DK0818274T3 - Surface treatment of aluminum alloy by spraying a grinding powder under pressure - Google Patents
Surface treatment of aluminum alloy by spraying a grinding powder under pressureInfo
- Publication number
- DK0818274T3 DK0818274T3 DK97420112T DK97420112T DK0818274T3 DK 0818274 T3 DK0818274 T3 DK 0818274T3 DK 97420112 T DK97420112 T DK 97420112T DK 97420112 T DK97420112 T DK 97420112T DK 0818274 T3 DK0818274 T3 DK 0818274T3
- Authority
- DK
- Denmark
- Prior art keywords
- spraying
- aluminum alloy
- surface treatment
- under pressure
- powder under
- Prior art date
Abstract
The surfaces of components made of aluminium or their alloys are treated by sand blasting, using an abrasive powder projected against the surfaces in a jet of compressed air. The powder is prepared by electro-melting a mix of corundum and 20-45% by weight of zirconia.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR9608901A FR2750909B1 (en) | 1996-07-11 | 1996-07-11 | TREATMENT OF ALUMINUM ALLOY SURFACES BY SPRAYING AN ABRASIVE POWDER UNDER PRESSURE |
Publications (1)
Publication Number | Publication Date |
---|---|
DK0818274T3 true DK0818274T3 (en) | 2002-02-18 |
Family
ID=9494115
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DK97420112T DK0818274T3 (en) | 1996-07-11 | 1997-07-09 | Surface treatment of aluminum alloy by spraying a grinding powder under pressure |
Country Status (7)
Country | Link |
---|---|
EP (1) | EP0818274B1 (en) |
AT (1) | ATE207399T1 (en) |
DE (1) | DE69707573T2 (en) |
DK (1) | DK0818274T3 (en) |
ES (1) | ES2166058T3 (en) |
FR (1) | FR2750909B1 (en) |
PT (1) | PT818274E (en) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE102004007361B4 (en) * | 2003-02-24 | 2005-10-06 | Innovent E.V. | Method for modifying galvanized steel surfaces and black steel surfaces |
CN106808372B (en) * | 2016-12-26 | 2019-04-12 | 广州市亿众金属制品有限公司 | A kind of aluminum alloy surface mechanical processing method |
Family Cites Families (9)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
FR2086972A5 (en) * | 1970-04-15 | 1971-12-31 | Pechiney | Abrasive grains by alpha alumina-in alumina zirconia eutectic - matrix |
US4035162A (en) * | 1973-11-09 | 1977-07-12 | Corning Glass Works | Fused abrasive grains consisting essentially of corundum, zirconia and R2 O3 |
DE2560066B1 (en) * | 1974-05-29 | 1979-12-13 | Treibacher Chemische Werke Ag | Process for the production of abrasive materials based on aluminum oxide, optionally together with other oxides |
FR2499061A1 (en) * | 1981-01-30 | 1982-08-06 | Sofrem | METHOD AND APPARATUS FOR RAPID CONTINUOUS CASTING SOLIDIFICATION AND COOLING OF MOLDED OXIDES BASED ON METAL OXIDES |
GB2137651A (en) * | 1983-04-05 | 1984-10-10 | Unicorn Ind Plc | Coated abrasives |
DE3609408A1 (en) * | 1986-03-20 | 1987-09-24 | Georg Norbert Fassel | Process for regenerating wheel rims of motor vehicles |
US5409415A (en) * | 1992-07-02 | 1995-04-25 | Nikkato Corp. | Shot method |
DE4306966C1 (en) * | 1992-10-19 | 1994-01-20 | Starck H C Gmbh Co Kg | Abrasive grain based on zirconium corundum, process for its production and its use |
DE4303339C2 (en) * | 1993-02-05 | 1995-03-30 | Ritter Aluminium Giesserei Gmb | Process for the treatment of aluminum die castings |
-
1996
- 1996-07-11 FR FR9608901A patent/FR2750909B1/en not_active Expired - Lifetime
-
1997
- 1997-07-09 ES ES97420112T patent/ES2166058T3/en not_active Expired - Lifetime
- 1997-07-09 DE DE69707573T patent/DE69707573T2/en not_active Expired - Lifetime
- 1997-07-09 AT AT97420112T patent/ATE207399T1/en active
- 1997-07-09 EP EP97420112A patent/EP0818274B1/en not_active Expired - Lifetime
- 1997-07-09 PT PT97420112T patent/PT818274E/en unknown
- 1997-07-09 DK DK97420112T patent/DK0818274T3/en active
Also Published As
Publication number | Publication date |
---|---|
EP0818274B1 (en) | 2001-10-24 |
ES2166058T3 (en) | 2002-04-01 |
DE69707573T2 (en) | 2002-07-11 |
FR2750909B1 (en) | 1998-10-16 |
FR2750909A1 (en) | 1998-01-16 |
DE69707573D1 (en) | 2001-11-29 |
PT818274E (en) | 2002-04-29 |
ATE207399T1 (en) | 2001-11-15 |
EP0818274A1 (en) | 1998-01-14 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AU1832497A (en) | Method and apparatus for honing an elongate rotary tool | |
ATE207806T1 (en) | METHOD FOR INCREASING THE WETABILITY OF THE SURFACE OF WORKPIECES | |
MY115702A (en) | Polishing composition for aluminum disk and polishing process therewith | |
CA2211281A1 (en) | Metal fluoride particles and a dental composition including said metal fluoride particles | |
ES2196338T3 (en) | PROCEDURE TO PRODUCE A PULVIMETALURGICAL BODY WITH COMPACTED SURFACE. | |
CA2041188A1 (en) | Nozzle unit and method for using wet abrasives to clean hard surfaces | |
DK0818274T3 (en) | Surface treatment of aluminum alloy by spraying a grinding powder under pressure | |
CA2286876A1 (en) | Dental abrading tool | |
GB9204034D0 (en) | Aircraft | |
GB2298382A (en) | Method for enhancing the rust resistance and the surface finish of a non-ferrous workpiece | |
AU5147293A (en) | The use of specular hematite as an impact material | |
Porter | Shot-Blasting Is Ideal Pre-Treatment | |
Huppatz et al. | Surface finishing of aluminium | |
EP0225765A3 (en) | Apparatus for abrading small objects | |
Thomas | Spray booths | |
Allister | Targeted Blasting--Effect of Various Parameters During Blasting Surfaces of Different Materials | |
Kuppinger | SURVEY OF SHOT BLASTING MATERIALS AND EQUIPMENT FOR THE TREATMENT OF ALUMINUM CASTINGS | |
AU2898600A (en) | Dental abrading tool | |
Sedlmair et al. | Method of surface treating structural components | |
KR940020312U (en) | Prevention of paint scattering and accelerated air inlet of the painting surface of the pipe | |
Landon-Browne | Coating Surfaces | |
GB2372039A (en) | Method for removing surface coatings | |
Horowitz | Blasting Technique and Rust-Proofing of Steel Structures | |
RU2001108007A (en) | METHOD FOR COATING OF POWDER MATERIALS | |
ES2123414A1 (en) | Procedure for treating aluminium surfaces |