DE734043C - Herstellung elektrischer Kontakte, insbesondere fuer Wellenschalter in Hochfrequenzkreisen - Google Patents
Herstellung elektrischer Kontakte, insbesondere fuer Wellenschalter in HochfrequenzkreisenInfo
- Publication number
- DE734043C DE734043C DES143162D DES0143162D DE734043C DE 734043 C DE734043 C DE 734043C DE S143162 D DES143162 D DE S143162D DE S0143162 D DES0143162 D DE S0143162D DE 734043 C DE734043 C DE 734043C
- Authority
- DE
- Germany
- Prior art keywords
- electrical contacts
- manufacture
- high frequency
- frequency circuits
- wave switches
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Herstellung elektrischer Kontakte, insbesondere für Wellenschalter in Hochfrequenzkreisen Das Hauptpatent beschreibt ein Glanzversilberungsbad, das dadurch gekennzeichnet ist, daß dem normalen cyankalischen oder cyanid- und nitrathaltigen Versilberungsbad ein Glanzzusatz, bestehend aus den drei Komponenten Türkischrotöl, Kaliumxanthogenat und einer cyanidischen Nickelverbindung, beigefügt ist.
- Dünne Silberschichten werden nicht nur in der Schmuckindustrie und zum Oberflächenschutz, sondern auch bei der Herstellung von elektrischen Kontakten verwendet. Bei diesem Verwendungszweck spielt allerdings der Glanz der Schicht keine Rolle. Bei den heute üblichen Konstruktionen besteht der Kontakt aus einem unedlen Grundmetall, wie z. B. Kupfer oder kupferhaltigen Legierungen und einer darauf galvanisch oder durch. Plattierung dünn aufgebrachten edlen Metallschicht. Solche Kontakte -müssen wegen ihrer starken mechanischen Beanspruchung, z. B. bei einem Wellenschalter in einem Rundfunkgerät, einerseits mechanisch sehr dauerhaft sein, anderseits aber auch dauernd eine gute elektrische Leitfähigkeit gewährleisten. Man hatte aus diesem Grund hochwertige Metalle für die Kontaktschicht angewendet, die aber fast durchweg vom Ausland eingeführt werden müssen und daher aus volkswirtschaftlichen Gründen möglichst zu vermeiden sind. Aus Gründen der Wirtschaftlichkeit müssen diese Schichten' sehr dünn aufgebracht werden. Ferner ist zu beachten, daß nur ein Verfahren in Betracht kommt, das einen guten Kontakt zwischen dem Grundmetall und der aufgebrachten Edelmetallsehicht sicherstellt.
- Da die galvanisch niedergeschlagenen Silberschichten diese Bedingungen nicht in hinreichendem Maße .erfüllen, hat man bereits vorgeschlagen, die Silberniederschläge durch eine ein- bis zweitägige Temperaturbehandlung bei i 6o bis -22O° und durch eine anschließende mechanische Behandlung, wie Walzen und Schlagen, zu verfestigen. Diese Behandlung ist jedoch sehr zeitraubend und teuer.
- Erfindungsgemäß lassen sich nun elektrische Kontakte, die allen Anforderungen entsprechen, dadurch herstellen, daß zur Aufbringung der Silberschichten das Glanzversüberungsbad gemäß dem Hauptpatent verwendet wird. Bei Anwendung .dieses Bades ergeben sich überraschende und technisch bedeutende Vorteile. Bei Dauerversuchen mit Wellenschaltern für Hochfrequenzkreise konnte gegenüber den bisher bekannten Ausführungen eine beträchtlich erhöhte Lebensdauer festgestellt werden.
- Ein wesentlicher Vorteil der Anwendung des Glanzversilberungsbades besteht darin, äaß besondere Maßnahmen für die Erhärtung :und Glättung der Kontaktschicht, wie sie bisher erforderlich waren, entfallen. Trotzdem ergeben sich bessere Werte sowohl in mechanischer als elektrischer Hinsicht.
Claims (1)
- PATENTANSPRUCH: Verwendung des elektrolytischen Glanzversilberungsbades nach Patent 731961 zur Herstellung der Kontaktflächen von elektrischen Kontakten, insbesondere für Wellenschalter in Hochfrequenzkreisen.