs
Publication of DK603374A publication Critical patent/DK603374A/da
Publication of DK141143B publication Critical patent/DK141143B/en
Application granted granted Critical
Publication of DK141143C publication Critical patent/DK141143C/da

Description

2 * t * « t * der består af to stive, mikroporøse, elektrisk isolerende plader, der er modstandsdygtige over for elektrolytten og er udformet med indvendige og udvendige noter til fri cirkulation af elektrolytten. Kanterne af de stive plader rager uden for akkumulatorpladernes kanter og presses mod hinanden, hvorpå de fastklemmes og sammensvejses. Ulempen ved denne udformning er, at lommen over hele omkredsen får en tyk og pladskrævende kantvulst.2 * t * «t * consisting of two rigid, microporous, electrically insulating plates resistant to the electrolyte and formed with inner and outer grooves for free circulation of the electrolyte. The edges of the rigid plates extend beyond the edges of the accumulator plates and are pressed against each other, whereupon they are clamped and welded together. The disadvantage of this design is that the pocket over the entire perimeter gets a thick and space-intensive edge bump.

Opfindelsen tager sigte på at afhjælpe disse ulemper, og med henblik herpå er fremgangsmåden ifølge opfindelsen ejendommelig ved, at der anvendes separator-plader af polyesterindeholdende fenolharpiks eller af polyvinylklorid, og at der langs pladernes kanter påføres i pastaagtig tilstand et hurtigt hærdende bånd af polyethylenkopolymer tilsat syntetisk akrylgummi.SUMMARY OF THE INVENTION The present invention aims to alleviate these disadvantages, and for this purpose the method according to the invention is characterized by the use of polyester-containing phenol resin or polyvinyl chloride separator plates and a fast-curing band of polyethylene copolymer is applied along the edges of the plates. synthetic acrylic rubber.

Ved at fremstille separatoren som ovenfor angivet undgår man støbeoperationer og de dermed forbundne vanskeligheder. Det hurtigt hærdende bånd giver en fast og stiv forbindelse, og fremstillingen er væsentligt enklere.By manufacturing the separator as stated above, it avoids molding operations and the associated difficulties. The fast curing band provides a firm and rigid connection, and manufacturing is significantly simpler.

Opfindelsen forklares nærmere i det følgende under henvisning til den skematiske tegning, hvor fig. 1 viser et perspektivisk, delvis skåret billede af en separator ifølge opfindelsen med indsat akkumulatorplade, og fig, 2 et snit langs linien A-A i fig. 1.The invention is explained in more detail below with reference to the schematic drawing, in which fig. 1 shows a perspective, partially cut view of a separator according to the invention with inserted accumulator plate, and fig. 2 is a section along the line A-A in fig. First

Tegningen viser en akkumulatorplade 1 med tilhørende pladefane 7.The drawing shows an accumulator plate 1 with associated plate tab 7.

Akkumnlatorpladen er indsat i en lomme, der danner separatoren ifølge opfindelsen, og som består af to stive, elektrisk isolerende plader 2 og 3, der er modstandsdygtige overfor elektrolyten 4, De mod akkumulatorpladen 1 vendende sider af disse to plader er udformet med ribber 10 og noter til bedre fjernelse af de gasser, der opstår som følge af den elektrokemiske reaktion. På ydersiden har pladerne 2 og 3 noter 11, som fremmer cirkulationen af elektrolyten mellem to ved siden af hinanden beliggende plader.The accumulator plate is inserted into a pocket forming the separator according to the invention, which consists of two rigid, electrically insulating plates 2 and 3 which are resistant to the electrolyte 4, the sides of the two plates facing the accumulator plate are formed with ribs 10 and notes for better removal of the gases generated by the electrochemical reaction. On the outside, plates 2 and 3 have grooves 11 which promote the circulation of the electrolyte between two adjacent plates.

Langs siderne og forneden er pladerne 2 og 3 forbundet med hinanden ved hjælp af et bånd 5 af plastmateriale. Foroven er pladernes kanter forbundet med hinanden ved hjælp af et bånd 6 af sanmte art som båndet 5, efter at akkumulatorpladen 1 er blevet anbragt inden i lommen.Along the sides and bottom, the plates 2 and 3 are connected to each other by means of a band 5 of plastic material. Above, the edges of the plates are connected to each other by means of a band 6 of the same kind as the band 5, after the accumulator plate 1 has been placed inside the pocket.

I en anden udførelsesform for opfindelsen behøver separatorlommen ikke at være lukket over hele sin omkreds.In another embodiment of the invention, the separator pocket need not be closed over its entire circumference.

Pladerne 2 og 3 kan bestå af en polyesterindeholdende phenolharpiks eller af mikroporøst PVC-skum med åbne porer med en radius mellem ca. 1 og ca. 7 μ, således at den samlede porøsitet for separatoren ifølge opfindelsen ligger mellem 75 og 80 %.Plates 2 and 3 may consist of a polyester-containing phenolic resin or of open-pore microporous PVC foam having a radius of between approx. 1 and approx. 7 µ so that the total porosity of the separator according to the invention is between 75 and 80%.

Til fremstilling af pladerne 2 og 3 kan man også anvende en blanding af PVC, pulverformet siliciumoxyd, vand og cyklohexanol til opnåelse af en porøsitetFor the preparation of plates 2 and 3, a mixture of PVC, powdered silica, water and cyclohexanol can also be used to obtain a porosity.

Claims (1)

føl i U1U3 i) / :>'Ί f på ca. 80 %. Til opnåelse af en udmærket vedhængning mellem pladerne 2 og 3 og ‘ g plastbåndene 5 og 6 kan båndet bestå af polyethylenkopolymer tilsat akrylisk / syntetisk gummi. Båndet i form af en pasta påføres kanterne af pladerne 2 og 3 J og stivner i løbet af 3-4 sek. /Med separatoren ifølge opfindelsen opnås, at akkumulatorpladerne indbyr-^ des holdes godt på plads inden i akkumulatorkarret og isoleres elektrisk godt fra hinanden, at der sikres en god beskyttelse af pladernes kanter, og at elek-trolyten frit kan cirkulere. En separator ifølge opfindelsen kan med fordel anvendes sammen med den negative plade i en blyakkumulator. Det bemærkes, at opfindelsen ikke er begrænset til denne anvendelse, og at man iøvrigt, inden for opfindelsens ramme, kan anvende for pladerne 2 og 3 et vilkårligt porøst, elektrisk isolerende materiale, der er kompatibelt med det isolerende bånd 5. Fremgangsmåde ved fremstilling af en separator til en elektrisk akkumulator og udformet som en lomme for en akkumulatorplade, og hvis flader udgøres af to mikroporøse, elektrisk isolerende plader, der er modstandsdygtige over for akkumulatorens elektrolyt, kendetegnet ved, at der anvendes separator-plader af polyesterindeholdende fenolharpiks eller af polyvinylklorid, og at der langs pladernes kanter påføres i pastaagtig tilstand et hurtigt hærdende band af polyethylenkopolymer tilsat syntetisk akrylgummi. Fremdragne publikationer: Britisk patent nr. 838310 < Tysk fremlæggelsesskrift nr. 1109751 • USA patenter nr. 1668404, 2490630, 2673230. i r ifoal in U1U3 i) /:> 'Ί f of approx. 80%. In order to obtain an excellent adhesion between the sheets 2 and 3 and the plastic strips 5 and 6, the strip may consist of polyethylene copolymer added with acrylic / synthetic rubber. The tape in the form of a paste is applied to the edges of plates 2 and 3 J and solidifies within 3-4 seconds. With the separator according to the invention, it is achieved that the accumulator plates are firmly held in place within the accumulator vessel and electrically insulated well from each other, that a good protection of the edges of the plates is ensured and that the electrolyte can circulate freely. A separator according to the invention can advantageously be used with the negative plate in a lead accumulator. It is to be noted that the invention is not limited to this application and that, within the scope of the invention, any porous, electrically insulating material compatible with the insulating band 5. can be used for the production of sheets. a separator for an electric accumulator and designed as a pocket for an accumulator plate, the surfaces of which are comprised of two microporous, electrically insulating plates that are resistant to the electrolyte of the accumulator, characterized in that separator plates of polyester-containing phenolic resin or of polyvinyl chloride are used. and that a fast-curing band of polyethylene copolymer added with synthetic acrylic rubber is applied along the edges of the plates in a paste-like state. Published Publications: British Patent No. 838310 <German Patent Publication No. 1109751 • United States Patents No. 1668404, 2490630, 2673230. i r
DK603374AA 1973-11-21 1974-11-20 Method of manufacturing a separator for an electric accumulator. DK141143B (en)